The invention relates to a cladding panel for floors, walls or ceilings or similar applications according to the preamble of claim 1.
These panels on their side surfaces have grooves and tongues in order to lay these panels in a structure. In order to achieve as stable a structure as possible, it can also be provided that the panels be cemented to one another.
The priority objective of the invention is to be able to produce panels of the initially mentioned type as easily and economically as possible, furthermore to enable their storage over longer time intervals without adverse effects and in a space-saving manner, and finally to make the installation and in any case disassembly as quick and simple as possible, in a manner that preserves the panels as much as possible. Another objective is to prepare a stable, durable and solid surface from panels that have been joined to one another; alignment of the panels over a certain time interval will also be possible during installation.
These objectives are achieved in a cladding panel of the initially mentioned type with the features cited in the characterizing part of claim 1.
According to the invention, in the tongue or on at least the inside surface of one of the legs of the groove and/or on at least one surface of the tongue, at least one bead or strip is applied, for the locking of which another bead or strip is applied on the respectively assigned, and especially contacting surface of the tongue and/or groove. In this way, in the course of installing the cladding panels or in the course of joining them together, the beads act as locking means; the bead and the other bead interact as catch and locking elements. In the formation of at least one of the two beads with a cement, an adhesive connection between the groove and the tongue can be achieved. The beads of plastic and/or cement are applied at the factory in a simple and quick procedure, e.g., sprayed on.
A material working process, e.g., milling, to form a locking element is eliminated.
It is simply more necessary to make another bead assigned to one bead in the wall surface of the groove and/or in the tongue surfaces. This type of connecting technology and optionally cementing technology can be used for cladding panels of any materials, wood, wood materials, especially MDF, HDF, chips, etc.
A series of plastics are known that can be applied as the corresponding bead or strip or the other bead or strip to the surfaces of the groove and/or tongue. In particular, silicone plastics, plastics based on polyalkylene, especially PVC, PE, PP and hot-melt cements based on neoprene can be used for this purpose. It should be possible to deform such plastics by heat or for them to seal by heat and to extrude or shape them in bead form and to make them solidify in an adhesive manner on the respective material of the panel. In use, they are to have corresponding elasticity and viscosity in order to be able to act as a catch element.
Especially thermoplastics, elastomers and thermoplastic elastomers are suitable as thermally deformable plastics. As thermoplastics, polyolefins, vinyl polymers, polyamides, polyesters, polyurethane and ionomers can be used. As elastomers, various types of rubber can be used. As thermoplastic elastomers, TPE, TPR, TPO, SPS, TP-Q, and TP-U are suitable. As plastics, hot-melt cements or hot-sealing cements based on ethylene vinyl chloride, PA, PU, and EVA can also be used. Other plastics can also be used.
A series of cements are known that have sufficient strength to not be removed or to be damaged in their surface configuration when the tongue is pushed into the groove, but based on the penetrating atmospheric humidity and/or by application of water in the course of installation or use, they can be sufficiently activated to fully develop their adhesive action. After setting of the cement of the cement bead(s), the latter take action, on the one hand, based on the adhesive action, and, on the other hand, based on the locking action that has developed; the beads either interact with respect to their adhesive action and/or interact with the material of the tongue or the groove. It should be possible to apply the cements and plastics used to the respective material of the panel using a nozzle and for them to adhere well there.
Such cladding panels have the advantage that the handling and manipulation steps are greatly reduced when installing the panels on site; it is simply necessary to introduce water into the groove using a corresponding device and/or apply it to the tongue in order to activate the cement if this is desired at all. If it is a cement that hardens as a result of the existing moisture in the air, this procedure also is not necessary.
One special advantage is that due to the mass of the cement that is provided in the cement bead at the factory, a correctly dimensioned or sufficient amount of cement is present, and handling or removal of cement that has been applied in excess in any case or emergence of the cement from the tongue-in-groove connection is eliminated.
To achieve the catch and/or adhesive connection, relatively small amounts of cement are sufficient. In particular, contact between the groove and the tongues over as large an area as possible is to be achieved.
Here, especially glues that consist of water-soluble, animal (glutin, casein), vegetable (starch, dextrin, cellulose ether) or synthetic (polyacrylic acid derivatives, polyvinyl alcohol, polyvinyl pyrrolidone) polymers and water as solvents are suitable as cements. The latter belong to the class of single-component cold-setting cements in which the solvent (water) during the process of cementing is absorbed or evaporated. These glues harden as they cool, especially in a gelatin-like manner, and generally dry to a transparent mass that dissolves into a gel with high adhesive strength upon contact with water.
