The present application is a national phase entry under 35 U.S.C. § 371 of the International Application No. PCT/KR2022/001335, filed on Jan. 25, 2022, which claims the benefit of Korean Patent Application No. 10-2021-0012231 filed on Jan. 28, 2021, all of which are incorporated herein by reference in their entireties.
The present disclosure relates to a battery cell and a battery cell manufacturing apparatus, and more particularly, to a battery cell with improved external emission of gas generated inside the battery cell, and a battery cell manufacturing apparatus.
As technology development and demand for mobile devices increase, the demand for secondary batteries as an energy source is rapidly increasing. In particular, secondary batteries are of great interest as energy sources not only for mobile devices such as mobile phones, digital cameras, notebooks and wearable devices, but also for power devices such as electric bicycles, electric vehicles and hybrid electric vehicles.
Depending on the shape of a battery case, these secondary batteries are classified into a cylindrical battery and a prismatic battery in which a battery assembly is included in a cylindrical or prismatic metal can, and a pouch-type battery in which the battery assembly is included in a pouch-type case of an aluminum laminate sheet. Here, the battery assembly included in the battery case is a power element including a positive electrode, a negative electrode, and a separator interposed between the positive electrode and the negative electrode, and capable of charging and discharging, and is classified into a jelly-roll type in which long sheet-type positive and negative electrodes coated with an active material are wound with a separator being interposed therebetween, and a stack type in which a plurality of positive and negative electrodes are sequentially stacked with a separator being interposed therebetween.
Among them, in particular, a pouch-type battery in which a stack-type or stack/folding-type battery assembly is included in a pouch-type battery case made of an aluminum laminate sheet is being used more and more due to low manufacturing cost, small weight, and easy modification.
However, as the energy density of the battery cell increases in recent years, there is a problem that the amount of gas generated inside the battery cell also increases. In the case of the conventional battery cell 10, a component capable of discharging the gas generated inside the battery cell is not included, so a venting may occur in the battery cell due to gas generation. In addition, moisture may penetrate into the battery cell damaged by the venting, which may cause side reactions, and there is a problem that battery performance deteriorates and additional gas is generated. Accordingly, there is an increasing need to develop a battery cell with improved external emission of gas generated inside the battery cell.
The present disclosure is directed to providing a battery cell with improved external emission of gas generated inside the battery cell, and a battery cell manufacturing apparatus.
The object to be solved by the present disclosure is not limited to the above-mentioned object, and the objects not mentioned here may be clearly understood by those skilled in the art from this specification and the accompanying drawings.
In one aspect of the present disclosure, there is provided a battery cell, comprising: a battery case having an accommodation portion in which an electrode assembly is mounted, and a sealing portion formed by sealing an outer periphery thereof; an electrode lead electrically connected to an electrode tab included in the electrode assembly and protruding out of the battery case via the sealing portion; and a lead film located at a portion corresponding to the sealing portion in at least one of an upper portion and a lower portion of the electrode lead, wherein the lead film has a dented portion that is recessed in an inner direction of the battery case, the dented portion is opened toward the outside of the battery case, the sealing portion located on a gas inlet portion of the dented portion has a recessed sealing portion that is recessed outward from an inner side of the battery case, and the recessed sealing portion does not overlap with at least a part of the gas inlet portion on a plane.
The gas inlet portion of the dented portion may be exposed to the inside of the battery case.
The dented portion may include a first dented portion and a second dented portion, the first dented portion may extend along a protruding direction of the electrode lead, and the second dented portion may extend along a length direction of the sealing portion.
One end of the first dented portion may be opened toward the outside of the battery case, and the other end of the first dented portion may communicate with the second dented portion.
The recessed sealing portion may be located on the second dented portion.
The recessed sealing portion may extend along a length direction of the second dented portion.
A length of the recessed sealing portion may be equal to or greater than a length of the second dented portion.
A width of the recessed sealing portion may be equal to or greater than a width of the second dented portion.
The lead film may have gas permeability of 20 Barrer to 60 Barrer at 60° C.
The lead film may have a moisture penetration amount of 0.02 g to 0.2 g for 10 years at 25° C., 50% RH.
The lead film may contain a polyolefin-based material.
An air ventilation layer may be inserted into the dented portion, and the air ventilation layer may have a material with higher air ventilation than the lead film.
