In at least one embodiment, the present invention relates to fuel cell bipolar plates with reduced contact resistances.
Fuel cells are used as an electrical power source in many applications. In particular, fuel cells are proposed for use in automobiles to replace internal combustion engines. A commonly used fuel cell design uses a solid polymer electrolyte (“SPE”) membrane or proton exchange membrane (“PEM”) to provide ion transport between the anode and cathode.
In proton exchange membrane type fuel cells, hydrogen is supplied to the anode as fuel, and oxygen is supplied to the cathode as the oxidant. The oxygen can either be in pure form (O2) or air (a mixture of O2 and N2). PEM fuel cells typically have a membrane electrode assembly (“MEA”) in which a solid polymer membrane has an anode catalyst on one face, and a cathode catalyst on the opposite face. The anode and cathode layers of a typical PEM fuel cell are formed of porous conductive materials, such as woven graphite, graphitized sheets, or carbon paper to enable the fuel to disperse over the surface of the membrane facing the fuel supply electrode. Each electrode has finely divided catalyst particles (for example, platinum particles), supported on carbon particles, to promote oxidation of hydrogen at the anode and reduction of oxygen at the cathode. Protons flow from the anode through the ionically conductive polymer membrane to the cathode where they combine with oxygen to form water, which is discharged from the cell. The MEA is sandwiched between a pair of porous gas diffusion layers (“GDL”), which in turn are sandwiched between a pair of non-porous, electrically conductive elements or plates referred to as flow field plates. The plates function as current collectors for the anode and the cathode, and contain appropriate channels and openings formed therein for distributing the fuel cell's gaseous reactants over the surface of respective anode and cathode catalysts. In order to produce electricity efficiently, the polymer electrolyte membrane of a PEM fuel cell must be thin, chemically stable, proton transmissive, non-electrically conductive and gas impermeable. In typical applications, fuel cells are provided in arrays of many individual fuel cell stacks in order to provide high levels of electrical power.
In order to maximize fuel cell performance, it is desirable to minimize contact resistances. For example, the contact resistance between the flow field plates and the gas diffusion layers should be as low as possible. Prior art methods use a bipolar plate coating consisting of a metal interlayer (Ti or Cr) and conductive amorphous carbon layer deposited by physical vapor deposition (PVD) processes on stainless steel substrates. The current state of the art contact resistance using a carbon coating is about 13-16 mΩcm2 at 200 psi. Inherent film non-uniformity is observed due to PVD process being a line of sight deposition technique. Moreover, the PVD processes have an associated high capital cost.
Accordingly, there is a need for improved methods for lowering the contact resistances in fuel cell components.
The present invention solves one or more problems of the prior art by providing, in at least one embodiment, a flow field plate for a fuel cell. The flow field plate includes an electrically conductive substrate at least partially defining a plurality of flow channels. A carbon layer is disposed over the flow field plate. The carbon layer includes graphene, carbon nanotubes, or combinations thereof and has a thickness of 1 to 10 nanometers.
In another embodiment, a method for forming the flow field plate set forth above having graphene layers is provided. The method includes a step of contacting an electrically conductive substrate with a vapor of a C1-18 hydrocarbon-containing compound at a temperature from 350° C. to about 600° C. to form a carbon layer. The carbon layer includes from 1 to 10 graphene monolayers. The electrically conductive substrate at least partially defines a plurality of gas flow channels. Advantageously, in accordance with this method, the carbon layer can be formed by chemical vapor deposition or atomic layer deposition. Growth of multi-layered graphene and carbon nanotubes on stainless steel substrates by atmospheric pressure CVD and ALD processes at temperatures lower than 400° C. can provide a low cost route to depositing highly conductive, corrosion resistant carbon for application as bipolar plate coating. Moreover, higher growth rates and coverage can be achieved by transition metal catalysts such as Ni, Cu and Ru. The graphene deposition process can be achieved with a range of pressures from less than or equal to 1 torr to atmospheric pressure.
Reference will now be made in detail to presently preferred compositions, embodiments and methods of the present invention which constitute the best modes of practicing the invention presently known to the inventors. The Figures are not necessarily to scale. However, it is to be understood that the disclosed embodiments are merely exemplary of the invention that may be embodied in various and alternative forms. Therefore, specific details disclosed herein are not to be interpreted as limiting, but merely as a representative basis for any aspect of the invention and/or as a representative basis for teaching one skilled in the art to variously employ the present invention.
