The present invention relates to canistered missile, and more particularly to covers for missile canisters.
It is well known in the art to launch a missile from a canister. The canisters are typically round or square tubes that contain a missile, missile-launch hardware such as rails and/or sabots, and electronics for initiating launch. In addition to functioning as a launch system, the canisters provide environmental protection for the missile, simplify missile-handling issues, and provide an efficient and long-term solution for missile storage.
In order to provide full environmental protection for the missile and other components within the canister, the canister must be sealed. This is typically done using a cap or cover. The cover is ideally able to protect or isolate the missile from a variety of environmental factors and must provide unimpeded passage of the missile upon launch.
A variety of canister covers are known. Some covers tear or shatter upon contact with the missile during launch. This is acceptable for some but not all types of missiles. In particular, some missiles (e.g., LAM, PAM, etc.) include fragile mechanisms in the nose that could be damaged on impact with the cover. For these types of missiles, the canister cover must blow off without making contact with the missile.
Non-contact covers are typically more elaborate than tear-through designs since they must be actuated to release. This usually equates to increased weight, complexity, and expense.
The present invention provides a cover for a missile canister that avoids some of the costs and disadvantages of the prior art.
The illustrative embodiment of the present invention is a launch system that includes a canister and a missile, in addition to the canister cover.
A canister cover in accordance with the present invention is capable of:
More particularly, in accordance with the illustrative embodiment, the capabilities described above are obtained by:
In the illustrative embodiment, the structural characteristic that differs between the regions of the cover is the thickness of the region. In particular, the marginal region is thinner than the main region.
Since the marginal region is thinner than the main region, and by virtue of the way in which the cover is attached to the canister, the cover breaks directly over the canister wall when exposed to an elevated internal canister pressure. The break occurs in the marginal region, or at the interface between the marginal region and the main region. As a consequence, a single large piece representing the main region of the cover is blown off of the canister.
When the cover is exposed to an external pressure, there is a relatively limited build-up of stress/strain at the interface of the marginal region and the main region. This is because the marginal region is attached to and supported by the forward end of the missile canister. In fact, on exposure to external pressure, the cover might fail at the main region, which is unsupported by the canister, before a failure occurs at the marginal region. On the other hand, to the extent that an internal pressure acts on the cover, high levels of stress/stain will build at the interface of the marginal region and the main region since this region of the cover is not supported against forces that are applied from the inside of the canister. As a consequence, the cover fractures at a relatively lower internal pressure than external pressure.
If an imperfection exists in the cover at some location along the marginal region, a gap or fracture might occur at that location when exposed to elevated internal pressure. Were that to occur, pressure would dissipate such that the cover would not blow off of the canister. To that end, the cover is physically adapted to equalize the response of the marginal region to internal pressure, regardless of location-to-location variations in the marginal region. In the illustrative embodiment, that adaptation is a ridge of material.
Canister 102 usually contains any one or more of a variety of internal elements or mechanisms, as is well known to those skilled in the art. Since these internals are not germane to an understanding of the present invention, they will not be described in this specification.
With continuing reference to
Marginal region 214 includes holes 216 for receiving a bolt, etc., by which canister cover 106 is attached to canister 102. Main region 210 includes a physical adaptation that enables cover 106 to resist pressure equally at all locations along the marginal region (when cover 106 is attached to canister 102). In the illustrative embodiment depicted in
As depicted in
It was previously disclosed that marginal region 214 is distinguished from main region 210 by a tendency to break or fragment before main region 210. In the embodiment that is depicted in
Cover 106 is coupled to missile canister 102 via bolts 322. In particular, bolt 322 extends through hole 216 in marginal region 214 and engages bolt-receiving hole 320 in forward portion 318 of canister 102. Gasket 324 is disposed between the bottom surface of cover 106 at marginal region 214 and the upper surface of forward portion 318 of canister 102. Gasket 324 provides a pressure-tight seal.