The air ventilation layer may have a thickness of 50 μm to 150 μm.
The air ventilation layer may have gas permeability of 1.6 e5 Barrer to 1.6 e7 Barrer.
The air ventilation layer may include a polyolefin-based resin, a fluorine-based resin, a natural material, a glass fiber, a ceramic fiber, a metal fiber, or two or more thereof.
The lead film and the electrode tab may be spaced apart from each other.
The lead film may further include an inner layer configured to cover at least one of inner surfaces of the dented portion.
A material of the inner layer may have a higher melting point compared to a material of the lead film and may not react with an electrolytic solution.
The inner layer may contain at least one of polyolefin-based materials, fluorine-based materials and porous ceramic-based materials.
Based on a protruding direction of the electrode lead, a width of the lead film surrounding a rear surface of the dented portion may be 2 mm or more.
A thickness of the lead film surrounding an upper surface of the dented portion may be 100 μm to 300 μm.
In another aspect of the present disclosure, there is also provided a battery cell manufacturing apparatus for manufacturing the battery cell described above, comprising: a first sealing tool in which a first sealing surface and a recessed surface are formed, wherein the recessed surface is configured to seal the battery case on at least a part of the gas inlet portion of the dented portion, and the first sealing surface is configured to seal the battery case on the dented portion except for a region sealed by the recessed surface.
The first sealing tool may include a first sealing surface, a recessed surface and a first inclined surface.
The battery cell manufacturing apparatus may further comprise a second sealing tool in which a second sealing surface is formed, and the second sealing surface may be configured to seal the battery case except for a region on the dented portion.
The second sealing tool may include a second sealing surface and a second inclined surface.
A length of the first sealing surface may be shorter than a length of the second sealing surface.
A length of the first sealing surface may extend along a length direction of the dented portion.
A width of the first sealing surface may extend along a width direction of the dented portion.
The first sealing tool and the second sealing tool may be integrated with each other.
According to the embodiments, the present disclosure provides a battery cell, which includes an electrode lead to which a lead film having a dented portion dented inward and opened toward the outside of the battery case is formed, and an apparatus for manufacturing the battery cell, thereby improving the external emission of gas generated inside the battery cell.
In addition, according to the embodiments, in the present disclosure, the sealing portion located on the gas inlet portion of the dented portion includes a recessed sealing portion that is recessed from the inside to the outside of the battery case and does not overlap with at least a part of the gas inlet portion on a plane, thereby improving the external emission of gas generated inside the battery cell.
The effect of the present disclosure is not limited to the above effects, and the effects not mentioned here will be clearly understood by those skilled in the art from this specification and the accompanying drawings.
Hereinafter, with reference to the accompanying drawings, various embodiments of the present disclosure will be described in detail so as to be easily implemented by those skilled in the art. The present disclosure may be implemented in various different forms and is not limited to the embodiments described herein.
In order to clearly explain the present disclosure, parts irrelevant to the description are omitted, and identical or similar components are endowed with the same reference signs throughout the specification.
In addition, since the size and thickness of each component shown in the drawings are arbitrarily expressed for convenience of description, the present disclosure is not necessarily limited to the drawings. In order to clearly express various layers and regions in the drawings, the thicknesses are enlarged. Also, in the drawings, for convenience of explanation, the thickness of some layers and regions is exaggerated.
In addition, when a part of a layer, a film, a region, a plate, or the like is explained to be “over” or “on” another part, this includes not only the case where it is “directly on” another part, but also the case where still another part is provided therebetween. Conversely, when a part is explained to be “right on” another part, it means that there is no other part therebetween. In addition, when a part is explained to be “over” or “on” a reference part, this means that the part is located on or below the reference part, and it does not mean that the part is located “over” or “on” the reference part in a direction opposite to gravity.
In addition, throughout the specification, when a part “includes” a certain component, it means that other components may be further included, rather than excluding other components, unless otherwise stated.
In addition, throughout the specification, when referring to “top view”, it means that the target part is viewed from above, and when referring to “cross-sectional view”, it means that a vertically-cut section of the target part is viewed from a side.
Hereinafter, a pouch battery cell 100 according to an embodiment of the present disclosure will be described. However, here, the description will be made based on one side surface of both side surfaces of the pouch battery cell 100, but it is not necessarily limited thereto, and the same or similar contents may be described in the case of the other side surface.
