Abstract
The present invention concerns a reinforced conductive layer (7). The layer is applied at a part (3a,b) of an electrical unit, e.g. a mobile telephone, which is to come into contact with another part (3a,b). The layer (7) will protect the covered material against corrosion due to formation of a galvanic element. In a preferred embodiment of the invention the layer (7) is made of the same material as the part (3a,b) which it will come into contact with. Furthermore, spaces (16) may be formed in assembly of a mobile telephone, which spaces (16) are surrounded by conductive material.
Description


TECHNICAL FIELD OF THE INVENTION

[0001] The present invention concerns a reinforced conductive layer, which is applied at a part of an electronic or electrical unit, e.g. a telephone, which is to come into contact with another part. The layer is mechanical, chemical and/or electrochemical resistant. The layer will protect the covered material against corrosion due to formation of a galvanic element.



DESCRIPTION OF THE PRIOR ART

[0002] In order to shield an electronic unit, preferably a telephone, against electromagnetic radiation such as ESD currents, it is at least partly surrounded by a conductive shield, This shield consists of a conductive material such as magnesium, aluminium, zinc or any other metal. It can also consists of a non-conductive material such as plastic, which is furnished with a conductive material, e.g. a conductive layer, which is able to conduct an electric current. The shield of the electronic unit will then be conductive in a desired extent.


[0003] In these contexts and for other reasons it is normal that different kinds of metals will come into contact with each other. This will lead to the creation of a galvanic element under influence of moisture or other fluids, whereby corrosion will result on at least one of the conductive materials. This will normally occur on the least noble metal. The different metals will come into contact when at least two parts of the electronic unit come into contact with each other. These parts may be placed at different parts of the electronic unit, e.g. at snaps, grooves, hooks, flanges, slots, screw joints, printed circuit carts or connectors.


[0004] For mobile telephones one part of the shield forms the rear of the mobile telephone, which part is made of e.g. magnesium. Another part of the shield forms the front of the mobile telephone, which part may be of plastic, coated on the inside with a conductive layer mainly of silver, aluminium or the like. This layer may be coated by means of vacuum evaporating, spraying, painting, attaching a foil or may be a separately inserted conductive layer.


[0005] When the different materials come into contact with each other a conductive unit will be formed as the shield parts are connected electrically. If this takes place in a damp environment a galvanic element is formed. This will cause corrosion of the least noble metal, which will be decomposed and pulverised. This means that the contact between the two shield parts deteriorates, impairing or breaking the desired electrical connection between the shield parts. Furthermore a damage is created in the material. This damage is unaesthetic and also forms openings which will make the telephone untight, and lets in foreign particles such as sand, dirt, moisture and gases, which all harm the function of the telephone.


[0006] Sometimes a packing is placed between the shield parts to enhance the tightness and the contact ability between these parts. The packing is conductive and may be of steel or another metal or may be of a conductive, rubber like material. Hereby further materials which may form a galvanic element are introduced. Furthermore there are a number of contact points where, as stated above, different metals come into contact with each other giving the above stated problems.



SUMMARY OF THE INVENTION

[0007] One object of the present invention is to reduce or eliminate the drawbacks of the above constructions. This is done by furnishing at least one of the parts which are to come into contact with each other with a protective conductive layer. The layer mechanically and electrically hinder/counteract corrosion due to the formation of galvanic elements The corrosion described above may of course arise anywhere in the electronic unit where two different metals come into contact with each other and where moisture is present and give rise to the above stated damages.


[0008] By the invention a reinforced conductive layer is provided, which layer is placed above one of the conductive materials which otherwise would have been susceptible to corrosion. The layer may be applied by tampon printing, screen printing, vacuum evaporation, painting, spraying or foiling. The layer may be applied in more than one layer. This protective layer can be made of any conductive metal. The most important is that the material has a mechanical and chemical resistance and that it will hinder moisture from reaching the underlying layer, which is to be protected, excluding any corrosion.


