Claims
- 1. A composition for hair treatment comprising:
- (a) 0.1-10 wt. % of a silicone polymer having at least one alkoxy group containing 12 to 22 carbon atoms in the molecule and having a melting point of not lower than 30.degree. C.;
- (b) 0.1-20 wt. % of a cationic surface active agent;
- (c) 0.1-30 wt. % of an alcohol having an alkyl group or alkenyl group of 12 to 26 carbon atoms;
- (d) 0.1-90 wt. % of an organic liquid compatible with water which is selected from the group consisting of propylene glycol, alkyl monoethers of diethylene glycol, and alkyl monoethers of dipropylene glycol, and
- (e) water.
- 2. The composition for hair treatment as defined in claim 1, wherein the modified silicone polymer has the following formula: ##STR11## wherein R.sup.1 represents an alkyl group having 1-28 carbon atoms, R.sup.2 represents methyl or phenyl, k is an integer of 0-6, l is an integer of 1-3,000, and m and n are integers satisfying the condition of m+n=1-500.
- 3. The composition for hair treatment as defined in claim 1, wherein the modified silicone polymer has the following formula: ##STR12## wherein R.sup.1 represents an alkyl group having 1-28 carbon atoms, l is an integer of 1-100, and m is an integer of 1-50.
- 4. The composition for hair treatment as defined in claim 1, wherein the cationic surface active agent has the following formula: ##STR13## wherein each of R.sup.9 and R.sup.10 is an alkyl group selected from the group consisting of branched alkyl groups expressed by the following formulae: ##STR14## wherein R.sup.13 is methyl or ethyl; p is an integer satisfying the condition that the total number of carbon atoms is within the range of 8-16;
- and the linear alkyl groups expressed by the following formula:
- CH.sub.3 (CH.sub.2).sub.q --
- wherein q is an integer satisfying the condition that the total number of carbon atoms is within the range of 8-16; and
- each of R.sup.11 and R.sup.12 is a group selected from the group consisting of an alkyl group having 1-3 carbon atoms and a hydroxyalkyl group having 1-3 carbon atom; and X.sup.- is a halogen ion or an organic anion.
- 5. The composition for hair treatment as defined in claim 1, wherein the cationic surface active agent has the following formula: ##STR15## wherein each of R.sup.14 and R.sup.15 is an alkyl group having 2-12 carbon atoms; R.sup.16 is the group expressed by the formula: ##STR16## wherein each of R.sup.14 and R.sup.15 is the same as defined above, or an alkyl group having 1-3 carbon atom; each of R.sup.17 and R.sup.18 is benzyl group, an alkyl group having 1-3 carbon atom or a hydroxyalkyl group having 1-3 carbon atom; and X.sup.- is halogen ion or an organic anion.
- 6. The composition for hair treatment as defined in claim 1, wherein the modified silicone polymer is contained in a amount of 0.2-5 wt. %.
- 7. A method for treating hair comprising applying to the hair a hair treating effective amount of a composition comprising:
- (a) 0.1-10 wt. % of a silicone polymer having at least one alkoxy group containing 12 to 22 carbon atoms in the molecule and having a melting point of not lower than 30.degree. C.:
- (b) 0.1-20 wt. % of a cationic surface active agent;
- (c) 0.1-30 wt. % of an alcohol having an alkyl group or alkenyl group of 12 to 26 carbon atoms;
- (d) 0.1-90 wt. % of an organic liquid compatible with water which is selected from the group consisting of propylene glycol, alkyl monoethers of diethylene glycol, and alkyl monoethers of dipropylene glycol, and
- (e) water.
Priority Claims (1)
Number |
Date |
Country |
Kind |
2-224113 |
Aug 1990 |
JPX |
|
Parent Case Info
This is a continuation of application Ser. No. 07/748,776 filed Aug. 22, 1991 now abandoned.
US Referenced Citations (3)
Number |
Name |
Date |
Kind |
4423041 |
Clum et al. |
Dec 1983 |
|
4658839 |
Dallal et al. |
Apr 1987 |
|
4711776 |
Suzuki et al. |
Dec 1987 |
|
Continuations (1)
|
Number |
Date |
Country |
Parent |
748776 |
Aug 1991 |
|