1. Technical Field
The present disclosure relates to surface acoustic wave (SAW) sensors for detecting the growth of biofilms. More particularly, the present disclosure relates to piezoelectric SAW sensors having passivation film layer.
2. Background of Related Art
Bacteria can attach to surfaces and form microcolonies as their population increases. The colonies eventually can form a community known as a bacterial biofilm [1, 2]. A biofilm is not simply a group of bacteria, but a complex collection of microorganisms encased in an extracellular matrix. The extracellular matrix is composed of exopolysaccharide polymers which promote irreversible adhesion of microcolonies on the surface and also prevent diffusion of antibiotics through the biofilm [1, 2]. Due to the complex extracellular matrix and heterogeneous bacterial composition, biofilms are resistant to bacteriophages in industry and to chemically diverse antibiotic treatments in clinical fields [3], in addition, bacterial corrosion of metals is an economically important consequence of bacterial biofilm formation that illustrates several fascinating aspects of the structure and physiology of these adherent bacterial populations. Therefore, environmental, clinical, and industrial long term reliable biofilm growth monitoring is critical to prevent contamination, severe infection, and corrosive problems due to the biofilm formation.
The measurement of bacterial biofilms with capacitive sensing has been applied by Yang and Li to monitor Salmonella typhimurium bacteria [4], and by Ghafar-Zadeh et al. to detect Escherichia coil (E. coli) [5]. In Yang and Li at al. [4], an interdigitated microelectrode was fabricated to provide detectable impedance signals in capacitance measurement during bacterial growth, S. typhimurium bacteria were grown over the microelectrode and the capacitance change was continuously measured. Capacitive sensing in a liquid environment, however, can be interfered with by a conductive media due to the current flow through the growth media [4].
The direct impedance measurement of the attachment of E. coli on an electrode is demonstrated by other groups [6, 7]. The change of impedance during bacterial growth is correlated with the biomass adhere on the electrode. This impedimetric sensing is particularly useful in detecting very early attachment of bacteria based on the significant impedance change observed upon attachment. However, long-term real-time biofilm monitoring by impedance measurement requires a continuous current source for bacterial detection which may cause interruption of bacterial growth.
Fluorescent methods have reported high sensitivity [8], but require fluorescent molecule labeling for sensing to occur. Labeling requires additional sample preparation and the fluorescent molecule can be degraded over long term exposure to liquid.
Electrochemical sensing can be used for selective detection a molecule without fluorescent labeling [9]. An electrochemical sensor array was integrated with a miniaturized bioreactor system for high throughput cell cultivation in 96 well plates [10]. Using a 100 μl working volume in the 96 well micro reactors, the sensor array can monitor temperature, pH, and oxygen concentration as well as total biomass. However, electrochemical sensors require a continuous power source for the operation and also require recalibration of the sensor due to the conductivity change of bacterial growth media in long term biofilm growth experiments.
Surface Acoustic Wave (SAW) sensors exhibit several advantages in small molecule detection including high sensitivity [11-22] and low power consumption [23]. A SAW sensor can detect mass or viscosity change due to the wave velocity attenuation, resulting in a resonant frequency shift at the output. A highly sensitive SAW sensor for detection of interleukin-6 (IL-6), which is one of key molecules in human immune system, was reported. In Krishnamoorthy et al. [19], a specific receptor for IL-6 was immobilized on the surface of the SAW sensor. Based on the resonant frequency shift due to the IL-6 binding, the detection limit of the SAW sensor was approximately 10−18 g (grams). A SAW sensor is also a passive device.
The power for operation of the SAW sensor can be delivered by an external device wirelessly which makes the SAW sensor useful for long term biofilm monitoring without a continuous power supply [23]. Furthermore, the SAW sensor can be fabricated using biocompatible materials [24-26]. The combination of extremely high sensitivity, biocompatibility, and low power consumption makes the SAW sensor a unique tool for real time monitoring of bacterial biofilm growth. However, it is also noted that piezoelectric materials used in the SAW sensor can be dissolved due to long term exposure to liquid [27].
The present disclosure relates to a novel inverted passivated SAW sensor for real time biofilm monitoring. A piezoelectric film is deposited by pulsed laser deposition, and the sensor is effectively passivated by a passivated film layer using atomic layer deposition to prevent damage to the piezoelectric layer in bacterial growth media and animal serum.
The SAW sensor can be reused after oxygen plasma cleaning, allowing for consecutive biofilm formation experiments using one sensor.
Therefore, the present disclosure relates to a novel surface acoustic wave (SAW) biofilm sensor comprising: a SAW transducer; a piezoelectric film layer; and a passivation film layer. The piezoelectric film layer is mounted over the SAW transducer and the passivation film layer is mounted over the piezoelectric film layer. In one embodiment, the passivation layer includes aluminum oxide, Al2O3. In yet another embodiment, the passivation layer defines a thickness of at least 45 nanometers (nm). In a still further embodiment, the piezoelectric layer includes zinc oxide, ZnO. In yet another embodiment, the piezoelectric layer defines a thickness of at least 40 nanometers (nm).
