U.S. application Ser. No. 08/755,439, Devlin et al., filed Nov. 26, 1996. |
Database WPI, “Semiconductor Energy Lab”, Derwent Publications Ltd., London, Abstract, Jul. 8, 1991, No page numbers. |
David J. Devlin, et al., “Diamond Like Carbon Coated “Kevlar” For Improved Mechanical Properties”, Electrochemical Society Proceedings, vol. 96, No. 5, 691-698, 1996. |
Iqbal S. Athwal, et al., “DLC Films By Plasma Assisted Chemical Vapor Deposition Near Room Temperature”, Diamond and Related Materials, vol. 2, No. 12, 1483-1489, Nov. 1, 1993. |
S. R. P. Silva, et al., “Diamond-Like Carbon Thin Film Deposition Using A Magnetically Confined r.f. PECVD System”, Diamond and Related Materials, vol. 4, No. 7, 977-983, May 15, 1995. |
F. J. McGarry, et al., “Ceramic Coated Rigid Rod Polymer Fibers”, SAMPE Quarterly, 35-38, Jul., 1992. |
S. R. Allen, “Tensile Recoil Measurement of Compressive Strength for Polymeric High Performance Fibres”, Journal of Materials Science, vol. 22, 853-859, 1987. |