The present application claims priority to Korean Patent Application No. 10-2020-0030940 filed on Mar. 12, 2020 in the Republic of Korea, the disclosures of which are incorporated herein by reference.
The present disclosure relates to an apparatus for inspecting swelling of a battery cell, and more particularly, to an apparatus for inspecting swelling of a battery cell, which may inspect swelling of a battery cell based on pressure distribution of the battery cell.
Recently, the demand for portable electronic products such as notebook computers, video cameras and portable telephones has increased sharply, and electric vehicles, energy storage batteries, robots, satellites and the like have been developed in earnest. Accordingly, high-performance batteries allowing repeated charging and discharging are being actively studied.
Batteries commercially available at present include nickel-cadmium batteries, nickel hydrogen batteries, nickel-zinc batteries, lithium batteries and the like. Among them, the lithium batteries are in the limelight since they have almost no memory effect compared to nickel-based batteries and also have very low self-charging rate and high energy density.
Such a battery may cause swelling in which gas is generated in the battery during charging and discharging or in a high temperature state to inflate the battery. Since there is a risk of fire or explosion due to battery swelling, it is important to accurately inspect the swelling behavior of the battery.
Conventionally, an evaluation system and a fixing jig for evaluating the state change of a battery caused by charging and discharging have been disclosed (Patent Document 1). Specifically, Patent Document 1 discloses a configuration in which a battery is fixed using the fixing jig and elastic deformation of a spring provided in the fixing jig is detected through a strain gauge based on the change in volume of the battery.
However, since the elastic deformation of the spring detected in Patent Document 1 is affected only by the change in volume of the battery, if the change in volume of the battery is too small, the elastic deformation of the spring may not reach a measurable range of the deformation rate of the strain gauge. That is, since Patent Document 1 does not measure the deformation rate by amplifying the elastic deformation of the spring, there is a problem in that the detection accuracy itself may be lowered by the volume change of the battery.
In addition, since Patent Document 1 uses a spring, if the change in volume of the battery is too large so that the deformation force of the spring exceeds an elastic limit, there is a problem in that the evaluation system and the fixing jig of Patent Document 1 cannot evaluate the condition of the battery any longer.
The present disclosure is designed to solve the problems of the related art, and therefore the present disclosure is directed to providing an apparatus for inspecting swelling of a battery cell, which may inspect swelling of a battery cell even based on a small force applied by the swelling of the battery cell by amplifying and measuring the force applied by the swelling of the battery cell.
These and other objects and advantages of the present disclosure may be understood from the following detailed description and will become more fully apparent from the exemplary embodiments of the present disclosure. Also, it will be easily understood that the objects and advantages of the present disclosure may be realized by the means shown in the appended claims and combinations thereof.
In one aspect of the present disclosure, there is provided an apparatus for inspecting swelling of a battery cell, comprising: a first plate configured in a plate shape; a second plate configured in a plate shape and located to face the first plate to be spaced therefrom by a predetermined interval, the second plate being configured so that the battery cell is interposed between the first plate and the second plate; a fixing frame configured so that a portion of the first plate is fixedly coupled thereto; a connection frame having one end fixedly coupled to the second plate and the other end fixedly coupled to the fixing frame; and a pressure measuring element attached to the connection frame and configured to measure a deformation rate of the connection frame.
The connection frame may be configured such that at least a portion thereof is bent.
The connection frame may include: a horizontal portion having one end connected to the fixing frame and configured to be elongated in one direction; and a vertical portion provided at a distal end of the horizontal portion and configured to have a distal end toward the second plate.
The connection frame may be configured such that the distal end of the vertical portion is fixedly coupled to an outer side surface of the second plate.
The connection frame may be configured such that the distal end of the vertical portion is fixedly coupled to a center portion of the outer side surface of the second plate.
The fixing frame may be configured so that the interval between the first plate and the second plate is adjusted.
An apparatus for inspecting swelling of a battery cell according to another aspect of the present disclosure may further comprise a pressure measuring unit connected to the pressure measuring element and configured to receive the deformation rate of the connection frame measured by the pressure measuring element and measure a pressure value of the battery cell based on the received deformation rate of the connection frame when the battery cell is interposed between the first plate and the second plate.