It is preferred when a cement that is dispersed in water or processed with water or a glue is applied as a cement bead and is dried in situ or at the factory. By the consumer applying water directly to this dried cement layer or by indirect intense contact with water that has been applied to the panel to be joined or its groove or tongue or by penetrating moisture, the dried cement is activated after the panels are joined to one another and returned into the active, adhesion-ready state. The application of the aqueous activator can take place by spraying or applying by means of a sponge or the like.
In one advantageous approach, first the cement beads are moistened with water, or a water film that at least wets the cement bead is applied or sprayed onto the tongues and/or into the grooves of the panels, and then the panels are joined to one another. The exposed time of the reactivated cement is chosen such that there is enough time for joining the panels to one another.
If the bead or strip is made of plastic, this embodiment has the advantage that the groove and the tongue can be easily locked to one another; if the bead or strip is formed from a cement, locking can take place accompanied by cementing.
It is advantageous if the features of claim 4 are implemented. In such an execution of the tongue and groove, the cohesion of the two cladding panels to be joined is improved and a coating with an essentially considerable stiffness is achieved. In this case, the cement of the cement beads can support the especially intimate connection between the groove and the tongue.
It is advantageous if the features of claim 6 are satisfied. In this way, the danger of damage or shearing-off of the cement beads or plastic beads when the tongue is inserted into the groove is reduced and their support on the surface to which the bead adheres is increased. Also, in this connection, it is advantageous if the cement bead adheres strongly in its recess and/or on the wall surfaces of the groove and/or the tongue surfaces. This strong adhesion is not to be entirely lost even when the cement is activated by contact with water; in particular this adhesion is to be made as strong as possible. The beads advantageously need project only slightly out of the recess.
Advantageously it is provided that the groove and the tongue are each made lengthwise or in one lengthwise side and/or lengthwise and in one transverse side of a panel, optionally the tongue and/or the groove and/or the beads or strips extending over the entire length of the respective side surface. Thus, optimum connectability and optimum coherence are achieved over all of the sides of the cladding panels during installation with the cladding panels to be connected.
The connection of the panels to be joined becomes simple when the features of claim 7 are used; joining of the flat surfaces is possible with little expenditure of force; it is simply necessary to overcome the elevations formed by the applied beads in order to insert them into the recesses. To do this, it is provided according to the invention that at least one leg, preferably the lower leg, of the groove can be widened or elastically bent up when the tongue is inserted and/or the plastic and/or cement used has the corresponding elastic behavior or viscosity.
The elastic widening of the legs of the groove undertaken by the locking cement beads can be partially, largely or completely cancelled again in the course of activation of the softening cement; thus the cross-sections of the cement beads can to a certain extent overlap. In this respect, the features of claim 19 are advantageous.
It is provided according to the invention that the cement of the cement beads or strips be water-soluble or upon contact with or supply of water and/or moisture can be partially dissolved and/or activated and/or formed by water-soluble glue, e.g., white glue, and/or by a pressure cement or a cement that can be activated by pressure or that develops an adhesive action when pressure is applied.
It is furthermore provided according to the invention that the panel is formed from wood material, MDF, HDF, plastic, recycled plastic, chips or chips bonded with resin (particle board) and optionally on its front surface or useful surface and/or on its back is provided in each case with at least one coating, e.g., a decorative coating, especially of plastic, decorative paper, wood, or the like.
The cross-sectional shape of the bead can be selected in a variety of ways; it is advantageous if the bead or strip and/or the recess and/or the recess in cross-section has a shape that is semicircular, lens-shaped, elliptical or elongated-rectangular, the transitions running rounded or bevelled from the plane surfaces to the beads.
Good coherence of two panels that are to be connected or of the groove and tongue arises when the features of claim 16 are implemented. In such an embodiment, the cement bead is in good contact with the parts that are to be joined, specifically the tongue and groove of two panels that are to be connected.
It is especially advantageous if according to the invention the features of the characterizing part of claim 10 are satisfied. In this way, the beads perform a double function, specifically they act as a locking element and as an element for connecting two panels.
The features of claim 29 are advantageous. With such a component that is designated an external tongue, it is simply necessary to mill out grooves on the peripheral surfaces of a panel; the components can be quickly produced in large amounts. The components are joined to the panels in part at the factory or this remains for the user to do.
