The invention relates to a composite film for packaging containers. The invention further relates to a method for producing a composite film as well as to a packaging container which is made from a composite film.
A composite film for packaging containers is known from the WIPO patent application WO96/19387 A. In this case, the composite film is part of a packaging container having a pouring aperture via which the liquid located inside the packaging container can be removed from said packaging container. In order to facilitate a simplified opening of the packaging container in the region of the opening device, provision is made to equip the known composite film with a weakened region on the side thereof facing the opening device. Two options are thereby described in the patent application mentioned above: on the one hand, a weakening resulting from two cuts arranged in the shape of a cross with respect to one another and on the other hand a reduction in the thickness of the composite film. By means of both measures, it is possible to weaken the packaging container in order to manually pierce or, respectively, open the composite film in the region of the opening device, wherein said composite film is kept intact during the transport or storage of the packaging container and thus the shelf life of the product situated in the packaging container is ensured. In addition, opening devices are addressed in the known patent application which devices have cutters that assist in severing the composite film. More detailed information with regard to the weakening region addressed above can be extracted from the aforementioned patent application.
Based on the prior art described above, it is the aim of the invention to embody a composite film for packaging containers in such a way that the composite film, in conjunction with an opening device comprising cutters for severing said composite film, allows for a reliable severing of the same while using relatively little effort and expense for implementing the geometry of the cutters being used or other measures. According to the invention, this aim is substantially met by a composite film for packaging containers by virtue of the fact that the weakened region is disposed on the side of the inner packaging material layer of the composite film and is implemented as an at least partial reduction in the layer thickness of the inner packaging material, wherein the shape of the weakened region, in particular having a circular cross section, is adapted to the arrangement of the cutters that are disposed on a partial circular diameter of the opening device as a part of the opening device.
It has become evident during trials that the inner packaging material layer, which typically consists of polyethylene (PE), is relatively difficult for the cutters of the opening device to sever on account of the toughness thereof. The consideration could, of course, then arise to replace the PE with another material; however, PE is particularly suited to being used as the inner packaging material layer in the relevant packaging containers or, respectively, composite films, in particular in tubular bag packagings, due to its sealing capability as well as other properties thereof. Another option could consist of designing the cutters especially sharp or with a specific geometry in order to make possible or facilitate the severing or, respectively, cutting of the inner packaging material layer consisting of polyethylene. This would, however, lead to an increase in costs for producing the opening devices. In contrast, it is possible by means of the composite film described in claim 1 to achieve a reliable severing of the film composite using conventional opening devices or, respectively, cutters.
As previously explained, the inner packaging material layer preferably consists of PE, wherein said PE can have a layer thickness between 50 μm and 200 μm, in particular between 60 μm and 120 μm.
The inner packaging material layer is reduced in the thickness thereof in the weakened region, wherein it is possible in principle to remove (at least partially) the inner packaging layer in the weakened region or to compress said layer, wherein the latter measure can, if need be, likewise lead to a simplified severing of the said inner packaging layer by means of the cutters in the opening device.
The invention also comprises a method for producing an inventive composite film. Provision is thereby made according to the invention for the weakened region to be produced using an anvil-like tool which is pressed with a contact pressing force against the inner packaging material layer and which interacts with an ultrasonic tool that is applied to the outer packaging material layer in alignment with said anvil-like tool. Such a method can be carried out relatively simply and exactly on an industrial scale and is therefore also particularly suited to packaging containers in which foodstuffs are packaged or, respectively, filled and which must be sealed off from ambient air.
It is proposed in one constructive embodiment of the invention that the tool has an annular cross section and that the diameter of the tool is adapted to the partial circular diameter of the cutters of the opening device.
A further aspect relates to the location where the weakened region is to be produced. To this end, it is proposed in a first method according to the invention that the weakened region be produced during the manufacturing process of the composite film. In other words, this means that the weakened regions are produced by the packaging material producer during the manufacture of the composite film. This has the advantage that the actual packaging machine for producing the packaging container or for filling the packaging container can be constructed relatively simply and cost effectively and that no process assurance measures for monitoring the proper production of the weakened regions have to be taken.
In an alternative embodiment, it is however possible for the weakened regions to be produced directly at the packaging machine during the manufacturing process of the packaging containers. This has the advantage that one and the same composite film can continue to be used, for example, when the format of the opening devices is changed, wherein the weakened regions are in each case adapted or, respectively, produced in a format-dependent manner directly at the packaging machine.
Packaging containers, in particular tubular bag packagings, which are produced from a composite film in accordance with the invention or are produced according to an inventive method for producing a composite film have the advantage that they can be easily and reliably opened by the user, wherein the packaged good or rather the foodstuff contained in the packagings is well protected against environmental damage during transport and/or storage thereof.
