Claims
- 1. A deinking medium for use in an aqueous washing method for deinking secondary fiber comprising water, 5-500 ppm of a water-soluble polymeric polyelectrolyte dispersant of the formula: ##STR5## wherein R.sub.1, R.sub.2, R.sub.4 and R.sub.5 are H, C.sub.1 -C.sub.4 lower alkyl, alkylcarboxy or mixtures thereof, R.sub.3 and R.sub.6 are H, carboxy, alkylcarboxy or mixtures thereof, and X is carboxy, CO.sub.2 NH.sub.2, acetyl or C.sub.6 H.sub.5 wherein a+b has a value so that the molecular weight of the polyelectrolyte dispersant is within the range of about 500-5,000; and an amount of a nonionic surfactant of the formula: nonylphenol(EtO).sub.9.5 (PrO).sub.6-24 -H effective to deink said fiber.
- 2. The deinking medium of claim 1 wherein the dispersant comprises a polyacrylate or a maleic acid-vinyl acetate copolymer.
- 3. The deinking medium of claim 2 wherein the molecular weight of the dispersant is about 750-3000.
- 4. The deinking medium of claim 1 further comprising a water-soluble cosolvent.
- 5. The deinking medium of claim 4 wherein the cosolvent is tetrahydrofurfuryl alcohol or ethoxylated derivatives thereof.
- 6. The deinking medium of claim 4 wherein the cosolvent is monoethoxylated-tetrahydrofurfuryl alcohol.
Parent Case Info
This is a continuation of application Ser. No. 206,142, filed Nov. 12, 1980, now abandoned, which is a continuation of application Ser. No. 458,432, filed Jan. 17, 1983, now U.S. Pat. No. 4,518,459, which is in turn a continuation of application Ser. No. 93,744, filed Nov. 13, 1979, now abandoned.
US Referenced Citations (6)
Foreign Referenced Citations (2)
Number |
Date |
Country |
729071 |
Mar 1966 |
CAX |
197607 |
Jul 1976 |
JPX |
Non-Patent Literature Citations (2)
Entry |
U.S. patent application Ser. No. 458,432, (filed Jan. 17, 1983). |
The "Condensed Chemical Dictionary", G. G. Hawley, ed. (p. 858). |
Continuations (3)
|
Number |
Date |
Country |
Parent |
206142 |
Nov 1980 |
|
Parent |
458432 |
Jan 1983 |
|
Parent |
93744 |
Nov 1979 |
|