In one especially advantageous embodiment of the invention the grooves and tongues are not aligned perpendicular to the side surfaces of the panels, but run perpendicular to the surface of the panels. Thus, locking of the groove and tongue when the panels are installed can take place by movement that takes place perpendicular to the panel surface. Regardless of this, all the advantages of the above-described tongue-in-groove connection possibilities can be used or provided.
The invention is explained in more detail below using the drawings that constitute, for example, schematic embodiments of the invention.
The shape of the groove and the shape of the tongue are matched to one another in order to ensure a good connection between the groove and the tongue. This shape allows the tongue 6 to be inserted into the groove 12 when the panels 1, 2 are aligned in the plane of the panel. It is possible to connect the panels 1, 2 in a checkerboard manner or offset against one another. Both the connection on the lengthwise sides and also on the narrow sides takes place by displacement essentially in the plane that is spanned by the panels 1, 2. The type of connection according to the invention could also be provided only on the transverse and narrow sides of panels that are connected on the lengthwise side in some other way, e.g., by swivelling or pivoting the panel to be connected.
On at least one tongue surface, in this case the tongue surface 7 near the surface, a bead 8 is applied or adheres especially securely to the tongue surface 7. At the corresponding or assigned location of the wall surface 5 of the groove 12 or of the leg 3, which wall surface is near the surface, when the panels have been joined, another bead 9 that is matched to the location of the bead 8 is formed in the otherwise preferably flat wall surface 5. When the two panels 1, 2 are joined or when the tongue 6 is inserted into the groove 12, the bead 8 comes to rest in the area behind the bead 9 or can lock with this other bead 9. The bead 8 has a rear surface 8a which is disposed behind a rear surface 9a of the second bead 9 so that the rear surfaces 8a and 9a face one another as seen in
It is advantageously provided that the cement of at least one of the cement beads or strips 8, 9 is water-soluble or upon contact with or supply of water and/or moisture can be partially dissolved and/or activated and/or is formed by water-soluble glue, e.g., white glue, and/or by a pressure cement or a cement that can be activated by pressure and that develops an adhesive action when pressure is applied. The cement of the cement beads 8, 9 can be activated by wetting the cement beads 8, 9 with water before joining the panels 1, 2 or by delivering water to the groove 12 and/or the tongue 6. Depending on the choice of the cement, it can also be provided that after locking of the cement bead 8 with the bead 9 by the atmospheric humidity that penetrates in the use of the panels 1, 2, the adhesive capacity of the cement beads 8, 9 is activated and thus an adhesive connection between the tongue 6 and the leg 3 of the groove 12 is produced. Fundamentally, cements can also be used that can be activated with substances other than water.
For joining the panels 1, 2 in this case for insertion of the tongue 6 provided with the bead 8 into the groove 12, it is provided according to the invention that at least one leg 3, 4 of the groove 12 can be elastically widened or elastically bent up when the tongue 6 is inserted.
Fundamentally, it is possible to form at least one or more bead(s) 8 or 9 that lie parallel next to one another on one or both tongue surfaces 7 or on one or both wall surfaces 5 of the groove 12. It must simply be watched that to each bead 8 is assigned a corresponding other bead 9 at the corresponding location in the wall opposite it, so that these two beads 8, 9 can lock, as is shown in
Accordingly, in
In one embodiment of the invention according to
It can apply to this and also to all other embodiments that advantageously the tongue 6 and the groove 12 can be connected at least over one part or optionally over the entire insertion area(s) of the tongue 6 by positive connection or with a snug fit and/or that the area of the tongue 6 that lies in front of the bead toward the free end of the tongue 6 can be inserted by a positive connection or with a snug fit into the groove 12. In all embodiments, it can be provided that the tongue 6 and/or the groove 12 and/or the beads 8 and 9 extend over the entire length of the respective side surface 17, and/or that the beads 8 and 9 and optionally the recess 10 (
As the material for the panels according to the invention, it is advantageously provided that the panel 1, 2 is formed from wood, wood material, MDF, HDF, plastic, recycled plastic, chips with synthetic resin or bonded chips (particle board) and optionally is provided on its front or useful surface and/or on its back in each case with at least one coating 13, 14, e.g., a decorative coating, especially of plastic or decorative paper. Furthermore, it can be advantageously provided that the groove 12 and the tongue 6 are made from the material of the panels 1, 2 or are milled out of them, or that the tongue 6 is formed integrally with the material of the panels 1, 2. For all embodiments and also in the embodiment according to
In the embodiment according to
In one embodiment according to
In the embodiment according to
It can be provided according to the invention that some of the bead or strip 8 and 9 is arranged countersunk in a recess 10 that is made in the wall surface 5 of the groove 12 and/or in the tongue surface 7. At the same time, the recess 10 helps the applied bead 8 or 9 to be joined securely to the respective wall surface and not to be sheared off when the tongue 6 is inserted into the groove 12. As shown in
The panels 1, 2 can be provided with coats 13 or 14, e.g., of wood, plastic, paper or the like, in order to configure the useful surface or bottom surface accordingly. These supports, however, do not have any effect on the connecting technique according to the invention.
