Galvanic corrosion causes voids and pits in conductive material of semiconductor device interconnects which reduces device reliability and useful device lifetime. Galvanic corrosion is caused by charge buildup on a wafer during a semiconductor device manufacturing process. Voids in semiconductor device interconnects contribute to electromigration defects, increased resistance between voltage sources and circuit elements, and mismatched circuit element performance. Galvanic corrosion and pitting are worsened by exposure to strong acids and bases during a manufacturing flow for a semiconductor device.
Aspects of the present disclosure are best understood from the following detailed description when read with the accompanying figures. It is noted that, in accordance with the standard practice in the industry, various features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or reduced for clarity of discussion.
The following disclosure provides many different embodiments, or examples, for implementing different features of the provided subject matter. Specific examples of components, values, operations, materials, arrangements, or the like, are described below to simplify the present disclosure. These are, of course, merely examples and are not intended to be limiting. Other components, values, operations, materials, arrangements, or the like, are contemplated. For example, the formation of a first feature over or on a second feature in the description that follows may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features may be formed between the first and second features, such that the first and second features may not be in direct contact. In addition, the present disclosure may repeat reference numerals and/or letters in the various examples. This repetition is for the purpose of simplicity and clarity and does not in itself dictate a relationship between the various embodiments and/or configurations discussed.
Further, spatially relative terms, such as “beneath,” “below,” “lower,” “above,” “upper” and the like, may be used herein for ease of description to describe one element or feature's relationship to another element(s) or feature(s) as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The apparatus may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein may likewise be interpreted accordingly.
Voids in interconnect structures of semiconductor devices have detrimental effects on the performance of the semiconductor devices. In some instances, voids lead to increased resistance between a voltage source and a circuit element of the semiconductor as the joint area between interconnect segments decreases. In some instances, voids also contribute to the electromigration of conductive material (copper, aluminum, and so forth), leading to breaks or “opens” in the interconnect structure of the semiconductor device, which increases a risk of failure of the semiconductor device. In some instances, voids also contribute to degraded device performance.
In some semiconductor devices, voids are a result of poor fill of a conductive material in an opening through a dielectric layer. In some embodiments, voids are a result of corrosion or pitting of a conductive material deposited in an opening through a dielectric layer. Pitting or corrosion results in a loss of conductive material at the site of the pit, or at corners of the interconnect segment, or electromigration of conductive material from other locations in the interconnect segment to the site of the pit or corrosion.
Copper is a conductive material used for semiconductor device interconnect segments. Copper diffusion into a dielectric layer or a semiconductor device base layer, or a semiconductor device substrate, is reduced by depositing a liner layer into openings which are later filled with copper. A liner layer slows diffusion of the copper into the dielectric layer of a semiconductor base layer.
One technique for reducing the formation of voids in copper interconnect segments includes protecting the exposed surface of the copper interconnect segment with a cap layer. A cap layer is a layer of conductive material which is deposited, or grown, on the top surface of the copper interconnect segment to reduce or prevent corrosion or pitting of the copper. Cobalt is used as a cap layer metal because the electropotential of a copper/cobalt junction is small: ΔE=ECo°−Cu20=(−0.28V)−(−0.34V)=−0.64V compared to the electropotential of other copper/metal junctions. For example, the copper/titanium junction electropotential is: ΔE(Ti/Cu)=−1.94V, and the copper/chromium junction electropotential is: ΔE(Cr/Cu)=−0.95V. Further, cobalt deposition on copper interconnect segments occurs without leaving a residue (or with minimal residue) over a top surface of the dielectric layer adjacent to the interconnect segment, which reduces the frequency of stringer defects and cobalt diffusion into the dielectric layer. A stringer defect is a short circuit between different interconnect segments. Cobalt is also more resistant to pitting than copper, and helps to protect copper interconnect segments from pitting and galvanic corrosion.
The present disclosure describes a method of modifying a top surface of a cap layer, including cobalt cap layers, to make the cap layer more resistant to pitting and galvanic corrosion. The present disclosure further describes a method of neutralizing charge buildup on a wafer during manufacturing of semiconductor devices to reduce pitting and galvanic corrosion. The present disclosure also describes a semiconductor device which reduces electromigration in interconnect structures to increase semiconductor device reliability and lifespan.
Method 100 includes an operation 102, wherein a first dielectric layer (see, e.g., dielectric layer 202 in
In some embodiments, the first dielectric layer comprises silicon dioxide (SiO2). Silicon dioxide has a dielectric constant (k) of about 3.9. In some embodiments, the first dielectric layer comprises a low-k dielectric material. A low-k dielectric layer has a dielectric constant below 3.9. In some embodiments, the first dielectric layer comprises a porous dielectric material (e.g., the dielectric layer includes pockets or voids formed after the first dielectric layer is deposited over the substrate). In some embodiments, the openings, or voids, in the first dielectric layer (see, e.g., dielectric layer 202 in
Method 100 includes an operation 104 in which an opening is formed in the first dielectric layer (see, e.g., dielectric layer 202 in
In some embodiments, the patterning material deposited over the dielectric layer includes photoresist or another material compatible with visible light lithography, ultra-violet light lithography (UV lithography, or UV patterning), electron beam lithography, and other methods of pattern transfer for semiconductor device manufacturing. In some embodiments, the patterning material is a visible-light compatible photoresist. In some embodiments, the patterning material is a UV lithography-compatible patterning material. In some embodiments, the patterning material is a mask material compatible with electron beam pattern transfer techniques. In some embodiments, the layer of patterning material is deposited over the dielectric layer by a spin-on technique and baking the spun-on material to cure the patterning material prior to developing.
In some embodiments, forming openings in the layer of patterning material includes developing the patterning material, where the developing process removes a portion of the layer of patterning material, and leaving behind a mask portion of the layer of patterning material. In some embodiments, the dielectric layer is below the layer of patterning material, and the dielectric layer is exposed within the openings. In some embodiments, a layer of hardmask material is between the layer of patterning material and the dielectric layer, and the layer of hardmask material is exposed at the bottom of the openings. In some embodiments, an etch process is performed to transfer the pattern directly to the dielectric layer. In some embodiments, a first etch process is performed to transfer the pattern to the layer of hardmask material, and a second etch process is performed to transfer the pattern to the dielectric layer. In some embodiments, multiple pattern transfer and etch steps are performed in order to form a dual-damascene type opening for an interconnect segment through the dielectric layer. In some embodiments, a first etch process forms trench openings in the dielectric layer, and a second etch process forms via openings aligned with the trench openings in the dielectric layer.
