The present invention relates to a color cathode ray tube and more specifically to a color cathode ray tube in which mechanical stress due to internal pressure made by evacuation is decreased.
The panel 1 comprises faceplate portion and peripheral sidewall portion sealed to the funnel 2. A phosphor screen 4 is formed on the inner surface of the faceplate portion. The phosphor screen 4 is coated by phosphor materials of R, G, and B. A multi-apertured color selection electrode, i.e., shadow mask 3 is mounted to the screen with a predetermined space. The shadow mask 3 is hold by main and sub frames 7 and 8. An electron gun is mounted within the neck 13 to generate and direct electron beams 6 along paths through the mask to the screen.
The shadow mask 3 and the frame 7 constitute a mask-frame assembly. The mask-frame assembly is joined to the panel 1 by means of springs 9.
The cathode ray tube further comprises an inner shield 10 for shielding the tube from external geomagnetism and a reinforcing band 12 attached to the sidewall portion of the panel 10 to prevent the cathode ray tube from being exploded by external shock. The cathode ray tube further comprises external deflection yokes 5 located in the vicinity of the funnel-to-neck junction and a magnet 11 attached to the rear side of the deflection yokes 5 for amending electron bean trajectory.
Process for making the color cathode ray tube comprises generally pre-process and post-process.
During the pre-process, phosphor materials are deposited on the inner surface of the panel.
The post-process comprises further sub processes as follows. Firstly, after the phosphor materials are deposited, sealing process is performed. In the sealing process, a panel to which mask-frame assembly is mounted and a funnel on the inner surface of which frit is deposited is sealed together in a high temperature furnace. Then, evacuating process is performed where electron gun is inserted in the neck. Thereafter, an evacuating and sealing process is performed, in which the cathode ray tube is evacuated and sealed.
Since the cathode ray tube is evacuated, it suffers from high tensile and compressive stress. Therefore, a reinforcing process is conducted where reinforcing band 12 is attached to the panel to distribute the stress over the panel.
In general, when a glass gets a shock from outside, cracks appear in the glass. Tensile stress may hasten increase of the cracks such that the glass may even be broken by the cracks. On the contrary, compressive stress disturbs increase of the cracks. As shown in
Moreover, the cathode ray tube becomes slim recently. As the cathode ray tube becomes slimmer, stress problem becomes more severe. This is because volume of the panel decreases while the degree of vacuum is not changed as the cathode ray tube becomes slimmer.
Further, the cathode ray tube where the funnel portion where yokes are attached are made to have rectangular shape to reduce power consumption suffers larger tensile stress. Those cathode ray tubes are easily broken during heat treatment processes.
In order to reduce the effect of the tensile stress on the funnel glass, heat treatment is conducted for the cathode ray tube to generate compressive stress for increasing shock tolerance. However, those treatments increase manufacturing costs.
An object of the present invention is to provide a cathode ray tube where stress is effectively reduced and shock tolerance is achieved.
According to an aspect of the present invention, a cathode ray tube comprises a panel on inner surface of which a phosphor screen is formed; a funnel joined to the panel; an electron gun generating electron beams; and a deflection yoke which is mounted within the funnel to deflect the electron beams, wherein said panel satisfies a condition: L1+(L2−L1)×0.35≦L≦L1+(L2−L1)×0.45 wherein L1 is distance between inner center P of said panel and yoke line plane; L2 is distance between the inner center P of said panel and neck line plane; and L is distance between the inner center P of said panel and reference line plane.
a and 4b show a diagram for showing stress and deflection angle distribution analysis.
Preferred embodiments of the present invention will be described in a more detailed manner with reference to the drawings.
According to an aspect of the present invention, a cathode ray tube comprises a panel on inner surface of which a phosphor screen is formed; a funnel joined to the panel; an electron gun generating electron beams; and a deflection yoke which is mounted within the funnel to deflect the electron beams, wherein said panel satisfies a condition: L1+(L2−L1)×0.35≦L≦L1+(L2−L1)×0.45 wherein L1 is distance between inner center P of said panel and yoke line plane; L2 is distance between the inner center P of said panel and neck line plane; and L is distance between the inner center P of said panel and reference line plane.
Hereinafter, the cathode ray tube structure is described by utilizing the following names or terminologies.
Deflection axis X means extension line of the central axis of the electron gun through the screen.
Deflection angle means an angle made with the deflection axis X and a line connecting the deflection center C and a diagonal end of the effective screen.
Panel inner center P means intersection of the deflection center C and the inner surface of the panel.
A cross section of the funnel is a horizontal cross section of the funnel sliced along a horizontal plane including the deflection axis X viewing from top.
A seal line plane is a vertical plane which is perpendicular to the deflection axis X and includes a closed line through which the panel and the funnel is sealed together.
A yoke line plane means a vertical plane which is perpendicular to the deflection axis X and includes a boundary line between the body and yoke portions of the funnel.
