Claims
- 1. The method of forming a tear strip in a container lid which comprises the steps of:
- depressing a section of a blank of metal away from its original plane to form a lid with a depressed section therein;
- reversing the outer surrounding edge between the lid and the depressed section whereby the lower terminal end of the reversed edge extends outwardly, substantially parallel to and beneath the surface of the lid; and
- thereafter coining the outer peripheral edge of the depressed section beneath the lid to reduce its cross-sectional thickness and form a weakened area of separation between the lid and the depressed section whereby the depressed section defines a tear strip.
- 2. The method of forming a tear strip in a container lid according to claim 1 further characterized by rolling the surrounding edge first upwardly above the surface of the lid then downwardly and outwardly beneath the lid surface.
- 3. The method according to claim 1 in which the weakened area of separation formed is scored through the coined area along the outer peripheral edge of the tear strip.
- 4. The method according to claim 3 in which the weakened area of separation is scored completely through its thickness and a temporary sealing composition is applied to the scored area.
- 5. The method according to claim 1 including the step of forming a raised stiffening rib out of the thickness of the lid and tear strip in a radial direction across the intersection of the lid and tear strip.
Parent Case Info
This application is a divisional of Ser. No. 241,642, filed 4-6-72 now U.S. Pat. No. 3,794,206.
US Referenced Citations (5)
Divisions (1)
|
Number |
Date |
Country |
Parent |
241642 |
Apr 1972 |
|