The invention relates generally to the protection and/or treatment of a submerged surface such as a ship hull.
More particularly, it relates to a device for the containment, protection and/or treatment of a submerged surface such as a ship hull (other non-limiting examples: surfaces in contact with water: finger pier, beacon, offshore platform, dock, barge, swimming pool, pond, floating homes) comprising an impervious or semi-impervious flexible shell made of several portions: a mainly submerged lower portion and a mostly emerged upper portion.
All of the surfaces of objects, structures, ships or buildings submerged in water cover with algae or molluscs. To avoid or minimize this problem, the most frequently used method is antifouling (most often through paint biocide). However, firstly, this technique forces to clean the hull and repaint it every year, thus drydocking the ship. Secondly, continuing contact between the anfoulings and surrounding water causes major direct and indirect pollution in ports and bays.
Many patents were filed relating to the protection of the hull that offer an alternative to this technique; a shell is slipped under the hull (
Some literature describes devices in which the residual water between the impervious film and the hull is pumped to allow the hull out of the water, the efficiency of which depends on the device. Other devices keep this residual water trapped, preventing the growth of the aforementioned organisms for lack of movement and light. Other devices add a product destroying living organisms to the residual water. All these devices exhibit the same drawback: providing a material the features of which are suitable for both the emerged and submerged portions and combining all the desired features essential for sustainability in the conditions of use is very difficult.
Still, some materials combine most of the desirable features, but at a very high cost and with an excessive specific gravity. For example, Teflon could be used if not for its price; the cost of production would not allow mass marketing, thus remaining mostly a technical solution.
Another issue occurred during previous development attempts. Marine organisms cling to the outer side of the shell. They grow all the easier as this surface is not coated with antifouling paint biocide. After about ten months, it is therefore covered with a very large amount of algae and molluscs. Thus, the surface should be cleaned; this procedure is not always practical. In addition, some films or webs are fragile; marine organisms have a high adhesion capacity, thus getting more difficult to dislodge over the years (the surface being altered and therefore facilitating their development and adhesion). Mechanical brushing is thus often necessary, leading to a fast degradation of the surfaces. Stronger webs, on the other hand, should be thickened or strengthened with a fabric or fiber, deteriorating flexibility and especially weight features.
Although the cleaning is easier than that of the hull of the ship, which requires drydocking and renewal of antifouling, this procedure remains unpractical. In order to demonstrate the difficulty of reconciling all the features and although
To overcome the aforementioned drawbacks of the prior art, the present invention provides a device hereinafter called “shell” which consists of at least two discrete portions: an emerged portion (1) and a submerged portion (2), with several variants. This simplifies the manufacture of the device by separating the abovementioned issues. The features of each portion can thus be optimized, allowing for the selection of materials with distinct properties, adapted to the respective media and desired characteristics.
In brief
For the upper emerged portion 1, the main features are: mechanical strength (for example tensile strength above 10N/mm2 or 10 MPa) and ultraviolet light resistance. The small surface area of this portion will allow for more expensive materials (specially formulated and optionally displaying a difference in specific gravity or weight vs. the submerged portion).
For the lower submerged portion 2, the main features are: flexibility, low specific gravity (less than 1), ease of cleaning, hydrophobicity, lightness, resistance to materials and substances with which it is in contact (propeller, rudder, antifouling or even detergent). Indeed, despite their dramatic evolution, some antifouling products remain polluting and aggressive. For special treatment of the hull, it will also be of interest to use the device as a containment device. The material can thus be chosen depending on the treatments.
Other advantageous and non-limiting features of the device according to the invention are as follows:
The following description, with reference to the appended drawings is given as a non limiting example and will allow for understanding the invention and how it can be embodied for a ship.
Appended drawings:
The entire device consists of
In the main embodiment, the device consists of at least two main portions 1 and 2 having features (physical or chemical) adapted to their respective different media: an emerged portion 1 surrounding the hull of the ship at or from the waterline, and secondly, a submerged portion 2 of a surface area always greater than the preceding, which includes the entirety of the submerged portion to protect 5 (in this example the hull of the ship), both portions 1 and 2 being assembled permanently, by stitching, gluing or welding fasteners, rivets 3 (
In this embodiment, the upper emerged portion 1 is made of a flexible material whose two main features are mechanical strength, (for example tensile strength above 10N/mm2 or 10 MPa), tear, lengthening and weathering resistance (particularly UV resistance). Flexibility is required as well as water resistance, but these features are less critical, the portion being only very partially in contact with water. Non limiting examples of materials: fabrics, films or PVC webs, nylon, polyurethane or polyurethane webbing, specially formulated PE or PP with additives or anti UV agents, reflective layer, complex combining the mentioned materials, . . .
In this embodiment, the constituent material of the outer side of at least the upper portion is thus selected for imparting to said upper portion a resistance to ultraviolet (UV) radiation that is higher than for the lower portion.