The selected cross-sections of the beads 8 and 9 and of the recesses 10 are optional; the region of the bead 8 or 9 that projects out of the recess 10 or over the wall surface 5 of the groove 12 or the tongue surface 7 is held by the recess 10 especially during cementing or softening or comes into contact with its surfaces and optionally cements the tongue 6 to the legs 3, 4 of the groove 12. The cross-sectional shape of the recess 10 can be oblong, rectangular, triangular, lens-shaped, triangularly elliptical or the like.
Fundamentally, at least as shown in
It is to be generally avoided that the legs 3, 4 of the groove 12 that are elastically widened when the tongue 6 is inserted into the groove 12 remain in the widened position. In the widened state, the joint 16 between the surfaces 18 of the two panels 1, 2 could form a step that would be subjected to increased wear, provided that not only the lower leg remains elastically widened. In one especially advantageous embodiment of the invention, it is provided that the leg 3 of the groove 12 that is near the surface is made more or less elastic, especially inelastic anyway, and only the leg near the bottom or the lower leg of the groove is made able to deflect elastically. Thus, it can be avoided that the upper leg 3 near the surface will be bent up by more or less deformable beads 8, 9, but only the lower, weaker or thinner leg 4 of the groove 12 is bent down. To prevent the upper leg 3 of a groove 12 from bending up, it can also be advantageously provided that the bead(s) 8, 9 is (are) made simply on the tongue surface 7 that is pointed down and on the wall surface 5 of the lower leg 4 of the groove 12. In this way, both the tongue 6 and also the upper leg 3 of the groove 12 would counteract the arching of the connecting site if the extent or the volume of the bead is made too large or, when a cement is used, the latter is not made soft enough and/or the volume stipulated for it between the groove and tongue is not made large enough.
The shape of recess 10 can be lens-shaped, triangular, semi-elliptical or oblong-rectangular. It is provided that this recess 10 is made as a depression in the otherwise flat tongue surface 7 or the flat wall surface 5 of the groove 12. Thus, the cement application or the amount of plastic for the beads 8, 9 should be defined or limited to certain areas.
In an embodiment of
Advantageously, the beads 8, 9, as shown in
It can be advantageous if the front edge areas of the tongue 6 have rounding or bevelling 19 as is shown in
In principle or in all embodiments, the tongue 6 can have rounding 19 directly in front of the beads 9. Thus, it also becomes possible to make the tongues 6 shorter and the groove 12 less deep. The joint 16 in the area of the panels 1, 2 that is near the surface is made such that the areas of the end face 17 that is near the surface adjoin one another and a gap is avoided as far as possible. In the area of the panels 1, 2 that is away from the surface or near the bottom, it is provided that the end faces 17 do not touch one another or that a gap 15 is formed between them. This is achieved especially in that the leg 4 of the groove 12 near the bottom is made slightly shorter than the leg 3 near the surface.
It is generally advantageous if the beads or strips 8, 9 are applied roughly in the middle or in the middle area on the tongue surface 7 or on the wall 5 of the groove 12 or of the legs 3, 5.