Referring to
The battery case 200 includes an accommodation portion 210 in which an electrode assembly 110 is mounted, and a sealing portion 250 formed by sealing an outer periphery thereof. The sealing portion 250 may be sealed by heat, laser, or the like. The battery case 200 may be a laminate sheet including a resin layer and a metal layer. More specifically, the battery case 200 may be made of a laminate sheet, and may include an outer resin layer forming the outermost layer, a barrier metal layer preventing penetration of materials, and an inner resin layer for sealing.
Also, the electrode assembly 110 may have a structure of a jelly-roll type (winding type), a stack type (lamination type), or a composite type (stack/folding type). More specifically, the electrode assembly 110 may include a positive electrode, a negative electrode, and a separator disposed therebetween.
Hereinafter, the electrode lead 300 and the lead film 400 will be mainly described.
Referring to
Referring to
In addition, referring to
For example, referring to
Accordingly, even if the lead film 400 is sealed together with the sealing portion 250 in a state of being located in at least one of the upper and lower portions of the electrode lead 300, the dented portion 450 may be preserved in a non-sealed state by the inner layer 410.
As another example, referring to
Accordingly, while the lead film 400 minimizes the inner layer 410 formed in the dented portion 450, the dented portion 450 may be preserved in a non-sealed state by the inner layer 410. In addition, the manufacturing process may be simplified and the cost may be reduced.
More specifically, the inner layer 410 may be made of a material having a higher melting point compared to the material constituting the lead film 400. In addition, the inner layer 410 may be made of a material that does not react with the electrolytic solution contained in the battery case 200. Accordingly, since the inner layer 410 is made of the above-described material, the inner layer 410 does not separately react with the electrolytic solution and does not cause heat fusion, thermal deformation, or the like in the high-temperature sealing process, so that the dented portion 450 may be kept blank. In addition, the gas generated in the battery case 200 may be easily discharged to the outside.
In one embodiment of the present disclosure, the thickness of the inner layer 410 may be 100 μm or less.
In one embodiment of the present disclosure, the gas permeability of the inner layer 410 may be 40 Barrer or more. For example, the carbon dioxide permeability of the inner layer 410 may satisfy the above range.
For example, the lead film 400 may include a polyolefin-based material, and the inner layer 410 may include at least one of polyolefin-based materials, fluorine-based materials, and porous ceramic-based materials. For example, the inner layer 410 may include at least one of polyolefin-based materials, fluorine-based materials, and porous ceramic-based materials that satisfies the above gas permeability value. The polyolefin-based material may include at least one material selected from the group consisting of polypropylene, polyethylene, and polyvinyl difluoride (PVDF). The fluorine-based material may include at least one material selected from the group consisting of polytetrafluoroethylene and polyvinylidene fluoride. In addition, the inner layer 410 may include a getter material, so that gas permeability may be increased while water permeability may be minimized As an example, the getter material may be calcium oxide (CaO), barium oxide (BaO), lithium chloride (LiCl), silica (SiO2), or the like, and any material reacting with water (H2O) can be used without being limited thereto.
The inner layer 410 may have an adhesive material between the lead film 400 and the inner layer 410 or may be extruded together with the lead film 400 and adhered to the lead film 400. The adhesive material may include an acryl-based material. In particular, when the inner layer 410 is extruded together with the lead film 400, the gas permeability of the inner layer 410 may be 40 Barrer or more.
Referring to
Accordingly, the lead film 400 may prevent the side surface of the electrode lead 300 from being exposed to the outside, while improving the sealing properties of the sealing portion 250 and the electrode lead 300.
For example, in the lead film 400, the dented portion 450 may be located in at least one of the first lead film and the second lead film. More specifically, in the lead film 400, the dented portion 450 may be formed in the first lead film or the second lead film based on the electrode lead 300, or the dented portion 450 may be formed in both the first lead film and the second lead film based on the electrode lead 300. However, the number of the dented portion 450 is not limited to the above, and the lead film 400 may be formed in an appropriate number.
Accordingly, by adjusting the number of the dented portions 450 formed in the lead film 400, the durability and airtightness of the lead film 400 may be controlled. In addition, by minimizing the number of the dented portion 450 as necessary, it is possible to simplify the manufacturing process and reduce the cost.
