Claims
- 1. An amine-modified homogeneous wax comprising 60-100% by weight of an unoxidized olefininc wax having a number average molecular weight of from 800 to 6,000 and a weight average molecular weight to number average molecular weight ratio of at least 1.05:1, being at least partially grafted with a tertiary amine unit-containing vinyl monomer selected from the group consisting of vinylpyridine, vinylpiperidine or a compound having the formula: ##STR2## wherein R.sub.1 is a hydrogen atom or a lower alkyl group, R.sub.2 is a lower alkylene group, R.sub.3 and R.sub.4 each is a lower alkyl group or an aryl group, and X is a linking group to the unsaturated carbon atom; in the presence of a radical initiator which does not generate a carboxyl radical, and which is used in an amount of from 0.1 to 1.2 moles per mole of the vinyl monomer; and 0 to 40% by weight of a polymer of the tertiary amine unit-containing vinyl monomer, wherein the total amount of the tertiary amine unit-containing vinyl monomer in the composition is about 0.3 to 40% by weight.
- 2. An amine-modified homogeneous wax according to claim 1, comprising 70 to 100% by weight of the wax, at least partially grafted with tertiary amine unit-containing vinyl monomer, and 30 to 0% by weight of the polymer of tertiary amine unit-containing vinyl monomer, the total amount of the tertiary amine unit-containing vinyl monomer in the composition being 0.3 to 30% by weight.
- 3. An amine-modified homogeneous wax according to claim 1, wherein said unoxidized olefinic wax is a polyethylene wax.
- 4. An amine-modified homogeneous wax according to claim 3, wherein said polyethylene wax has a number average molecular weight of from 900 to 5,000.
- 5. An amine-modified homogeneous wax according to claim 1, wherein said weight-average molecular weight to number-average molecular weight ratio is at least 1.15:1.
- 6. An amine-modified homogeneous wax according to claim 1, wherein said radical initiator has a decomposition temperature of from 60.degree. C. to 100.degree. C., whereby the decomposition percentage of radical initiator reaches 50% when 0.1 mole of the radical initiator is added to one liter of benzene and the mixture is allowed to stand at a given temperature for 10 hours.
- 7. An amine-modified homogeneous wax according to claim 6, wherein said radical initiator is an organic peroxide or an azo compound having a decomposition temperature of from 60.degree. C. to 100.degree. C.
- 8. An amine-modified homogeneous wax according to claim 6, wherein said radical initiator is an azo compound.
- 9. An amine-modified homogeneous wax according to claim 1, wherein said radical initiator is used in an amount of from 0.15 mole to 0.9 moles per mole of the vinyl monomer.
- 10. An amine-modified homogeneous wax according to claim 1, wherein said linking group is a direct bond or an amide group.
- 11. An amine-modified homogeneous wax comprising 60 to 100% by weight of an unoxidized olefinic wax having a number average molecular weight of from 800-6,000 and a weight average molecular weight to number average molecular weight ratio of at least 1.05:1, and wherein the total amount of the tertiary amine unit-containing vinyl monomer in the composition is about 0.3 to 40% by weight, and which is prepared by a process consisting essentially of radically grafting to said polyethylene wax a tertiary amine unit-containing vinyl monomer selected from the group consisting of vinylpyridine, vinylpiperidine or a compound having the formula: ##STR3## wherein R.sub.1 is a hydrogen atom or a lower alkyl group, R.sub.2 is a lower alkylene group, R.sub.3 and R.sub.4 each is a lower alkyl group or an aryl group, and X is a linking group to the unsaturated carbon atom; in the presence of a radical initiator which does not generate a carboxyl radical, and which is used in an amount of from 0.1 to 1.2 moles per mole of the vinyl monomer.
- 12. An amine-modified homogeneous wax according to claim 11, wherein during said radical grafting, said vinyl monomer is fed at a rate of 2.times.10.sup.-3 to 5.times.10.sup.2 moles/hr per kg of said wax and the radical initiator is fed at a rate of 2.times.10.sup.-4 to 5.times.10.sup.2 moles/hr per kg of said wax.
- 13. An amine-modified homogeneous wax according to claim 11, wherein said radical grafting reaction is conducted in a non-aqueous system.
- 14. An amine-modified homogeneous wax according to claim 11, which further contains up to 40% by weight of a polymer of the tertiary amine unit-containing vinyl monomer.
- 15. An amine-modified homogeneous wax according to claim 11, wherein said radical initiator has a decomposition temperature in the range of 60.degree.-120.degree. C.
Priority Claims (1)
Number |
Date |
Country |
Kind |
59-60142 |
Mar 1984 |
JPX |
|
CROSS REFERENCE TO THE RELATED APPLICATION
This application is continuation-in-part application of Ser. No. 712,654, filed Mar. 18, 1985 entitled "Amine-modified wax", now pending.
US Referenced Citations (4)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
712654 |
Mar 1985 |
|