[0009] A preferred embodiment of the invention is provided if the protective layer is made of the same conductive material as the material it will come into contact with. In this way no galvanic element will be formed. Moisture or other chemical materials cannot go in under the reinforced conductive layer, and thus no corrosion will be formed Accordingly the invention stops the harmful influences.


[0010] At e.g. the edges of a shield part of a mobile telephone, consisting of magnesium, the connecting parts are furnished with a conductive layer of a colour including silver, which layer is applied by e.g. tampon printing. The other shield part of the mobile telephone is made of a plastic, the inside of which is furnished with a conductive paint layer through tampon printing and which layer mainly consists of silver. As the magnesium will not come in direct contact with the silver, silver will meet silver and no galvanic element will be formed, The magnesium is protected by the silver paint, forming a reinforced conductive layer and moisture will not reach the magnesium.


[0011] The reinforced layer should be mechanically resistant and have an adhesiveness which is enough to guarantee that no holes will form in the layer and that the layer will not come off due to mechanical wear. Furthermore, the layer may be furnished with coarse metallic grains, in order to have better electrical contact between the connecting parts. The layer has a structure in which the metal grains are protected from mechanical influence and corrosion of a binder, preferably a plastic, e.g. acrylic, PVC, or a resin, whereby the metal grains will not be decomposed in any large extent. The thickness of the layer is normally 4 to 20 micrometers.


[0012] If a metal packing is placed between the shield parts the reinforced conductive layer will still fill a function, as the metal of the packing and the magnesium material will not come into contact with each other.







BRIEF DESCRIPTION OF THE DRAWINGS

[0013] The invention will be described more closely below by way of examples with reference to the accompanying drawings, of which:


[0014]
FIG. 1 shows a section through a detail of two shield parts of a mobile telephone according to the present invention,


[0015]
FIG. 2 shows a section through a detail of the two shield parts of a mobile telephone according to the present invention and which are connected as a snap lock,


[0016]
FIG. 3 shows a section through a detail of a mobile telephone, where two connectors meet at a printed circuit card, a screw joint, pogo pin or other fastener, and


[0017]
FIG. 4 shows a perspective view of a shield part of a mobile telephone, where the connectors at the edges of the shield are covered with a reinforcing conductive layer.







DETAILED DESCRIPTION OF THE INVENTION

[0018] As is obvious from the embodiments shown in FIGS. 1, 2 and 3, a detail of an electronic unit is shown, preferably a mobile telephone lo comprising at least two shield parts 2a,b, which are to be joined. The shield parts 2a,b have edges 14 showing connecting parts 3a,b which will come into contact when the shield parts 2a,b are united creating an electric contact. One shield part 2a forms the back 4 of the mobile telephone 1 and is made of a metallic material, e.g. magnesium, zinc, aluminium or any other metal. The other shield part 2b of the mobile telephone 1 forms the front 5 of the telephone and is made of a plastic covered on the inside with a conductive layer 6, The conductive layer 6 covers the connecting part 3b of the front 5, which connecting part 3b is made of a different metal compared to the connecting part 3a of the back 4. The connecting part 3a of the back 4 is covered with a reinforced conductive layer 7, which protects the connecting part 3a of the back 4 against corrosion and mechanical influence. In order to improve the electric contact and/or the sealing effect between the joined shield parts 2a,b, an intermediate packing 6 may be provided prior to assembly. This packing 8 is made of a conductive material.


[0019] Further as shown in the embodiment of FIG. 2 the mobile telephone 1 has a variant of two connecting parts 3a,b which in an assembled state has the form of a snap lock 15. The connecting parts 3a,b form the electric contact by means of the reinforced conductive layer 7. The packing 8 is not shown in this embodiment.


