Claims
- 1. A hermetically sealed primary electrochemical cell comprising:
- a hollow outer cell casing having a single opening therein, the outer cell casing being formed of a conductive material and being a first terminal of the primary electrochemical cell;
- an electrochemical system being disposed within the outer casing and including
- an anode in mechanical and electrical contact with the outer cell casing,
- a cathode spaced from the anode material, and
- a liquid electrolytic solution in contact with the anode and cathode, said electrolytic solution including a solvent and a solute dissolved therein,
- an electrically, non-conductive separator being interposed between the anode and cathode;
- a glass-to-metal seal being welded into the opening in the outer cell casing to seal hermetically the primary electrochemical cell, the glass-to-metal seal having a metallic feedthrough in the central portion thereof the internal end of which engages the cathode thereby serving as a current collector therefor, the external end serving as a second terminal of the primary elecytrochemical cell, and
- means for establishing a temporary seal within the outer cell casing between the weld and the electrochemical system, whereby escape of any volatilized solvent during welding of the glass-to-metal seal is generally prevented.
- 2. A hermetically sealed primary electrochemical cell according to claim 1, wherein there is further included means for partially thermally insulating the electrolytic solution from heat generated while welding the glass-to-metal seal in the opening in the outer cell casing.
- 3. A hermetically sealed primary electrochemical cell according to claim 1, wherein the cathode is a preformed porous carbon cathode.
- 4. A hermetically sealed primary electrochemical cell according to claim 1, wherein a cathode current collector is attached to the internal end of the metallic feedthrough, the cathode current collector being a tortuously formed strip of conductive material a major portion of which extends into the preformed porous carbon cathode.
- 5. A hermeticaly sealed primary electrochemical cell according to claim 2, wherein the means for establishing a temporary seal and the means for partially thermally insulating the electrolytic solution are a plastic washer which is press fitted within the outer cell casing above the electrochemical system and which has a central opening therein the edge of which bears against the glass-to-metal seal to complete the temporary seal.
- 6. A hermetically sealed primary electrochemical cell according to claim 5, wherein the plastic washer is formed of a fluorocarbon polymer.
- 7. A method of producing a hermetically sealed primary electrochemical cell comprising the steps of:
- forming an electrically conductive hollow outer casing having a single opening therein;
- placing an anode of a selected electrochemical system within the outer casing and in mechanical and electrical contact with the outer casing so that the outer casing forms one terminal of the primary electrochemical cell;
- placing a cathode of the selected electrochemical system and a separator of non-conducting material within the outer casing so that physical contact between the anode and cathode materials is prevented;
- filling the outer casing with an effective amount of an electrolytic solution compatible with the selected electrochemical system, said electrolytic solution including a solvent and a solute dissolved therein;
- placing a layer of barrier material in sealing contact with the inner wall of the casing to temporarily seal the electrolytic solution from the casing opening;
- inserting a glass-to-metal seal into the opening in the outer casing, the glass-to-metal seal having a solid metallic feedthrough in the central portion thereof which engages the cathode material upon insertion and which serves as a current collector therefor; and
- welding the glass-to-metal seal to the outer casing to form a hermetic seal, the temporary seal generally preventing volatilization of electrolyte during the welding step.
- 8. A method according to claim 7, wherein the primary electrochemical cell assembly is chilled prior to welding to reduce the vapor pressure of the electrolytic solution.
- 9. A method according to claim 8, wherein the temporary seal is established by pressing a plastic washer into the opening in the outer casing prior to insertion of the glass-to-metal seal so that upon insertion of the glass-to-metal seal a portion thereof bears against the washer to complete the temporary seal.
CROSS-REFERENCE TO RELATED PATENT APPLICATION
This patent application, is a continuation-in-part of application Ser. No. 539,752, filed Jan. 9, 1975, and assigned to the same assignee as in the present patent application, now abandoned.
US Referenced Citations (7)
Continuation in Parts (1)
|
Number |
Date |
Country |
| Parent |
539752 |
Jan 1975 |
|