Method 100 includes an operation 106 wherein a liner (a liner layer, or a layer of liner material) is deposited on a sidewall of the opening through the first dielectric layer. In a non-limiting example,
Method 100 includes an optional operation 108 wherein a seed layer is deposited over the liner. In some embodiments, a seed layer is deposited over the liner in order to promote a smooth growth or deposition pattern of the layer of conductive material deposited for the interconnect segment formed in the opening through the dielectric layer. In a non-limiting example, seed layer 208 in
Method 100 includes an operation 110 wherein a first interconnect segment is formed in the opening in the first dielectric layer. Forming a first interconnect segment includes steps related to adding a conductive material to an opening through a dielectric layer. In some embodiments, adding a conductive material to an opening through a dielectric layer includes electroplating. In some embodiments, adding a conductive material to an opening includes performing a sputtering process in some embodiments, adding a conductive material includes performing a PVD process (a sublimation or evaporation-type process). In some embodiments, the conductive material is a pure metal. In some embodiments, the conductive material is a metal alloy. In some embodiments, the conductive material deposited in the opening to form the first interconnect segment comprises copper, aluminum, tungsten, or alloys thereof. According to some embodiments, the conductive material for the interconnect segment is deposited both in the opening through the dielectric layer, and over a top surface of the dielectric layer. Subsequent to deposition of the conductive material, a chemical-mechanical polishing (CMP) step is performed to remove conductive material from the top surface of the dielectric layer, leaving behind a portion of conductive material in the opening (now filled) through the dielectric layer. Thus, after performing a CMP step, interconnect segments embedded in the dielectric layer are electrically isolated from each other and have exposed top surfaces.
In some embodiments, the first interconnect segment includes a via portion and a trench portion. In some embodiments, the first interconnect segment includes a via portion but no trench portion. In some embodiments, the first interconnect segment includes a trench portion but no via portion. In a non-limiting example, a conductive material 210 of
Method 100 includes an operation 112 wherein a cap layer is formed on a top surface of the first interconnect segment. A cap layer is formed on a top surface of the first interconnect segment in order to help protect conductive material of the first interconnect segment from pitting or galvanic corrosion. According to some embodiments, the cap layer is formed by depositing a blanket layer of material over a top surface of the dielectric layer and over the interconnect segment, and performing a chemical mechanical polishing step to remove material from over the top surface of the dielectric layer while leaving a portion of the material over the interconnect segment. According to some embodiments, dishing of the conductive material for the interconnect segment recesses the conductive material slightly below the top surface of the dielectric layer, making a blanket deposition/CMP-style process feasible. According to some embodiments, material for a cap layer is grown selectively over a top surface of the conductive material for an interconnect segment using atomic layer deposition (ALD) or some other selective growth process.
In some embodiments, the cap layer is a pure metal. In some embodiments, the cap layer is a metal alloy. In some embodiments, the cap layer is cobalt. In some embodiments, the cap layer is a cobalt alloy. In some embodiments, the cap layer includes one or more of tantalum, titanium, nickel, niobium, and other metals suitable for copper deposition. In some embodiments, the cap layer is made of a same material as the seed layer. In some embodiments of optional operation 108, described above, the cap layer is made from a different material as the seed layer. In some embodiments, the cap layer is formed over a top side of an interconnect segment having a liner and no seed layer.
In some embodiments, a tantalum nitride liner is covered with a cobalt seed layer. A semiconductor device having both a cobalt seed layer and a cobalt cap layer (described below) experiences a significant decrease in the frequency of electromigration defects in the semiconductor device during electrical testing or operation of the semiconductor device, as compared to semiconductor devices which have only a cobalt cap layer, or which have a seed layer which does not include cobalt. In a non-limiting embodiment, semiconductor device 355 of
In some embodiments, the thickness of the cap layer ranges from 10 Å to 80 Å. Cap layer thicknesses of less than 10 Å are subject to increased frequency of pitting and erosion. Cap layers larger than 80 Å are unnecessarily thick and result in increased manufacturing cost and decreased productivity of a manufacturing process.
Method 100 includes an operation 114 wherein a top surface of the cap layer is modified to reduce galvanic corrosion. In some embodiments, uneven deposition of cap layer material, or defects in the cap layer material after deposition, are associated with pitting or galvanic corrosion of the conductive material below the cap layer, as water or cleaning agents penetrate through the cap layer to the conductive material of the interconnect segment. When water or cleaning agents penetrate through the cap layer to the conductive material, galvanic corrosion results in dissolution of the cap material and/or the conductive material of the interconnect segment. Modifying a top surface of a cap layer is effective at reducing the amount of pitting or galvanic corrosion in a semiconductor device.
Modification of a top surface of the cap layer includes several steps which produce an organometallic coating resistant to water penetration through the cap layer to the conductive material of the interconnect segment. In a non-limiting embodiment, a cobalt cap layer is modified by exposing the cobalt cap layer to ammonia (NH3). According to theory and belief, ammonia forms a van der Waals complex with cobalt atoms at the top surface of the cobalt cap layer. A monolayer of ammonia, complexed with the cobalt atoms at the top surface of the cap layer, provides coverage of the cobalt and prepares for other surface modification treatments to prevent corrosion of the cobalt layer. According to theory and belief, the unbonded valence electrons of the ammonia molecules form van der Waals complexes with the cobalt atom valence electrons which lock the ammonia molecules in place for subsequent processing operations.
Modifying the top surface of cap layer also includes exposing the ammonia-covered cobalt cap layer to methyl radicals (CH3⋅). According to theory and belief, methyl radicals react with the hydrogen atoms of the ammonia molecules in van der Waals complexes. Methyl radicals remove hydrogen atoms, promoting formation of cobalt-nitrogen bonds between the cobalt cap layer and the complexed ammonia molecules. Further reactions between methyl radicals and hydrogen atoms proceed by continuing to remove hydrogen from the ammonia molecule's nitrogen atom (now bonded to the cobalt). During some reactions of methyl radicals, the carbon atom of the methyl radical forms a C—N single bond, which undergoes “promotion” to a double bond or a triple bond according to the amount of hydrogen removed from the ammonia nitrogen atom. According to theory and belief, in some embodiments of the reactions between methyl radicals and the ammonia atoms complexed to the cobalt cap layer, the C—N bond (single, or double) rearranges to a lower energy state and the carbon atom directly bonds to the cobalt cap layer with the nitrogen atom extending outward from the cobalt cap layer (e.g., Co—C—NH2 or Co—C═N—H). According to theory and belief, the final bond structure of the cobalt cap layer is a mixture of Co—N+≡C− (a higher energy state configuration) and Co—C≡N (a lower energy state configuration), although some hydrogen atoms are present in some embodiments, especially embodiments manufactured without an excess of methyl radicals for hydrogen removal.