It can be provided according to the invention that the width B of the bead or strip 8 or 9 is one to nine times, preferably one to seven times, especially two to five times, as great as its height H. Furthermore, according to the invention, it can be provided that the cement bead or strip 8, 9 comprises an adhesive-latent cement material, preferably a polymer cement that can be emulsified with water, and the cement material can be converted into the adhesive-ready or adhesive state by wetting with water, and/or that the plastic or the cement material of the cement bead or strip 8 and 9 that can be (re)activated by means of water or moisture is applied with an essentially uniform layer thickness of 0.1 to 0.6 mm, especially from 0.2 to 0.5 mm, at thickness tolerances in the range from ±0.05 to 0.1 mm, and/or that the cement of the cement bead or strip 8 is formed by a quick-setting or mounting glue based on polyvinyl acetate, such as, for example, DORUS MDO 55 from the Henkel Company, or a commercial wood glue, e.g., based on starch and protein. It can be advantageous if the width B of the cement bead or strip 8 corresponds to 5 to 25%, preferably 9 to 21%, especially 12 to 17%, of the thickness D of the groove 12.
It should be noted that the attachment of the beads 8, 9 to the corresponding surfaces 5, 7 can take place either directly on these surfaces 5, 7 or in the recesses 10 that were made in the especially flat surfaces 5, 7. Advantageously, the applied beads 8, 9 project roughly 0.1 to 0.2 mm over the respective surface 5, 7.
Advantageously, the tongue 6 on each tongue surface 7 bears a bead 9 and on each leg 3, 4 of the groove 12, a cement bead 8 is optionally applied in a recess 10.
The important action of the applied beads 8, 9 consists in their locking action that is used especially in the course of installing and matching of the panels to be joined.
When the edges of the free end of the tongue 6 are rounded accordingly and/or the inner edges of the wall surfaces 5 of the legs 3, 4 of the groove 12 are rounded, it is also possible during installation to first lay the panels 1, 2 to be joined to one another at a certain angle on one another in order to attain entry of the tongue 6 into the groove 12 to a certain extent. The final locking of the tongue 6 and the groove 12 or the last interlocking step that ends with contact of the end faces 17 in the area near the surface is in any case only possible when the panels 1, 2 are moved relative to one another in the plane of the panels.
Care should be taken that the cement is softened or becomes soft accordingly so that no unevenness is formed in the joint area of the panels 1, 2 that are to be joined to one another. The amount of cement to be applied in the cement beads 8, 9 depends mainly on the geometrical circumstances between the tongue 6 and the groove 12 or on the size of the recesses 10 and especially also on the viscosity of the reactivated cement.
The component 6′ constitutes a double tongue 6. The advantage of this so-called external tongue is that the panels 1, 2 can be made solely with the corresponding grooves 12 all around on their side surfaces and the external tongues 6′ can be inserted into the grooves 12 at the factory or just during installation. The insertion of an external tongue 6′ also takes place in the plane of the respective panel 1, 2. The panels 1, 2 are also joined when the external tongues 6′ are inserted at least in the last joining step by displacement in the plane of the panel.
All statements regarding the tongues 6 apply both to the left part and also to the right part of the component 6′ that is shown in
As already described above in conjunction with
Furthermore, the area B can also be defined as a groove area that has been turned by 90° and that is formed in the panel 2 in the sense of the preceding description and
If it is provided that the panel 2 in its side end area ends with a boundary surface 30 at a distance from the outside leg 4 of the groove 12 in order to facilitate joining of the panels 1, 2, the corresponding beads 8 and 9 are provided simply on the tongue 6 that can be inserted into the groove 12 of the area A of the panel 1.
The leg 3 of the groove 12 in the panel 1 is integrated into the panel body of the panel 1 or is represented by the panel body.
The beads 8 and 9 can also be located in recesses 10 here; however, such recesses 10 are not indicated in
The grooves 12, tongues 6 and recesses 10 are preferably produced by milling.
The shape of the grooves 12 and the tongues 6 are advantageously matched to one another, but this is not absolutely essential. Grooves and tongues that have not been matched to one another in terms of shape can also be held together with the beads 8, 9 provided according to the invention.
The beads 8 and/or 9 can also be applied in the form of successive partial pieces, i.e., optionally with interruptions.
It is advantageous if at least one bead extends parallel to or along the edge of the end face 17 or in the lengthwise direction of the panel 1, 2. Fundamentally, the path of the bead, optionally dictated by production or by intention, can deviate from a parallel course with respect to the lengthwise extension of the panel.
In this case, the tongue on its tongue surfaces bears at least one bead or strip 8 that can be locked to at least one other bead 9 on the groove side surfaces 5, as is shown in
The mutual connection of the panels 1, 2, as is shown in
It is advantageous here if the radii of curvature of the inside surfaces of the groove 12 and of the surfaces of the tongue 6 are made the same size, or the thickness of the tongue 6 corresponds to the width of the groove 12 or is kept somewhat smaller.
