This application claims priority to German Patent Application DE102007022468.2 filed May 8, 2007, the entirety of which is incorporated by reference herein.
This invention relates to a bore serration for locking externally serrated threaded inserts against rotation, with the external serration comprising several teeth, and more particularly, for use with components made of hard, brittle materials.
It is generally known to provide threaded connections on a component, for example a casing, by use of a threaded insert retained in a bore. In the case of damage to the thread, the threaded insert can then simply be replaced, with the same thread size being applied again. In order to lock the threaded insert against rotation, an internal serration (a bore serration of star-type configuration to match and engage a conformal external serration of the threaded insert), is produced in the respective bore of the component by gradual penetration of a wobble (rotary) broaching tool. However, production of the bore serration is problematic with hard materials—such as Inconel 718 or titanium aluminide, as used, for example, in engine manufacture—in that surface damage and cracking may occur in the component and, moreover, the tool itself is stressed to such an extent that the serration is incomplete or, at least, its dimensional accuracy is not ensured, with the tool being subject to severe wear, so that it has to be replaced after only one application. When producing the bore serration by wobble (rotary) broaching, chipping may occur at the bottom end of the serrated bore. If a chip gets lodged in the thread, it must be removed with considerable effort, again with the hazard of crack formation. Production of the serration by special casting methods is also to be ruled out due to the crack-initiating effect of the casting structure and the resultant negative consequences on service-life.
The present invention, in a broad aspect, provides for completeness and dimensional accuracy of the bore serration produced in components made of hard, brittle materials to lock the threaded inserts against rotation, while avoiding damage to the workpiece and ensuring low wear of the tool.
The essence of the present invention is that the bore serration has arcuate recesses produced by plunge or circumferential surface milling, with each recess being positively engaged by at least two teeth of the threaded insert. The arcuate serration is also producible in hard, brittle materials, for example titanium aluminide as used in engine manufacture, with high dimensional accuracy and without damaging the workpiece and, compared to the known wobbling process, with low wear of the tool.
The arcuate serration can preferably be provided such that up to four teeth of the threaded insert engage one arcuate recess each. If the number of teeth is not an integral multiple of the recesses, at least one of the recesses can be widened or narrowed such that the number of teeth of the threaded insert, which positively engage the arcuate serration, is maximised. The bottom end of the arcuate recesses is provided with preferably radially arcuate runout.
The arcuate serration according to the present invention is advantageously applicable to components made of hard materials and high-temperature resistant alloys and to thin-walled threaded inserts as used in engine manufacture.
The present invention is more fully described in the light of the accompanying drawing showing a preferred embodiment. On the drawing,
A casing 1 made of titanium aluminide is provided with a bore 2 into which a standard threaded insert 3 is fitted. The threaded insert 3 has a serration 4 with an even number of teeth 5 on the outer circumference and an internal thread 6. In a partial area of the bore 2, arcuate recesses 7 are provided on the inner circumference which are dimensioned such that two teeth 5 each engage one recess 7 and the outer flanks 8 of the two adjacent teeth 5 at least partly locate on the arcuate surface of the respective recess 7. As shown in
The arcuate serration 10, including arcuate recesses 7 rowed up on the inner surface of the bore 2 and provided with an arcuate runout 9 at the bottom (radiused arcuate internal edge), is producible with high dimensional accuracy in the brittle, hard material used here by plunge milling without surface damage or crack formation. The arcuate recesses can be milled in one or several passes of a single cutter or a plurality of cutters. The arcuate recesses can also be electrochemical machined or machined in other manners. Chipping, with the resultant negative consequences, will not occur. For the first time, thin-walled threaded inserts can be inserted in components made of brittle materials, such as titanium aluminide, with these inserts being safely retained in the arcuate serration and with adequate service-life being ensured.
If the number of teeth of the threaded insert is odd, one of the arcuate recesses is dimensioned such that it can accommodate three teeth. Basically, the arcuate recess 7 can also accommodate three or four adjacent teeth 5.
1 Casing, component
2 Bore in 1
3 Threaded insert
4 Serration of 3
5 Teeth of 4
6 Internal thread of 3
7 Arcuate recess
8 Outer flanks of 5
9 Arcuate runout of 7 (radiused edge)
10 Arcuate serration in 2
Number | Date | Country | Kind |
---|---|---|---|
10 2007 022 468 | May 2007 | DE | national |
Number | Name | Date | Kind |
---|---|---|---|
2490594 | Madden | Dec 1949 | A |
4210372 | McGee et al. | Jul 1980 | A |
6017177 | Lanham | Jan 2000 | A |
20020021948 | Stumpf et al. | Feb 2002 | A1 |
Number | Date | Country |
---|---|---|
4 77 633 | Aug 1969 | CH |
87 03 981 | Apr 1987 | DE |
0 080 558 | Jun 1983 | EP |
1 134 439 | Sep 2001 | EP |
Number | Date | Country | |
---|---|---|---|
20080279652 A1 | Nov 2008 | US |