Thus, treatment of ammonia-complexed cobalt cap layer surfaces is understood to produce an organometallic (e.g., carbon atoms bonded to metal atoms of the cobalt surface) protective layer which significantly reduces the likelihood of pitting in semiconductor manufacturing processes. According to theory and belief, the organometallic cobalt/carbon/nitrogen cap layer coating at the top surface of the cap layer is understood to be moderately hydrophobic, repelling water and other liquids from the top surface by, e.g., a surface tension modification, to reduce intrusion into the cap layer and to the conductive material. Modifying the top surface of the cap layer includes treating the covered top surface of the cobalt cap layer with carbonated deionized (DI) water to clean the surface before deposition of etch stop layers, as described below in operation 116. In some embodiments of semiconductor devices having modified cobalt cap layers, the loss of cobalt in the cap layer, and seed layers at the sides of the interconnect segment, and void formation in the interconnect segment, is reduced.
A semiconductor device having both a cobalt seed layer and a cobalt cap layer (a “cobalt all around” interconnect segment, including both surface-modified layers and unmodified cap layers) is better able to carry electrical current along an exterior of an interconnect segment, rather than through a bulk structure, resulting in reduced electromigration of the conductive material comprising the bulk of the interconnect segment. In some embodiments, semiconductor devices having interconnect segments both a cobalt seed layer and a cobalt cap layer have up to 100 times reduction in the frequency of electromigration defects in the semiconductor devices in comparison to semiconductor devices having: [1] no cobalt seed layer and no cobalt cap layer, [2] no cobalt seed layer, or [3] no cobalt cap layer.
Method 100 includes an operation 116 wherein at least one etch stop layer is deposited over the conductive material of the first interconnect segment. According to some embodiments, the bottom etch stop layer deposited over the dielectric layer and the first interconnect segment includes an aluminum oxy-nitride or aluminum oxide layer. In some embodiments, a middle etch stop layer deposited over the dielectric layer and the first interconnect segment includes an oxygen doped carbon layer. In some embodiments, a top etch stop layer deposited over the dielectric layer and the first interconnect segment includes an aluminum oxide (AlOx) layer. Semiconductor devices having at least one etch stop layer have more uniform openings for second and subsequent interconnect segments than semiconductor devices without etch stop layer. Etch stop layers protects materials and layers below the etch stop layer while etch processes are being performed above the etch stop layer.
According to some embodiments, etch stop layers as described above are deposited by chemical vapor deposition (CVD) or PVD processes. According to some embodiments, each of the etch stop layers deposited over the dielectric layer and the first interconnect segment has different degrees of resistance to plasma etch layers above the etch stop layer. According to some embodiments, multiple etching processes are performed above and each etch process stop on, or penetrate through, one of etch stop layers before exposing the first interconnect segment and/or dielectric layer. In a non-limiting embodiment, semiconductor device 200 in
Method 100 includes an operation 118 wherein a second dielectric layer is deposited over the at least one etch stop layer. According to some embodiments, the second dielectric layer is a silicon dioxide layer. According to some embodiments, the second dielectric layer is a low-k dielectric layer and is deposited in a manner similar to the manner described above in the description of operation 102. In some embodiments, the second dielectric layer is a porous dielectric layer. In some embodiments, the second dielectric layer is a solid material without holes or openings therein.
Method 100 includes an operation 120 wherein an opening is formed through the second dielectric layer. Forming an opening in a dielectric layer includes steps of depositing a layer of patterning material over the dielectric layer, transferring a pattern to the layer of patterning material, forming openings in the layer of patterning material to expose the dielectric layer, and performing an etch process to remove exposed portions of the dielectric layer at the bottom of the openings in the layer of patterning material. In a non-limiting example, semiconductor device 200 of
In some embodiments, the patterning material deposited over the dielectric layer includes photoresist or another material compatible with visible light lithography, ultra-violet light lithography (UV lithography, or UV patterning), electron beam lithography, and other methods of pattern transfer for semiconductor device manufacturing. In some embodiments, the patterning material is a visible-light compatible photoresist. In some embodiments, the patterning material is a UV lithography-compatible patterning material. In some embodiments, the patterning material is a mask material compatible with electron beam pattern transfer techniques. In some embodiments, the layer of patterning material is deposited over the dielectric layer by a spin-on technique and baking the spun-on material to cure the patterning material prior to developing.
In some embodiments, forming openings in the layer of patterning material includes developing the patterning material, where the develop process removes a portion of the layer of patterning material, and leaving behind a mask portion of the layer of patterning material. In some embodiments, the dielectric layer is below the layer of patterning material, and the dielectric layer is exposed within the openings. In some embodiments, a layer of hardmask material is between the layer of patterning material and the dielectric layer, and the layer of hardmask material is exposed at the bottom of the openings. In some embodiments, an etch process is performed to transfer the pattern directly to the dielectric layer. In some embodiments, a first etch process is performed to transfer the pattern to the layer of hardmask material, and a second etch process is performed to transfer the pattern is to dielectric layer. In some embodiments, multiple pattern transfer and etch steps are performed in order to form a dual-damascene type opening for an interconnect segment through the dielectric layer. In some embodiments, a first etch process forms trench openings in the dielectric layer, and a second etch process forms via openings aligned with the trench openings in the dielectric layer.
In some embodiments, forming an opening through the second dielectric layer includes wet processing steps to selectively remove one or more of the etch stop layers (e.g., after performing a plasma etch, performing a wet etch to remove the etch stop layer exposed by the plasma etch), to give a clean surface for subsequent operations of the manufacturing process of the semiconductor device.
In some embodiments, forming an opening through the second dielectric layer includes etching through the entirety of the second dielectric layer in an opening of the pattern over the second dielectric layer with the opening of the pattern offset from the position of the first interconnect segment below the second dielectric layer. By offsetting the opening through the second dielectric layer from the first interconnect segment [1] the second interconnect segment (to be formed in the opening through the second dielectric layer, see operation 130, below) makes contact with part of the top surface of the first interconnect segment, and [2] part of the sidewall of the first interconnect segment. In
Method 100 includes an operation 122 wherein a charge neutralization process is performed on the semiconductor device. In a non-limiting embodiment, semiconductor device 200 of
Charge builds up on semiconductor wafers during manufacturing processes. The charge buildup on a semiconductor wafer triggers pitting and galvanic corrosion of interconnect segments when the exposed metal of unmodified cap layers, or the bare interconnect segment, is exposed to moisture (water or other liquids capable of conducting an electric current).