[0020] As shown in the embodiment of FIG. 3 the two shield parts 2a,b are connected by a screw joint 9, comprising a connector 10 which in this case is a pogo pin 11 in electrical contact with e.g. a battery and a printed circuit card 13. Different connecting parts 3a,b are present at different locations around the screw joint 9, whereby different metals meet which may form a galvanic element, Electric contact is formed with the front 5 and the back 4 by means of washers 12 at the screw joint 9 and at the printed circuit card 13. At these connecting parts 3a,b a reinforced conductive layer 7 is applied, which protect against galvanic corrosion.


[0021] As show in the embodiment according to FIG. 4, the shield part 2a, forming the back 4 of a mobile telephone 1 has edges 14 and connecting parts 3a, extending mainly along the extent of the edges 14, When the back 4 is assembled with the front 5 the connecting parts 3a of the back 4 will come into electric contact with the connecting parts 3b of the front 5, which connecting parts 3b have a reinforced conductive layer 7 preventing corrosion. The inside of the front 5 is covered by a conductive layer 6. The edges 14 of the back 4 and the front 5 will form spaces 16 when they are assembled. These spaces 16 are almost completely surrounded by conductive surfaces, whereby electromagnetic radiation will be limited as it mainly is enclosed in each space 16 when the edges 14 of the shields 2a,b are in contact with each other. The edges 14 have normally a height of just a few millimetres, in order to have a thin back 4 of the mobile telephone 1. A battery 17 (indicated with dashed lines) is attached to this back.


[0022] Even tough the invention is described in connection with a mobile telephone, a person skilled in the art will realise that the invention is applicable for all kinds of equipment where different conductive materials come into contact with each other.


Claims
  • 1. A means at an electrical unit having at least one conductive material on a first part (3a) and an other conductive material on a second part (3b) and which first and second parts (3a,b) are to be connected with each other, characterized in that at least one of the parts (3a,b) is furnished with a reinforced conductive layer (7).
  • 2. The means of claim 1, characterized in that the electrical unit is a mobile telephone (1), comprising two shield parts (2a,b), which shield parts have edges (14).
  • 3. The means of claim 2, characterized in that at least one of the parts (3a,b) to be connected is placed on a shield part (2a,b) or is the shield part (2a,b).
  • 4. The means of any of the previous claims, characterized in that the parts (3a,b) to be connected are placed at a printed circuit board (13), a conductive layer (6), a screw joint (9), a connector (10), a pogo pin (11) or a snap lock (15).
  • 5. The means of any of the claims 2 to 4, characterized in that the edges (14) of at least one of the shield parts (2a,b) have parts to be connected with other parts mainly covered by the reinforced conductive layer (7).
  • 6. The means of claims 2 to 5, characterized in that spaces (16) are formed during assembly of the shield parts (2a,b), which spaces (16) are totally surrounded by conductive material.
  • 7. The means of any of the previous claims, characterized in that the reinforced conductive layer (7) at least partly is made of a conductive foil, a conductive paint, a vacuum evaporated surface or a separately placed, reinforced conductive layer (7) and that the conductive layer (7) is able to keep moisture out.
  • 8. The means of any of the previous claims, characterized in that a conductive packing (8) is placed between the parts (3a,b) to be connected, of which parts at least one is covered by the reinforced conductive layer (7).
  • 9. The means of any of the previous claims, characterized in that the reinforced conductive layer (7) is applied in at least two layers.
  • 10. The means of any of the previous claims, characterized in that the reinforced conductive layer (7) has a thickness of 4 to 20 micrometers.
  • 11. The means of any of the previous claims, characterized in that the conductive layer (7) is made of the same material as one of the connecting parts (3a,b) which it is to come into contact with.
  • 12. The means of any of the previous claims, characterized in that the reinforced conductive layer (7) is made of metal particles in a binder, that the binder is acrylic, PVC, resin or the like and that the metal particles are coarse.
Priority Claims (2)
Number Date Country Kind
0000711-2 Mar 2000 SE
0000907-6 Mar 2000 SE