Flexible pipes currently used in offshore oil and gas fields for the transport of fluids underwater between the subsea wellhead and the surface facilities are designed to retain a circular cross-section when subject to external hydrostatic pressure. This is usually achieved by the inclusion of metallic layers which extend around and support a polymer fluid barrier layer and which resists collapsing under the external hydrostatic pressure. However, for deep water applications, the strength and the weight of the metallic layers required to resist collapse becomes a limiting factor in flexible pipe design.
Also, in these designs the innermost barrier layer is designed to contain the fluid or gas. Thus, when the pipe collapses or is squashed, the barrier wall will experience excessive localized over-bending, which can cause structural damage to the barrier layer and result in failure of the pipe.
Therefore, what is needed is a flexible pipe that can tolerate relatively high hydrostatic pressure yet eliminate the disadvantages of the metallic layers discussed above while avoiding potential structural damage to the barrier layer.
Referring to
The barrier layer 12 can be fabricated from a material that has reasonable ductility and elasticity such as a plastic or elastic polymer. The material forming the inner layer 14 can also be a plastic or elastic polymer, and preferably is selected so that it has sufficient ductility to survive after being subjected to large strain levels a number of times, and sufficient elasticity to tend to recover from a collapsed state when the pipe is repressurized.
The wall thickness of the inner layer 14 relative to the wall thickness of the layer 12 is selected so that damage to the barrier layer 12 is prevented when both the barrier layer and the inner layer are collapsed in response to a hydrostatic load placed on the pipe. For example, and assuming the layers 12 and 14 are fabricated from a polymer material as discussed above, their relatively thicknesses are selected so that, when the pipe 10 collapses under a hydrostatic load, a maximum strain on the layer 12 will occur that is no greater than approximately 7% which is below the value that will cause damage to the barrier layer for most polymer material. Thus, the thickness of the inner layer 14 relative to the thickness of the layer 12 is selected to limit the bending of the outer layer to within safe levels of strain. In this context, it is understood that the thickness of the inner layer 14 relative to the barrier layer 12 can vary from a value in which the former is less or greater than the latter based on the relative dimensions of the layer 12 and 14 and the material of the layers. Thus, the relative thicknesses of the layers 12 and 14 shown in the drawing are for the purposes of a non-limitative example only.
If the external pressure acting on the pipe 10 remains sufficiently high after the initial collapse shown in
The collapse of the pipe 10 can also result in small gaps G at two ends of the cross section of the pipe, as shown in
In each of these situations, the inner layer 14 can suffer localized structural damage, such as crazing or localized yielding, especially after several collapses, but this damage will not affect the function of the pipe and can be tolerated. When the inner layer 14 is, in fact, damaged, it functions as a sacrificial layer.
The accumulation of permeated fluid and/or gas in the interface between the barrier layer 12 and inner layer 14 can cause separation between the barrier layer 12 and inner layer 14 prior to collapse of the pipe 10. This separation could result in an undesirable collapse mode other than those shown in
Specifically, a series of small radially-extending and axially and angularly-spaced holes 14a are formed through the inner layer 14 in any known manner, such as by drilling. During operation, the holes 14a will promote the flow of the trapped fluid/gas from the interface F, and into the interior of the inner layer 14 as shown by the solid arrows. This is caused by two effects—a “vacuum” effect due to low pressure at the inner side of the holes 14a which is generated by the flowing fluid/gas inside the inner layer 14 in the direction shown by the dashed arrow, and a “squeezing” effect as the internal flow pressure (with possible external pressure on the outer surface of the inner layer 12) pushes the inner layer 14 and the barrier layer 12 against each other. This flow through the holes 14a avoids separation of the barrier layer 12 and inner layer 14 so that they will thus remain in contact in their designed, abutting, coaxial configuration, thus avoiding the undesirable separation and enabling the pipe 10 to return from its collapsed condition to its normal condition shown in
The pipe 10 thus can tolerate relatively high hydrostatic pressures while eliminating the disadvantages of the metallic layers discussed above and avoiding potential structural damage to the barrier layer. In addition, the pipe 10 can be wound on a storage reel in a collapsed, substantially flat form, an advantage from a storage and transportation standpoint.
The pipe 20 according to an alternate embodiment is shown in
A protective layer 26 extends over the barrier layer 22, a reinforcement layer 28 extends over the protective layer 26 and an additional protective layer 30 extends over the layer 28. Although only one layer 26, 28, and 30 are shown, it is understand that additional layers 26, 28, and 30 can be provided. The protective layers 26 and 30 can be made from plastic or elastic polymer, or plastic or elastic polymer tapes with or without reinforcement fibers. The reinforcement layer(s) can be made from metallic or composite strips with or without interlocking.
The pipe 20 thus enjoys all of the advantages of the pipe 10 and, in addition, enjoys additional protection and reinforcement from the layers 26, 28, and 30.
It is understood that variations may be made in the foregoing without departing from the scope of the invention. For example, the pipe can be provided with one or more protective layers and/or one or more reinforcement layers extending over the outer layer.
The foregoing descriptions of specific embodiments of the present invention have been presented for purposes of illustration and description. They are not intended to be exhaustive or to limit the invention to the precise forms disclosed, and obviously many modifications and variations are possible in light of the above teaching. The embodiments were chosen and described in order to best explain the principles of the invention and its practical application, to thereby enable others skilled in the art to best utilize the invention and various embodiments with various modifications as are suited to the particular use contemplated. It is intended that the scope of the invention be defined by the claims appended hereto and their equivalents.