The amount of charge buildup (e.g., the wafer electrical potential with respect to ground) changes during a semiconductor device manufacturing process, as the charge buildup is bled off (by, e.g., grounding the wafer) or added to during wafer handling. A charge neutralization process is a liquid treatment of the semiconductor wafer to remove or reduce the charge buildup without triggering pitting or galvanic corrosion of the exposed conductors (e.g., cap layers, interconnect segments, and so forth) during a manufacturing process. The liquid treatment for charge neutralization comprises [1] preparing a dilute solution of ionic solutes (a charge neutralization wash) which precipitate on exposure to the static electricity buildup on the semiconductor wafer, [2] applying the charge neutralization wash to the wafer or semiconductor device, and [3] rinsing the charge neutralization wash from the wafer or semiconductor device. A charge neutralization wash includes ionic solutes which receive electrons from the wafer substrate to convert the dissolved ions into a suspended precipitate which is removed from the semiconductor device in a rinse step after charge neutralization. According to some embodiments, charge neutralization washes include a solution containing one or more of: BF3, CO2, SO32−, Cu+, Ag+, GaCl3, CN−, RS−, and CO, wherein RS− is a thiol compound and R is an aliphatic chain having a main chain length L of 1 to 12 carbon atoms.
According to some embodiments, charge neutralization washes leave a neutralization residue behind on the exposed sidewalls of the dielectric layer. Further discussion of the charge neutralization residues is presented below in the discussion of
In some embodiments, the charge neutralization wash is applied to the opening through the second dielectric layer (see dielectric layer 222 of
According to some embodiments, a charge neutralization wash has a pH of at least 8 and not more than 12. By maintaining the pH at not less than least 8 and not more than 12, the charge neutralization wash has a pH which [1] promotes removal of aluminum oxide (e.g., a common etch stop material, see etch stop layer 216 in
Charge neutralization wash is adjusted to the pH of at least 8 and not more than 12 by adding ammonium hydroxide (NH4OH) to the solution. The semiconductor device is rinsed using a combination of ammonium hydroxide (NH4OH) with hydrogen peroxide (H2O2), followed by a dilute solution of carbonic acid (CO2 in water, or H2CO3) in Di water to neutralize residual ammonium hydroxide over the wafer surface after the charge neutralization. In some embodiments, charge neutralization is performed after every liquid etch/wet processing step to neutralize charge buildup on a wafer. Charge neutralization, as described hereinabove, is compatible with liquid etch manufacturing steps throughout the semiconductor device manufacturing flow and is effective at reducing voids (especially copper interconnect voids) at all layers of the semiconductor device interconnect structure. In some embodiments, oxygen-depleted (degassed, or oxygen-purged) deionized water containing a sodium sulfide solution is used as a rinsing agent in a charge neutralization process to remove charge buildup, to remove precipitate atoms, and to neutralize residual acid or peroxide on a wafer surface.
Performing charge neutralization of a semiconductor device is effective at reducing a charge buildup on a wafer from more than 3 Volts to less than 0.5 Volts after the charge neutralization wash. A charge neutralization wash is effective at reducing the charge buildup over an entire wafer, and is non-uniform across the wafer, to a lower, more uniform value. For example, in some embodiments, a charge buildup on a wafer is largest (e.g., most negative) at a center of a wafer, decreases gradually along a mid-radius portion of the wafer, and drops off sharply at a wafer perimeter. Performing a charge neutralization wash on a wafer reduces the charge buildup on the wafer to a lower, more uniform level across the entire mid-radius and center regions of the wafer, with a drop-off at the wafer perimeter.
Method 100 includes an operation 124, wherein a top surface the interconnect segment (see
In some embodiments, the top surface of the interconnect segment is exposed by performing a liquid etch process after performing the charge neutralization wash described above in operation 122. In some embodiments, both the charge neutralization wash (operation 122) and opening the etch stop layer to expose the interconnect segment (operation 124) are performed in a same wet etch processing tool, and the liquid stream applied to the surface of the wafer is switched smoothly between [1] charge neutralization wash, [2] rinse, and [3] etch chemistry to expose the underlying interconnect segment without removing the wafer from the processing tool. By reducing the processing time between performing the charge neutralization wash and etch to expose the interconnect segment, an amount of time for pitting and galvanic corrosion is reduced, further decreasing the likelihood of void formation in the semiconductor device during a manufacturing flow for the semiconductor device.
Method 100 includes an operation 126, wherein a liner is deposited in the opening through the second dielectric layer. In
Method 100 includes an optional operation 128, wherein a seed layer is deposited in the opening through the second dielectric layer. A seed layer is deposited over the liner in order to promote a smooth growth or deposition pattern of the layer of conductive material deposited for the interconnect segment formed in the opening through the dielectric layer. In some embodiments, a seed layer is a pure metal. In some embodiments, the seed layer is a metal alloy. In some embodiments, the seed layer comprises cobalt, tantalum, titanium, nickel, niobium, copper, or another seed layer metal compatible with copper deposition in the opening through the dielectric layer. According to some embodiments, the thickness of the seed layer is different on sidewalls of the opening that over the bottom of the opening. According to some embodiments, thickness of the seed layer on a sidewall ranges from about 5 Angstroms (Å) to about 50 Å. In some embodiments, thickness of the seed layer is about 20 Å. A thickness of a seed layer less than 5 Å (or, an average thickness of less than 5 Å) is likely to have incomplete coverage of the liner, where the liner will make electrical contact with conductive material of an interconnect segment after the opening is filled. A thickness of the seed layer greater than 50 Å does not produce additional benefits to a semiconductor device, and merely prolongs manufacturing time and increases manufacturing costs.
Method 100 includes an operation 130, wherein a second interconnect segment is formed in the opening in the second dielectric layer. A second interconnect segment is formed in a manner similar to the formation of the first interconnect segment, as described in operation 110, above. Forming a second interconnect segment includes steps related to adding a conductive material to an opening through a dielectric layer. In some embodiments, adding a conductive material to an opening through a dielectric layer includes electroplating. In some embodiments, adding a conductive material to an opening includes performing a sputtering process in some embodiments, adding a conductive material includes performing a PVD process (a sublimation or evaporation-type process). In some embodiments, the conductive material is a pure metal. In some embodiments, the conductive material is a metal alloy. In some embodiments, the conductive material deposited in the opening to form the second interconnect segment comprises copper, aluminum, tungsten, or alloys thereof. According to some embodiments, the conductive material for the interconnect segment is deposited both in the opening through the dielectric layer, and over a top surface of the dielectric layer. Subsequent to deposition of the conductive material, a chemical-mechanical polishing (CMP) step is performed to remove conductive material from the top surface of the dielectric layer, leaving behind a portion of conductive material in the opening (now filled) through the dielectric layer. Thus, after performing a CMP step, interconnect segments embedded in the dielectric layer are electrically isolated from each other and have exposed top surfaces.