The present disclosure relates also to a surface acoustic wave (SAW) biofilm sensor that includes a transmitting electric to acoustic wave transducer defining an upper surface and a lower surface, a receiving acoustic wave to electric transducer defining an upper surface and a lower surface, a piezoelectric film layer defining an upper surface and a lower surface and a passivation film layer defining an upper surface and a lower surface. A portion of the lower surface of the piezoelectric film layer is disposed on the upper surface of the transmitting electric to acoustic wave transducer and another portion of the lower surface of the piezoelectric film layer is disposed on the upper surface of the receiving acoustic wave to electric transducer and the lower surface of the passivation film layer is disposed on the upper surface of the piezoelectric film layer. The upper surface of the passivation film layer thereby configured to enable contact with a biofilm.
In one embodiment, the SAW biofilm sensor may further include a piezoelectric SAW loss reduction film layer defining an upper surface and a lower surface wherein the lower surface of the transmitting electric to acoustic wave transducer is disposed on a portion of the upper surface of the piezoelectric SAW loss reduction film layer and wherein the lower surface of the receiving acoustic wave to electric transducer is disposed on another portion of the upper surface of the piezoelectric SAW loss reduction film layer.
In still another embodiment, the SAW biofilm sensor may further include a substrate defining an upper surface and a lower surface, wherein the lower surface of the piezoelectric SAW loss reduction film layer is disposed on the upper surface of the substrate.
In yet another embodiment, a portion of the lower surface of the piezoelectric film layer is disposed on a portion of the upper surface of the piezoelectric SAW loss reduction film layer and disposed between the transmitting electric to acoustic wave transducer and the receiving acoustic wave to electric transducer.
In a still further embodiment, another portion of the lower surface of the piezoelectric film layer may be disposed between the transmitting electric to acoustic wave transducer and the receiving acoustic wave to electric transducer.
In one embodiment of the SAW biofilm sensor, wherein the piezoelectric layer defines an upper sub-layer and a lower sub-layer, wherein the lower sub-layer defined by the portion of the lower surface of the piezoelectric film layer is disposed on the portion of the upper surface of the lower piezoelectric film layer and is disposed between the transmitting electric to acoustic wave transducer and the receiving acoustic wave to electric transducer. The upper sub-layer is defined by the portion of the piezoelectric layer between the passivation film layer and the lower sub-layer. The lower sub-layer has a shear modulus and density to define a first SAW velocity. The upper sub-layer has a shear modulus and density to define a second SAW velocity wherein the second velocity differs from the first velocity.
In one embodiment, the second velocity is equal to or greater than the first velocity.
In still another embodiment, the SAW biofilm sensor the passivation layer includes aluminum oxide, Al2O3. In one embodiment, the passivation layer defines a thickness between the upper surface of the passivation layer and the lower surface of the passivation layer wherein the thickness of the passivation layer has a dimension of at least 45 nanometers (nm).
In yet another embodiment, the piezoelectric layer may include zinc oxide, ZnO. In one embodiment, the piezoelectric layer defines a thickness between the upper surface of the piezoelectric layer and the lower surface of the piezoelectric layer and the thickness of the piezoelectric layer has a dimension of at least 40 nanometers (nm).
The present disclosure relates also to a method of assembling a biofilm surface acoustic wave (SAW) sensor that includes depositing a piezoelectric layer on a SAW transducer electrode pattern and depositing a passivation layer on the piezoelectric layer.
In one embodiment, the depositing of the piezoelectric layer may include depositing a layer of zinc oxide ZnO on the SAW transducer electrode pattern. In a still further embodiment, the depositing a layer of zinc oxide ZnO on the SAW transducer electrode pattern may include depositing a layer of zinc oxide ZnO having a thickness of at least 40 nanometers (nm).
In yet another embodiment, the depositing a passivation layer on the piezoelectric layer may include depositing a layer of aluminum oxide Al2O3 on the piezoelectric layer.
In a still further embodiment, the depositing of the layer of aluminum oxide Al2O3 on the piezoelectric layer may include depositing a layer of aluminum oxide Al2O3 having a thickness of at least 45 nanometers (nm) on the piezoelectric layer.
In one embodiment, the method of assembling may further include depositing the SAW transducer electrode pattern on a piezoelectric SAW loss reduction film layer. The method may further include depositing the piezoelectric SAW loss reduction film layer on a substrate.
In another embodiment, the step of depositing the piezoelectric layer on the SAW transducer electrode pattern includes pulsed laser deposition.
In still another embodiment, the step of depositing the passivation layer on the piezoelectric layer includes atomic layer deposition.
