A PROCESS FOR PRODUCING SALT BY MEANS OF STRONG BRINE CONCENTRATION AFTER SEA WATER DESALINATION BY USING A TWO-WAY CIRCULATION METHOD AND BROMINE EXTRACTION

Information

  • Patent Application
  • 20170152160
  • Publication Number
    20170152160
  • Date Filed
    January 04, 2015
    9 years ago
  • Date Published
    June 01, 2017
    7 years ago
  • Inventors
    • CAI; Panmin
  • Original Assignees
    • WEIFANG NORTHSEA OASIS SOLAR POWERED TECHNOLOGY CO., LTD.
Abstract
A process produces salt by way of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction. The process includes the following steps: A, preparing fresh water and strong brine from sea water in a high-pressure reverse osmosis unit by using a reverse osmosis method, wherein the concentration of the prepared strong brine is 70000 to 80000 PPM; and B, performing fresh and concentrated separation on the strong brine with the concentration of 70000 to 80000 PPM in a two-way circulation manner by using a concentration difference method till the strong brine is crystallized.
Description
TECHNICAL FIELD

The present invention relates to a process for separating and extracting salt, bromine, potassium chloride and magnesium chloride from sea water, particularly a process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction, and it belongs to the technical field of sea water desalination coupled with industrial salt production.


BACKGROUND TECHNOLOGY

The current salt pan solar evaporation technology method is disadvantaged by large floor space, low production efficiency, high cost and poor quality. However, the sea water desalination engineering implemented in areas in shortage of fresh water will cause pollution due to external discharge of strong brine cannot be utilized after extraction of fresh water since the water preparation cost is high and is unable to adapt to the market price.


CONTENT OF INVENTION

The problem to be solved in the present invention is to provide a process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction which can reduce the current production cost of fresh water, salt and bromine, improve quality and protect environment.


In order to solve the aforesaid problems, the present invention adopts the following technical solution:


A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction, comprising the following steps:


A. Preparing fresh water and strong brine from sea water in a high-pressure reverse osmosis unit by using a reverse osmosis method, wherein the concentration of the prepared strong brine is 70000˜80000 PPM;


B. Performing fresh and concentrated separation on the strong brine with the concentration of 70000˜80000 PPM in a two-way circulation manner by using a concentration difference method till the strong brine is crystallized.


The following is a further optimization of the aforesaid solution:


The aforesaid technology also includes the following step:


C. In the process of performing fresh and concentrated separation on the strong brine, extracting the magnesium chloride, potassium chloride and bromine in strong brine in sequence.


Further optimization:


In the said Step B, the process of performing fresh and concentrated separation in a two-way circulation manner by using a concentration difference method includes the following steps:


a. Setting several 12 m deep brine tanks and numbering them: I-XVII; divide every brine tank into three areas, among which the upper 4 m is low salinity area, the middle 4 m is medium salinity area and the lower 4 m is high salinity area; separating concentration difference of every area is 0.2˜1.5°, and the concentration difference of the same area of neighboring brine tanks is 1˜3°; the several brine tanks are divided into salt areas with the brine concentration of 4-29°;


b. Firstly, inject the strong brine with the concentration of 70000˜80000 ppm in the location 6 m deep in brine tank XV with the concentration of 7° in the medium salinity area;


c. Then, slowly pump the brine at the bottom of every brine tank into the medium salinity area of the upper brine tank with high salt content, and the brine of low concentration at the top of the upper brine tank will overflow to the lower brine tank, forming a two-way circulation;


d. After the crystallization of sodium chloride at around 29°, extracting sodium chloride crystals in the strong brine area at 27˜29°.


Further optimization:


In the aforesaid technology, magnesium chloride is extracted with a physical method and the extraction is performed in the 14˜16° strong brine area; after the crystallization of magnesium chloride at around 15°, magnesium chloride crystals are extracted.


Further optimization:


In the aforesaid technology, potassium chloride is extracted with a physical method and the extraction is performed in the 25˜26° strong brine area; after the crystallization of potassium chloride at around 25°, potassium chloride crystals are extracted.


Further optimization:


In the aforesaid technology, the extraction technology of bromine is performed in brine tanks III and IV, and the steps are as follows:


1) Introduce chlorine into the strong brine to blow bromine out, and the reaction formula is as follows:





MgBr2+Cl2→MgCl2+Br2


2) The bromine is absorbed by alkali liquor and is fixed in the form of sodium bromate, and the reaction formula is as follows:





3Br2+6NaOH→5NaBr+NaBrO3+3H2O


3) Bromine can be obtained from the aqueous solution of sodium bromate through distillation after neutralizing treatment of sulfuric acid.


Further optimization:


The said bromine extraction adopts full-automatic supergravity bromine extraction equipment and a chemical method, and the steps are as follows:


1) Respectively introduce strong brine and chlorine into the water distributor in the shell through the brine and chlorine inlets at the bottom of shell, and then they will enter the motor-driven rotating packed bed loaded with filler, and in the water distributor and rotating packed bed, bromine in strong brine will react with chlorine:


The reaction formula is as follows:





MgBr2+Cl2→MgCl2+Br2


Blow out the bromine generated after reaction through the fan and send it to the alkali liquor tank;


2) The bromine is absorbed by alkali liquor and is fixed in the form of sodium bromate, and the reaction formula is as follows:





3Br2+6NaOH→5NaBr+NaBrO3+3H2O


3) Bromine can be obtained from the aqueous solution of sodium bromate through distillation after neutralizing treatment of sulfuric acid.