The pressure measuring element may be configured to measure the deformation rate of the connection frame based on a force applied to the vertical portion by the pressure of the battery cell and a length of the horizontal portion in the one direction.
An apparatus for inspecting swelling of a battery cell according to still another aspect of the present disclosure may further comprise a control unit connected to the pressure measuring unit and configured to receive the pressure value of the battery cell from the pressure measuring unit, compare the received pressure value of the battery cell with a reference pressure value and determine at least one of the presence of swelling and a swelling degree of the battery cell according to the pressure value comparison result.
The connection frame may include a plurality of unit connection frames so that the plurality of unit connection frames are coupled to the second plate at a predetermined interval.
The pressure measuring element may be provided in plural and configured to be attached to each of the plurality of unit connection frames.
The pressure measuring unit may be configured to measure a pressure value of each section of the battery cell, based on a deformation rate of each of the plurality of unit connection frames measured by each of the plurality of pressure measuring elements.
The control unit may be configured to determine at least one of a swelling distribution of the battery cell and a swelling degree of each section, based on the pressure value of each section of the battery cell measured by the pressure measuring unit.
The pressure measuring unit may be configured to calculate a pressure value of each section of the battery cell from the deformation rate of each of the plurality of unit connection frames, in consideration of a length of the horizontal portion of the plurality of unit connection frames.
The second plate may be configured to include a plurality of second unit plates.
The plurality of unit connection frames may be configured to be coupled to a corresponding second unit plate among the plurality of second unit plates.
The plurality of unit connection frames may be configured to be coupled to a center portion of an outer side surface of the corresponding second unit plate.
An apparatus for inspecting swelling of a battery cell according to still another aspect of the present disclosure may further comprise a temperature measuring unit configured to measure a temperature of each of the plurality of second unit plates by using a temperature measuring element attached to each of the plurality of second unit plates.
The control unit may be configured to receive the temperature value of each of the plurality of second unit plates from the temperature measuring unit and further determine a temperature of each section of the battery cell.
According to one aspect of the present disclosure, the magnitude of the force applied by the swelling of the battery cell may be amplified as much as the length of the horizontal portion of the connection frame. Therefore, even if a small force is applied by swelling, there is an advantage of precisely determining the presence of swelling of the battery cell.
The effects of the present disclosure are not limited to the effects mentioned above, and other effects not mentioned will be clearly understood by those skilled in the art from the description of the claims.
The accompanying drawings illustrate a preferred embodiment of the present disclosure and together with the foregoing disclosure, serve to provide further understanding of the technical features of the present disclosure, and thus, the present disclosure is not construed as being limited to the drawing.
It should be understood that the terms used in the specification and the appended claims should not be construed as limited to general and dictionary meanings, but interpreted based on the meanings and concepts corresponding to technical aspects of the present disclosure on the basis of the principle that the inventor is allowed to define terms appropriately for the best explanation.
Therefore, the description proposed herein is just a preferable example for the purpose of illustrations only, not intended to limit the scope of the disclosure, so it should be understood that other equivalents and modifications could be made thereto without departing from the scope of the disclosure.
Additionally, in describing the present disclosure, when it is deemed that a detailed description of relevant known elements or functions renders the key subject matter of the present disclosure ambiguous, the detailed description is omitted herein.
The terms including the ordinal number such as “first”, “second” and the like, may be used to distinguish one element from another among various elements, but not intended to limit the elements by the terms.
Throughout the specification, when a portion is referred to as “comprising” or “including” any element, it means that the portion may include other elements further, without excluding other elements, unless specifically stated otherwise.
Furthermore, the term “control unit” described in the specification refers to a unit that processes at least one function or operation, and may be implemented by hardware, software, or a combination of hardware and software.
In addition, throughout the specification, when a portion is referred to as being “connected” to another portion, it is not limited to the case that they are “directly connected”, but it also includes the case where they are “indirectly connected” with another element being interposed between them.
Hereinafter, preferred embodiments of the present disclosure will be described in detail with reference to the accompanying drawings.