These and other advantages will become more apparent from the following detailed description of the various embodiments of the present disclosure with reference to the drawings wherein:
The present disclosure relates to the design of a passivated piezoelectric SAW transducer biofilm sensor according to embodiments of the present disclosure without loss of sensitivity for biosensing applications.
First, to illustrate the advantages of the embodiments of the present disclosure,
The substrate 32 may be made from silicon Si and the common piezoelectric loss reduction film 30 may be made from silicon dioxide SiO2.
Since the biofilm 40 is in direct contact with the elevated portions 23 and 25 of the transmitting electrode transducer 22 and the receiving electrode transducer 24, respectively, the configuration of a SAW sensor such as SAW sensor 10 in
In contrast, the present disclosure relates to a successfully passivated ZnO based SAW sensor for long term biofilm growth monitoring in an animal serum or bacterial growth media. Atomic Layer Deposition (ALD) was applied for high density and conformal aluminum oxide (Al2O3) film deposition to protect the ZnO of the SAW sensor from media. The SAW sensor was used for the in vitro real time study of E. coli static biofilm growth in Lysogeny Broth (LB) media and in 10% Fetal Bovine Serum (FBS), the latter of which is the most widely used serum for mammalian cell culture due to similarities to in vivo environments [28].
The remainder of the present disclosure presents the design of the inverted SAW sensor for the targeted mode of the wave and fabrication process. The material and experimental procedures for biofilm detection in the sensor are presented. The results show the biofilm detection using the sensor in consecutive testing both in bacterial growth media and animal serum.
More particularly,
As noted, the transmitting electric to acoustic wave transducer 110 also includes the second transmitting electrode comb-like or prong-like electrically conductive member 122 that interlocks or interdigitated with the first transmitting electrode comb-like electrically conductive member 112. The second transmitting conductive member 122 includes a rectangularly-shaped base 124 from which extend orthogonally first rectangularly-shaped prong 126a and second rectangularly-shaped prong 126b. The rectangularly shaped base 124 defines a first end 124a and a second end 124h. The first prong 126a is positioned at a distance away from first end 124a and the second prong 1261 is positioned at a distance away from the second end 126b to define a central rectangularly-shaped aperture 128 between the first prong 126a and the second prong 126b.
The first transmitting electrically conductive member 112 includes a voltage input terminal Vin that is in direct electrical communication with, for example, the rectangularly-shaped base 114 such that the entire first transmitting electrically conductive member 112 is in electrical communication with the voltage input terminal Vin. The first and second electrically conductive members 112 and 122 are arranged such that the prongs 116a, 116b, 116c are adjacent to and intermesh with prongs 126a and 126h. The second transmitting electrically conductive member 122 includes a ground terminal 130 that is in direct electrical communication with, for example, the rectangularly-shaped base 124 such that the entire second transmitting electrically conductive member 122 is in electrical communication with the ground terminal 130.
The receiving acoustic wave to electric transducer 110′ includes the same components as, and is arranged in the same manner as, transmitting electric to acoustic wave transducer 110 and for convenience the components are designated with primes.
Consequently, receiving acoustic wave to electric transducer 110′ includes a first transmitting electrode comb-like or prong-like electrically conductive member 112′ that interlocks or interdigitates with a second transmitting electrode comb-like electrically conductive member 122′. The first receiving electrically conductive member 112′ includes rectangularly-shaped base 114 from which extend orthogonally first rectangularly-shaped peripheral prong 116a′, rectangularly-shaped central prong 116b′ and second rectangularly-shaped peripheral prong 116c′.
The receiving electric to acoustic wave transducer 110′ also includes the second receiving electrode comb-like or prong-like electrically conductive member 122′ that interlocks or interdigitates with the first receiving electrode comb-like electrically conductive member 112′. The second receiving conductive member 122′ includes a rectangularly-shaped base 124′ from which extend orthogonally first rectangularly-shaped prong 126a′ and second rectangularly-shaped prong 126b′. The rectangularly-shaped base 124′ defines a first end 124a′ and a second end 124b′. The first prong 126a′ is positioned at a distance away from first end 124a′ and the second prong 126b′ is positioned at a distance away from the second end 126b′ to define a central rectangularly-shaped aperture 128′ between the first prong 126a′ and the second prong 126b′.
The first receiving electrically conductive member 112′ includes a voltage output terminal Vout that is in direct electrical communication with, for example, the rectangularly-shaped base 114′ such that the entire first receiving electrically conductive member 112′ is in electrical communication with the voltage output terminal Vout. The first and second electrically conductive members 112′ and 122′ are arranged such that the prongs 116a′, 116b′, 116c′ are adjacent to and intermesh with prongs 126a′ and 126h′. The second receiving electrically conductive member 122′ includes a ground terminal 130′ that is in direct electrical communication with, for example, the rectangularly-shaped base 124′ such that the entire second receiving electrically conductive member 122′ is in electrical communication with the ground terminal 130′.
