Abstract
This invention relates to a composite panel for a rooftop surface having a core material board having a top surface and a bottom surface with a plurality of openings through said core material board extending from said top surface to said bottom surface; a rigid outer shell of solid material that encapsulates said core material board; a plurality of supports of said solid material wherein each of said plurality of supports extends through one of said plurality of openings in said core material board; and a plurality of legs on a portion of said rigid outer shell covering said bottom surface of core board material.
Description
TECHNICAL FIELD

The present invention relates to composite cement panel for use in a roof deck or similar structure, and a fabricating method of the cement panel.


BACKGROUND ART


FIG. 1 illustrates a typical construction 100 of a cladding construction system of a concrete roof deck 102. A cement sand base 104 is formed over the roof deck 102, the base 104 being screed to form a slope or slope-to-fall gradient to create a drainage fall into a drain 106 and downpipe 108. A waterproof membrane 110 is laid over the cement sand base 104, interrupted only by downpipe 108, and extending a height 112 of 300 mm (0.98 feet) up the inside surface of walls 114. Where the deck 102 meets some walls 114, the transition of the waterproof membrane from the horizontal surface to the vertical surface may be effected by use of waterproof filler such as poly foam 116. A thermal insulating layer 118 is constructed on top of the membrane 110, the layer 118 comprising extruded polystyrene insulation board of 50 mm (2 inches) thickness. A separation fleece layer 120 overlies the thermal insulating layer 118. Finally an overlying protective screed concrete layer 122 of 75 mm (2.9 inches) thickness is provided, comprising 4.5 m (4.9 yards) by 4.5 m (4.9 yards) panels separated by joints filled with bituminous compound. Plastering 124 is applied to walls 114.


The thermal insulating material 118 reduces heat transfer through the concrete roof deck 102 into the building below. The protective cement screed 122 protects the thermal insulating material 118 and the waterproofing membrane 110, and bears the human traffic on the roof deck. Such a construction 100 is constructed in-situ on site, with an expansion joint provided at regular intervals.


Construction 100 suffers from a range of problems. The expansion joints in concrete screed layer 122 are a weak point in the construction and a source of leaks. Residual water becomes lodged between the thermal insulating material 118 and the waterproofing membrane 110 after rain. When exposed to heat from the sun, the water expands and evaporates, exerting pressure on the thermal insulating material 118 which in turn exerts pressure onto the protective screed concrete 122. Both the protective screed concrete 122 and thermal insulating material 118 will generally crack due to such stress, leading to leakage and/or “sickness” in the construction 100.


A further problem is that on site cladding construction makes quality control difficult, can cause damage to the waterproofing system, and is subject to the vagaries of inclement weather during construction leading to time delay. In addition, mixing, handling and/or applying concrete slurry on site can be messy and laborious.


Still further, in the event that maintenance is required to the underlying roof deck 102, waterproofing membrane 110 and/or components of the built-up waterproofing system 104, 118, 120, 122, the protective screed 122 and some or all underlying layers need to be destructively removed such as by being cut away, effectively destroying the construction 100. The entire process of building up the waterproofing system must then be repeated to re-establish a waterproof cladding.


Any discussion of documents, acts, materials, devices, articles or the like which has been included in the present specification is solely for the purpose of providing a context for the present invention. It is not to be taken as an admission that any or all of these matters form part of the prior art base or were common general knowledge in the field relevant to the present invention as it existed before the priority date of each claim of this application.


Throughout this specification the word “comprise”, or variations such as “comprises” or “comprising”, will be understood to imply the inclusion of a stated element, integer or step, or group of elements, integers or steps, but not the exclusion of any other element, integer or step, or group of elements, integers or steps.





BRIEF DESCRIPTION OF THE DRAWINGS


FIG. 1 illustrates a typical roof cladding construction;



FIG. 2 is a perspective view of a formwork for cement casting for a composite cement panel according to one embodiment of the present invention;



FIG. 3 is a perspective view of a foam board placed in the formwork of FIG. 2 for fabricating a composite cement panel according to one embodiment of the present invention.



FIG. 4 is a flowchart showing a process for fabricating a cement panel using the formwork of FIG. 2.



FIG. 5A is a top view of a composite cement panel according to one embodiment of the present invention.



FIG. 5B is a bottom view of FIG. 5A.



FIG. 6A is a front view of FIG. 5A.



FIG. 6B is a cross sectional side view of FIG. 5A.



FIG. 6C is a partially enlarges view of FIG. 6B.



FIG. 7A is a perspective bottom view of FIG. 5A.



FIG. 7B is a partially cross sectional perspective view of FIG. 5A.





DETAILED DESCRIPTION OF THE INVENTION

Throughout this specification, SI units are followed by corresponding English units. Where a discrepancy exists, the SI units control.



