Claims
- 1. A prevulcanization process for producing elastomer blends having improved green strength, comprising,
- mixing a semi-crystalline butene polymer having a number average molecular weight of from about 30,000 to about 500,000 with an elastomer and reclaimed rubber to produce the blend, said butene polymer selected from the class consisting of polybutene and interpolymers made from 1-butene monomer and at least one monomer selected from the class consisting of alpha-olefins having 2 through 16 carbon atoms; non-conjugated dienes having the general formula: ##STR8## where R.sub.1, R.sub.2, and R.sub.3 is a hydrogen, a lower alkyl group containing from one to four carbon atoms, or an aryl group; where R.sub.4 is an aryl group or a lower alkyl group containing from one to nine carbon atoms, and n is an integer having a value of from 1 to 6, and wherein the said R.sub.1 's in the ##STR9## group may be similar to dissimilar; and non-conjugated alpha, omega-polyenes having from 6 to 36 carbon atoms which may or may not contain internal unsaturation, wherein butene in said interpolymers comprises from 99.9 to 65 mole percent of the total monomers,
- said elastomer selected from the group consisting of natural cis-1,4-polyisoprene and elastomers made from monomers selected from the group consisting of conjugated dienes having from 4 to 10 carbon atoms, interpolymers of said dienes among themselves or with monomers selected from the group consisting of vinyl substituted aromatic hydrocarbon compounds having from 8 to 12 carbon atoms, and polyalkenylenes, the amount of said butene polymer ranging from about 2 parts to about 25 parts per 100 parts of said elastomer and said reclaimed rubber, the amount of said elastomer based upon said elastomer and said reclaimed rubber being greater than 5 percent by weight.
- 2. A process according to claim 1, wherein said butene polymer is selected from the class consisting of polybutene, a copolymer of 1-butene and ethylene, a copolymer of 1-butene and propylene, a copolymer of 1-butene and 1-hexene, a copolymer of 1-butene and 1-octene, a terpolymer of 1-butene, 1-octene and 1,7-octadiene, and a terpolymer of 1-butene, 1-hexene and 1-octene, and wherein said elastomer is selected from the class consisting of natural cis-1,4-polyisoprene, synthetic cis-1,4-polyisoprene, cis-1,4-polybutadiene and a copolymer of styrene and butadiene.
- 3. An elastomer blend composition having improved green strength, comprising;
- a blend of a semi-crystalline butent polymer having a number average molecular weight of 30,000 to about 500,000 with an elastomer and reclaimed rubber, said butene polymer selected from the class consisting of polybutene and interpolymers made from 1-butene monomer and at least one monomer selected from the class consisting of alpha-olefins having 2 through 16 carbon atoms, non-conjugated dienes having the general formula: ##STR10## where R.sub.1, R.sub.2 and R.sub.3 is a hydrogen, a lower alkyl group containing from one to four carbon atoms, or an aryl group; where R.sub.4 may be an aryl group or a lower alkyl group containing from one to nine carbon atoms, and n is an integer having a value of from 1 to 6, and wherein the said R.sub.1 's in the ##STR11## group may be similar or dissimilar; and non-conjugated alpha, omega-polyenes having from 6 to 36 carbon atoms which may or may not contain internal unsaturation, wherein butene in said interpolymers comprises from 99.9 to 65 mole percent of the total monomers,
- said elastomer selected from the group consisting of natural cis-1,4-polyisoprene and elastomers made from monomers selected from the group consisting of conjugated dienes having from 4 to 10 carbon atoms, interpolymers of said dienes among themselves or with monomers selected from the group consisting of vinyl substituted aromatic hydrocarbon compounds having from 8 to 12 carbon atoms, and polyalkenylenes, the amount of said butene polymer ranging from about 2 parts to about 25 parts per 100 parts of said elastomer and said reclaimed rubber, the amount of said elastomer based upon said elastomer and said reclaimed rubber being greater than 5 percent by weight.
- 4. An elastomer blend composition according to claim 3, wherein said butene polymer is selected from the class consisting of polybutene, a copolymer of 1-butene and ethylene, a copolymer of 1-butene and propylene, a copolymer of 1-butene and 1-hexene, a copolymer of 1-butene and 1-octene, a terpolymer of 1-butene, 1-octene and 1,7-octadiene, a terpolymer of 1-butene, 1-hexene and 1-octene, and wherein said elastomer is selected from the class consisting of natural cis-1,4-polyisoprene, synthetic cis-1,4-polyisoprene, cis-1,4-polybutadiene, a copolymer of styrene and butadiene, and a copolymer of cyclopentene and dicyclopentadiene.
CROSS REFERENCE
This application is a divisional application of my copending application, U.S. Ser. No. 779,382 filed on Mar. 21, 1977 for "COMPOSITION AND METHOD OF IMPROVED GREEN STRENGTH AND UNVULCANIZED ELASTOMERS" now U.S. Pat. No. 4,198,324.
US Referenced Citations (4)
Foreign Referenced Citations (2)
Number |
Date |
Country |
946224 |
Jan 1964 |
GBX |
1120572 |
Jul 1968 |
GBX |
Non-Patent Literature Citations (1)
Entry |
B. Mehr et al., "Influence of Additions of Polybutylene with Different Mol. Wgt. on the Properties of Compositions of Cis-Polyisoprene Synthetic Rubber" Materiale Plastice, No. 10(11), 604-607, (1973). |
Divisions (1)
|
Number |
Date |
Country |
Parent |
779382 |
Mar 1977 |
|