In
It is quite generally advantageous if the beads 8 and 9 are directly opposite one another with respect to the tongue 6 and the groove 12.
It is possible to make several beads 8 and other beads 9 interacting with one another on the curved tongue surfaces and on the curved groove side surfaces.
It is furthermore possible for the tongue surfaces and the side surfaces of the groove 12 to have straight and curved segments, the straight segments not preventing or allowing swivelling of the attached panel 2 when two panels 1, 2 are being joined.
Quite generally, the beads 8 and the other beads 9 extend behind one another, or the beads 8 on the tongues 6 extend behind the other beads 9 in the groove 12. The location of the beads 8 and of the other beads 9 on the tongue surfaces and the side wall surfaces of the grooves 12 is chosen accordingly. The beads 8, 9 that extend behind one another adjoin one another or can be connected to one another.
The other beads 9 on the wall surfaces of the groove 12 hold the beads 8 securely on the tongue surfaces and thus in the groove 12.
When the tongue 6 is inserted into the groove 12, the groove legs can be slightly, optionally permanently, widened or bent up.
The catch function of the beads 8 and the other beads 9 is essentially the same when they are being inserted and pivoted in.
In particular, in
All features relating to the panels that can be joined for insertion in a plane can also be implemented for panels that can be joined by swivelling. This relates especially to the materials as well as the shape and position of the beads.
Number | Date | Country | Kind |
---|---|---|---|
A 358/2003 | Mar 2003 | AT | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/AT2004/000049 | 2/18/2004 | WO | 00 | 6/23/2006 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2004/079128 | 9/16/2004 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
1540128 | Houston | Jun 1925 | A |
1575821 | Daniels | Mar 1926 | A |
1602256 | Sellin | Oct 1926 | A |
1602267 | Karwisch | Oct 1926 | A |
1660480 | Daniels | Feb 1928 | A |
1718702 | Pfiester | Jun 1929 | A |
1778069 | Fetz | Oct 1930 | A |
1846658 | Rockwell | Feb 1932 | A |
2736930 | Longley | Mar 1956 | A |
2839790 | Collings | Jun 1958 | A |
2894292 | Gramelspacher | Jul 1959 | A |
3719015 | Misawa | Mar 1973 | A |
3943022 | Susnjara | Mar 1976 | A |
3998024 | Frandsen | Dec 1976 | A |
4037377 | Howell et al. | Jul 1977 | A |
4095388 | Breault | Jun 1978 | A |
4769963 | Meyerson | Sep 1988 | A |
4944416 | Petersen et al. | Jul 1990 | A |
5165816 | Parasin | Nov 1992 | A |
5216861 | Meyerson | Jun 1993 | A |
5362560 | Ehrhart et al. | Nov 1994 | A |
5381638 | Andersson | Jan 1995 | A |
5497589 | Porter | Mar 1996 | A |
5502939 | Zadok et al. | Apr 1996 | A |
5618602 | Nelson | Apr 1997 | A |
5755068 | Ormiston | May 1998 | A |
5827592 | Van Gulik et al. | Oct 1998 | A |
5830549 | Sweet et al. | Nov 1998 | A |
5899038 | Stroppiana | May 1999 | A |
6006486 | Moriau et al. | Dec 1999 | A |
6021615 | Brown | Feb 2000 | A |
6029416 | Andersson | Feb 2000 | A |
6101778 | Mårtensson | Aug 2000 | A |
6131355 | Groh et al. | Oct 2000 | A |
6209278 | Tychsen | Apr 2001 | B1 |
6216409 | Roy et al. | Apr 2001 | B1 |
6314701 | Meyerson | Nov 2001 | B1 |
6324809 | Nelson | Dec 2001 | B1 |
6345481 | Nelson | Feb 2002 | B1 |
6397547 | Mårtensson | Jun 2002 | B1 |
6418683 | Martensson et al. | Jul 2002 | B1 |
6421970 | Martensson et al. | Jul 2002 | B1 |
6438919 | Knauseder | Aug 2002 | B1 |