In one embodiment of the present disclosure, the gas permeability of the lead film 400 may be 20 Barrer to 60 Barrer, or 30 Barrer to 40 Barrer at 60° C. For example, the carbon dioxide permeability of the lead film 400 may satisfy the above range. In addition, the gas permeability may satisfy the above range at 60° C. based on the thickness of the lead film 400 of 200 μm. If the gas permeability of the lead film 400 satisfies the above range, the gas generated inside the secondary battery may be more effectively discharged.
In this specification, the gas permeability may be measured by ASTM F2476-20.
In one embodiment of the present disclosure, the moisture penetration amount of the lead film 400 may be 0.02 g to 0.2 g, or 0.02 g to 0.04 g, or 0.06 g, or 0.15 g for 10 years at 25° C., 50% RH. If the moisture penetration amount of the lead film 400 satisfies the above range, the penetration of moisture from the lead film 400 may be more effectively prevented.
In this embodiment, the moisture penetration amount may be measured by adopting the ASTM F 1249 method. At this time, the moisture penetration amount may be measured using equipment officially certified by MCOON.
In one embodiment of the present disclosure, the lead film 400 may have a gas permeability of 20 Barrer to 60 Barrer at 60° C. and a moisture penetration amount of 0.02 g to 0.2 g at 25° C., 50% RH for 10 years. If the gas permeability and the moisture penetration amount of the lead film 400 satisfy the above ranges, the penetration of moisture from the outside may be more effectively prevented while discharging the gas generated inside the secondary battery.
In one embodiment of the present disclosure, the lead film 400 may include a polyolefin-based resin. For example, the lead film 400 may include a polyolefin-based resin satisfying the gas permeability and/or moisture penetration amount values described above. The polyolefin-based resin may include at least one material selected from the group consisting of polypropylene, polyethylene, and polyvinyl difluoride (PVDF). While the lead film 400 contains polypropylene, the gas permeability of the lead film 400 may be 20 Barrer to 60 Barrer at 60° C. Also, the moisture penetration amount may be 0.06 g to 0.15 g. In this case, the gas generated inside the secondary battery may be more effectively discharged, and the penetration of moisture from the outside may be easily prevented.
In addition, since the lead film 400 is made of the above-described material, the lead film 400 may maintain the airtightness of the battery cell 100 and prevent leakage of the internal electrolytic solution.
Referring to
In addition, the recessed sealing portion 250H is located on a gas inlet portion of the dented portion 450.
Referring to
Referring to
However, the shape of the dented portion 450 is not limited to the above, and the dented portion 450 may be formed in an appropriate shape within the lead film 400.
Here, one end of the first dented portion 451 may be opened toward the outside of the battery case 200, and the other end of the first dented portion 451 may communicate with the second dented portion 455. More specifically, the first dented portion 451 and the second dented portion 455 may be integrated with each other. That is, the second dented portion 455 may serve as a gas inlet through which the gas generated in the battery case 200 is introduced, and the first dented portion 451 may serve as a gas outlet through which the gas introduced into the second dented portion 455 is discharged to the outside.
Also, referring to
More specifically, the recessed sealing portion 250H may extend along the length direction of the second dented portion 455. Here, the length of the second dented portion 455 means a maximum value of the distance between one end and the other end of the second dented portion 455 in a direction orthogonal to the protruding direction of the electrode lead 300. In addition, the length of the recessed sealing portion 250H may be equal to or greater than the length of the second dented portion 455. Here, the length of the recessed sealing portion 250H means a maximum value of the distance between one end and the other end of the recessed sealing portion 250H in a direction orthogonal to the protruding direction of the electrode lead 300.
In addition, the width of the recessed sealing portion 250H may be equal to or greater than the width of the second dented portion 455. Here, the width of the second dented portion 455 means a maximum value of the distance between one end and the other end of the second dented portion 455 in the protruding direction of the electrode lead 300, and the width of the recessed sealing portion 250H means a maximum value of the distance between one end and the other end of the recessed sealing portion 250H in the protruding direction of the electrode lead 300. However, the size of the recessed sealing portion 250H is not limited to the above, and the recessed sealing portion 250H may be formed in an appropriate size within the lead film 400.