A neck line plane means a vertical plane which is perpendicular to the deflection axis X and includes a closed line through which the neck portion and the funnel is sealed together.
A reference line plane means a vertical plane which is perpendicular to the deflection axis X and includes the deflection center.
The present invention relates to the structural aspect of the cathode ray tube defined by position of the yoke line plane, the reference line plane, and the neck line plane by which stress is reduced.
Hereinafter, following parameters are used in the description of the present invention.
D is distance between the panel inner center P and the diagonal end of the effective screen.
L1 is distance between inner center P of the panel and the yoke line plane.
L2 is distance between the panel inner center P and the neck line plane.
L is distance between the panel inner center P and the reference line plane.
Table 1 is the result of an experiment where stress was measured across the funnel for various values of L, L1, and L2 according to the present invention and stress values of the prior art.
As shown in Table 1, in the conventional cathode ray tube, deflection angle was 100° and stress was 48.8 MPa. According to the cathode ray tube made by the first parameter sets of the present invention, deflection angle was 120° and stress was 13.4 MPa. According to the first parameter sets, deflection angle was increased while stress was reduced remarkably. Considering the result of the experiment, when following Eqn. 1 is satisfied, L is decreased such that a color cathode ray tube becomes slim, deflection angle is widened, and stress is reduced remarkably.
L1+(L2−L1)×0.35≦L≦L1+(L2−L1)×0.45 Eqn. 1:
Moreover, as shown in Table 1, in the conventional cathode ray tube, L=287.11 mm, D=337.56 mm, and TAN-1(D/L)=0.87. According to the cathode ray tube made by the first parameter sets of the present invention, L=193.71 mm, D=337.56 mm, and TAN-1(D/L)=1.05. According to the cathode ray tube made by the second parameter sets of the present invention, TAN-1(D/L)=1.11. According to the cathode ray tube made by the third parameter sets of the present invention, TAN-1(D/L)=1.16. Therefore, not only limiting L value, but also making TAN-1(D/L)≧1.06. the color cathode ray tube becomes slim, deflection angle is widened, and stress is reduced remarkably.
Further, as shown in Table 1, in the conventional cathode ray tube, deflection angle was 100°. According to the cathode ray tube made by the first parameter sets of the present invention, deflection angle is 120°. According to the cathode ray tube made by the second parameter sets of the present invention, deflection angle is 125°. According to the cathode ray tube made by the third parameter sets of the present invention, deflection angle is 135°. Therefore, not only limiting L value, but also making deflection angle be in the range of 120° to 135°, the color cathode ray tube becomes slim, deflection angle is widened, and stress is reduced remarkably.
a and 4b shows a diagram for showing stress and deflection angle distribution analysis. As shown in
As shown in
Hereinafter, in the cross section of the neck portion, radius of curvature at one outer corner of the cross section is called Rdo. Whereas, radius of curvature at the inner corner of the cross section is called Rdi.
Table 2 is the result of an experiment where stress was measured across the funnel for various values of Rdo and Rdi according to the present invention and stress values of the prior art.
As shown in Table 2, when Rdi/Rdo satisfies Rdi/Rdo≦0.54, stress is reduced remarkably in comparison with the prior art. Therefore, if Rdi/Rdo is maintained 0.54 or below, a cathode ray tube may be provided where stress is remarkably reduced.
Hereinafter, thickness of central panel portion which is intersected by the deflection axis X is defined as a. Thickness of panel at the corner portion is defined as b. Then, b/a is called wedge ratio. According to the present invention, if wedge ratio is no smaller than 1.5, stress is reduced and, additionally, tolerance against shock is increased.
In
Table 3 is the result of an experiment where stress was measured across the panel for various values of CFT, OAH, and SET according to the present invention and stress values of the prior art.
As shown in Table 3, when CFT/SET satisfies CFT/SET≦1.04, stress is remarkably reduced in comparison with the prior art. Thus, if CFT/SET is 1.04 or below, a cathode ray tube may be provided where stress is remarkably reduced.
Moreover, in addition to making CFT/SET to satisfy CFT/SET≦1.04, Rdi/Rdo≦0.54 may further be satisfied. Then, stress is reduced more remarkably.
Further, the every embodiments described hereinabove may be applied to flat type color cathode ray tube where front face surface of panel is substantially flat. Therefore, the effect of the present invention is still effective for the flat type color cathode ray tube.
According to the present invention, a panel and funnel structure is provided which have wide deflection angle and slimmer shape while stress over the funnel is reduced remarkably. Further, the cathode ray tube in accordance with the present invention has larger tolerance against shock in comparison with the prior art.
Number | Date | Country | Kind |
---|---|---|---|
10-2003-0062155 | Sep 2003 | KR | national |
10-2003-0079500 | Nov 2003 | KR | national |