The apparatus 100 for inspecting swelling of a battery cell according to an embodiment of the present disclosure is a device for inspecting swelling of a battery cell 10, and may inspect the presence of swelling and/or a swelling degree.
Here, the battery cell 10 refers to one independent cell that has a negative electrode terminal and a positive electrode terminal and is physically separable. For example, one pouch-type lithium polymer cell may be regarded as the battery cell 10.
Referring to
The first plate 110 may be configured in a plate shape.
Specifically, the first plate 110 may be configured in a plate shape so that the battery cell 10 may be seated thereon. In addition, the first plate 110 may be configured to have a wider horizontal area than the battery cell 10 so that a lower surface of the battery cell 10 may be seated thereon.
For example, the first plate 110 may be a lower plate on which the battery cell 10 may be placed.
The second plate 120 may be configured in a plate shape.
Specifically, the second plate 120 may be seated or attached to an upper surface of the battery cell 10.
For example, in the embodiment of
In addition, in order to increase the placing stability or the attachment stability of the second plate 120 on the upper surface of the battery cell 10, the horizontal area of the second plate 120 may be equal to or smaller than the horizontal area of the battery cell 10.
For example, in the embodiment of
That is, one surface of the first plate 110 and one surface of the second plate 120 may face each other. Preferably, one surface of the first plate 110 and one surface of the second plate 120 may be parallel to each other.
In addition, the second plate 120 may be configured such that the battery cell 10 is interposed between the second plate 110 and the first plate 110.
For example, in the embodiment of
The fixing frame 130 may be configured such that a portion of the first plate 110 is fixedly coupled thereto.
Specifically, the first plate 110 may be fixedly coupled to the fixing frame 130, but the second plate 120 may not be fixedly coupled to the fixing frame 130.
Preferably, the first plate 110 may be coupled to the fixing frame 130 at a right angle. In addition, the first plate 110 may be fixed by the fixing frame 130 so as not to shake or rotate. Hereinafter, “fixed” or “fixed coupling” refers to a coupled state in which the coupled state is maintained with shaking or rotating.
In the embodiment of
The connection frame 140 may be configured such that one end is fixedly coupled to the second plate 120 and the other end is fixedly coupled to the fixing frame 130.
For example, in the embodiment of
The pressure measuring element 150 may be configured to be attached to the connection frame 140.
For example, in the embodiment of
In addition, the pressure measuring element 150 may be configured to measure a deformation rate of the connection frame 140. To this end, the connection frame 140 may be made of a metal that elastically moves when a force is applied thereto.
For example, a strain gauge for measuring the deformation of the connection frame 140 may be applied to the pressure measuring element 150.
As in the embodiment of
The connection frame 140 may be configured such that at least a portion thereof is bent.
Here, the “bent form” may mean a shape that the connection frame 140 is bent. For example, the connection frame 140 may be bent at an angle of greater than 0 degrees and less than or equal to 90 degrees in a form elongated in one direction.
For example, in the embodiments of
The connection frame 140 will be described in more detail with reference to
The connection frame 140 may include a horizontal portion 140a and a vertical portion 140b.
For example, in the embodiment of
The horizontal portion 140a may be configured such that one end thereof is connected to the fixing frame 130 and elongated in one direction.
Here, “horizontal” may mean a direction parallel to the first plate 110. That is, the horizontal portion 140a of the connection frame 140 may be parallel to the first plate 110. Also, the horizontal portion 140a of the connection frame 140 may also be parallel to the second plate 120.
For example, in the embodiment of
The vertical portion 140b may be configured to be provided at a distal end of the horizontal portion 140a.
Here, “vertical” may mean a direction perpendicular to the first plate 110. That is, the vertical portion 140b of the connection frame 140 may be perpendicular to the first plate 110.
Specifically, the vertical portion 140b may be provided at the distal end of the horizontal portion 140a and configured to be elongated in a direction perpendicular to the longitudinal direction of the vertical portion 140b. For example, in the embodiment of
Both the vertical portion 140b and the horizontal portion 140a may include one end and the other end. For example, in the embodiment of
The other end of the horizontal portion 140a may be coupled to the fixing frame 130, and the other end of the vertical portion 140b may be provided at one end of the horizontal portion 140a. In addition, the vertical portion 140b may be configured such that the distal end thereof faces the second plate 120. That is, one end of the vertical portion 140b may be configured to face the second plate 120.