Accordingly, in the lead film 400, the second dented portion 455 on the lead film 400 may not be in contact with the sealing portion 250. In other words, a region of the lead film 400 where the second dented portion 455 is located may avoid interference with the sealing portion 250. Accordingly, the second dented portion 455 may be exposed to the inside of the battery case 200. Since the second dented portion 455 serves as a gas inlet through which the gas generated in the battery case 200 is introduced, the area in which the second dented portion 455 is exposed to the inside of the battery case 200 within the lead film 400 increases, so that gas may be smoothly introduced into the second dented portion 455 from the inside of the battery case 200.
Referring to
For example, as shown in
As another example, as shown in
Accordingly, by adjusting the position of the dented portion 450 formed in the lead film 400, the durability and airtightness of the lead film 400 may be controlled. In addition, if necessary, by adjusting the size of the dented portion 450 according to the position of the dented portion 450, it is possible to simplify the manufacturing process and reduce the cost.
In addition, referring to
Accordingly, it is possible to prevent a step from being created as the lead film 400 and the electrode tab 115 overlap with each other, and it is also possible to prevent poor adhesion performance from occurring due to the step and to prevent the battery cell 100 from being damaged at high pressure.
Referring to
Accordingly, the gas generated inside the battery cell 100 may be discharged toward the dented portion 450, and the gas introduced into the dented portion 450 may be easily discharged toward the outside. In addition, the external emission of gas generated inside the battery cell 100 may also be increased.
In addition, since the dented portion 450 is recessed in the inner direction of the battery case 200 and is opened toward the outside of the battery case 200, the dented portion 450 may not be exposed to the electrolytic solution inside the battery case 200, and airtightness and durability of the pouch may also be secured.
At this time, the recessed end of the dented portion 450 may serve as a gas inlet through which the gas generated in the battery case 200 is introduced, and the end of the dented portion 450 that is open toward the outside of the battery case 200 may serve as a gas outlet through which the gas introduced into the dented portion 450 is discharged to the outside.
Referring to
Referring to
If the sealing portion 250 comes into contact with the gas inlet portion when the gas generated in the battery case 200 flows into the dented portion 450, the inflow of gas from the inside of the battery case 200 into the dented portion 450 may be disturbed by the sealing portion 250. Accordingly, there is a problem in that the amount of gas flowing into the dented portion 450 is greatly reduced. For example, in the lead film 400, the gas inside the battery case 200 may be introduced into the dented portion 450 due to gas permeation on the lead film at the upper surface of the recessed end of the dented portion 450. Here, if the lead film on the upper surface of the recessed end of the dented portion 450 comes into contact with the sealing portion 250, the inflow of gas from the inside of the battery case 200 into the dented portion 450 may be disturbed by the sealing portion 250.
Referring to
In addition, in the lead film 400, the gas inlet portion of the dented portion 450 may be exposed to the inside of the battery case 200. In this specification, the inside of the battery case 200 means a space in the inner direction of the battery case 200 rather than the end of the sealing portion 250 at the inner side of the battery case. That is, in the lead film 400, since the area in which the gas inlet portion of the dented portion 450 is exposed to the inside of the battery case 200 is increased, gas may be smoothly introduced into the dented portion 450 from the inside of the battery case 200.
Referring to
For example, the air ventilation layer 500 may include a material that is more porous than the lead film 400. That is, the air ventilation layer 500 may include a material having a higher ratio of pores per unit volume than the lead film 400.
In one embodiment of the present disclosure, the gas permeability of the air ventilation layer 500 may be 1.6 e5 Barrer to 1.6 e7 Barrer, or 1 e6 Barrer to 3 e6 Barrer. For example, the carbon dioxide permeability of the air ventilation layer 500 may satisfy the above range.
In one embodiment of the present disclosure, the air ventilation layer 500 may include at least one material selected from the group consisting of a polyolefin-based resin, a fluorine-based resin, a natural material, a glass fiber, a ceramic fiber, and a metal fiber. For example, the air ventilation layer 500 may include at least one material selected from the group consisting of a polyolefin-based resin, a fluorine-based resin, a natural material, glass fiber, a ceramic fiber, and a metal fiber that satisfy the gas permeability described. The polyolefin-based resin may include at least one material selected from the group consisting of polypropylene, polyethylene, and polyvinyl difluoride (PVDF). The fluorine-based resin may include at least one material selected from the group consisting of polytetrafluoroethylene and polyvinylidene fluoride, and the natural material may include at least one material selected from the group consisting of cotton and wool.
