The invention relates to a method of forming a cooling channel in a wall, to an electrode used for implementing the method, to a wall element in which a cooling channel is formed, and to a hollow turbomachine blade including a wall element of this type.
More precisely, the invention relates to a wall element of the type comprising an inside surface and an outside surface, the outside surface being suitable for being cooled by cool air flowing in said cooling channel. In addition, the cooling channel is of the type comprising a hole and a diffusion portion, the hole opening out at one end into the inside surface of the wall and at its other end substantially into the bottom of the diffusion portion by forming an orifice, and the diffusion portion flaring away from said orifice and opening out into the outside surface of the wall.
U.S. Pat. No. 6,183,199 B1 shows an example of a wall element for a hollow blade of a turbojet turbine, the element being pierced by a cooling channel of the above-specified type. In that example, the hole of the channel and its diffusion portion are made by electro-erosion in a single step, using a single electrode whose tip presents a front portion of a shape that corresponds to that of the hole and a rear portion of a shape corresponding to that of the diffusion portion of the channel.
An electrode of that type is described and shown in U.S. Pat. No. 4,197,443 to which reference is made in U.S. Pat. No. 6,183,199 B1. As can be seen, the shape of that electrode is particularly complex. In addition, in general manner, forming a channel by electroerosion using known methods remains an operation that is lengthy and expensive.
An object of the invention is thus to provide an alternative to known methods, making it possible to form a cooling channel of the above-specified type, more quickly and at lower cost.
To achieve this object, the invention provides a method wherein said wall is pierced to make said hole, and wherein an indentation is formed in said wall in order to form said diffusion portion, in two distinct steps.
In the method of the invention, it is thus possible to use techniques and materials that are different for making the hole and for making the diffusion portion.
To make the hole, it is possible to pierce the wall by electroerosion or by using a laser.
Advantageously, laser piercing techniques are used, since these techniques are much faster and much less expensive than electroerosion techniques. Thus, to pierce a wall of a hollow turbine blade by laser, generally only a few tenths of a second are required.
Nevertheless, if it is desired to perform the piercing and the diffusion portion by electroerosion, then two different electrodes are used for each of said portions. The electrodes are simpler in shape than the electrodes that have been used in the past, so they are easier and less expensive to make. For example, for the piercing, it is possible to use an electrode that is cylindrical.
According to another aspect of the invention, in order to make the diffusion portion, an electrode is used in which the tip of the electrode is in the form of a cone with a rounded end and with a conical side surface that presents a flat, the axis of the cone not intersecting the flat.
The above-specified shape for the electrode makes it possible firstly to avoid creating a sharp angle in the bottom of the diffusion portion, where sharp angles generally constitute starter zones for cracks.
Secondly, an electrode of that shape and of appropriate dimensions relative to the hole makes it possible to form a diffusion portion of a shape that is sufficiently broad and flared to ensure that, given the tolerances involved in making the hole and the diffusion portion, and regardless of the position of the hole relative to the diffusion portion, the diffusion portion provides good diffusion (i.e. good guidance and good spreading) of the stream of air leaving the hole.
The invention also provides a wall element having a new type of cooling channel formed therein. Such a channel may be obtained using the method and the electrode of the invention.
The channel includes a diffusion portion with a bottom whose front end is substantially flat, sloping in the thickness of the wall and extending in front of the orifice in the flow direction of the cool air, and a rearwardly-extending margin on the sides and at the front of the orifice, said margin joining the sides of the front end of the bottom.
Advantageously, the angle formed between the margin and the front end of the bottom in a plane perpendicular to the bottom is not “sharp” in the sense that it is strictly greater than 90°. This avoids creating crack-starter zones.
Finally, the invention provides a hollow gas-turbine blade including a wall element of the above-specified type.
The invention and its advantages can be better understood on reading the following detailed description. The description refers to the accompanying figures, in which:
With reference to
Said wall element presents an inside surface 3 and an outside surface 5. This element belongs to a wall 1 of a hollow gas-turbine blade, such as a high pressure turbine blade of a turbojet. This type of hollow blade has an internal cooling passage 4 defined in part by the inside surface 3, said passage being fed with cool air.
The outside surface 5 of the wall is subjected to the hot gas passing through the turbine and it therefore needs to be cooled. For this purpose, cooling channels are provided in the wall 1. At least some of these channels are of the same type as the channel shown in
The hole is said to be an adjustment portion since the minimum section of the hole 7 serves to adjust the rate at which air flows along the channel 6. Advantageously, the hole 7 is simple in shape. In the example shown, the hole 7 is inscribed in a circular cylinder. In addition, the axis B of the hole 7 is inclined at an angle G relative to the outside surface 5 (or if this surface 5 is not plane, relative to the tangent thereto on the axis B). The angle G is less than 90°, and preferably lies in the range 15° to 80°, so as to direct the stream of air F towards the outside surface 5 so that it remains as close as possible thereto. In other words, it is desired to make the velocity vectors of the air stream F at the outlet from the channel 6 as nearly parallel as possible to the plane of the outside surface 5.
