This application is the National Stage of PCT/DE2009/001167 filed on Aug. 19, 2009 which claims priority under 35 U.S.C. §119 of German Application No. 10 2008 038 323.6 filed on Aug. 19, 2008, the disclosure of which is incorporated by reference. The international application under PCT article 21(2) was not published in English.
The invention relates to a coating mask for electrolytic coating of a circumferential region on the mantle surface of a cylindrical body in accordance with the preamble of claim 1, and the use of the coating mask for coating of a piston ring groove of a piston for an internal combustion engine in accordance with claim 7.
A device for anodic oxidation of a circumferential region on the mantle surface of a cylindrical body, particularly the piston ring groove of a piston for an internal combustion engine, is known from the U.S. Pat. No. 6,821,408, whereby the region to be coated is hermetically sealed off, on both sides, by two circumferential sealing rings, which are at first round in section, in that pressure is exerted on the sealing rings by a sleeve, in each instance, until the sealing rings deform to become oval, whereby this ovality is oriented perpendicular to the mantle surface of the piston. In this way, the sealing rings come to lie against the mantle surface on both sides of the piston ring groove and seal this region off hermetically. Subsequently, an electrolyte is introduced into this region and the piston ring groove situated within it is anodically oxidized. It is disadvantageous that a very complicated mechanism for deformation of the sealing rings is required. In this connection, the sleeves are put into motion parallel to the piston axis, by multiple pressure rods that can be moved perpendicular to the piston axis, by way of a slanted contact surface.
It is the task of the invention to overcome this disadvantage of the state of the art. This task is accomplished with the characteristics that stand in the characterizing part of the main claim. Practical embodiments are the object of the dependent claims.
Since the coating mask according to the invention consists of an elastically resilient material, this mask merely has to be stretched outward radially, using a simple mechanism, in order to make room for a piston whose piston ring groove is supposed to be coated.
The invention will be described in the following, using the drawings. The figures show:
Between the openings 3 to 10, the coating mask 1 has regions 24 to 31 having a thinner wall, which regions increase the elasticity of the coating mask 1, so that the coating mask 1 can be stretched more easily in the direction of the arrows 20 to 23.
In
In this connection, the electrolyte gets into the lower ring line 32′ by way of the inflow channel 33, flows into the coating groove 37 that is closed off by the piston to be coated, by way of the lower feed channels 35′, from here into the upper ring line 32, by way of the upper feed channels 35, and is passed out of the coating mask 1 from here, by way of the outflow channel 40. In
As can be clearly seen in
However, the coating mask 1 can also be used to anodically oxidize the flanks of the piston ring groove 39 of the piston 38. For this purpose, the piston 38 is switched as an anode, i.e. connected with the positive pole of a direct-voltage source, and the ring electrodes 42 and 43 are switched as cathodes, i.e. connected with the negative pole of a direct-voltage source by way of the connectors 53 and 54, and sulfuric acid, for example, is supplied to the coating mask 1 as an electrolyte, by way of the inflow channel 33.
If the piston ring groove 39 of a piston 38 is supposed to be coated, first the coating mask 1 is pushed onto the mandrels 11 to 18 of the stretching device 19 by way of its openings 3 to 9, as shown in
Subsequently, if the flanks of the piston ring groove 39 are supposed to be coated with iron, an electrolyte that contains iron is introduced into the coating mask 1 by way of the inflow channel 33, the ring electrodes 42 and 43 are connected with the plus pole of a direct-voltage source by way of the electrical connectors 53 and 54, the piston 38 is connected with the minus pole of the direct-voltage source by way of an electrical connector 55, and the excess electrolyte is passed out of the coating mask 1 by way of the outflow channel 40.
After a certain period of time, the flanks of the piston ring groove 39 of the piston 38 are coated to a sufficient degree, so that after the electrolyte was completely passed out of the ring lines 32 and 32′, the ring lines 32 and 32′ and the coating groove 37 are flushed with hot steam, heated to 130° C. Subsequently, the mandrels 11 to 18 of the stretching device 19 are moved radially outward, so that the diameter of the inner opening 2 is also enlarged, and the piston 38 can be removed from the coating mask 1.
The coating mask 1 is produced using a casting method, whereby first, two ring line templates 50 that consist of sintered plastic are laid into a casting mold 49, as shown in
The ring line templates 50 remain in the coating mask 1 after the casting process, and have planned breaking points 52 that break open during the first coating process, when the coating mask 1 and therefore also the ring line template 50 are widened radially outward for the first time, so that in this way, the elasticity of the coating mask 1 is not hindered. It is advantageous to install one ring electrode, in each instance, into the ring line templates 50, during the production of the ring line templates 50.
Number | Date | Country | Kind |
---|---|---|---|
10 2008 038 323 | Aug 2008 | EP | regional |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/DE2009/001167 | 8/19/2009 | WO | 00 | 9/26/2011 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2010/020235 | 2/25/2010 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
6821408 | Sasaki et al. | Nov 2004 | B2 |
20020100695 | Sasaki et al. | Aug 2002 | A1 |
Number | Date | Country |
---|---|---|
10 2006 020 593 | Nov 2007 | DE |
2 027 054 | Feb 1980 | GB |
01-073080 | Mar 1989 | JP |
WO 2007124728 | Nov 2007 | WO |
Entry |
---|
International Search Report of PCT/DE2009/001167, Apr. 7, 2010. |
German Search Report dated Nov. 18, 2008 in German Application No. 10 2008 038 323.6 with English translation of relevant parts. |
Number | Date | Country | |
---|---|---|---|
20120085654 A1 | Apr 2012 | US |