Except in the examples, or where otherwise expressly indicated, all numerical quantities in this description indicating amounts of material or conditions of reaction and/or use are to be understood as modified by the word “about” in describing the broadest scope of the invention. Practice within the numerical limits stated is generally preferred. Also, unless expressly stated to the contrary: percent, “parts of,” and ratio values are by weight; the description of a group or class of materials as suitable or preferred for a given purpose in connection with the invention implies that mixtures of any two or more of the members of the group or class are equally suitable or preferred; description of constituents in chemical terms refers to the constituents at the time of addition to any combination specified in the description and does not necessarily preclude chemical interactions among the constituents of a mixture once mixed; the first definition of an acronym or other abbreviation applies to all subsequent uses herein of the same abbreviation and applies mutatis mutandis to normal grammatical variations of the initially defined abbreviation; and, unless expressly stated to the contrary, measurement of a property is determined by the same technique as previously or later referenced for the same property.
It is also to be understood that this invention is not limited to the specific embodiments and methods described below, as specific components and/or conditions may, of course, vary. Furthermore, the terminology used herein is used only for the purpose of describing particular embodiments of the present invention and is not intended to be limiting in any way.
It must also be noted that, as used in the specification and the appended claims, the singular form “a,” “an,” and “the” comprise plural referents unless the context clearly indicates otherwise. For example, reference to a component in the singular is intended to comprise a plurality of components.
Throughout this application, where publications are referenced, the disclosures of these publications in their entireties are hereby incorporated by reference into this application to more fully describe the state of the art to which this invention pertains.
“CVD” means chemical vapor deposition.
“EDX” means energy-dispersive X-ray spectroscopy.
“GDL” means gas diffusion layer.
“PEM” means proton exchange membrane.
“sccm” means standard cubic centimeters per minute.
“SEM” means scanning electron microscopy.
“SS” means stainless steel.
“slpm” means standard liters per minute.
With reference to
With reference to
In the variation set forth in
Advantageously, the fuel cell flow field plates of
In another embodiment, a method for forming the graphene and/or carbon nanotube layers set forth above on a bipolar plate is provided. The method includes a step of contacting an electrically conductive substrate with a vapor of a C1-18 hydrocarbon-containing compound at a temperature from 350° C. to about 600° C. to form a carbon layer. The carbon layer includes from 1 to multiple graphene monolayers. In a refinement, the graphene deposition process is accomplished at pressures from less than or equal to 1 torr to atmospheric pressure. As set forth above, the electrically conductive substrate at least partially defines a plurality of gas flow channels. In one variation, the carbon layer is formed by chemical vapor deposition in which the substrate is contacted with a reaction mixture. Characteristically, the reaction mixture includes the C1-18 hydrocarbon-containing compound and reaction products of the C1-18 hydrocarbon-containing compound. In a refinement, the reaction mixture further includes a reducing agent such as molecular hydrogen.
In another variation, the carbon layer set forth above is formed by atomic layer deposition (ALD) in which graphene monolayers are formed by one or a plurality of ALD deposition cycles. Characteristically, each ALD deposition cycle produces a monolayer of graphene so that a multilayer graphene coating is constructed layer by layer. An ALD deposition cycle includes a step where an electrically conductive substrate is contacted with the vapor of the C1-18 hydrocarbon-containing compound in an ALD reaction chamber. Optionally, the ALD reaction chamber is purged with an inert gas (e.g., argon, helium, nitrogen, etc.) after this step. In a refinement, the ALD deposition cycle further includes a step of contacting the substrate with a reducing agent (e.g., molecular hydrogen) followed again by an optional purging of the ALD reaction chamber with an inert gas.