When a voltage source, not shown, is placed across the terminals Vin and Vout, a surface acoustic wave 150 is generated by the transmitting electric to acoustic wave transducer 110 and travels in the direction of arrow 152 towards the receiving acoustic wave to electric transducer 110′.
The lower surface 110a of the transmitting electric to acoustic wave transducer 110 is disposed on a portion 301a of the upper surface 30a of the piezoelectric SAW loss reduction film layer 30 and the lower surface 110a′ of the receiving acoustic wave to electric transducer 110′ is disposed on another portion 302a of the upper surface 30a of the piezoelectric SAW loss reduction film layer 30.
A piezoelectric film layer 160 defines an upper surface 160a and a lower surface 160b. A portion 1601b of the lower surface 160b of the piezoelectric film layer 160 is disposed on the upper surface 110a of the transmitting electric to acoustic wave transducer 110. Another portion 1602b of the lower surface 160b of the piezoelectric film layer 160 is disposed on the upper surface 110′a of the receiving acoustic wave to electric transducer 110′.
A passivation film layer 170 defines an upper surface 170a and a lower surface 170b, The lower surface 170b of the passivation film layer 170 is disposed on the upper surface 160a of the piezoelectric film layer 160. Thus, the upper surface 160a of the passivation film layer 170 is thereby configured to enable contact with a biofilm 40.
In a similar manner as described with respect to
A portion 1603b of the lower surface 160b of the piezoelectric film layer 160 is disposed on a portion 303a of the upper surface 30a of the piezoelectric SAW loss reduction film layer 30 and disposed between the transmitting electric to acoustic wave transducer 110 and the receiving acoustic wave to electric transducer 110′.
The lower sub-layer 161 is defined by the portion 1603b of the lower surface 160b of the piezoelectric film layer 160 that is disposed on the portion 303a of the upper surface 30a of the lower piezoelectric film layer 30 and is disposed between the transmitting electric to acoustic wave transducer 110 and the receiving acoustic wave to electric transducer 110′. The upper sub-layer 162 is defined by the portion of the piezoelectric layer 160 between the passivation film layer 170 and the lower sub-layer 161 of the piezoelectric layer.
The lower sub-layer 161 has a shear modulus and density to define a first SAW velocity V1. The upper sub-layer 162 has a shear modulus and density to define a second SAW velocity V2. Although the second velocity V2 may differ from the first velocity V1, for the purposes of simplifying the design analysis, the two velocities may be set equal to one another. Alternatively, the second velocity V2 may be equal to or greater than the first velocity V1.
The passivation layer 170 defines a thickness h between the upper surface 160a of the passivation layer 160 and the lower surface 160b of the passivation layer 160 while the biofilm 40 defines a thickness x.
In one embodiment, the piezoelectric layer 160 includes zinc oxide, ZnO and the thickness d of the piezoelectric layer 160 has a dimension of at least 40 nanometers (nm).
In one embodiment, the passivation layer includes aluminum oxide, Al2O3, and the thickness h of the passivation layer 170 has a dimension of at least 45 nanometers (nm).
The specific design for the selection of the material and thickness of the piezoelectric layer 160 and the passivation layer 170 is described in more detail below.
Materials and Methods
Design of the SAW Sensor
For applications of a SAW sensor in liquid environments, selecting the proper mode of propagation is crucial to prevent severe attenuation or the wave. In a SAW sensor, the surface of the piezoelectric layers is set to a high frequency oscillation governed by the design of the interdigitated transducers (IDT) and the SAW velocity of the piezoelectric material. This no-load oscillation frequency is affected by environmental changes at the surface of the SAW sensor. These effects are observed experimentally as changes in resonant frequency, representing a shift in the SAW phase velocity. However, one of the challenges for biosensor applications is the extremely high attenuation damping of the SAW in liquid environments, when Rayleigh mode waves are generated. In this mode the acoustic wave displacement is perpendicular to the surface and causes significant attenuation of the oscillations in liquid environments. Unlike Rayleigh mode waves, Love mode SAW generation demonstrates displacement planar to the surface and the oscillations are not attenuated in liquid environments [11-15, 18-20, 29-31]. The generation of Love or Rayleigh mode waves depends on the crystallographic orientation of the piezoelectric film. Therefore, it is highly advantageous to deposit piezoelectric material with a specific orientation for generating Love mode SAW [16-22, 29-31]. ZnO with a high piezoelectric coefficient is capable of generating very high frequency (GHz, gigahertz, where Hz is hertz or 1 cycle/sec) SAW, and it has been shown to grow along the crystallographic orientation that favors Love mode propagation on a SiO2/Si substrate [19-22]. Love mode waves are predominantly generated with the SAW IDT aligned perpendicular to the c-axis of the ZnO film [16-22].