Here, the longitudinal direction (−y direction) of the horizontal portion 140a and the longitudinal direction (−z direction) of the vertical portion 140b may be perpendicular to each other.
Referring to
The connection frame 140 may be configured such that the distal end of the vertical portion 140b is fixedly coupled to the outer side surface of the second plate 120.
Specifically, in the embodiment of
For example, referring to the structure of the connection frame 140 shown in
Accordingly, the second plate 120 is fixedly coupled to the connection frame 140 and thus may not be shaken or rotated. In addition, if the battery cell 10 is interposed between the first plate 110 and the second plate 120, the force applied to the second plate 120 due to the swelling of the battery cell 10 may be transferred to the connection frame 140.
If the second plate 120 and the vertical portion 140b of the connection frame 140 are not perpendicular to each other and are coupled to be inclined by a predetermined angle θ relative to the z direction, the force applied to the second plate 120 by the swelling of the battery cell 10 may be reduced in proportion to Cos θ and transferred to the vertical portion 140b of the connection frame 140. In addition, the pressure measuring element 150 may measure the deformation rate of the connection frame 140 based on the force applied to the connection frame 140. Therefore, if the second plate 120 and the vertical portion 140b of the connection frame 140 are fixedly coupled as being inclined by the predetermined angle θ based on the z direction, since the force transferred to the connection frame 140 is reduced, the error of the deformation rate of the connection frame 140 measured by the pressure measuring element 150 may increase. Accordingly, preferably, the second plate 120 and the vertical portion 140b of the connection frame 140 may be fixedly coupled to be perpendicular to each other.
Referring to
Preferably, the connection frame 140 may be configured such that the distal end of the vertical portion 140b is fixedly coupled to a center portion of the outer side surface of the second plate 120.
In general, the swelling of the battery cell 10 may occur not only in the center portion of the battery cell 10 but also in a peripheral portion thereof. Here, the peripheral portion refers to a region excluding the center portion. That is, the force applied to each part of the second plate 120 may be different depending on the location where the swelling occurs in the battery cell 10.
For example, if swelling occurs in the center portion of the battery cell 10, the greatest force may be applied to the center portion of the second plate 120. In addition, the force applied to the second plate 120 by the swelling may be evenly distributed to the peripheral portion of the second plate 120.
Meanwhile, if swelling occurs in a peripheral portion of the battery cell 10, the greatest force may be applied to a region corresponding to the peripheral portion of the battery cell 10 among the peripheral portions of the second plate 120.
That is, if the vertical portion 140b of the connection frame 140 is coupled to the peripheral portion of the outer side surface of the second plate 120, the deformation rate of the connection frame 140 measured by the pressure measuring element 150 may be inaccurate according to the location where the swelling occurs in the battery cell 10.
For example, in the embodiment of
As another example, in the embodiment of
That is, since the pressure measuring element 150 may measure the deformation rate of the connection frame 140 based on the force F applied to the connection frame 140, as the deviation of the force F applied to the connection frame 140 is greater, the deformation rate of the connection frame 140 measured by the pressure measuring element 150 may have a larger error.
Therefore, since the apparatus 100 for inspecting swelling of a battery cell according to an embodiment of the present disclosure is configured such that the connection frame 140 is fixedly coupled to the center portion of the outer side surface of the second plate 120, it is possible to minimize the error of the measured deformation rate of the connection frame 140 caused by the position where swelling occurs in the battery cell 10.
The fixing frame 130 may be configured to adjust the interval between the first plate 110 and the second plate 120.
Specifically, the fixing frame 130 may be configured to adjust a location where the connection frame 140 and/or the first plate 110 is coupled. Preferably, the location in the fixing frame 130 at which the connection frame 140 and/or the first plate 110 are fixedly coupled may be adjusted so that the battery cell 10 may be fixed between the first plate 110 and the second plate 120. Accordingly, the interval between the first plate 110 and the second plate 120 may be adjusted.