FIG. 2 shows a formwork 2, made of metal for example, for casting a composite cement panel 800 shown in FIG. 7A. Formwork 2 has an array of recesses 3 formed on the base surface 4. Recesses 3 are positioned spaced apart from each other across the base surface 4 of the formwork 2. Guide abutments 6 are provided on two adjacent inner surfaces 214, 215 of the metal formwork 2. Formwork 2 further includes pins 8 positioned on the bottom surface 4. Pins 8 extend upwardly from the base surface 4 of formwork 2. Formwork 2 ends with an upturn skirting 7 along the peripheral edge, allowing ease of handling the formwork 2 during casting or transportation of the cement panel 800.



FIG. 3 illustrates a light-weight core material board, such as a foam board 200, placed in formwork 2 before the process of cement casting of the composite cement panel 800. Foam board 200 has through holes 202 formed thereon by, for example, drilling, stamping, cutting, punching or pre-made integratedly during a molding process forming the foam board. Through holes 202 are configured such that, when foam board 200 is placed in formwork 2, each through hole faces one recess of formwork 2. When placed in formwork 2, foam board 200 sits on pins 8, leaving a gap between foam board 2 and bottom surface 4 of formwork 2.



FIG. 4 is a flowchart of a process 300 for fabricating a cement panel using the formwork 2 shown in FIG. 2. At step 302, foam board 200 having through holes 2 formed there on, is placed in the formwork 2, with two adjacent sides of the form board acting against a respective guide abutment 6. This way, there is remained a side gap between the periphery of foam board and inner surfaces 214 and 215 of formwork 2.


At step 312 a pre-mixed self-levelling high strength cement grout, with or without concrete hardener or chemical additive, is prepared. At step 306, the cement grout is poured onto foam board 200 and into formwork 2. During this step, cement grout will fill up the round recesses 3 in the formwork 2, the gap between the foam board and the bottom surface 4 of formwork 2, the gap between the periphery of foam board 200 and inner surfaces 214, 215, 216 and 217 of formwork 2, and the holes 202 of the foam board 200. At step 308, the cement grout fills formwork fully, and is trowelled and finished. At step 310 the cement grout is left to dry and harden, hence to form a cement casing 502 encapsulating foam board 200, and form the composite cement panel. At step 314 the formed cement panel is removed from the formwork 2.


Depending on the building roof conditions and the finishing requirements, the composite cement panel may be fabricated with a suitable finishing layer on its top surface. For example, at an optional pre-dry finishing step 318, pebbles may be poured onto the top surface of the wet composite cement panel. The pebbles are then attached onto the top surface of the panel, and dried together with the panel. Alternatively, color cement powders may be supplied onto the top surface of the wet composite cement panel and dried together, so as to form a colored finishing layer. Imprints with predetermined patterns may also be formed, by molding or pressing the patterns on the top surface of the composite cement panel. In a further optional after-dry step 320, as an alternative of step 318, the dried composite cement panel may be covered by tiles, wood panels or natural/artificial stones and/or a layer of heat-insulating or waterproof coating.



FIGS. 5A, 5B, 6A, 6B, 6C, 7A and 7B illustrate a composite cement panel 800 produced after step 314 of process 300 (shown in FIG. 4). With reference to FIG. 6A and FIG. 6B, it can be seen that the foam board 200 is encapsulated in the cement casing 502. Also, it can be seen from FIG. 6C that the top portion and bottom portion of the cement casing is bound by portions of cement 502a surrounding the foam board 200 as well as the portions 502b filling the holes 202 of the foam board 200. Portions of cement casing 502 fills in the holes 202 of foam board 200, forming columns 570. These columns 570 increase the strength and rigidity of the cement panel 800, and serve to distribute applied weight, such as foot traffic, to reduce the likelihood of foam board 200 being crushed. Portions of the cement casing filling in the round recess 3 of formwork 2 form legs 220 at the bottom side 250 of the composite cement panel 800. Additionally, the foam board 200 is chemically bonded to the cement casing 502 by additives in the cement grout.


With reference to FIGS. 7A and 7B, legs 220 extend downwardly from the bottom surface 250 of the cement panel 800. When leveled on top the roof top surface of a building, legs 220 rests on the roof top surface, providing a network of multi-directional free-flow paths between the spaces of the legs 220 for draining water along the underside of the cement panel 800. Provision of legs 220 of cylinder shape and multi-directional flow paths reduces trapping of residual water in the cement panel 800, and at the same time allows the water to flow in multiple-directions on the roof top surface level. Thus, better drainage of water can be achieved even in heavy rainfall. By encapsulating the foam board in the cement casing, water or moisture is prevented from penetrating into the panel and wet the foam board, hence the likelihood of the foam board deformation or damage caused by water or moisture content is avoided.