6505452 | Hannig et al. | Jan 2003 | B1 |
6536178 | Pålsson et al. | Mar 2003 | B1 |
6581351 | DeVivi | Jun 2003 | B2 |
6588166 | Martensson et al. | Jul 2003 | B2 |
6601359 | Olofsson | Aug 2003 | B2 |
6606834 | Martensson et al. | Aug 2003 | B2 |
6675544 | Ou et al. | Jan 2004 | B1 |
6682254 | Olofsson et al. | Jan 2004 | B1 |
6808777 | Andersson et al. | Oct 2004 | B2 |
6823638 | Stanchfield | Nov 2004 | B2 |
6880307 | Schwitte et al. | Apr 2005 | B2 |
7037024 | Steinwender | May 2006 | B2 |
7093399 | Thiers et al. | Aug 2006 | B2 |
7121058 | Palsson et al. | Oct 2006 | B2 |
7188456 | Knauseder | Mar 2007 | B2 |
7441384 | Miller et al. | Oct 2008 | B2 |
20010034991 | Martensson et al. | Nov 2001 | A1 |
20020020127 | Thiers et al. | Feb 2002 | A1 |
20020046526 | Knauseder | Apr 2002 | A1 |
20020100242 | Olofsson | Aug 2002 | A1 |
20020108343 | Knauseder | Aug 2002 | A1 |
20020112429 | Niese et al. | Aug 2002 | A1 |
20020148551 | Knauseder | Oct 2002 | A1 |
20020152707 | Martensson | Oct 2002 | A1 |
20020189747 | Steinwender | Dec 2002 | A1 |
20030003258 | Durso et al. | Jan 2003 | A1 |
20030033777 | Thiers et al. | Feb 2003 | A1 |
20030041545 | Stanchfield | Mar 2003 | A1 |
20030079425 | Morgan et al. | May 2003 | A1 |
20030101681 | Tychsen | Jun 2003 | A1 |
20030141004 | Palmblad et al. | Jul 2003 | A1 |
20030208980 | Miller et al. | Nov 2003 | A1 |
20030213211 | Morgan et al. | Nov 2003 | A1 |
20040031227 | Knauseder | Feb 2004 | A1 |
20040107665 | Faxe et al. | Jun 2004 | A1 |
20040211143 | Hanning | Oct 2004 | A1 |
20040250492 | Becker | Dec 2004 | A1 |
20060236643 | Moriau et al. | Oct 2006 | A1 |
Number | Date | Country |
---|---|---|
2 434 168 | Jul 2002 | CA |
202 16 584 | Jan 2003 | DE |
1229181 | Aug 2002 | EP |
2205079 | May 1974 | FR |
2647837 | Dec 1990 | FR |
2256023 | Nov 1992 | GB |
2 377 457 | Jan 2003 | GB |
58 14185 | Mar 1983 | JP |
59 005744 | Jan 1984 | JP |
6 8587 | Jan 1994 | JP |
7 44657 | Feb 1995 | JP |
8 261640 | Oct 1996 | JP |
2001 73535 | Mar 2001 | JP |
2001 193175 | Jul 2001 | JP |
2001 234016 | Aug 2001 | JP |
WO9821428 | May 1998 | SE |
WO-97 47834 | Dec 1997 | WO |
Entry |
---|
Abstract of DE 202 16 584—Published Jan. 16, 2003—Kaindl Wals. |
Sekisui Chemical Co. Ltd., “Floor Finishing Structure,” Data Supplied from the espacenet worldwide database, Publication Date: Mar. 21, 2001; English Abstract of JP 2001-073535. |
Unilin Beheer BV, “Floor Covering, Consisting of Hard Floor Panels and Method for Manufacturing such Floor Panels,” Data Supplied from the espacenet worldwide database, Publication Date: Dec. 18, 1997; English Abstract of WO97 47834. |
Mannington Mills, “Thermoplastic Plank and Method for Producing the Same,” Data Supplied from espacenet worldwide database, Publication Date: Aug. 28, 2001; English Abstract of JP 2001 234016. |
Showa Aluminum Corp., “Joining Device for Panels,” Data Supplied from the espacenet worldwide database, Publication Date: Oct. 11, 1996; English Abstract of JP 8 261640. |
Daiken Trade & Industry, “Connecting Structure of Wooden Building Plate,” Data Supplied from the espacenet worldwide database, Publication Date: Jul. 17, 2001; English Abstract of JP 2001 193175. |
English Translation of the Reason for Rejection for Japanese Patent Application No. 2004 528159 dispatched on Feb. 26, 2010. |
Office Action for Related Canadian Application No. 2 517 907 dated Mar. 22, 2011. |
Number | Date | Country | |
---|---|---|---|
20060272262 A1 | Dec 2006 | US |