In
In some embodiments, the dielectric layer is a low-k dielectric material, with a dielectric constant of less than 3.9. In some embodiments, the dielectric layer is a porous low-k material. In some embodiments, the low-k dielectric material is a solid dielectric layer, with no voids.
In
In some embodiments, the liner comprises a metal nitride. According to some embodiments, the liner comprises tantalum nitride (TaN), titanium nitride (TiN), niobium nitride (NbN), or another metal nitride which slows or blocks metal diffusion into a dielectric layer. Other liner materials which slow or block metal diffusion into a dielectric layer are also within the scope of the present disclosure.
In some embodiments, the liner material comprises tantalum nitride (TaN), titanium nitride (TiN), niobium nitride (NbN), or another metal nitride which slows or blocks diffusion of interconnect segment metal (e.g., copper, aluminum, and so forth) into dielectric layers of a semiconductor device.
In some embodiments, the seed layer is a pure metal. In some embodiments, the seed layer is a metal alloy. According to some embodiments, the seed layer comprises cobalt, tantalum, titanium, nickel, niobium, copper, or another seed layer metal compatible with deposition of a conductive material the opening of the dielectric layer. Seed layer 208 has a non-uniform thickness, with a smaller thickness on the sidewalls, and a larger thickness on the bottom of the opening through the dielectric layer. According to some embodiments, thickness of the seed layer on a sidewall ranges from about 5 Angstroms (Å) to about 50 Å. In some embodiments, thickness of the seed layer is about 20 Å. A thickness of a seed layer less than 5 Å (or, an average thickness of less than 5 Å) is likely to have incomplete coverage of the liner, where the liner will make electrical contact with conductive material of an interconnect segment after the opening is filled. A thickness of the seed layer greater than 50 Å does not produce additional benefits to a semiconductor device, and merely prolongs manufacturing time and increases manufacturing costs.
In
Conductive material 210 is copper. In some embodiments, the conductive material is a copper alloy, or a tungsten alloy, or some other material suitable for filling trench structures in a dielectric layer. According to some embodiments, the copper for conductive material 210 is deposited by electroplated, and thinned off of the top surface of dielectric layer 202 by a chemical mechanical polishing (CMP) step.
Cap layer 212 comprises a same material as seed layer 208. In some embodiments, the cap layer includes a different metal than the seed layer. In some embodiments, the cap layer is a cobalt cap layer, and the seed layer is a cobalt seed layer. In some embodiments, the thickness of the cap layer ranges from 10 Å to 80 Å. Cap layer thicknesses of less than 10 Å are subject to increased frequency of pitting and erosion. Cap layers larger than 80 Å are unnecessarily thick and result in increased manufacturing cost and decreased productivity of a manufacturing process.
Cap layer 212 is modified to have an organometallic film thereon by steps described above in operation 114. The organometallic cobalt/carbon/nitrogen coating at the top surface of the cap layer is understood to be moderately hydrophobic, repelling water and other liquids from the top surface by, e.g., preventing “wetting” of the surface due to an increased contact angle of the organometallic film on the cap layer, to reduce liquid intrusion into the cap layer and down to the conductive material. According to some embodiments, the addition of methyl radicals to ammonia/cobalt van der Waals complexes produces C—N bonds, C—Co bonds, and N—Co bonds. In some embodiments, the addition of methyl radicals to the Co—NH3 van der Walls complexes produces Co—CN complexes on the top surface of the cobalt cap layer.
In
Etch stop layers 216, 218, and 220 are deposited by, e.g., a PVD process. According to some embodiments, etch stop layer 216 is an aluminum oxy-nitride (AlON) layer or an aluminum oxide (Al2O3) layer. According to some embodiments, etch stop layer 218 is an oxide-doped carbon layer (e.g., silicon carbide with oxygen inclusions). According to some embodiments etch stop layer 220 is an aluminum oxide layer (Al2O3 or AlOx). Etch stop layers 216, 218, and 220 are configured to provide different selectivity to plasma and liquid etch chemistries during the manufacturing process of semiconductor device 200.
In some embodiments, dielectric layer 222 is a silicon dioxide layer deposited by a CVD process. In some embodiments, dielectric layer 222 is a low-k dielectric material deposited by, e.g., a spin-on coat process, followed by a bake process to drive off solvent in the spin-on material and harden or polymerize the low-k dielectric material precursor into a solid form.
In
In some embodiments, the etch processes are plasma etch processes configured to have straight sidewalls. Opening 224 extends through dielectric layer 222, etch stop layer 220, etch stop layer 218, and partly into etch stop layer 216. A remaining portion of etch stop layer 216 separates opening 224 from cap layer 212. A trench opening 224B is at an upper portion of the opening 224, and a via opening 224A is at a lower portion of the opening 224. In some embodiments, two plasma etch processes are used to form trench opening 224B and via opening 224A. In some embodiments, a single plasma etch process is used to form both trench opening 224B and via opening 224A.
Charge neutralization residues 225 are on a sidewall of opening 224, including on both trench opening 224B and via opening 224A. Charge neutralization residue 225A is on etch stop layer 216 at the bottom of via opening 224A. In some embodiments, the charge neutralization residue includes one or more of silver (Ag), carbon (C), gallium (Ga), boron (B), and fluorine (F) at a concentration of about 5×1016 atoms/cm3. A concentration of the neutralization residue ranges from about 1×1016 atoms/cm3 to about 1×1017 atoms/cm3. A neutralization residue concentration of less than about 1×1016 atoms/cm3 is indicative of insufficient exposure of the semiconductor device, or the interconnect segment, to the charge neutralizing chemicals in the charge neutralization wash, leaving static electricity buildup on the semiconductor device and promoting corrosion of the interconnect segment (e.g., the cap layer, the liner, and/or the conductive material filled into the opening in the dielectric layer). A neutralization residue concentration of greater than about 1×1017 atoms/cm3 is indicative of overexposure of the semiconductor device, or the interconnect segment, or the cap layer (modified or unmodified) to the charge neutralizing chemicals, with an elevated likelihood of charge neutralization residues contaminating the opening for the interconnect segment, or contaminating the dielectric layer before a new liner (or new seed layer) is deposited in the opening through the second dielectric layer.
