Claims
- 1. A method for manufacturing an adsorbent, supple, filter fabric, comprising the steps of:
- a) mixing at room temperature 70 to 95% by weight adsorbent particles having an average particle size of 100 to 5,000 .mu.m with 5 to 30% by weight binding-agent particles having an average particle size of 90 to 5% that of the adsorbent particles, wherein the binding-agent particles melt over a temperature range that is lower than the lowest temperature at which the adsorbent particles begin to melt, and the binding agent does not spread on the adsorbent surface below 100.degree. C., and with 15 to 70% by weight water, relative to the total mixture of adsorbent, binding agent and water;
- b) sprinkling the mixture as loose pour on a textile carrier material which withstands temperatures of at least 180.degree. C. free of destruction;
- c) heating the mixture on the carrier material in an open device for 20 to 120 seconds to at least 100.degree. C. and at least 5.degree. C. above the lower end of the temperature range over which the binding melts, however below the lower end of the temperature range over which the adsorbent melts, accompanied by simultaneous escape of the water vapor from the mixture to form a supple filter fabric;
- d) cooling off and rolling up of the resultant supple filter fabric.
- 2. The method according to claim 1, wherein before the step of heating, a textile covering material having at least the same heat resistance as that of the carrier material is placed on the mixture such that the mixture is sandwiched between the textile carrier material and the textile covering material.
- 3. The method according to claim 1, wherein the adsorbent particles are activated-carbon.
- 4. The method according to claim 2, wherein the adsorbent particles are activated-carbon.
- 5. The method according to claim 1, further comprising the step of adding a first substance that promotes sorbtion by the adsorbant particles, which is dispersible or soluble in water, to the water before the mixing step.
- 6. The method according to claim 2, further comprising the step of adding a first substance that promotes sorbtion by the adsorbant particles, which is dispersible or soluble in water, to the water before the mixing step.
- 7. The method according to claim 3, further comprising the step of adding a first substance that promotes sorbtion by the adsorbant particles, which is dispersible or soluble in water, to the water before the mixing step.
- 8. The method according to claim 5, further comprising the step of bonding together a first filter fabric and a second filter fabric after their manufacture, wherein the first filter fabric contains a first substance that promotes sorbtion by the adsorbant particles, and the second filter fabric contains a second substance, different from the first substance, that promotes sorbtion by the adsorbant particles.
- 9. The method according to claim 1, wherein the loose pour includes a first layer sprinkled on the textile carrier material and a second layer sprinkled on the first layer, and the first layer contains a first substance that promotes sorbtion by the adsorbant particles, and the second layer contains a second substance, different from the first substance, that promotes sorbtion by the adsorbant particles.
- 10. The method according to claim 2, wherein the loose pour includes a first layer sprinkled on the textile carrier material and a second layer sprinkled on the first layer, and the first layer contains a first substance that promotes sorbtion by the adsorbant particles, and the second layer contains a second substance, different from the first substance, that promotes sorbtion by the adsorbant particles.
- 11. The method according to claim 3, wherein the loose pour includes a first layer sprinkled on the textile carrier material and a second layer sprinkled on the first layer, and the first layer contains a first substance that promotes sorbtion by the adsorbant particles, and the second layer contains a second substance, different from the first substance, that promotes sorbtion by the adsorbant particles.
- 12. The method according to claim 1, wherein the step of mixing is conducted for at least about 5 min.
Priority Claims (1)
Number |
Date |
Country |
Kind |
195 14 887 |
Apr 1995 |
DEX |
|
Parent Case Info
This application is a division of Ser. No. 08/615,009, filed Mar. 12, 1996, now abandoned.
US Referenced Citations (10)
Divisions (1)
|
Number |
Date |
Country |
Parent |
615009 |
Mar 1996 |
|