In one embodiment of the present disclosure, the thickness of the air ventilation layer 500 may be 50 μm to 150 μm, or 50 μm to 100 μm. If the thickness of the air ventilation layer 500 satisfies the above range, the gas inside the battery case 200 may be more easily discharged to the outside of the battery case 200.
Referring to
The recessed surface 1050H seals the battery case 200 on at least a part of the gas inlet portion of the dented portion 450. Accordingly, the recessed sealing portion 250H may be formed.
The first sealing surface 1050 seals the battery case 200 on the dented portion 450 except for the region sealed by the recessed surface 1050H.
By using the first sealing tool 1000, it is possible to form the recessed sealing portion 250H by the recessed surface 1050H while maintaining the sealing property or adhesion performance between the sealing portion 250 and the lead film 400. The shape of the recessed surface 1050H is not limited thereto, and the recessed surface 1050H may have a structure recessed in a rectangular shape, a semi-circular shape, or the like having a size capable of maintaining the sealing property of the battery case 200.
In one embodiment of the present disclosure, the length of the first sealing surface 1050 may extend along the length direction of the dented portion 450. However, the first sealing surface 1050 does not extend to the gas inlet portion of the dented portion 450. Here, the length of the first sealing surface 1050 means a maximum value of the distance between one end and the other end of the first sealing surface 1050 in the protruding direction of the electrode lead 300, and the length of the dented portion 450 means a maximum value of the distance between one end and the other end of the dented portion 450 in the protruding direction of the electrode lead 300.
In addition, the width of the first sealing surface 1050 may extend along the width direction of the dented portion 450. Here, the width of the first sealing surface 1050 means a maximum value of the distance between one end and the other end of the first sealing surface 1050 in a direction orthogonal to the protruding direction of the electrode lead 300, and the width of the dented portion 450 means a maximum value of the distance between one end and the other end of the dented portion 450 in a direction orthogonal to the protruding direction of the electrode lead 300. The width of the first sealing surface 1050 may be equal to or greater than the width of the dented portion 450.
Referring to
Referring to
Referring to
The second sealing surface 2050 seals the battery case 200 except for the region on the dented portion 450. Accordingly, even if the dented portion 450 is located in the lead film 400, a portion of the lead film 400 where the dented portion 450 is not located and the sealing portion 250 may be sealed with each other, so that the sealing force of the battery case 200 may be improved by the second sealing tool 2000.
In one embodiment of the present disclosure, the length of the first sealing surface 1050 may be shorter than the length of the second sealing surface 2050. That is, the length of the sealing portion 250 formed by the first sealing surface 1050 may be shorter than the length of the sealing portion 250 formed by the second sealing surface 2050. Accordingly, the sealing portion 250 is not positioned on the gas inlet portion of the dented portion 450, so that gas may be smoothly introduced into the dented portion 450 from the inside of the battery case 200.
Referring to
In one embodiment of the present disclosure, the inclination angle of the first inclined surface 1010 may be identical or similar to the inclination angle of the second inclined surface 2010. Accordingly, the inclination angles of the outer surfaces of the accommodation portion 210 respectively in contact with the first inclined surface 1010 and the second inclined surface 2010 may be identical or similar to each other.
In one embodiment of the present disclosure, the first sealing tool 1000 and the second sealing tool 2000 may be integrated with each other. For example, the first sealing tool 1000 and the pair of second sealing tools 2000 are integrated, and the first sealing tool 1000 may be located between the pair of second sealing tools 2000. Here, depending on the position of the dented portion 450, the pair of second sealing tools 2000 may have the same width or different widths.
Accordingly, depending on the position of the dented portion 450, the first sealing tool 1000 and the second sealing tool 2000 are integrated, thereby simplifying the manufacturing process of the battery cell 100 and reducing the cost.
Referring to
More specifically, in the first upper sealing tool 1100, the upper recessed surface 1150H may be located on at least a part of the gas inlet portion of the dented portion 450, and the first upper sealing surface 1150 may be located on the battery case 200 on the dented portion 450 except for the region sealed by the upper recessed surface 1150H. That is, the upper recessed surface 1150H may be in contact with the outer surface of the accommodation portion 210 to form the recessed sealing portion 250H on the lead film in which the gas inlet portion of the dented portion 450 is positioned. In addition, the first upper sealing surface 1150 may be in contact with the sealing portion 250 to seal the battery case 200.