The present invention adopts the said solution, and it has the following advantages:


1. Through this invention, salt is produced from the strong brine by means of sea water desalination, solving the problem of contamination caused by discharge of strong brine after sea water desalination, and the yield of salt in unit area is 30˜50 times of the yield of salt in a salt pan producing method, and the cost is far lower than that of salt pan production.


2. The quality of salt depends on purity. It is hard to extract magnesium chloride and potassium chloride with the salt pan producing, while the technical solution adopted in the present invention is convenient for the separation and extraction of magnesium chloride, potassium chloride and bromine, and it can realize effective separation of various inorganic salts, so the quality of salt is of high grade.


3. The bromine extraction by use of supergravity centrifuge at high salinity adopted in the present invention is in the highest level of the industry by virtue of its high efficiency, low cost, automation and safety.


The following figures and embodiments further illustrate the present invention.





DESCRIPTION OF FIGURE


FIG. 1 is the flow diagram of embodiments 1-5 in the present invention;



FIG. 2 is the schematic diagram of bromine extractor in embodiment 5 in the present invention;





Where, 1—Shell; 2—Rotating packed bed; 3—Fan; 4—Motor; 5—Chlorine and brine inlet; 6—Effluent outlet; 7—Alkali liquor tank; 8—Water distributor.


SPECIFIC EMBODIMENTS

Embodiment 1, a process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction, comprising the following steps:


A. Preparing fresh water and strong brine from sea water in a high-pressure reverse osmosis unit by using a reverse osmosis method, wherein the concentration of the prepared strong brine is 70000˜80000 PPM (7˜8°);


B. Performing fresh and concentrated separation on the strong brine with the concentration of 70000˜80000 PPM in a two-way circulation manner by using a concentration difference method till the strong brine is crystallized.


C. In the process of performing fresh and concentrated separation on the strong brine, extracting the magnesium chloride, potassium chloride and bromine in strong brine in sequence.


In the said Step B, the process of performing fresh and concentrated separation in a two-way circulation manner by using a concentration difference method includes the following steps:


a. Setting several 12 m deep brine tanks and numbering them: I-XVII; divide every brine tank into three areas, among which the upper 4 m is low salinity area, the middle 4 m is medium salinity area and the lower 4 m is high salinity area; separating concentration difference of every area is 0.2˜1.5°, and the concentration difference of the same area of neighboring brine tanks is 1˜3°; the several brine tanks are divided into salt areas with the brine concentration of 4-29°;


The capacity of brine tank of every stage is 3˜5 times of the daily brine output Q of anti-penetration equipment (keep the standing time above 70 h).


b. Firstly, inject the strong brine with the concentration of 70000˜80000 ppm in the location 6 m deep in brine tank XV with the concentration of 7° in the medium salinity area;


c. Then, slowly pump the brine at the bottom of every brine tank into the medium salinity area of the upper brine tank with high salt content, and the brine of low concentration at the top of the upper brine tank will overflow to the lower brine tank, forming a two-way circulation.


d. After the crystallization of sodium chloride at around 29°, extracting sodium chloride crystals in the strong brine area at 27˜29°.


Embodiment 2, in the said Embodiment 1, magnesium chloride is extracted with a physical method and the extraction is performed in the 14˜16° strong brine area; after the crystallization of magnesium chloride at around 15°, magnesium chloride crystals are extracted.


Embodiment 3, in the said Embodiment 1, potassium chloride is extracted with a physical method and the extraction is performed in the 25˜26° strong brine area; after the crystallization of potassium chloride at around 25°, potassium chloride crystals are extracted.


Embodiment 4, in the said Embodiment 1, the extraction technology of bromine is performed in the optimal brine tank (III and IV) after the demonstration of several tests, and the steps are as follows:


1) Introduce chlorine into the strong brine to blow bromine out, and the reaction formula is as follows:





MgBr2+Cl2→MgCl2+Br2


2) The bromine is absorbed by alkali liquor and is fixed in the form of sodium bromate, and the reaction formula is as follows:





3Br2+6NaOH→5NaBr+NaBrO3+3H2O


3) Bromine can be obtained from the aqueous solution of sodium bromate through distillation after neutralizing treatment of sulfuric acid.


Embodiment 5, in the said Embodiment 1, the said bromine extraction can adopt full-automatic supergravity bromine extraction equipment and a chemical method, as shown in FIG. 2:


1) Respectively introduce strong brine and chlorine into the water distributor 8 in Shell 1 through the brine and chlorine inlets 5 at the bottom of Shell 1, and then enter the rotating packed bed 2 loaded with filler driven by the motor 4, and in the water distributor 8 and rotating packed bed 2, bromine in strong brine will react with chlorine:


The reaction formula is as follows:





MgBr2+Cl2→MgCl2+Br2


Blow out the bromine generated after reaction through the fan 3 and send it to the alkali liquor tank 7;


2) The bromine is absorbed by alkali liquor and is fixed in the form of sodium bromate, and the reaction formula is as follows:





3Br2+6NaOH→5NaBr+NaBrO3+3H2O


3) Bromine can be obtained from the aqueous solution of sodium bromate through distillation after neutralizing treatment of sulfuric acid.