Further advantages, features and details of the invention ensue from the following description of exemplary embodiments as well as with the aid of the drawings.
In the drawings:
The same components or components serving the same function are denoted in the figures with the same reference numerals.
In
The opening device 10 is shown in more detail in
Such an opening device 10 is known per se from the prior art just as the cutters 13 thereof as well as the mechanism required to actuate said cutters 13. The aforementioned components are therefore not explained in detail below as they are not considered to be essential to the invention.
In
It should be additionally noted that the described layer configuration of the composite film 100 is only presented by way of example and can be changed in a variety of ways by the use or omission of individual layers. It is also possible if need be to dispense with the adhesive layers 103, 105, 107 and to connect the individual layers to one another, for example, by means of extrusion lamination. It is only essential to the invention that the outside 5 of the OPP layer 101 forming the outside 5 of the tubular bag packaging is suitable for connecting to the opening device 10, whereas the inner PE layer 108 is designed for processing on the aforementioned tubular bag machine in a heat-sealing manner.
Provision is made according to the invention for the (inner) PE layer 108 to be equipped with a weakening zone 20, which is annular in the exemplary embodiment, in the region of the opening device 10 to be attached. The weakening zone 20 is characterized in that the original thickness D of the PE layer 108 is reduced to a thickness d in the region of said weakening zone 20. Provision can be made in the extreme case for at least the entire PE layer 108 to be completely removed in the region of the weakening zone 20.
The reduction in the thickness in the weakening zone 20 preferably results by means of removing the material of the PE layer 108 or as an alternative if need be by means of a compression of the PE layer 108 for the purpose of a reduction in thickness. It is of importance thereby that the region of the reduced thickness of the PE layer 108 is disposed so as to line up or align with the partial circular diameter T of the cutters 13. Hence, when the cutters 13 are actuated, said cutters only have to sever a PE layer 108 having a reduced thickness when the same make contact with PE layer 108.
In
In alignment with the anvil 30, a sonotrode 25 is pressed from the outer OPP layer 101 against the composite film 100 which preferably has a cylindrical or tapered end 26. The sonotrode 25 is coupled at least indirectly to an ultrasonic source (not depicted) and is operated with a frequency of, for example, 30 kilohertz or 35 kilohertz.
In
The weakening zone 20 can, for example, be produced by a packaging material manufacturer (who manufactures the composite film 100) by the weakening zones 20 being spaced apart at equal distances corresponding to the printed image or size of the tubular bag packagings 1 in a composite film web. The composite film 100 built-up as a packaging material roll can subsequently be delivered to the packaging plant for the manufacture of the tubular bag packagings 1. The packer forms the tubular bag packagings 1 on the tubular bag machine previously mentioned and fills said packagings with the bulk good 7. As an alternative, it is, however, also possible to dispose the device for forming the weakening zone 20 directly at the tubular bag machine or at least in the region of the packaging line in the packaging plant.
The composite film 100 described to this point as well as the tubular bag packaging 1 can be altered or modified in a variety of ways without deviating from the concept of the invention. Said concept consists of a selected weakening of the inner packaging material layer of the tubular bag packaging 1 in order to facilitate the severing of the inner packaging material layer by means of the cutters 13 of the opening device 10.
Number | Date | Country | Kind |
---|---|---|---|
10 2011 075 481 | May 2011 | DE | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP2012/054906 | 3/20/2012 | WO | 00 | 11/11/2013 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2012/152492 | 11/15/2012 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
4072233 | Kramer et al. | Feb 1978 | A |
4429828 | Farber | Feb 1984 | A |
5141133 | Ninomiya et al. | Aug 1992 | A |
5839627 | Hicks et al. | Nov 1998 | A |
6382462 | Ostergaard-Nielsen et al. | May 2002 | B1 |
6398075 | Laciacera et al. | Jun 2002 | B1 |
6598757 | Stillinger et al. | Jul 2003 | B2 |
7036683 | Dubach | May 2006 | B2 |
7757894 | Kluczynski | Jul 2010 | B2 |
20030128899 | Dennis | Jul 2003 | A1 |
20050175800 | Staffetti et al. | Aug 2005 | A1 |
20140233871 | Barron et al. | Aug 2014 | A1 |
Number | Date | Country |
---|---|---|
1182144 | Feb 2002 | EP |
2154200 | Sep 1985 | GB |
9619387 | Jun 1996 | WO |
WO 9746459 | Dec 1997 | WO |
2007127982 | Nov 2007 | WO |
Entry |
---|
International Search Report for Application No. PCT/EP2012/054906 dated Jun. 21, 2012 (3 pages). |
Number | Date | Country | |
---|---|---|---|
20140086513 A1 | Mar 2014 | US |