In
In
In method 100, a liner is deposited into the opening through the second dielectric layer in operation 126. In method 100, a description of depositing a seed layer over the liner is provided in operation 128. In method 100, a description of depositing conductive material over the seed layer is provided in operation 130.
Liner 226 is a tantalum nitride layer. In some embodiments, other liner materials such as titanium nitride (TiN), niobium nitride (NbN), or another metal nitride which slows or block metal diffusion in to a dielectric layer are used instead of tantalum nitride. Seed layer 227 is a cobalt seed layer. In some embodiments, other metals are used for the seed layer, according to the discussion of operation 108, above.
Conductive material 228 is copper metal. In some embodiments, a copper alloy is used for filling the opening and forming interconnect segments through the dielectric layer 222. Further discussion of conductive materials suitable for deposition into an opening through a dielectric layer is provided above in the discussion of operation 110.
Charge neutralization residues 225 are embedded between dielectric layer 222 and liner 226. In some embodiments, the charge neutralization residue includes one or more of silver (Ag), carbon (C), gallium (Ga), boron (B), and fluorine (F) at a concentration of about 5×1016 atoms/cm3. A concentration of the neutralization residue ranges from about 1×1016 atoms/cm3 to about 1×1017 atoms/cm3. A neutralization residue concentration of less than about 1×1016 atoms/cm3 is indicative of insufficient exposure of the semiconductor device, or the interconnect segment, to the charge neutralizing chemicals in the charge neutralization wash, leaving static electricity buildup on the semiconductor device and promoting corrosion of the interconnect segment (e.g., the cap layer, the liner, and/or the conductive material filled into the opening in the dielectric layer). A neutralization residue concentration of greater than about 1×1017 atoms/cm3 is indicative of overexposure of the semiconductor device, or the interconnect segment, or the cap layer (modified or unmodified) to the charge neutralizing chemicals, with an elevated likelihood of charge neutralization residues contaminating the opening for the interconnect segment, or contaminating the dielectric layer before a new liner (or new seed layer) is deposited in the opening through the second dielectric layer.
Interconnect segment 213 and interconnect segment 215 are non-overlapping interconnect segments, where the interconnect segments meet at an interface which corresponds to an interface between a dielectric layer and an etch stop layer. Interconnect segment 215 includes contact 230 and conductive line 232.
In
In
In interconnect segment 315A, liner 326 is in direct contact with conductive material 328. Semiconductor device 345 includes a cap layer 312 which is modified to have reduced pitting and protect conductive material 310 from galvanic corrosion. Semiconductor device 345 has charge neutralization residues 325 on sides of dielectric layer 322 and the between the liner 326 and etch stop layers 316, 318, and 320. Interconnect segment 315A includes a via 330 and a trench 332. Via 330 is in lower opening 324A, and trench 332 is in upper opening 324B.
In
In
The method and embodiments described above are adjusted using an EDA system to compensate for the effect of charge neutralization on the wafer and seed layer deposition and offset of some interconnect segments (or, openings for the patterning and etch process described above). Variations of the embodiments and method described above, and in the EDA system instructions and the manufacturing flow described below, will be familiar to those having skill in the art.
In some embodiments, EDA system 500 includes an APR system. Methods described herein of designing layout diagrams represent wire routing arrangements, in accordance with one or more embodiments, are implementable, for example, using EDA system 500, in accordance with some embodiments.
In some embodiments, EDA system 500 is a general purpose computing device including a hardware processor 502 and a non-transitory, computer-readable storage medium 504. Storage medium 504, amongst other things, is encoded with, i.e., stores, computer program code 506, i.e., a set of executable instructions. Execution of instructions 506 by hardware processor 502 represents (at least in part) an EDA tool which implements a portion or all of the methods described herein in accordance with one or more embodiments (hereinafter, the noted processes and/or methods).
Processor 502 is electrically coupled to computer-readable storage medium 504 via a bus 508. Processor 502 is also electrically coupled to an I/O interface 510 by bus 508. A network interface 512 is also electrically connected to processor 502 via bus 508. Network interface 512 is connected to a network 514, so that processor 502 and computer-readable storage medium 504 are capable of connecting to external elements via network 514. Processor 502 is configured to execute computer program code 506 encoded in computer-readable storage medium 504 in order to cause system 500 to be usable for performing a portion or all of the noted processes and/or methods. In one or more embodiments, processor 502 is a central processing unit (CPU), a multi-processor, a distributed processing system, an application specific integrated circuit (ASIC), and/or a suitable processing unit.
In one or more embodiments, computer-readable storage medium 504 is an electronic, magnetic, optical, electromagnetic, infrared, and/or a semiconductor system (or apparatus or device). For example, computer-readable storage medium 504 includes a semiconductor or solid-state memory, a magnetic tape, a removable computer diskette, a random access memory (RAM), a read-only memory (ROM), a rigid magnetic disk, and/or an optical disk. In one or more embodiments using optical disks, computer-readable storage medium 504 includes a compact disk-read only memory (CD-ROM), a compact disk-read/write (CD-R/W), and/or a digital video disc (DVD).
In one or more embodiments, storage medium 504 stores computer program code 506 configured to cause system 500 (where such execution represents (at least in part) the EDA tool) to be usable for performing a portion or all of the noted processes and/or methods. In one or more embodiments, storage medium 504 also stores information which facilitates performing a portion or all of the noted processes and/or methods. In one or more embodiments, storage medium 504 stores library 507 of standard cells including such standard cells as disclosed herein. In one or more embodiments, storage medium 504 stores one or more layout diagrams 509 corresponding to one or more layouts disclosed herein.
EDA system 500 includes I/O interface 510. I/O interface 510 is coupled to external circuitry. In one or more embodiments, I/O interface 510 includes a keyboard, keypad, mouse, trackball, trackpad, touchscreen, and/or cursor direction keys for communicating information and commands to processor 502.
EDA system 500 also includes network interface 512 coupled to processor 502. Network interface 512 allows system 500 to communicate with network 514, to which one or more other computer systems are connected. Network interface 512 includes wireless network interfaces such as BLUETOOTH, WIFI, WIMAX, GPRS, or WCDMA; or wired network interfaces such as ETHERNET, USB, or IEEE-1364. In one or more embodiments, a portion or all of noted processes and/or methods, is implemented in two or more systems 500.
System 500 is configured to receive information through I/O interface 510. The information received through I/O interface 510 includes one or more of instructions, data, design rules, libraries of standard cells, and/or other parameters for processing by processor 502. The information is transferred to processor 502 via bus 508. EDA system 500 is configured to receive information related to a UI through I/O interface 510. The information is stored in computer-readable medium 504 as user interface (UI) 542.