For example, in the embodiment of
If the interval between first plate 110 and the second plate 120 is not adjustable, there is a problem that the type of the battery cell 10 to be inspected is limited.
Therefore, since the apparatus 100 for inspecting swelling of a battery cell according to an embodiment of the present disclosure includes the fixing frame 130 configured to adjust the interval between the first plate 110 and the second plate 120, there is an advantage in that swelling of battery cells 10 having various thicknesses (for example, z direction length of the battery cell 10 in
Hereinafter, a configuration in which the pressure of the battery cell 10 (the pressure generated due to the swelling of the battery cell 10) is measured by a pressure measuring unit 160 and a pressure measuring element 150 will be described.
Referring to
The pressure measuring unit 160 may be connected to the pressure measuring element 150 and configured to receive the deformation rate of the connection frame 140 measured by the pressure measuring element 150.
For example, the pressure measuring unit 160 may be connected to the pressure measuring element 150 through a wired line. In addition, the pressure measuring unit 160 may be configured to receive data on the deformation rate of the connection frame 140 measured by the pressure measuring element 150 through the wired line.
Specifically, the pressure measuring element 150 may be configured to measure the deformation rate of the connection frame 140 based on the force applied to the vertical portion 140b due to the pressure of the battery cell 10 and the length of the horizontal portion 140a in the one direction.
Here, the force applied to the vertical portion 140b of the connection frame 140 may be a force applied from the battery cell 10 to the vertical portion 140b of the connection frame 140 due to the swelling of the battery cell 10. More specifically, the force applied to the vertical portion 140b of the connection frame 140 may be a force applied to the portion where the second plate 120 and the vertical portion 140b of the connection frame 140 are coupled, among the forces applied to the second plate 120 due to the swelling of the battery cell 10.
In the embodiment of
For example, if the force F is applied to the connection frame 140, the horizontal portion 140a of the connection frame 140 may be slightly bent. At this time, the pressure measuring element 150 may calculate the degree to which the horizontal portion 140a is slightly bent, as the deformation rate of the connection frame 140.
That is, the pressure measuring element 150 may measure the deformation rate of the connection frame 140 based on the moment M applied to the connection frame 140 due to the swelling of the battery cell 10.
For example, unlike the embodiment of
Meanwhile, in the embodiment of
In addition, the pressure measuring unit 160 may be configured to measure a pressure value of the battery cell 10 based on the received deformation rate of the connection frame 140, if the battery cell 10 is interposed between the first plate 110 and the second plate 120.
Specifically, the pressure measuring unit 160 may replace the deformation rate of the connection frame 140 received from the pressure measuring element 150 with the pressure value of the battery cell 10 in consideration of the length L of the horizontal portion 140a of the connection frame 140.
Therefore, by using the connection frame 140 having a bent form to include the horizontal portion 140a and the vertical portion 140b, even if the force F applied due to the swelling of the battery cell 10 is less than a predetermined size, the apparatus 100 for inspecting swelling of a battery cell according to an embodiment of the present disclosure may measure the pressure value according to the swelling of the battery cell 10. That is, the apparatus 100 for inspecting swelling of a battery cell may measure the pressure value of the battery cell 10 precisely by greatly expanding the range in which the swelling of the battery cell 10 can be measured by using the connection frame 140.
Referring to
Here, the control unit 170 may selectively include processors known in the art, application-specific integrated circuit (ASIC), other chipsets, logic circuits, registers, communication modems, data processing devices, and the like to execute various control logic performed in the present disclosure. Also, when the control logic is implemented in software, the control unit 170 may be implemented as a set of program modules. At this time, the program module may be stored in a memory and executed by the control unit 170. The memory may be located inside or out of the control unit 170 and may be connected to the control unit 170 by various well-known means.
The control unit 170 may be connected to the pressure measuring unit 160 and configured to receive the pressure value of the battery cell 10 from the pressure measuring unit 160.
For example, the control unit 170 and the pressure measuring unit 160 may be communicatively connected by wire or wirelessly. In addition, the control unit 170 may receive the pressure value of the battery cell 10 measured by the pressure measuring unit 160.