In some variations of the methods set forth above, the C1-18 hydrocarbon containing compound includes a component selected from the group consisting of C6-12 aromatic compounds, C1-8 alkanes, C2-8 alkenes, C2-8 alkynes, C1-8 amines and C1-8 alcohols. Examples of C6-12 aromatic compounds include, but are not limited to, benzene, toluene, xylenes, and the like. Examples of C1-8 alkanes include, but are not limited to, methane, ethane, propane, butanes, pentanes and the like. Examples of C2-8 alkenes include, but are not limited to, ethylene, propylene, butylenes, and the like. Examples of C2-8 alkynes include acetylene, propyne, butyne, and the like. Examples of C1-8 amines include methyl amine, ethyl amine, propyl amines, dimethyl amine, diethyl amine, and the like. Finally, examples of C1-8 alcohols include methanol, ethanol, propanols, butanols, and the like.
In still other variations of the methods set forth above, the carbon layer is densified. For example, the carbon layer can be densified by a process selected from the group consisting of post-deposition thermal treatment, chemical treatment or plasma treatment, and combinations thereof.
In yet other variations, a metal layer is deposited on the electrically conductive substrate prior to forming the carbon layer. In a refinement, the metal layer includes a transition metal catalyst. In particular, the metal layer includes Ni, Cu, or Ru. In another refinement, metal layer 36 is a Ni layer, Cu layer, or Ru layer. The metal layer can be deposited CVD, ALD, and PVD processes such as evaporation and sputtering. In still another refinement, the metal layer 36 has a thickness from about 50 to 500 nanometers. In a further refinement, the metal layer 36 has a thickness from about 10 to 300 nanometers or about 300 nanometers. In a particular refinement, the metal layer does not include any chromium and/or titanium. In a refinement, the amount of chromium and titanium in the metal layer is less than or equal to, in increasing order of preference, 5.0 weight percent, 2.0 weight percent, 1.0 weight percent, 0.5 weight percent, 0.3 weight percent, 0.1 weight percent, 0.05 weight percent, or 0.01 weight percent or substantially equal to 0 weight percent. Growth on transition metal catalyst layer and lower growth temperatures lead to improved uniformity of the graphene or carbon nanotubes layer. Since the growth of the film is a surface property, the catalyst layer would provide a uniform composition surface irrespective of metal migration in underlying electronically conductive substrate, and in particular, when the substrate is stainless steel. Moreover, the transition metal catalyst layer lowers the range of the carbon layer deposition temperatures.
The following examples illustrate the various embodiments of the present invention. Those skilled in the art will recognize many variations that are within the spirit of the present invention and scope of the claims.
An initial set of CVD depositions at temperatures >650° C. on SS 304L results in non-uniform coating on the stainless steel substrates due to the migration of Cr in the underlying stainless steel. Metal grain rearrangement presents differences in atomic composition, thereby promoting or hindering carbon layer growth, depending on the alloy composition lying underneath.
Test samples are cut in pieces of 2″×2″, cleaned in an ultrasonic bath for 5 minutes each, first in acetone, then in isopropanol. The samples are then dried under a nitrogen gun flow. The dried foils are coated with 300 nm film of nickel using e-beam evaporation. The foils are then inserted in a CVD furnace. After a full power ramp up and a 15 min annealing under hydrogen flow, chemical vapor deposition is performed at 425° C., 450° C., and 475° C. for 60 minutes each, at a C2H2 flow rate of 12 sccm diluted in 5 slpm argon.
Rc=VA
gdl
/I
where V is the voltage drop, Agdl is the area of the gas diffusion layers, and I is the applied current.
SEM and EDX are performed on each sample at multiple points. Raman mapping is performed using a 633 nm laser to acquire spectra at about 50 points on a nearly 40 μm2 area of each sample. The average, variance, and overall range are then evaluated and are shown below. The elemental analysis performed using EDX seems to support the claims that higher chromium content leads to lower carbon synthesis. A steady rise in chromium can be observed in Table 1 as the temperature is raised above 500° C.
The amount of carbon produced in the graphene coatings is proportional to the intensity of the G peak of the sample's Raman spectra.
While exemplary embodiments are described above, it is not intended that these embodiments describe all possible forms of the invention. Rather, the words used in the specification are words of description rather than limitation, and it is understood that various changes may be made without departing from the spirit and scope of the invention. Additionally, the features of various implementing embodiments may be combined to form further embodiments of the invention.
Number | Date | Country | |
---|---|---|---|
Parent | 14735791 | Jun 2015 | US |
Child | 15863341 | US |