It accordance with the illustrative embodiment, cover 106 is released from canister 102 and blown away from canister 102 during launch but before the nose of missile 108 has a chance to contact the cover. The cover releases due to the pressure generated from exhaust gases on when the missile fires. The design of cover 106 is, therefore, a function of the internal pressure that is developed when the missile ignites and materials composition of cover 106. The internal pressure that develops depends on missile type and the dimensions of the canister. Those skilled in the art will be able to design and build cover 106, after reading the present disclosure, as a function of desired materials of construction, missile type and canister dimensions. Suitable materials for cover 106 include for example, aluminum or glass-filled nylon. More generally suitable materials include any isotropic or quasi-isotropic material with predictable mechanical properties.
As previously described, marginal region 214 is less able to withstand pressure than main region 210. As a consequence, cover 106 fractures at marginal region 214 due to launch pressure.
Launch system 100 must be able to withstand elevated external pressure. In particular, it is important that when cover 106 is exposed to such elevated external pressures, it does not fracture. In fact, it is possible that cover 106 will be exposed to external pressures that are as high as the internal pressure that is developed by the missile plume (which causes cover 106 to blow off of canister 102). As a consequence, cover 106 must be able to withstand a higher level of external pressure (i.e., pressure against its outside surface 107) than internal pressure (i.e., pressure against its inside surface 105). In other words, assume that cover 106 fractures when the internal canister pressure reaches magnitude P1, wherein the elevated pressure results from the release into canister 102, on ignition, of missile exhaust gases. Cover 106 will not fracture, however, when exposed to an external pressure of the same magnitude, P1.
In accordance with the illustrative embodiment, this differential response to pressure is achieved by the way cover 106 is supported. In particular, in the illustrative embodiment, inside surface 105 of cover 106 is supported at marginal region 214, but outside surface 107 is not supported.
Specifically, to the extent an external pressure is applied, marginal region 214, the interface of the marginal region and the main region, and peripheral portion 430 of main region 210 deflect only a minimal distance (i.e., the thickness of gasket 324) until they abut upper surface 432 of forward end 318 of canister 102. They are, therefore, prevented from deflecting to any substantial degree. As a consequence, there is a relatively limited build-up of stress/strain in the interface of main region 210 and marginal region 214. As a result, a break does not occur. To the extent that an internal pressure acts on cover 106, high levels of stress/stain will build at the interface of marginal region 214 and main region 210. This occurs since cover 106 is not supported against forces that are applied against it from the inside of the canister. As a consequence, cover 106 has a diminished ability to resist internal pressure as compared to its ability to resist external pressure.
As previously described, ridge 212 equalizes the response of marginal region 214 to internal canister pressure. In particular, ridge 212 prevents cover 106 from fracturing at a single location along marginal region 214, as might otherwise occur if marginal region 214, at that location, were structurally compromised relative to other locations along the marginal region. If marginal region 214 were to fracture at a single location, then pressure would rapidly dissipate at that fracture and cover 106 would not blow off, as desired.
It is to be understood that the above-described embodiments are merely illustrative of the present invention and that many variations of the above-described embodiments can be devised by those skilled in the art without departing from the scope of the invention. It is therefore intended that such variations, and others that will occur to those skilled in the art in view of the present disclosure, be included within the scope of the following claims and their equivalents.
This invention was made with Government support under contract DAAH01-03-C-0035 awarded by the US Army. The Government has certain rights in the invention.
Number | Name | Date | Kind |
---|---|---|---|
2576431 | White | Nov 1951 | A |
3670916 | Alpert | Jun 1972 | A |
4207913 | Fike, Jr. | Jun 1980 | A |
4389938 | Sigrist | Jun 1983 | A |
4471684 | Johnson et al. | Sep 1984 | A |
5375503 | Breugnot et al. | Dec 1994 | A |
5542333 | Hagelberg et al. | Aug 1996 | A |
5993921 | Hunn | Nov 1999 | A |
6123005 | Kuchta et al. | Sep 2000 | A |
6363855 | Kim et al. | Apr 2002 | B1 |
20040083878 | Paul | May 2004 | A1 |
Number | Date | Country |
---|---|---|
0022756 | Jan 1981 | EP |
2124741 | Feb 1984 | GB |
Number | Date | Country | |
---|---|---|---|
20060207416 A1 | Sep 2006 | US |