Claims
- 1. An absorbent article comprising:
a topsheet; a backsheet; an intermediate layer between the topsheet and the backsheet; wherein at least one of the topsheet, backsheet, and intermediate layer comprises a three-dimensional vacuum formed film with a male side void volume of at least 350 cc/m2; and the absorbent article having a first minute decrease in temperature of at least 8° F. on a Third Insult Test.
- 2. The absorbent article of claim 1 wherein the topsheet comprises the three-dimensional vacuum formed film.
- 3. The absorbent article of claim 1 wherein the backsheet comprises the three-dimensional vacuum formed film.
- 4. The absorbent article of claim 1 wherein the intermediate layer comprises the three-dimensional vacuum formed film and said intermediate layer is adjacent an absorbent core.
- 5. The absorbent article of claim 1 wherein the male side void volume of the at least one three-dimensional formed film is greater than 450 cc/m2.
- 6. The absorbent article of claim 1 wherein the first minute decrease in temperature is at least 9° F.
- 7. The absorbent article of claim 3 wherein the three-dimensional film is fluid impervious.
- 8. The absorbent article of claim 4 wherein the three-dimensional film is between the absorbent core and the topsheet.
- 9. The absorbent article of claim 1 wherein the intermediate layer comprises a three-dimensional formed film, an absorbent core, and a separation layer between the absorbent core and said three-dimensional formed film to maintain the male side void volume.
- 10. The absorbent article of claim 2 wherein the intermediate layer comprises an absorbent core and a separation layer, the separation layer being between the topsheet and the absorbent core to maintain the male side void volume.
- 11. The absorbent article of claim 3 wherein the intermediate layer comprises an absorbent core and a separation layer, the separation layer being between the backsheet and the absorbent core to maintain the male side void volume.
- 12. An absorbent article comprising:
an absorbent core with a body facing side and an opposite clothing facing side; and a three-dimensional formed film having a male side void volume of at least 350 cc/m2; wherein the absorbent article has a first minute decrease in temperature of at least 8° F. on a Third Insult Test with the three-dimensional formed film on either the body facing side or the clothing facing side of the absorbent core.
- 13. The absorbent article of claim 12 wherein the three dimensional film has a male side void volume of at least 450 cc/m2.
- 14. The absorbent article of claim 12 wherein the first minute decrease in temperature is at least 9° F.
- 15. The absorbent article of claim 12 further comprising a separation layer between the absorbent core and the three-dimensional formed film to maintain the male side void volume.
- 16. The absorbent article of claim 15 wherein the three-dimensional formed film is on the body facing side of the absorbent core.
- 17. The absorbent article of claim 15 wherein the three-dimensional formed film is on the clothing facing side of the absorbent article.
Parent Case Info
[0001] This application is a continuation-in-part of U.S. patent application Ser. No. 09/668,649 filed on Sep. 22, 2000, which is hereby incorporated by reference as if reproduced herein.
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
09668649 |
Sep 2000 |
US |
Child |
10422703 |
Apr 2003 |
US |