Higher resistance to ultraviolet (UV) radiation refers to the fact that the material comprising at least the outer portion of the upper portion retains a mechanical strength (tensile, break, shear) that is at least 3 times that of the lower portion, when they (emerged upper portion and lower portion) are directly exposed in an identical manner (same intensity, same duration, same wavelength) equaling a mean exposition in southern France for three years.
Other method of UV resistance characterization.
After being exposed for 3 years to the above described conditions, the material comprising at least the outer surface of the upper portion must retain at least 70% of its tensile strength, its tear resistance or its shear strength. Example: this material comprising at least the outer surface of the upper portion and having before exposition a tensile strength of 10N/mm2 (10 MPa) must retain a tensile strength of at least 7N/mm2 (7 MPa) after 3 years of exposition to the above described conditions.
On the other hand, after being exposed for 3 years to the same above described conditions, the material comprising at least the outer surface of the lower portion must retain less than 70% of its tensile strength, its tear resistance or its shear strength.
In this embodiment, the submerged portion 2 is made of a material whose main features are flexibility, resistance to water (hydrophobic), light weight (weight of preferably less than 500 g/m2) and a specific gravity of less than 1. Another advantageous feature is to provide a very low adhesion to marine organisms. This feature could optionally be improved in the case of a durable device because these organisms must be dislodged as easily as possible for ease of cleaning. Example: PE, reinforced or not, can be specifically formulated or surface-treated to improve the desired features.
In this embodiment, the submerged portion 2 may be partially or totally reinforced with woven or non-woven fibers.
In this main embodiment, the complete device is provided with means for attachment 6 (loop, hole, grommet) and fastening 8 (straps, ropes, sandow cords, hooks . . . ) mainly placed on the emerged portion 1 which allow for its placement and holding in place.
In another main embodiment, the emerged portion 1 and the submerged portion 2 are assembled together by a fastening system 4 which is reversible (
The two main embodiments detailed above allow for variants that can be applied to both embodiments. We therefore define variants for the emerged portion 1 and for the submerged portion 2. These variants may be advantageously blended in one or the other of the two main embodiments of the complete device we call a shell.
Below are detailed variants of the emerged portion 1 for the two main embodiments
Below are given several examples of embodiments of the emerged portion 1 of the device according to the invention:
The emerged portion 1 may consists of at least one outer film (exposed to ultraviolet light) and mostly opposite to the portion to protect, to be selected from any of the following non-limiting materials: PVC, polyurethane, hypalon, nylon, with an ultraviolet resistance that is superior to the materials making up portion 2, trapping a foamed material 7, see
Below are detailed variants of the submerged portion 2 for the two main embodiments
Below are given several examples of embodiments of the submerged portion 2 of the device according to the invention:
In another variant, the submerged portion 2 or 2b is may be completely disposable and recyclable (
In another embodiment, the submerged portion 2 has a thickness of less than 500 μm.
In another embodiment, the submerged portion 2 is partially reinforced by a strip of non-woven fibers or another additional film or layer 9 (
In another embodiment, the submerged portion 2 is reinforced in areas suffering from friction or additional strain (propeller, keel . . . ) by a layer of non-woven fibers or another film to increase their resistance.
In another embodiment, the submerged portion 2 may have imprints or embossings or is padded (e.g. geogrids or textiles) on its inner portion to allow for movement of fluids in the spaces created after contact with the hull (
In one embodiment, the attachment means 6 are mainly placed on the upper portion 1 of the shell.
In another embodiment, the attachment means 6 are exclusively placed on the upper portion 1 of the shell.
In another embodiment, the shell is open on the rear and the lower portion 2 is in line with the upper portion 1 (
In one embodiment, the shell is open on the rear and the lower portion 2 is set back with respect to the upper portion 1 (
In one embodiment, the shell is open on the rear and the lower portion 2 is set forward with respect to the upper portion 1 (
In another embodiment, the shell may be closed on the rear by upward folding (
In one embodiment, the shell is closed by crossing both sides of the shell and/or covering one side with the other on the rear (
In another embodiment, the rear closing of the shell may be hood-shaped (
In another embodiment, the shell may be closed on the rear by closing a flap downwards (
In another embodiment, the submerged portion 2 is impervious and provided with at least one check valve to let the trapped water leave out and to preclude or minimize flow in the opposite direction.
In another embodiment, the submerged portion 2 is impervious and provided with at least one valve or adjustable opening.
In another embodiment, portions 1 and 2 may have backing hems 11 through which ropes or straps can be passed to adjust, place or tighten the entire device against the hull (
The device is set up and maintained by ropes, sandow cords, carabiners 8.
Number | Date | Country | Kind |
---|---|---|---|
1003335 | Aug 2010 | FR | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|