For example, when the dented portion 450 includes the first dented portion 451 and the second dented portion 455 as shown in
In addition, the widths of the first upper sealing surface 1150 and the upper recessed surface 1150H may extend along the length direction of the second dented portion 455. Here, the width of the first upper sealing surface 1150 means a maximum value of the distance between one end and the other end of the first upper sealing surface 1150 in a direction orthogonal to the protruding direction of the electrode lead 300, and the width of the upper recessed surface 1150H means a maximum value of the distance between one end and the other end of the upper recessed surface 1150H in a direction orthogonal to the protruding direction of the electrode lead 300.
Accordingly, in the manufacturing apparatus according to the present embodiment, the recessed sealing portion 250H may be formed on the region where the gas inlet of the dented portion 450 is located, by the first sealing tool 1000. Accordingly, gas may be smoothly introduced into the dented portion 450 from the inside of the battery case 200.
Referring to
More specifically, in the second upper sealing tool 2100, the second upper sealing surface 2150 may be located on the region of the sealing portion 250 where the dented portion 450 is not located. That is, in the second sealing tool 2000, the second sealing surface 2050 may be located on the battery case 200 except for the region on the dented portion 450 based on the lead film 400, so that the lead film 400 and the sealing portion 250 may be sealed.
Accordingly, even if the dented portion 450 is located in the lead film 400, the region of the lead film 400 where the dented portion 450 is not located and the sealing portion 250 may be sealed with each other, so that the sealing force of the battery case 200 may be improved by the second sealing tool 2000.
A battery module according to another embodiment of the present disclosure includes the battery cell described above. Meanwhile, one or more battery modules according to this embodiment may be packaged in a pack case to form a battery pack.
The battery module described above and the battery pack including the same may be applied to various devices. These devices may be transportation means such as electric bicycles, electric vehicles, hybrid electric vehicles, and the like, but the present disclosure is not limited thereto, and the present disclosure may be applied various devices that can use a battery module and a battery pack including the same, which is also within the scope of the right of the present disclosure.
Although the preferred embodiment of the present disclosure has been described in detail above, the scope of the right of the present disclosure is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present disclosure defined in the appended claims also fall within the scope of the right of the present disclosure.
Number | Date | Country | Kind |
---|---|---|---|
10-2021-0012231 | Jan 2021 | KR | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/KR2022/001335 | 1/25/2022 | WO |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2022/164182 | 8/4/2022 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
20060238162 | Cheon et al. | Oct 2006 | A1 |
20140199581 | Ryu et al. | Jul 2014 | A1 |
20160315301 | Kim et al. | Oct 2016 | A1 |
20180114955 | Robert et al. | Apr 2018 | A1 |
20180114964 | Kim et al. | Apr 2018 | A1 |
20200028128 | Hwang et al. | Jan 2020 | A1 |
20200321577 | Kim et al. | Oct 2020 | A1 |
20210074977 | Ko et al. | Mar 2021 | A1 |
Number | Date | Country |
---|---|---|
107968167 | Apr 2018 | CN |
111656570 | Sep 2020 | CN |
S58-046824 | Oct 1983 | JP |
S61063761 | Apr 1986 | JP |
2009-146812 | Jul 2009 | JP |
2012-089532 | May 2012 | JP |
2015-510240 | Apr 2015 | JP |
2018525804 | Sep 2018 | JP |
2020-509553 | Mar 2020 | JP |
100684724 | Feb 2007 | KR |
101011807 | Feb 2011 | KR |
20130014253 | Feb 2013 | KR |
20140087773 | Jul 2014 | KR |
20150062688 | Jun 2015 | KR |
20160126157 | Nov 2016 | KR |
20170027150 | Mar 2017 | KR |
20170096852 | Aug 2017 | KR |
20190022196 | Mar 2019 | KR |
20190123059 | Oct 2019 | KR |
Entry |
---|
International Search Report for PCT/KR2022/001335 dated May 18, 2022. 3 pgs. |
Search Report dated Sep. 18, 2023 from the Office Action for Chinese Application No. 202280003343.6 issued Sep. 21, 2023, pp. 1-2. [See p. 1, categorizing the cited references]. |
Number | Date | Country | |
---|---|---|---|
20230187748 A1 | Jun 2023 | US |