Some important parameters, such as the SiO2 thickness, the IDT electrode dimensions, and the ZnO deposition method, had to be considered in the design of a highly sensitive SAW sensor. In order to confine the propagation of the SAW on the surface of the device, a thin film that can prevent acoustic wave loss from the piezoelectric material to Si substrate was required between ZnO film and Si. SiO2 was previously shown [15, 18] to be an appropriate loss blocking film for thicknesses around 50 nm and was selected in this work. For the best resonance of the SAW at the designed operational frequency, the IDT separation d should be equal to half of the operational wavelength λ. (See
To achieve advantages over prior art biofilm sensors for biofilm detection, it was necessary to provide an inverted structure for the saw sensor 200, as shown in
The material of the IDT, traditionally aluminum in the SAW sensor, can be selected by the acoustic impedance match theory [34]. Potential materials, such as aluminum and gold, were selected and the acoustic power reflective coefficient (R) was calculated based on the theory. The reflective coefficient of the aluminum and gold were 0.058 and 0.012 respectively. The lower reflective coefficient in IDT represents more energy transmission to the piezoelectric material which makes a highly sensitive SAW sensor. Therefore, the IDT material was chosen to be gold based on the low R value.
Selection of Passivation Film
Since the bare ZnO layer 160 without a passivation film layer 170 was damaged both in LB media and 10% FBS, selection of the proper material to protect ZnO while considering future biomedical applications is important to maintain the sensitivity of the sensor. The sensitivity of the passivated SAW sensor is decreased as compared to the unpassivated sensor due to the initial mass loading and dispersion of the wave in the passivation film [12, 29, 35-40]. To investigate the effect of the added material on the SAW sensitivity in addition to the material selection, we consider only the mass loading effect of the passivation film based on the assumption that the dispersion in the passivation film is minimal due to a much thinner passivation layer (45 nm) as compared to the wavelength of the SAW [35, 38, 40]. As noted, the schematic cross section view of the inverted passivation SAW sensor 200 is shown in
where v0 is the initial velocity of the wave, m is the amount of the additional mass, and Δv is the wave velocity changes due to Δm. The SAW velocity (v), shown in equation (2), is defined by the shear modulus of the piezoelectric material and local area density based on the one-dimensional acoustic wave equation (3) [15, 18-20].
where C is the shear modulus of the surface material, u is the mechanical displacement of the piezoelectric substrate, ρ is material density of the surface, y is the axis of the mechanical displacement propagation, and v is the velocity of the SAW in equations (2) and (3). In order to simplify the modeling of passivation effects on the sensitivity of the SAW sensor, the bacterial growth over the sensor was assumed uniform, so that bacterial mass loading only depended on the thickness of the biofilm. Based on this assumption, the sensitivity of the SAW sensor from equation (1) was proportional to the velocity change as biofilm thickness (x) approaches zero as shown in equation (4).
The biofilm formed on the sensor also has a comparatively low shear modulus that can be neglected in the calculation of the total shear modulus of the passivated SAW sensor. The total shear modulus including the ZnO and the passivation film was calculated based on a mechanical spring series connection because the SAW is transferred from ZnO film to the passivation layer sequentially. Based on the assumptions and the total shear modulus calculation, the SAW velocity on a sensor coated with a biofilm was determined by the following equation (5).
where Cfilm and CZno are the shear moduli of the passivation film and ZnO, ρZno and ρfilm are the densities of the ZnO and passivation film, h is the thickness of the passivation film, d is the thickness of the ZnO film, and x is the biofilm thickness. All parameters except the biofilm thickness (x) were determined by selecting potential passivation materials (i.e. Al2O3, Si3N4, SiO2 and Teflon) and their thicknesses which were assumed to be 40 nm for all passivation films considered. Potential passivation materials with mechanical properties similar to the ZnO film, such as shear modulus and density, were selected [41, 42]. The sensitivity of the SAW sensor with different passivation films was calculated by differentiating equation (5) with respect to x, and letting x approach zero, based on equation (4).
The application of this fundamental theoretical treatment showed that an Al2O3 film was best suited as a passivation layer and it was selected. The thickness of the passivation film (h) in equation (5) is important for our application. The film should be thick enough for effective passivation, but should not be too thick that the added layer causes a significant attenuation both due to mass loading and dispersion of the SAW resulting in substantial loss in sensitivity. The minimum required thickness of Al2O1 film (45 nm) was empirically determined. The detailed studies were presented in the film characterization section.
Fabrication
As described below in more detail with respect to
The fabrication process flow is shown in
Referring to
In
For simplicity, in
Returning to
The transducer mounting structure 35 is positioned directly opposite to the target 312 on the target platform 310 and the target carousel 304. The structure 35 is positioned on a heatable sample stage 314 that is supported by a second shaft 316 that passes through a second penetration 318 in the vacuum chamber 302.