In some embodiments, a portion or all of the noted processes and/or methods is implemented as a standalone software application for execution by a processor. In some embodiments, a portion or all of the noted processes and/or methods is implemented as a software application that is a part of an additional software application. In some embodiments, a portion or all of the noted processes and/or methods is implemented as a plug-in to a software application. In some embodiments, at least one of the noted processes and/or methods is implemented as a software application that is a portion of an EDA tool. In some embodiments, a portion or all of the noted processes and/or methods is implemented as a software application that is used by EDA system 500. In some embodiments, a layout diagram which includes standard cells is generated using a tool such as VIRTUOSO® available from CADENCE DESIGN SYSTEMS, Inc., or another suitable layout generating tool.
In some embodiments, the processes are realized as functions of a program stored in a non-transitory computer readable recording medium. Examples of a non-transitory computer readable recording medium include, but are not limited to, external/removable and/or internal/built-in storage or memory unit, e.g., one or more of an optical disk, such as a DVD, a magnetic disk, such as a hard disk, a semiconductor memory, such as a ROM, a RAM, a memory card, and the like.
In
Design house (or design team) 620 generates an IC design layout diagram 622. IC design layout diagram 622 includes various geometrical patterns designed for an IC device 660. The geometrical patterns correspond to patterns of metal, oxide, or semiconductor layers that make up the various components of IC device 660 to be fabricated. The various layers combine to form various IC features. For example, a portion of IC design layout diagram 622 includes various IC features, such as an active region, gate electrode, source and drain, metal lines or vias of an interlayer interconnection, and openings for bonding pads, to be formed in a semiconductor substrate (such as a silicon wafer) and various material layers disposed on the semiconductor substrate. Design house 620 implements a proper design procedure to form IC design layout diagram 622. The design procedure includes one or more of logic design, physical design or place and route. IC design layout diagram 622 is presented in one or more data files having information of the geometrical patterns. For example, IC design layout diagram 622 can be expressed in a GDSII file format or DFII file format.
Mask house 630 includes data preparation 632 and mask fabrication 644. Mask house 630 uses IC design layout diagram 622 to manufacture one or more masks 645 to be used for fabricating the various layers of IC device 660 according to IC design layout diagram 622. Mask house 630 performs mask data preparation 632, where IC design layout diagram 622 is translated into a representative data file (“RDF”). Mask data preparation 632 provides the RDF to mask fabrication 644. Mask fabrication 644 includes a mask writer. A mask writer converts the RDF to an image on a substrate, such as a mask (reticle) 645 or a semiconductor wafer 653. The design layout diagram 622 is manipulated by mask data preparation 632 to comply with particular characteristics of the mask writer and/or requirements of IC fab 650. In
In some embodiments, mask data preparation 632 includes optical proximity correction (OPC) which uses lithography enhancement techniques to compensate for image errors, such as those that can arise from diffraction, interference, other process effects and the like. OPC adjusts IC design layout diagram 622. In some embodiments, mask data preparation 632 includes further resolution enhancement techniques (RET), such as off-axis illumination, sub-resolution assist features, phase-shifting masks, other suitable techniques, and the like or combinations thereof. In some embodiments, inverse lithography technology (ILT) is also used, which treats OPC as an inverse imaging problem.
In some embodiments, mask data preparation 632 includes a mask rule checker (MRC) that checks the IC design layout diagram 622 that has undergone processes in OPC with a set of mask creation rules which contain certain geometric and/or connectivity restrictions to ensure sufficient margins, to account for variability in semiconductor manufacturing processes, and the like. In some embodiments, the MRC modifies the IC design layout diagram 622 to compensate for limitations during mask fabrication 644, which may undo part of the modifications performed by OPC in order to meet mask creation rules.
In some embodiments, mask data preparation 632 includes lithography process checking (LPC) that simulates processing that will be implemented by IC fab 650 to fabricate IC device 660. LPC simulates this processing based on IC design layout diagram 622 to create a simulated manufactured device, such as IC device 660. The processing parameters in LPC simulation can include parameters associated with various processes of the IC manufacturing cycle, parameters associated with tools used for manufacturing the IC, and/or other aspects of the manufacturing process. LPC takes into account various factors, such as aerial image contrast, depth of focus (“DOF”), mask error enhancement factor (“MEEF”), other suitable factors, and the like or combinations thereof. In some embodiments, after a simulated manufactured device has been created by LPC, if the simulated device is not close enough in shape to satisfy design rules, OPC and/or MRC are be repeated to further refine IC design layout diagram 622.
It should be understood that the above description of mask data preparation 632 has been simplified for the purposes of clarity. In some embodiments, data preparation 632 includes additional features such as a logic operation (LOP) to modify the IC design layout diagram 622 according to manufacturing rules. Additionally, the processes applied to IC design layout diagram 622 during data preparation 632 may be executed in a variety of different orders.
After mask data preparation 632 and during mask fabrication 644, a mask 645 or a group of masks 645 are fabricated based on the modified IC design layout diagram 622. In some embodiments, mask fabrication 644 includes performing one or more lithographic exposures based on IC design layout diagram 622. In some embodiments, an electron-beam (e-beam) or a mechanism of multiple e-beams is used to form a pattern on a mask (photomask or reticle) 645 based on the modified IC design layout diagram 622. Mask 645 can be formed in various technologies. In some embodiments, mask 645 is formed using binary technology. In some embodiments, a mask pattern includes opaque regions and transparent regions. A radiation beam, such as an ultraviolet (UV) beam, used to expose the image sensitive material layer (e.g., photoresist) which has been coated on a wafer, is blocked by the opaque region and transmits through the transparent regions. In one example, a binary mask version of mask 645 includes a transparent substrate (e.g., fused quartz) and an opaque material (e.g., chromium) coated in the opaque regions of the binary mask. In another example, mask 645 is formed using a phase shift technology. In a phase shift mask (PSM) version of mask 645, various features in the pattern formed on the phase shift mask are configured to have proper phase difference to enhance the resolution and imaging quality. In various examples, the phase shift mask can be attenuated PSM or alternating PSM. The mask(s) generated by mask fabrication 644 is used in a variety of processes. For example, such a mask(s) is used in an ion implantation process to form various doped regions in semiconductor wafer 653, in an etching process to form various etching regions in semiconductor wafer 653, and/or in other suitable processes.