The size and thicknesses of foam boards 200 are kept in appropriate ratio to the size and thickness of the finished cement panel 800 to achieve a satisfactory effect of thermal insulating. In one embodiment, the dimensions of foam board 200 are 18 mm (0.7 inches) thick by 480 mm (18.9 inches) width by 480 mm (18.9 inches) length. Specifications of the one exemplary polystyrene foam board 200 are listed in Table 1 below.









TABLE 1







Specification of foam board










Property
Test Method
Unit(s)
Typical Value(s)





Density

kg/m3
40-50





(2.5-3.1 lb/ft3)


Thermal
ASTM C518:
W/m/ ° K.
0.02207


Conductivity
1991
kcal/mm/ ° K.
0.01897 (0.012





BTU/ft/





hour/ft2/° F.


10% Compressive
ASTM D 1621:
N/mm2
0.30 (144.5 psi)


Strength (Average)
2000




Flammability
ASTM C635: 91
%
10.0 (3.94 inches/





minute)


Classification





(Average burning





rate)





Water Absorption
ASTM C272:

0.01


(Average)
2001




Temperature of Hot

° C.
40.77 (105.39° F.)


Surface





Temperature of

° C.
19.95 (67.91° F.)


Cold Surface





Mean Temperature

° C.
30.36 (86.65° F.)









The composition of an exemplary pre-mixed, self-leveling, high strength cement grout is listed in Table 2 below.









TABLE 2







Composition of cement grout











Name
CAS
Proportion






Portland Cement
65997-15-1
10-60%



Sand (Crystalline Quartz)
14808-60-7
10-60%



Flow Aid, Plasticiser

0-1%



Concrete Strengthener Additive

250 ml (15.26 in3)










The specification of an exemplary concrete strengthener is listed in Table 3 below.









TABLE 3







specification of the concrete strengthener











Property
Unit
Typical Value






Solid Content
%
>40



Density
kg/m3
1.16 ± 0.04 (1.15 ± 0.04 oz/ft3)



Crack Filing
mm
0.1-2 (3.9-78 mil)



Depth of Absorption (for
mm
1-8 (39-314 mil)



Grade 20 Concrete)





Flash Point Waterborne

Not flammable



Drying Time
hours
1-3



Weather Condition
° C.
10-50 (50-122° F.)



UV Resistance

Stable









It will be appreciated by persons skilled in the art that numerous variations and/or modifications may be made to the invention as shown in the specific embodiments without departing from the spirit or scope of the invention as broadly described. The present embodiments are, therefore, to be considered in all respects as illustrative and not restrictive.