In order to direct the stream of air F better against the outside surface 5 and in order to spread this stream of air F in the plane of the outside surface 5, the channel 6 presents a diffusion portion 9 following the hole 7. This diffusion portion 9 flares around the orifice 11 through which the cool air leaves the hole 7. This orifice 11 is situated preferably substantially in the bottom of the diffusion portion 9 relative to the outside surface 5. In front of the orifice, in the flow direction of the stream F, the diffusion portion 9 has a bottom whose front end 13 is substantially plane, sloping in the thickness of the wall at an angle g relative to the outside surface 5. The angle g preferably lies in the range 2° to 45°, and in any event it is smaller than the angle G so that the stream of air F, as guided by the front end 13 of the bottom is directed towards the outside surface 5.
The front end 13 of the bottom encourages the stream of cool air F leaving the hole 7 to come close to the outside surface 5. This air stream thus remains in contact with the outside surface 5, thus making it possible firstly to cool the surface 5 by heat exchange and secondly to create a protective film of air on said surface 5 that keeps the hot gas of the medium in which the wall 1 is situated at a distance from said surface 5.
Advantageously, the outline of the front end 13 of the bottom is generally triangular in shape, having one of its vertices pointing towards said orifice 11 (see
At the rear end, on the sides and in front of the orifice 11, there is a margin 15. The margin 15 goes around the orifice 11 in part and towards the front it joins the sides of the front end 13 of the bottom.
In the example shown in
It is also possible to provide rounding in each junction zone in order to avoid creating any edges. Under such circumstances, the angle P is measured between the general direction of the margin 15 and the front end 13 of the bottom.
In the example of
The front end 13 of the bottom and the margin 15 are inscribed in a cone 23 having a rounded end 24 and a conical surface 25 that presents a flat 26. The front end 13 of the bottom corresponds to the flat 26, and as can be seen in
With the shape of the cooling channel 6 in the wall element 1 described fully above, there follows a description of an implementation of the method of, the invention enabling a channel of this type to be formed.
In a first step of the method, the wall 1 is pierced by means of a laser. Laser piercing techniques are known to the person skilled in the art and they present the advantage of being fast and less expensive than electro-erosion techniques.
Then, in a second step, the recess corresponding to the diffusion portion 9 is formed in the wall 1 in its outside surface 5 by electroerosion. Naturally, this second step could be undertaken before the first.
For this second step, an electrode 20 is used that is of the type shown in
As shown in
It should be observed that the presence and the size of the lip 12 of the margin 15 (i.e. the extent to which it extends rearwards) depends on the radius of the curvature of the end 24 and on the depth to which the electrode 20 is pushed in.
In general, when forming the indentation, the following are selected: the shape of the electrode 21 and more particularly the shape of the cone 23, the radius of the curvature of the rounded end 24 and the position of the flat 26 (half-angles Y of the flare); the position of the electrode, and more particularly the orientation of the axis E of the cone 23 relative to the axis B of the hole 7; and the penetration depth of the electrode 20 into the wall 1; so as to form the front end 13 of the bottom in front of the orifice 11 and a flared margin 15 behind and on the side of the orifice 11 that meet the sides of the front end 13 where they form two edges 17. These edges are sufficiently rounded to avoid creating zones of weakness (see
The presence of the rear margin 15 enables the diffusion portion 9 to be made with a certain amount of tolerance relative to the hole 7. This is shown in
Number | Date | Country | Kind |
---|---|---|---|
05 07924 | Jul 2005 | FR | national |
06 50103 | Jan 2006 | FR | national |
Number | Name | Date | Kind |
---|---|---|---|
4197443 | Sidenstick | Apr 1980 | A |
4650949 | Field | Mar 1987 | A |
4653983 | Vehr | Mar 1987 | A |
4664597 | Auxier et al. | May 1987 | A |
4672727 | Field | Jun 1987 | A |
4684323 | Field | Aug 1987 | A |
4738588 | Field | Apr 1988 | A |
4762464 | Vertz et al. | Aug 1988 | A |
4819325 | Cross et al. | Apr 1989 | A |
5043553 | Corfe et al. | Aug 1991 | A |
5368441 | Sylvestro et al. | Nov 1994 | A |
5609779 | Crow et al. | Mar 1997 | A |
5683600 | Kelley et al. | Nov 1997 | A |
6183199 | Beeck et al. | Feb 2001 | B1 |
6206638 | Glynn et al. | Mar 2001 | B1 |
6287075 | Kercher | Sep 2001 | B1 |
6307175 | Blochlinger et al. | Oct 2001 | B1 |
6368060 | Fehrenbach et al. | Apr 2002 | B1 |
6573474 | Loringer | Jun 2003 | B1 |
6630645 | Richter et al. | Oct 2003 | B2 |
6759621 | Varin | Jul 2004 | B2 |
6897401 | Kildea | May 2005 | B2 |
6994514 | Soechting et al. | Feb 2006 | B2 |
7019257 | Stevens | Mar 2006 | B2 |
7041933 | Forrester et al. | May 2006 | B2 |
20020187039 | Rinck et al. | Dec 2002 | A1 |
Number | Date | Country |
---|---|---|
0 267 718 | May 1988 | EP |
1 228 832 | Aug 2002 | EP |
1 517 003 | Mar 2005 | EP |
2000-064806 | Feb 2000 | JP |
2000-141069 | May 2000 | JP |
2000-141069 | May 2000 | JP |
2005-090511 | Apr 2005 | JP |
Number | Date | Country | |
---|---|---|---|
20070025852 A1 | Feb 2007 | US |