In addition, the control unit 170 may be configured to compare the received pressure value of the battery cell 10 with a reference pressure value and to determine at least one of the presence of swelling and a swelling degree of the battery cell 10 according to the pressure value comparison result.
Here, the reference pressure value may be a reference value for determining whether swelling occurs in the battery cell 10. The reference pressure value may be stored in an internal memory of the control unit 170 or an external memory.
The control unit 170 may determine the presence of swelling of the battery cell 10 by comparing the pressure value of the battery cell 10 received from the pressure measuring unit 160 with the reference pressure value.
For example, if the pressure value of the battery cell 10 is less than the reference pressure value, the control unit 170 may determine that the swelling of the battery cell 10 does not occur. Conversely, if the pressure value of the battery cell 10 is equal to or greater than the reference pressure value, the control unit 170 may determine that the swelling of the battery cell 10 occurs.
In addition, the control unit 170 may determine the swelling degree of the battery cell 10 through the difference between the pressure value of the battery cell 10 received from the pressure measuring unit 160 and the reference pressure value.
For example, the control unit 170 may determine the swelling degree of the battery cell 10 as any one of normal, warning and dangerous, based on the difference between the pressure value of the battery cell 10 and the reference pressure value.
More specifically, the control unit 170 may calculate a pressure difference value according to the difference between the pressure value of the battery cell 10 and the reference pressure value. In addition, the control unit 170 may determine the swelling degree of the battery cell 10 according to a section to which the calculated pressure difference value belongs among a plurality of preset pressure sections.
Here, the plurality of pressure sections may be set as a normal section, a warning section and a dangerous section in advance. The plurality of pressure sections may be stored in an internal memory of the control unit 170 or an external memory.
In addition, the control unit 170 may determine the swelling degree of the battery cell 10 so that the calculated pressure difference value corresponds to a section to which it belongs, among the plurality of pressure sections.
Referring to
For example, in the embodiment of
In addition, the connection frame 140 may be configured such that the plurality of unit connection frames 140 are coupled to the second plate 120 at a predetermined interval.
Preferably, the plurality of unit connection frames 140 may be coupled to the second plate 120 at a predetermined interval based on a midpoint of the outer side surface of the second plate 120.
For example, in the embodiment of
Preferably, the interval between the −y-directional edge of the upper surface of the second plate 120 and the third unit connection frame 143, the interval between the third unit connection frame 143 and the second unit connection frame 142, the interval between the second unit connection frame 142 and the first unit connection frame 141, and the interval between the +y-directional edge of the upper surface of the second plate 120 and the first unit connection frame 141 may be the same.
In addition, the pressure measuring element 150 is provided in plural and may be configured to be attached to each of the plurality of unit connection frames 140.
For example, in the embodiment of
The plurality of pressure measuring elements 150 may measure a deformation rate of each of the plurality of unit connection frames 140. Therefore, if swelling occurs in the battery cell 10, the deformation rate of the first unit connection frame 141, the deformation rate of the second unit connection frame 142, and the deformation rate of the third unit connection frame 143 may be measured, respectively.
The pressure measuring unit 160 may be configured to measure a pressure value of each section of the battery cell 10, based on the deformation rate of each of the plurality of unit connection frames 140 measured by each of the plurality of pressure measuring elements 150.
Specifically, the plurality of pressure measuring elements 150 may be connected to the pressure measuring unit 160. The pressure measuring unit 160 may receive the deformation rate of each of the plurality of unit connection frames 140 from the plurality of pressure measuring elements 150.
In addition, the pressure measuring unit 160 may be configured to calculate the pressure value of each section of the battery cell 10 from the deformation rate of each of the plurality of unit connection frames 140 in consideration of the length of the horizontal portion 140a of the plurality of unit connection frames 140.
Specifically, the pressure measuring unit 160 may replace the deformation rate of each of the plurality of unit connection frames 140 with the pressure value of each section of the battery cell 10, based on the length of the horizontal portion 140a of the plurality of unit connection frames 140.