Claims
  • 1. A composite panel for a rooftop surface, said composite panel comprising: a core material board having a top surface and a bottom surface with a plurality of openings through said core material board extending from said top surface to said bottom surface; a rigid outer shell of solid material that encapsulates said core material board; a plurality of supports of said solid material, wherein each of said plurality of supports extends through one of said plurality of openings in said core material board; a plurality of legs on a portion of said rigid outer shell covering said bottom surface; said plurality of legs supporting said composite panel over a surface of a structure defining a gap between said surface of said structure and a portion of said rigid outer shell over said bottom surface of said core material board; and wherein said plurality of legs define a network of multi-directional flow paths under said composite panel in said gap defined by said plurality of legs, wherein each of said flow paths directs a flow of material in a different direction, said network of flow paths including at least a first flow path and a second flow path, wherein said first flow path and said second flow path are in different directions, wherein each of said legs is cylinder shaped, and wherein each of said supports is substantially aligned with one of said legs.
  • 2. The composite panel of claim 1, wherein said supports are integral to said rigid outer shell.
  • 3. The composite panel of claim 1, wherein each of said supports is a column.
  • 4. The composite panel of claim 1, wherein said core material board is chemically bonded to said rigid outer shell.
  • 5. The composite panel of claim 1, wherein said core material board comprises a polystyrene foam board.
  • 6. The composite panel of claim 1, wherein said rigid outer shell comprises a cement mixture.
  • 7. The composite panel of claim 1, further comprising: a covering over a surface of a portion of said rigid outer shell covering said top surface of said core material board.
  • 8. A method for producing a composite panel comprising: placing-a core material board having a top surface, a bottom surface, and a plurality of openings through said core material board from said top surface to said bottom surface-in a formwork having a base surface with a plurality of recesses defined in said base surface, a rigid outer shell of solid material that encapsulates said core material board, a plurality of supports of said solid material, wherein each of said plurality of supports extends through one of said plurality of openings in said core material board, a plurality of legs on a portion of said rigid outer shell covering said bottom surface, said plurality of legs supporting said composite panel over a surface of a structure defining a gap between said surface of said structure and a portion of said rigid outer shell over said bottom surface of said core material board, and wherein said plurality of legs define a network of multi-directional flow paths under said composite panel in said gap defined by said plurality of legs, wherein each of said flow paths directs a flow of material in a different direction, said network of flow paths including at least a first flow path and a second flow path, wherein said first flow path and said second flow path are in different directions, wherein each of said legs is cylinder shaped, and wherein each of said supports is substantially aligned with one of said legs, filling said formwork with a viscous material that fills said plurality of recesses, fills said plurality of openings in said core material board and surrounds said core material board in said formwork; and allowing said viscous material to harden into a rigid outer shell encapsulating said core material board.
  • 9. The method of claim 8 further comprising: trowelling a top surface of said viscous material to create a smooth surface responsive to pouring said viscous material into said formwork.
  • 10. The method of claim 8 further comprising: pouring pebbles onto a surface of said viscous material after pouring said viscous material into said formwork.
  • 11. The method of claim 8 further comprising: pouring a colored powder onto a top surface of said viscous material after pouring said viscous material into said formwork.
  • 12. The method of claim 8 further comprising: covering a top surface of said rigid outer shell with a material after hardening said viscous material into said rigid outer shell.
  • 13. The method of claim 8 further comprising: removing said composite panel from said formwork after said viscous material has hardened into said rigid outer shell.
  • 14. The method of claim 8 wherein said core material board is made of polystyrene foam.
  • 15. The method of claim 8 further comprising: aligning each of plurality of openings through said core material board with one of said plurality of recesses in said formwork.
  • 16. The method of claim 8 wherein said viscous material is a cement mixture.
  • 17. The method of claim 16 further comprising: preparing said cement mixture prior to pouring said cement mixture into said formwork.
Priority Claims (1)
Number Date Country Kind
200703691-6 May 2007 SG national
PCT Information
Filing Document Filing Date Country Kind 371c Date
PCT/SG2008/000174 5/9/2008 WO 00 3/15/2010
Publishing Document Publishing Date Country Kind
WO2008/143591 11/27/2008 WO A
US Referenced Citations (51)
Number Name Date Kind
3288998 Press, Jr. Nov 1966 A
3387420 Long Jun 1968 A
3412513 Gosele Nov 1968 A
4206267 Jungbluth Jun 1980 A
4449336 Kelly May 1984 A
4658554 Riley et al. Apr 1987 A
4674249 Bennett, Jr. Jun 1987 A
4677800 Roodvoets Jul 1987 A
4835034 Cruz May 1989 A
4937990 Paquette Jul 1990 A
5088259 Myers Feb 1992 A
5104715 Cruz Apr 1992 A
5369926 Borland Dec 1994 A
5377468 Repasky Jan 1995 A
5473847 Crookston Dec 1995 A
5561958 Clement et al. Oct 1996 A
5699643 Kinard Dec 1997 A
5775039 McPherson Jul 1998 A
5884446 Hageman Mar 1999 A
5887397 Repasky Mar 1999 A
6079166 Mason et al. Jun 2000 A
6233892 Tylman May 2001 B1
6256957 Kelly Jul 2001 B1
6298620 Hatzinikolas Oct 2001 B1
6449915 Park Sep 2002 B1
6457288 Zambelli et al. Oct 2002 B2
6487830 Robertson Dec 2002 B2
7454876 Kelly Nov 2008 B2
7493733 Kelly Feb 2009 B2
7493738 Bui Feb 2009 B2
7591114 Herron, III Sep 2009 B2
7658052 Kelly Feb 2010 B2
7770354 Bui Aug 2010 B2
7805900 Kelly Oct 2010 B2
7877955 Kelly Feb 2011 B2
8028483 Carolan Oct 2011 B2
20010015039 Zambelli et al. Aug 2001 A1
20020028318 Clark Mar 2002 A1
20020110666 McCollough et al. Aug 2002 A1
20040137195 Stephens, Jr. Jul 2004 A1
20050146068 Liu Jul 2005 A1
20080041004 Gibbar et al. Feb 2008 A1
20080276557 Rapaz Nov 2008 A1
20090007509 Jordan et al. Jan 2009 A1
20090064617 Montoya et al. Mar 2009 A1
20090193738 Kortuem et al. Aug 2009 A1
20120047839 Walker Mar 2012 A1
20120047844 Walker Mar 2012 A1
20120227343 Curtin et al. Sep 2012 A1
20120285116 Walker Nov 2012 A1
20120324814 Amend Dec 2012 A1
Foreign Referenced Citations (8)
Number Date Country
0410528 Jan 1991 EP
1111146 Jun 2001 EP
2223520 Apr 1990 GB
491317 Jun 2002 TW
493646 Jul 2002 TW
9207695 May 1992 WO
WO 2006002451 Jan 2006 WO
WO 2007040461 Apr 2007 WO
Related Publications (1)
Number Date Country
20100189953 A1 Jul 2010 US