A quartz window 320 is positioned in the vacuum chamber 302 at an angle to enable a beam of laser light 324 to impact the target 312. As a result of the beam of laser light 324 impacting the target 312, a plume 326 of target material is created within the vacuum chamber and deposits on the transducer mounting structure 35 which includes substrate 32.
The laser deposition system used a KrF excimer laser at a wavelength of 248 nm with pulse duration of 25 ns to ablate a high purity (99.99%) ZnO ceramic target. The ZnO layer was grown at 250° C. with an ambient oxygen partial pressure of ˜1.0×10−4 Torr. After ZnO film deposition, electrical contact pad areas were patterned by photolithography and the ZnO was etched using a solution that consisted of phosphoric acid, acetic acid, and deionized water (1:1:30).
As shown in
In view of the foregoing, those skilled in the art will understand that embodiments of the present disclosure relate to a surface acoustic wave (SAW) biofilm sensor 200 that includes SAW transducer 105, piezoelectric film layer 160, and passivation film layer 170. The piezoelectric film layer 160 is mounted over the SAW transducer 105 and the passivation film layer 170 is mounted over the piezoelectric film layer 160. In one embodiment, the passivation layer 170 includes aluminum oxide, Al2O3. In yet another embodiment, the passivation layer 170 defines a thickness h of at least nanometers (nm). In a still further embodiment, the piezoelectric layer 160 includes zinc oxide, ZnO. In yet another embodiment, the piezoelectric layer 160 defines a thickness d of at least 40 nanometers (nm).
Further, in view of the foregoing, those skilled in the art will understand that embodiments of the present disclosure relate to a method of assembling a biofilm surface acoustic wave (SAW) sensor, e.g., biofilm SAW sensor 200, that includes depositing a piezoelectric layer, e.g., piezoelectric layer 160, on a SAW transducer electrode pattern, e.g., IDT electrode pattern 105, and depositing a passivation layer, e.g., passivation layer 170, on the piezoelectric layer 160. The depositing a piezoelectric layer may include depositing a layer of zinc oxide ZnO on the SAW transducer electrode pattern 105. In one embodiment, the depositing a layer of zinc oxide ZnO on the SAW transducer electrode pattern 105 may include depositing a layer of zinc oxide ZnO having a thickness d of at least 40 nanometers (nm).
Further, the depositing a passivation layer, e.g., passivation layer 170, on the piezoelectric layer, e.g., piezoelectric layer 160, may include depositing a layer of aluminum oxide Al2O3 on the piezoelectric layer 160. The depositing a layer of aluminum oxide Al2O3 on the piezoelectric layer includes depositing a layer of aluminum oxide Al2O3 having a thickness h of at least 45 nanometers (nm) on the piezoelectric layer.
Additionally, the method of assembling the SAW biofilm sensor 200 may further include depositing the SAW transducer electrode pattern, e.g., IDT electrode pattern 105, on a piezoelectric SAW loss reduction film layer, e.g., piezoelectric SAW loss reduction film layer 30.
The method of assembling may further include depositing the piezoelectric SAW loss reduction film layer, e.g., piezoelectric. SAW loss reduction film layer 30, on a substrate, e.g. substrate 32.
The step of depositing a piezoelectric layer, e.g., piezoelectric layer 160, on a SAW transducer electrode pattern, e.g., IDT electrode pattern 105, may include pulsed laser deposition. Additionally, the step of depositing a passivation layer, e.g., passivation layer 170, on a piezoelectric layer, e.g., piezoelectric layer 160, may include atomic layer deposition.
Device Characterization and Testing
Before the SAW sensor was used to measure biofilm growth, the performance of the passivation film was characterized using an optical microscope to inspect the surface of the ZnO layer after exposure to growth media. The results were used to optimize the film thickness and fabrication process. The sensitivity of the sensor was studied by loading the sensor surface with &ionized (DI) water since its viscosity is negligible. After these characterization studies, the sensor response was tested using E. coli static biofilm growth.
Al2O3 Film Characterization
Based on the theoretical modeling calculation presented previously and the results shown in
More particularly,
Based on these experiments, the minimum required thickness of ALD Al2O3 film for the passivation of ZnO was 45 nm. Since thicker passivation films caused a high loss of sensitivity due to more initial mass loading, the 45 nm thick Al2O3 film was selected to passivate the SAW sensor.
In addition to ALD, other Al2O3 film deposition methods were investigated in order to evaluate the dependence of passivation layer performance on the fabrication process. E-beam evaporation and RF-sputtering were used to deposit 45 nm of Al2O3 film. However, after two days in an LB media bacterial suspension, these two passivation films were not able to protect the ZnO layer as shown in
More particularly,
This result can be due to non-uniform or lower density film deposition of IE-beam evaporation and RF-sputtering as compared to ALD. Therefore, ALD is a highly advantageous fabrication process for effective passivation of the ZnO using Al2O3.