For example, in the embodiment of
Similarly, the pressure measuring unit 160 may measure a pressure value for the second section of the battery cell 10 corresponding to a portion of the second plate 120 to which the second unit connection frame 142 is coupled, based on the length of the horizontal portion 140a of the second unit connection frame 142 and the deformation rate of the second unit connection frame 142. Specifically, the second unit connection frame 142 may be coupled to the center of the upper surface (the x-y plane in the +z direction) of the second plate 120. In addition, the center of the battery cell 10 may be aligned perpendicular to the center of the upper surface of the second plate 120. Accordingly, the pressure measuring unit 160 may measure a second pressure value of the center portion of the battery cell 10, based on the length of the horizontal portion 140a of the second unit connection frame 142 and the deformation rate of the second unit connection frame 142.
In addition, the pressure measuring unit 160 may measure a third pressure value for the third section (the section in the −y direction) of the battery cell 10 corresponding to a portion of the second plate 120 to which the third unit connection frame 143 is coupled, based on the length of the horizontal portion 140a of the third unit connection frame 143 and the deformation rate of the third unit connection frame 143.
The control unit 170 may be configured to determine at least one of a swelling distribution of the battery cell 10 and a swelling degree of each section, based on the pressure value of each section of the battery cell 10 measured by the pressure measuring unit 160.
Specifically, the control unit 170 may receive the pressure value of each section of the battery cell 10 corresponding to each of the plurality of unit connection frames 140 from the pressure measuring unit 160. In addition, the control unit 170 may determine the swelling distribution of the battery cell 10 according to the received pressure value of each section of the battery cell 10.
In the embodiment of
In addition, the control unit 170 may calculate a first pressure difference value between the first pressure value and a reference pressure value, calculate a second pressure difference value between the second pressure value and the reference pressure value, and calculate a third pressure difference value between the third pressure value and the reference pressure value. In addition, the control unit 170 may determine the swelling degree for each of the first region, the second region and the third region of the battery cell 10 by matching the first pressure difference value, the second pressure difference value and the third pressure difference value with a plurality of preset pressure sections.
For example, it is assumed that among the plurality of pressure sections, the first pressure difference value belongs to the danger section, the second pressure difference value belongs to the warning section, and the third pressure difference value belongs to the normal section. The control unit 170 may determine that the swelling degree of the first region of the battery cell 10 is the danger level, the swelling degree of the second region is the warning level, and the swelling degree of the third region is the normal level.
More preferably, the control unit 170 may be configured to determine the swelling distribution of each region of the battery cell 10 first and then determine the swelling degree of only the region of the battery cell 10 that is determined to have swelling.
In the former embodiment, it is assumed that the control unit 170 determines that swelling occurs in the first region and the second region of the battery cell 10. The control unit 170 may determine the swelling degree for the first region by matching the first pressure difference value for the first region of the battery cell 10 with the plurality of preset pressure sections. In addition, the control unit 170 may determine the swelling degree for the second region of the battery cell 10 by matching the second pressure difference value for the second region of the battery cell 10 with the plurality of preset pressure sections. Here, the control unit 170 may compare the sizes of the plurality of received pressure values and the reference pressure value, and determine that swelling occurs if the received pressure value is greater than or equal to the reference pressure value.
That is, the apparatus 100 for inspecting swelling of a battery cell according to another embodiment of the present disclosure may determine the swelling distribution of the battery cell 10 and/or the swelling degree of each region of the battery cell 10 by using the plurality of unit connection frames 140 and the plurality of pressure measuring elements 150. Accordingly, a region in which swelling occurs in the battery cell 10 may be specifically specified.
In addition, since the apparatus 100 for inspecting swelling of a battery cell may specifically determine the swelling degree of each region of the battery cell 10, there is an advantage of providing information for analyzing the cause of the swelling of the battery cell 10.
For example, based on the swelling distribution of the battery cell 10 and the swelling degree of each region obtained from the apparatus 100 for inspecting swelling of a battery cell, it is possible to distinguish whether the swelling is caused by an increase in pressure due to gas generation or an increase in pressure due to inflow of foreign substances.
In the embodiment of
Then, each of the nine pressure measuring elements 150 may be attached to each of the plurality of unit connection frames 140 to measure the deformation rate of each of the plurality of unit connection frames 140.