IC fab 650 is an IC fabrication business that includes one or more manufacturing facilities for the fabrication of a variety of different IC products. In some embodiments, IC Fab 650 is a semiconductor foundry. For example, there may be a manufacturing facility for the front end fabrication of a plurality of IC products (front-end-of-line (FEOL) fabrication), while a second manufacturing facility may provide the back end fabrication for the interconnection and packaging of the IC products (back-end-of-line (BEOL) fabrication), and a third manufacturing facility may provide other services for the foundry business.
IC fab 650 includes fabrication tools 652 configured to execute various manufacturing operations on semiconductor wafer 653 such that IC device 660 is fabricated in accordance with the mask(s), e.g., mask 645. In various embodiments, fabrication tools 652 include one or more of a wafer stepper, an ion implanter, a photoresist coater, a process chamber, e.g., a CVD chamber or LPCVD furnace, a CMP system, a plasma etch system, a wafer cleaning system, or other manufacturing equipment capable of performing one or more suitable manufacturing processes as discussed herein.
IC fab 650 uses mask(s) 645 fabricated by mask house 630 to fabricate IC device 660. Thus, IC fab 650 at least indirectly uses IC design layout diagram 622 to fabricate IC device 660. In some embodiments, semiconductor wafer 653 is fabricated by IC fab 650 using mask(s) 645 to form IC device 660. In some embodiments, the IC fabrication includes performing one or more lithographic exposures based at least indirectly on IC design layout diagram 622. Semiconductor wafer 653 includes a silicon substrate or other proper substrate having material layers formed thereon. Semiconductor wafer 653 further includes one or more of various doped regions, dielectric features, multilevel interconnects, and the like (formed at subsequent manufacturing steps).
Details regarding an integrated circuit (IC) manufacturing system (e.g., system 600 of
A system of one or more computers can be configured to perform particular operations or actions by virtue of having software, firmware, hardware, or a combination of them installed on the system that in operation causes or cause the system to perform the actions. One or more computer programs can be configured to perform particular operations or actions by virtue of including instructions that, when executed by data processing apparatus, cause the apparatus to perform the actions.
One general aspect includes a device. The device also includes a first dielectric layer over a device base layer, the first dielectric layer having a first opening therethrough, the first opening having a first sidewall; a first interconnect segment extending through the first opening; and a cap layer over a top surface of the first interconnect segment, where the cap layer may include a first metal, carbon, and nitrogen. Other embodiments of this aspect include corresponding computer systems, apparatus, and computer programs recorded on one or more computer storage devices, each configured to perform the actions of the methods.
Implementations may include one or more of the following features. The device may include: a second dielectric layer over the first dielectric layer and the first interconnect segment, where the second dielectric layer has a second opening extending therethrough; and a second interconnect segment extending through the second opening and electrically connected to the first interconnect segment. The cap layer is between the first interconnect segment from the second interconnect segment. The first metal may include cobalt. The liner layer is between the first sidewall of the first opening and the first interconnect segment; and a seed layer may include the first metal, where the seed layer is between the liner layer and the first interconnect segment. The first metal may include cobalt, and the second metal may include tantalum. The first dielectric layer may include a low-k dielectric layer. The first dielectric layer may include a porous low-k dielectric layer. The charge neutralization wash residue may include one or more of boron, fluorine, gallium, silver, and copper ranging from 1×1016 atoms/(cubic centimeter (cm3)) to 1×1017 atoms/(cm3). Implementations of the described techniques may include hardware, a method or process, or computer software on a computer-accessible medium.
One general aspect includes a method of making a semiconductor device. The method also includes depositing a first dielectric layer over a base layer of the semiconductor device; forming a first opening through the first dielectric layer to expose the base layer of the semiconductor device, forming a first interconnect segment in the first opening, forming a cap layer may include a first metal over a top surface of the interconnect segment, and modifying the cap layer to have an organometallic film. Other embodiments of this aspect include corresponding computer systems, apparatus, and computer programs recorded on one or more computer storage devices, each configured to perform the actions of the methods.
Implementations may include one or more of the following features. The method may include: depositing a liner layer in the first opening; and depositing a seed layer over the liner layer, where the seed layer may include the first metal. The first interconnect segment is exposed at a bottom of the second opening; and forming a second interconnect segment in the second opening. Modifying the cap layer further may include: binding ammonia to the top surface of the cap layer; reacting a portion of the ammonia with methyl radicals; and removing hydrogen from the ammonia and the methyl groups to form an organometallic film on the cap layer. Implementations of the described techniques may include hardware, a method or process, or computer software on a computer-accessible medium.
One general aspect includes a method of making a semiconductor device. The method also includes depositing a dielectric layer over an interconnect segment; forming an opening through the dielectric layer to expose the interconnect segment, where the opening forms a sidewall of the dielectric layer; neutralizing a charge buildup on the semiconductor device; depositing a liner on the sidewall of the dielectric layer; and filling the opening with a conductive material. Other embodiments of this aspect include corresponding computer systems, apparatus, and computer programs recorded on one or more computer storage devices, each configured to perform the actions of the methods.
Implementations may include one or more of the following features. The method may include depositing an etch stop layer over the interconnect segment, where forming an opening through a dielectric layer further may include etching through the dielectric layer to expose the etch stop layer, and etching partially through the etch stop layer; and neutralizing the charge buildup on the semiconductor device further may include etching partially through the etch stop layer to expose the interconnect segment. Neutralizing the charge buildup on the semiconductor device further may include applying a neutralization wash to the dielectric layer and the etch stop layer, and rinsing the neutralization wash from the dielectric layer and the etch stop layer after charge neutralization. The method neutralizing the charge buildup on the semiconductor device further may include: maintaining a pH of the neutralization wash between pH=8 and pH=12 during applying the neutralization wash to the dielectric layer and the etch stop layer; and maintaining a pH between pH=8 and pH=12 during rinsing the neutralization wash from the dielectric layer and the etch stop layer after charge neutralization. Neutralizing a charge buildup on the semiconductor device further may include: applying a charge neutralization wash having one or more of BF3, CO2, SO32−, Cu+, Ag+, GaCl3, CN−, RS−, and CO at a pH of not less than 8 and not more than 12. Neutralizing a charge buildup on the semiconductor device further may include rinsing with a basic solution having a pH of not less than 8 and not more than 12. Implementations of the described techniques may include hardware, a method or process, or computer software on a computer-accessible medium.
The foregoing outlines features of several embodiments so that those skilled in the art may better understand the aspects of the present disclosure. Those skilled in the art should appreciate that they may readily use the present disclosure as a basis for designing or modifying other processes and structures for carrying out the same purposes and/or achieving the same advantages of the embodiments introduced herein. Those skilled in the art should also realize that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they may make various changes, substitutions, and alterations herein without departing from the spirit and scope of the present disclosure.