A comparison between the refined salt produced by use of the said technology and the refined salt produced with other methods, and the comparison results are shown in the table below:


















Refined salt





produced by



Solar industrial salt
Refined industrial salt
use of this














Index
Premium
Grade I
Grade II
Premium
Grade I
Grade II
technology

















Sodium chloride
96.00
94.50
92.00
99.10
98.50
97.50
99.40


(%)≧









Moisture (%)≦
3.00
4.10
6.00
0.30
0.50
0.80
0.20


Water insoluble
0.20
0.30
0.40
0.05
0.10
0.20
0.05


substance (%)≦









Calcium and
0.30
0.40
0.60
0.25
0.40
0.60
0.15


magnesium









ion (%)≦









Sulfate ion (%)≦
0.05
0.70
1.00
0.30
0.50
0.90
0.20









Through the aforesaid comparison, it can be known that the quality grade of salt produced by use of this technology is far higher than that of refined salt produced with other methods.


In the said embodiments, the number of stages of brine tanks depends on the required concentration of the final brine; if it is required to reach the concentration of salt crystallization, 18˜20 stages shall be set (designed by increasing 1° per stage).

Claims
  • 1. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction, comprising the following steps: A. Preparing fresh water and strong brine from sea water in a high-pressure reverse osmosis unit by using a reverse osmosis method, wherein the concentration of the prepared strong brine is 70000˜80000 PPM;B. Performing fresh and concentrated separation on the strong brine with the concentration of 70000˜80000 PPM in a two-way circulation manner by using a concentration difference method till the strong brine is crystallized.
  • 2. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 1, wherein the process also includes the following step: C. In the process of performing fresh and concentrated separation on the strong brine, extracting the magnesium chloride, potassium chloride and bromine in strong brine in sequence.
  • 3. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 2, wherein in the said Step B, performing fresh and concentrated separation in a two-way circulation manner by using a concentration difference method includes the following steps: a. Setting several 12 m deep brine tanks and numbering them: I-XVII; divide every brine tank into three areas, among which the upper 4 m is low salinity area, the middle 4 m is medium salinity area and the lower 4 m is high salinity area; separating concentration difference of every area is 0.2˜1.5°, and the concentration difference of the same area of neighboring brine tanks is 1˜3°; the several brine tanks are divided into salt areas with the brine concentration of 4˜29°;b. Firstly, inject the strong brine with the concentration of 70000˜80000 ppm in the location 6 m deep in brine tank XV with the concentration of 7° in the medium salinity area;c. Then, slowly pump the brine at the bottom of every brine tank into the medium salinity area of the upper brine tank with high salt content, and the brine of low concentration at the top of the upper brine tank will overflow to the lower brine tank, forming a two-way circulation;d. After the crystallization of sodium chloride at around 29°, extracting sodium chloride crystals in the strong brine area at 27˜29°.
  • 4. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 3, wherein in the aforesaid process, magnesium chloride is extracted with a physical method and the extraction is performed in the 14˜16° strong brine area; after the crystallization of magnesium chloride at around 15°, magnesium chloride crystals are extracted.
  • 5. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 3, wherein in the aforesaid process, potassium chloride is extracted with a physical method and the extraction is performed in the 25˜26° strong brine area; after the crystallization of potassium chloride at around 25°, potassium chloride crystals are extracted.
  • 6. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 3, wherein in the aforesaid process, the extraction technology of bromine is performed in brine tanks III and IV, and the steps are as follows: 1) Introduce chlorine into the strong brine to blow bromine out, and the reaction formula is as follows: MgBr2+Cl2→MgCl2+Br2 2) The bromine is absorbed by alkali liquor and is fixed in the form of sodium bromate, and the reaction formula is as follows: 3Br2+6NaOH→5NaBr+NaBrO3+3H2O3) Bromine can be obtained from the aqueous solution of sodium bromate through distillation after neutralizing treatment of sulfuric acid.
  • 7. A process for producing salt by means of strong brine concentration after sea water desalination by using a two-way circulation method and bromine extraction according to claim 6, wherein the said bromine extraction adopts full-automatic supergravity bromine extraction equipment and a chemical method, and the steps are as follows: 1) Respectively introduce strong brine and chlorine into the water distributor in Shell through the brine and chlorine inlets at the bottom of Shell, and then enter the rotating packed bed loaded with filler driven by the motor, and in the water distributor and rotating packed bed, bromine in strong brine will react with chlorine:
Priority Claims (1)
Number Date Country Kind
201410248591.4 Jun 2014 CN national
PCT Information
Filing Document Filing Date Country Kind
PCT/CN2015/000002 1/4/2015 WO 00