Claims
- 1. A cutting insert comprising:
- (a) a support member; and
- (b) at least one cutting member brazed to the support member, the cutting member having at least one cutting surface and comprising a selfbonded polycrystalline superabrasive material being formed such that the cutting member has a width substantially less than its depth ad attached to the support member such that the width is the cutting surface, such that the brazing conditions minimize thermal damage to the support member ad superabrasive materials.
- 2. A cutting insert as recited in claim 1 wherein the insert has a means for indexing the insert to different cutting surfaces.
- 3. A cutting insert as recited in claims 1 or 2 wherein the selfbonded polycrystaline superabrasive material is selected from the group consisting of cubic boron nitride, polycrystaline diamond, thermally stable polycrystaline diamond and coated thermally stable polycrystaline diamond.
- 4. A cutting insert as recited in claim 1 or 2 wherein the support member is a cemented metal carbide.
- 5. A cutting insert as recited in claim 4 wherein the cemented metal carbide is selected from the group consisting of cemented tungsten carbide, cemented titanium carbide, cemented tungsten carbide and cemented tantalum carbide.
- 6. A cutting insert comprising:
- (a) a support member having at least one pre-cut slot therein; and
- (b) at least one cutting member brazed to the support member, the cutting member having at least one cutting surface and being formed as to mate to the pre-cut slot and comprising a selfbonded polycrystaline superabrasive material being formed such that the cutting member has a width substantially less than its depth and attached to the support member such that the width is the cutting surface, such that the brazing conditions minimize thermal damage to the support member and superabrasive material.
- 7. A cutting insert as recited in claim 6 wherein the insert has a means for indexing the insert to different cutting surfaces.
- 8. A cutting insert as recited in claims 6 or 7 wherein the selfbonded polycrystaline superabrasive material is selected from the group consisting of cubic boron nitride, polycrystaline diamond, thermally stable polycrystaline diamond and coated thermally stable polycrystaline diamond.
- 9. A cutting insert as recited in claims 6 or 7 wherein the support member is a cemented metal carbide.
- 10. A cutting insert as recited in claim 9 wherein the cemented metal carbide is selected from the group consisting of cemented tungsten carbide, cemented titanium carbide, cemented tungsten-molybdenum carbide and cemented tantalum carbide.
- 11. A cutting insert as recited in claims 6 or 7 wherein the support member and the cutting member are attached to each other by brazing.
- 12. A method for making a cutting insert, which comprising brazing a support member to at least one cutting member, the cutting member having at least one cutting surface and comprising a selfbonded polycrystalline superabrasive material being formed having a width substantially less than its depth and attached to the support member such that the width is the cutting surface, such that the brazing conditions minimize thermal damage to the support member and superabrasive material.
- 13. A method for making a cutting insert as recited in claim 12 wherein the insert has a means for indexing the insert to different cutting surfaces.
- 14. A method for making a cutting insert as recited in claims 12 or 13 wherein the selfbonded polycrystaline superabrasive material is selected from the group consisting of cubic boron nitride, polycrystaline diamond, thermally stable polycrystaline diamond and coated thermally stable polycrystaline diamond.
- 15. A method for making a cutting insert as recited in claims 12 or 13 wherein the support member is a cemented metal.
- 16. A method for making a cutting insert as recited in claim 15 wherein the cemented metal is selected from the group consisting of cemented tungsten carbide, cemented titanium carbide, cemented tungsten-molybdenum carbide and cemented tantalum carbide.
- 17. A method for making a cutting insert as recited in claims 12 or 13 wherein the support member and cutting member are attached by brazing.
- 18. A cutting insert consisting essentially of:
- (a) a support member; and
- (b) at least one cutting member brazed to the support member, the cutting member having at least one cutting surface and comprising a selfbonded polycrystalline superabrasive material being formed such that the cutting member has a width substantially less than its depth and attached to the support member such that the width is the cutting surface, such that the brazing conditions minimize thermal damage to the support member and superabrasive material.
Parent Case Info
This is a continuation of U.S. patent application Ser. No. 07/888,245 filed on May 22, 1992, now abandoned, which is a continuation of U.S. patent application Ser. No. 07/557,906 filed on Jul. 28, 1990 also abandoned.
US Referenced Citations (4)
Continuations (2)
|
Number |
Date |
Country |
Parent |
888245 |
May 1992 |
|
Parent |
557906 |
Jul 1990 |
|