Claims
- 1. A cement composition for cementing in a well penetrating subterranean formations and having an aqueous drilling fluid containing at least one cement retarder comprising:
- a major proportion of the drilling fluid from the well as it was drilled said fluid having a density in the range of about 9.0-18.0 ppg;
- water;
- a lesser proportion of dry cementitious material;
- About 0.5 to about 10.0 ppb. of a dispersant selected from the group consisting of sulfonated styrene maleic anhydride, sulfonated styrene imide, and sulfonate styrene itaconic acid; and
- a compatible accelerator selected from the group consisting of acetic acid; the first 4 carbon esters thereof; acetamide; monoethanolamine; and diethanolamine.
- 2. The composition of claim 1 wherein said dispersant is provided in a quantity of less than about 5.0 ppb.
- 3. The composition of claim 1 wherein said cementitious material of claim 1 comprises of Portland cement.
- 4. The composition of claim 3 wherein said Portland cement is provided in a concentration within the range of about 100 ppb. to about 600 ppb.
- 5. The composition of claim 1 wherein said accelerator is selected from a group consisting of methyl acetate, ethyl acetate, isopropyl acetate, normal propyl acetate, normal butyl acetate, iso-butyl acetate; tertiary butyl acetate; monoethanolamine and diethanolamine.
- 6. A cement composition for cementing space in a wellbore wherein said space is occupied by drilling fluid prior to displacement of said drilling fluid by said cement composition, said cement composition comprising:
- a quantity of a water based drilling fluid said fluid having a density in the range of about 9.0-18.0 ppg;
- Portland cement in the range of concentration of from 100 pounds per original 42 U.S. gallon barrel of drilling fluid (ppb) to about 600 ppb;
- about 0.5 to about 10.0 ppb of a dispersant comprising a material selected from the group consisting of sulfonated styrene maleic anhydride, sulfonated styrene imide, and sulfonate styrene itaconic acid;
- a calcium sulfate hemihydrate in the range of about 10.0 ppb to about 50.0 ppb;
- an accelerator selected from the group consisting of acetic acid, first four carbon esters of acetic acid, acetamide; monoethanolamine and diethanolamine; and
- finely ground silica in the amount of up to 100 percent by weight of the Portland cement.
Parent Case Info
This application is a division of application Ser. No. 07/556,011 U.S. Pat. No. 5,038,863, filed 7/20/90.