As the number of the unit connection frames 140 and the pressure measuring elements 150 increases as above, the swelling distribution of the battery cell 10 may be determined more specifically and precisely. In addition, the sections of the battery cell 10, where the swelling degree is determined, may be further subdivided. Therefore, the section where swelling occurs in the battery cell 10 may be specified more concretely.
The second plate 120 may be configured to include a plurality of second unit plates 121.
For example, in the embodiment of
Preferably, the plurality of second unit plates 121 may be spaced apart from each other at a predetermined interval so as not to overlap each other.
Each of the plurality of unit connection frames 140 may be configured to be coupled to a corresponding second unit plate 121 among the plurality of second unit plates 121. Preferably, the plurality of unit connection frames 140 may be configured to be fixedly coupled to the center portion of the outer side surface of the corresponding second unit plate 121.
Each of the plurality of pressure measuring elements 150 attached to the plurality of unit connection frames 140 may measure a deformation rate of each of the plurality of unit connection frames 140.
In addition, the pressure measuring unit 160 may calculate the pressure value of each section of the battery cell 10 corresponding to each of the plurality of second unit plates 121, based on the deformation rate of each of the plurality of unit connection frames 140 measured by each of the plurality of pressure measuring elements 150. In this case, since the plurality of second unit plates 121 are positioned to be spaced apart from each other by a predetermined distance, the influence between them may be minimized.
For example, in the embodiment of
That is, since the plurality of second unit plates 121 are located to be spaced apart from each other, the influence between the adjacent second unit plates 121 may be excluded in the process of measuring the deformation rate of each of the plurality of unit connection frames 140.
In other words, the deformation rate of each of the plurality of unit connection frames 140 may be measured by reflecting the swelling pressure generated in the corresponding section of the battery cell 10 more accurately.
The embodiment of
Referring to the swelling distribution of the battery cell 10 shown in
That is, since the apparatus 100 for inspecting swelling of a battery cell according to still another embodiment of the present disclosure includes a plurality of second unit plates 121 and a plurality of unit connection frames 140, there is an advantage in the swelling distribution of the battery cell 10 and the swelling degree of each section of the battery cell 10 may be determined more specifically.
Referring to
The temperature measuring element 180 may be provided in plural and attached to each of the plurality of second unit plates 121.
In addition, the temperature measuring unit 190 may be configured to measure the temperature of each of the plurality of second unit plates 121 by using the plurality of temperature measuring element 180.
The control unit 170 may be configured to receive the temperature value of each of the plurality of second unit plates 121 from the temperature measuring unit 190 and further determine the temperature of each section of the battery cell 10.
For example, in the embodiment of
The control unit 170 may further determine the temperature of each section of the battery cell 10, together with at least one of the swelling distribution of the battery cell 10 and the swelling degree of each section of the battery cell 10.
If the internal temperature of the battery cell 10 rises to evaporate the electrolyte inside the battery cell 10, the pressure inside the battery cell 10 may increase, thereby causing swelling.
Therefore, the apparatus 100 for inspecting swelling of a battery cell according to still another embodiment of the present disclosure may determine the cause of swelling of the battery cell 10 more specifically, since not only the swelling distribution of the battery cell 10 and the swelling degree of each section of battery cell 10 but also the temperature of each section of the battery cell 10 are further considered.
The embodiments of the present disclosure described above may not be implemented only through an apparatus and a method, but may be implemented through a program that realizes a function corresponding to the configuration of the embodiments of the present disclosure or a recording medium on which the program is recorded. The program or recording medium may be easily implemented by those skilled in the art from the above description of the embodiments.
The present disclosure has been described in detail. However, it should be understood that the detailed description and specific examples, while indicating preferred embodiments of the disclosure, are given by way of illustration only, since various changes and modifications within the scope of the disclosure will become apparent to those skilled in the art from this detailed description.
Additionally, many substitutions, modifications and changes may be made to the present disclosure described hereinabove by those skilled in the art without departing from the technical aspects of the present disclosure, and the present disclosure is not limited to the above-described embodiments and the accompanying drawings, and each embodiment may be selectively combined in part or in whole to allow various modifications.
Number | Date | Country | Kind |
---|---|---|---|
10-2020-0030940 | Mar 2020 | KR | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|