This application is a continuing application of U.S. patent application Ser. No. 08/850,319 now abandoned, which was filed with the United States Patent and Trademark office on May 2, 1997. The entire disclosure of the U.S. patent application Ser. No. 08/850,319 is incorporated herein by reference.
Number | Name | Date | Kind |
---|---|---|---|
4442062 | Fujii et al. | Apr 1984 | A |
5010145 | Ikada et al. | Apr 1991 | A |
5142023 | Gruber et al. | Aug 1992 | A |
5180765 | Sinclair | Jan 1993 | A |
5216050 | Sinclair | Jun 1993 | A |
5247059 | Gruber et al. | Sep 1993 | A |
5252642 | Sinclair et al. | Oct 1993 | A |
5274073 | Gruber et al. | Dec 1993 | A |
5294469 | Suzuki et al. | Mar 1994 | A |
5338822 | Gruber et al. | Aug 1994 | A |
5391423 | Wunk et al. | Feb 1995 | A |
5424346 | Sinclair | Jun 1995 | A |
5437918 | Taniguchi et al. | Aug 1995 | A |
5444113 | Sinclair et al. | Aug 1995 | A |
5475080 | Gruber et al. | Dec 1995 | A |
5484881 | Gruber et al. | Jan 1996 | A |
5502158 | Sinclair et al. | Mar 1996 | A |
5525706 | Gruber et al. | Jun 1996 | A |
5536807 | Gruber et al. | Jul 1996 | A |
5545371 | Lu | Aug 1996 | A |
5567510 | Patnode et al. | Oct 1996 | A |
5594095 | Gruber et al. | Jan 1997 | A |
Number | Date | Country |
---|---|---|
0 597 427 | May 1994 | EP |
637641 | Feb 1995 | EP |
0 669 358 | Aug 1995 | EP |
723043 | Jul 1996 | EP |
731198 | Sep 1996 | EP |
747065 | Dec 1996 | EP |
765959 | Feb 1997 | EP |
2725731 | Apr 1996 | FR |
2732196 | Apr 1996 | FR |
07008520 | Jan 1995 | JP |
07133569 | May 1995 | JP |
08283558 | Oct 1996 | JP |
9077124 | Mar 1997 | JP |
9077863 | Mar 1997 | JP |
9095605 | Apr 1997 | JP |
9095847 | Apr 1997 | JP |
9095852 | Apr 1997 | JP |
WO 9001521 | Feb 1990 | WO |
WO 9204412 | Mar 1992 | WO |
WO 9204413 | Mar 1992 | WO |
WO 9406856 | Mar 1994 | WO |
WO 9408078 | Apr 1994 | WO |
WO 9630576 | Oct 1996 | WO |
Entry |
---|
Matsui, M., “Biodegradable fibers made of poly-lactic acid”, Chemical Fibers International, 46(5):318 (Oct. 1996). |
R. M. Ikeda, Shrinkage Measurements of Stress-Induced Crystallization in Oriented Amorphous Pet, Journal of Polymer Science: Polymers Letters Edition, v. 18, pp. 325-331 (1980). |
W. Hoogsteen et al., Crystal Structure, Conformation, and Morphology of Solution-Spun Poly(L-lactide) Fibers, Macromolecules, v. 23, pp. 634-642 (1990). |
S. D. Long et al., Shrinkage Force Studies of Oriented Polyethylene Terephthalate, Journal of Applied Polymer Science, v. 42, 1921-1929 (1991). |
P. B. Rim et al., Properties of PET Fibers with High Modulus and Low Shrinkage (HMLS). I. Yarn Properties and Morphology, Journal of Applied Polymer Science, v. 42, pp. 1807-1813 (1991). |
S. R. Malkan et al., A Review on Melt Blowing Technology, INB Nonwovens, pp. 46-52 (Feb. 1991). |
S. R. Malkan et al., A Review of Melt Blowing Technology (Part II), INB Nonwovens, pp. 22-28 (Mar. 1991). |
S. R. Malkan et al., A Review on SpunbondTechnology Part I, INB Nonwovens, pp. 4-14 (Mar. 1992). |
Seung Jin Kim et al., Effects of Textile Processing and Fabric Structural Parameters to the Physical Properties of New Synthetic Fabrics, Journal of the Korean Fiber Society, v. 32, No. 8, pp. 760-765 (1995). |
S. R. Malkan, An Overview of Spunbonding and Meltblowing Technologies, Tappi Journal, v. 78, No. 6, pp. 185-190 (Jun. 1995). |
Dr. Ronald Smorada, Spunbonded and Melt Blown Nonwovens: The Basics, Nonwovens Industry, pp. 48-56 (Oct. 1996). |
H. R. Borkar, Effect of Spinning Speed on Physical Properties and Dyability of Polyester Filaments, pp. 31-37. |
Number | Date | Country | |
---|---|---|---|
Parent | 08/850319 | May 1997 | US |
Child | 09/072326 | US |