Passivated SAW Sensor Characterization
The mass sensitivity and detection limit of the SAW sensor were studied by loading 10 μl of deionized (DI) water onto the sensor. A volume of 10 μl was used since that was the minimum volume of DI water required to cover the area between the two IDTs of the sensor. By measuring the resonant frequency shift upon mass loading, the sensitivity of the SAW sensor was calculated based on equations (3) and (6). The mass detection limit of the sensor was also calculated using the equipment resolution and the sensitivity.
Real-Time Resonant Frequency Monitoring
As illustrated in
Biofilm Growth Experiments with the SAW Sensor
E. coli W3110 was cultured in a shaking incubator for about 16 hours. The grown bacterial suspension was diluted with LB media or 10% FBS to make the initial OD600 approximately 0.21-0.23. The total volume of the diluted bacterial suspension in the growth well 502 was 20 ml in experiments with both types of media. The FBS solution was prepared to a 10% concentration by diluting with Dulbecco/Vogt modified Eagle's minimal essential medium (Invitrogen Inc, USA). After filling the bacterial growth well 502 with the diluted bacterial suspension, the well was sealed by paraffin film to prevent evaporation of the media during the experiment. The package 500 was placed on a 37° C. hotplate 530, and a polystyrene container (not shown) covered the whole package to reduce the temperature gradient near the test setup. After each biofilm growth experiment, the sensor 200 was recalibrated using DI water loading. The thickness of biofilm was measured optically by the distance difference between the focal plane of the sensor surface and the focal plane of the top of any accumulated biofilm.
Results and Discussion
ZnO Film Characterization
The generation of Love mode SAW was confirmed by investigating the lattice orientation of the deposited ZnO thin film, X-ray diffraction (XRD) was employed for crystal structure characterization of the ZnO layer after PLD deposition on a SiO2/Si substrate by measuring the diffraction angle (2θ). The diffraction angles of the in the ZnO film at 34.25° and 72.25°, corresponding to c-axis (002) and (004) lattice orientations, were the most intensive reflections in the PLD prepared ZnO film. This c-axis orientation of ZnO crystal lattice ((00L) direction) was perpendicular to the substrate so that the Love mode of SAW generation was dominant on the surface of the sensor [15-22].
Photoluminescence (PL) spectroscopy was used to investigate the crystal quality of the ZnO film. The peak wavelength of the emitted light was approximately 380 nm, corresponding to the characteristic ZnO bandgap energy (3.3 eV). Therefore, the PL spectroscopy result confirmed that the PLD-prepared ZnO film had a low number of impurities.
Biofilm Cleaning
Consecutive biofilm growth tests using the same device are essential to investigate the reliability and repeatable operation of the SAW sensor. To test the sensor over multiple biofilm growth experiments, surface cleaning after a biofilm growth experiment was crucial for subsequent biofilm growth; cleaning not only sterilized the sensor, but also prevented initial mass loading due to the uncleaned biofilm and the resulting significant loss of sensitivity. Oxygen plasma applied for 30 s at 150 W RF-power was successfully employed to clean any remaining biofilm as shown in
The 45 nm ALD Al2O3 film passivation and oxygen plasma biofilm cleaning method enable SAW sensor 200 to be reusable over consecutive biofilm growth experiments.
Sensor Sensitivity
The sensitivity and detection limit of the SAW sensor were studied and calculated by loading 10 μl of DI water on the sensor and monitoring the magnitude of the resonant frequency shift. After loading 10 si of DI water, the resonant frequency shift of the SAW sensor was measured to be about 188 KHz by the network analyzer. Hence, the sensitivity of the sensor was 1.88×1010 Hz/g. Based on the network analyzer resolution (0.1 Hz), the detection limit of the sensor (resolution/sensitivity) was approximately 5.3 pg (picograms). Since the mass of a bacterium is known to be approximately 1 pg [44], this detection limit validates the SAW sensor application for bacterial biofilm monitoring.
Biofilm Growth Experiments in the SAW Sensor
The resonant frequency shift results of the SAW sensor due to the biofilm growth in LB media and in 10% PBS are shown in
In nature, bacterial growth in hatch culture begins with a lag phase where bacteria are not dividing but are actively adapting to the culture conditions. After this period, bacteria divide at a fast rate during the exponential phase of growth. Eventually, once the reactor contains a high population density and a limited supply of nutrients, the culture reaches stationary phase [45].
As shown in Table 1, the detection limit of the sensor changed minimally after consecutive biofilm growth experiments, demonstrating excellent sensitivity recovery of the sensor. Therefore, the large variance in the final resonant frequency shift seen in LB media is not a result of sensor degradation, but can be due to non-uniform growth of the biofilm based on the results shown in
The standard deviation of the measured biofilm thickness in LB media (62 μm, about 46% of the average biofilm thickness) was significantly more than the standard deviation in 10% FBS (6.4 μm, about 20% of average biofilm thickness).
