Claims
- 1. A process of manufacturing powdered copolymers of maleic anhydride and methyl vinyl ether in a single reaction vessel, essentially consisting of the steps of:
- preparing a reaction mixture by mixing maleic anhydride with an excess of methyl vinyl ether, said excess being in a range from about 3 to about 20 mol methyl vinyl ether per mol maleic anhydride and adding a radical initiator in a quantity of from about 0.001 to about 1 weight % with respect to the maleic anhydride;
- initiating a polymerization reaction by heating said reaction mixture in said reaction vessel to a decomposition temperature of the radical initiator, initiating said polymerization reaction at said decomposition temperature in the reaction vessel with intensive stirring and in the absence of other solvents;
- heating said reaction mixture in said reaction vessel to a reaction temperature at least 5.degree. C. higher than said decomposition temperature to complete said polymerization reaction and maintaining said reaction temperature by external cooling;
- evaporating excess methyl vinyl ether after reaction of maleic anhydride; and
- collecting a powdered copolymer of maleic anhydride and methyl vinyl ether, said copolymer having a mole ratio of maleic anhydride:methyl vinyl ether of about 1:1 and having a specific viscosity in a range from about 2 to about 5.
- 2. A process as defined in claim 1, wherein the quantity of radical initiator is in a range from about 0.01 weight % to about 0.5 weight % with respect to the maleic anhydride.
- 3. A process as defined in claim 1, wherein the excess of methyl vinyl ether is in a range from about 6 to about 15 mol methyl vinyl ether per mol maleic anhydride.
- 4. A process as defined in claim 1, wherein said polymerization reaction takes place at a temperature in a range from about 40.degree. to about 80.degree. C.
- 5. A process as defined in claim 1 wherein the reaction takes place at a pressure corresponding to the vapor pressure of the reaction mixture developing at the corresponding temperature.
- 6. A process as defined in claim 1, wherein the polymerization is performed in an inert gas atmosphere and the total pressure during the process is a maximum of 50 bar.
- 7. A process as defined in claim 1, wherein the polymerization is performed over a time period from 1 to 20 hours.
- 8. A process as defined in claim 1, wherein the polymerization is performed over a time period from 3 to 8 hours.
- 9. A powdered copolymer of maleic anhydride and methyl vinyl ether made by the process of claim 1.
- 10. A process as defined in claim 1, wherein in the initiating step said reaction vessel is a closed reaction vessel.
Priority Claims (1)
Number |
Date |
Country |
Kind |
3712265 |
Apr 1987 |
DEX |
|
Parent Case Info
This application is a continuation of application Ser. No. 07/180,079, filed Apr. 11, 1988, now abandoned.
US Referenced Citations (5)
Foreign Referenced Citations (5)
Number |
Date |
Country |
59446 |
Sep 1982 |
EPX |
68847 |
Jan 1983 |
EPX |
1299119 |
Mar 1970 |
DEX |
3042471 |
Jun 1982 |
DEX |
DE3514367 |
Oct 1986 |
DEX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
180079 |
Apr 1988 |
|