Claims
- 1. A rubber stock comprising (1) a rubber selected from the group consisting of natural rubber, rubbers derived from a diene monomer or mixtures thereof, and (2) a polymeric resin composition consisting essentially of the reaction product of the polymerization between dicyclopentadiene and limonene, said resin having a softening point ranging from about 50 to about 220° C., and an average molecular weight ranging from about 500 to about 42,000.
- 2. The rubber stock of claim 1 wherein said rubber derived from a diene monomer or mixtures thereof is selected from the group comprising natural rubber, polyisoprene, polybutadiene, polychloroprene, copolymers of isoprene and butadiene, copolymers of styrene and butadiene, copolymers of acrylonitrile and butadiene, copolymers of acrylonitrile and isoprene and blends thereof.
- 3. The rubber stock of claim 1 wherein said polymeric resin composition is present in an amount ranging from about 5 to about 50 parts per hundred parts of rubber.
- 4. The rubber stock of claim 3 wherein said polymeric resin composition is present in an amount ranging from about 10 to about 25 parts per hundred parts of rubber.
- 5. The rubber stock of claim 1 wherein the resin composition comprises a blend of four individual resins.
- 6. The rubber stock of claim 1 wherein said resin composition comprises a blend of three individual resins.
- 7. The rubber stock of claim 5 wherein the first resin has a softening point ranging from about 55 to about 75° C., the second resin has a softening point ranging from about 80 to about 131° C., the third resin has a softening point ranging from about 126 to about 168° C., and the fourth resin has a softening point ranging from about 168 to about 195° C.
- 8. The rubber stock of claim 6 wherein the first resin has a softening point ranging from about 135 to about 156° C., the second resin has a softening point ranging from about 138 to about 180° C., and the third resin has a softening point ranging from about 188 to about 208° C.
- 9. The rubber stock of claim 5 wherein the first resin has a molecular weight ranging from about 500 to about 15,000, the second resin has a molecular weight ranging from about 700 to about 15,000, the third resin has a molecular weight ranging from about 3,000 to about 15,000, and the fourth resin has a molecular weight ranging from about 4,000 to about 15,000.
- 10. The rubber stock of claim 6 wherein the first resin has a molecular weight ranging from about 700 to about 24,000, the second resin has a molecular weight ranging from about 700 to about 36,000, and the third resin has a molecular weight ranging from about 700 to about 42,000.
Parent Case Info
This is a Divisional of application Ser. No. 09/246,391, filed on Feb. 9, 1999, now U.S. Pat. No. 6,245,873.
US Referenced Citations (16)
Foreign Referenced Citations (2)
Number |
Date |
Country |
0063092 |
Oct 1982 |
EP |
0249904 |
Dec 1987 |
EP |
Non-Patent Literature Citations (4)
Entry |
Chemical Abstract 56109, vol. 90, 1979 p. 60. |
Chemical Abstracts, Section Ch. Week 198709, Abstract No. 002136270. |
Chemical Abstracts, Section Ch. Week 198841, Abstract No. 002136271. |
European Search Report. |