These results correspond to the large growth variance in LB media measured by the resonant frequency shift of the SAW sensor. Based on these experimental biofilm growth variance results and the sensitivity characterization work as shown in Table 1, the stationary phase resonant frequency shift variation in LB media in
After biofilm growth experiments in each media, the presence of bacterial biofilm on the SAW sensor was confirmed by optical microscopy as shown images in
As shown by the data, the 45 nm ALD Al2O3 passivated SAW sensor was able to measure biofilm growth repeatably using oxygen plasma cleaning between experiments. The final frequency shift results in LB media were more variable than those in 10% FBS since the composition of the LB media was a more favorable environment to E. coli, thereby indicating non-uniform biofilm growth in each experiment [47]. The observed SAW sensor outputs in both media followed the same growth trends. Moreover, the 10% FBS results suggest that the SAW sensor can be applied to in vivo biofilm detection in the future. Since the FBS is composed of blood proteins and plasma, the serum can be used to mimic an in vivo environment. The resonant frequency shift results of the SAW sensor in 10% HIS are more repeatable than results in LB media, rendering reliable operation of the sensor in an in vivo environment more likely. The effective passivation of the sensor using an ALD Al2O3 film also contributed to reliable sensing in 10% FBS.
The results indicated by
In view of the foregoing description, those skilled in the art will understand and appreciate that a novel ALD Al2O3 film passivated SAW sensor for real time biofilm monitoring has been successfully demonstrated. A high quality c-axis oriented ZnO film was deposited by PLD, and the sensor was effectively passivated by 45 nm of Al2O3 film using ALD to prevent ZnO damage in the bacterial growth media and animal serum. For the reliable passivation of the ZnO SAW sensor, ALD was an important fabrication method based on its highly dense and conformal film deposition capabilities. The SAW sensor can be reused after oxygen plasma cleaning, allowing for consecutive biofilm formation experiments using one sensor. The detection limit of the SAW sensor was approximately 5.3 pg. The resonant frequency shift results of the SAW sensor followed natural bacterial biofilm growth properties not only in LB media which provided a favorable bacterial growth environment, but also in 10% FBS as a simulated in vivo environment. These results validate the application of the SAW sensor for real-time bacterial growth monitoring.
This SAW sensor 600 combined with RF wireless communication techniques can be used to detect in vivo biofilm growth, which is the groundwork for developing an implantable sensor for early biofilm detection and prevention of major infections.
Although the present disclosure has been described in considerable detail with reference to certain preferred version thereof, other versions are possible and contemplated. Therefore, the spirit and scope of the appended claims should not be limited to the description of the preferred versions contained therein.
Any element in a claim that does not explicitly state “means for” performing a specified function or “step for” performing a specified function, is not to be interpreted as a “means” or “step” clause as specified in 35 U.S.C. §112, ¶6. In particular, the use of “step of” in the claims is not intended to invoke the provisions of 35 U.S.C. §112, ¶6.
While several embodiments of the disclosure have been shown in the drawings, it is not intended that the disclosure be limited thereto, as it is intended that the disclosure be as broad in scope as the art will allow and that the specification be read likewise. Therefore, the above description should not be construed as limiting, but merely as exemplifications of particular embodiments. Those skilled in the art will envision other modifications within the scope of the claims appended hereto.
In the claims, any reference signs placed between parentheses shall not be construed as limiting the claim. The word “comprising” does not exclude the presence of elements or steps other than those listed in a claim. The word “a” or “an” preceding an element does not exclude the presence of a plurality of such elements. The embodiments of the present disclosure may be implemented by means of hardware comprising several distinct elements, and/or by means of a suitably programmed processor. In the device claim enumerating several means, several of these means may be embodied by one and the same item of hardware. The mere fact that certain measures are recited in mutually different dependent claims does not indicate that a combination of these measures cannot be used to advantage.
The entire contents and teachings of the following references are incorporated herein by reference.
These references are identified as source documents for the particular portion of the foregoing description by indication of the number or numbers in parentheses [1]-[47] corresponding to one or more of the references below.
This application claims the benefit of, and priority to, U.S. Provisional Patent Application Ser. No. 61/753,332, filed on Jan. 16, 2013, entitled “ALD Passivated Bacterial Biofilm Sensor Using Inverted Surface. Acoustic Wave” by Young Wook Kim et al., the entire contents of which is hereby incorporated by reference herein.
This invention was made with U.S. government support under EFRI1042881 awarded by the National Science Foundation. The U.S. government has certain rights in the invention.
Number | Date | Country | |
---|---|---|---|
61753332 | Jan 2013 | US |