The present disclosure claims priority from a Chinese patent application filed with the National Intellectual Property Administration on Jun. 19, 2020, with application number 202010566142.X, and titled “DISPLAY DEVICE”, which is incorporated by reference in the present application in its entirety.
The present disclosure relates to the field of display technologies, and particularly relates to a display device.
With more and more models of foldable mobile phones, foldable mobile phones have not been quickly promoted to enter mass market due to obvious defects and lack of good solutions. Please refer to
Therefore, in order to improve impact resistance of the display device and ensure products pass falling ball test successfully, so as to achieve a purpose of improving product yield, it is now necessary to provide a display device.
The present disclosure provides a display device. A buffer layer is disposed on a side of a back plate away from a cover plate. The buffer layer includes at least one of at least one first sub-buffer layer, at least one second sub-buffer layer, and at least one third sub-buffer layer. The first sub-buffer layer is made of a foamed material with a completely closed hole structure, the second sub-buffer layer is made of a foamed material with a half-open and half-closed hole structure, and the third sub-buffer layer is made of a foamed material with a completely open hole structure, which can improve point impact resistance of falling pen test.
In a first aspect, an embodiment of the present disclosure provides a display device, including: a back plate, a display module disposed on a side of the back plate, a cover plate disposed on a side of the display module away from the back plate, and a buffer layer disposed on a side of the back plate away from the cover plate. Wherein, the buffer layer includes at least one of at least one first sub-buffer layer, at least one second sub-buffer layer, and at least one third sub-buffer layer, and the first sub-buffer layer is made of a foamed material with a completely closed hole structure, the second sub-buffer layer is made of a foamed material with a half-open and half-closed hole structure, and the third sub-buffer layer is made of a foamed material with a completely open hole structure.
In some embodiments, the buffer layer includes at least one first sub-buffer layer and at least one second sub-buffer layer, the second sub-buffer layer is disposed on a side of the first sub-buffer layer away from the back plate.
In some embodiments, the buffer layer includes at least one first sub-buffer layer and at least one third sub-buffer layer, the third sub-buffer layer is disposed on a side of the second sub-buffer layer away from the back plate.
In some embodiments, the buffer layer includes at least one first sub-buffer layer, at least one second sub-buffer layer, and at least one third sub-buffer layer, wherein the second sub-buffer layer is disposed on a side of the first sub-buffer layer away from the back plate, and the third sub-buffer layer is disposed on a side of the second sub-buffer layer away from the first sub-buffer layer.
In a second aspect, an embodiment of the present disclosure further provides a display device, wherein, the display device includes: a back plate, a display module disposed on one side of the back plate, a cover plate disposed on a side of the display module away from the back plate, and a buffer layer disposed on a side of the back plate away from the cover plate. Wherein, the buffer layer comprises at least one first sub-buffer layer, and the first sub-buffer layer is made of a foamed material with a completely closed hole structure.
In some embodiments, the buffer layer further includes at least one second sub-buffer layer, the second sub-buffer layer is disposed on a side of the first sub-buffer layer away from the back plate, and the second sub-buffer layer is made of a foamed material with a half-open and half-closed hole structure.
In some embodiments, the buffer layer further includes at least one third sub-buffer layer, and the third sub-buffer layer is made of a foamed material with a completely open hole structure.
In some embodiments, the third sub-buffer layer is disposed on a side of the first sub-buffer layer away from the back plate.
In some embodiments, the third sub-buffer layer is disposed on a side of the second sub-buffer layer away from the first sub-buffer layer.
In some embodiments, a buffer rate of the first sub-buffer layer ranges from 12.76% to 16.84%.
In some embodiments, a buffer rate of the second sub-buffer layer ranges from 2.61% to 9.11%.
In some embodiments, a buffer rate of the third sub-buffer layer ranges from 1.53% to 1.95%.
In some embodiments, a bore diameter of the half-open and half-closed hole structure ranges from 20 μm to 50 μm.
In some embodiments, a bore diameter of the completely open hole structure ranges from 70 μm to 110 μm.
Advantages of the present disclosure are: a buffer layer is disposed on a side of a back plate away from a cover plate in the display device described in the present disclosure, the buffer layer includes at least one of at least one first sub-buffer layer, at least one second sub-buffer layer, and at least one third sub-buffer layer, the first sub-buffer layer is made of a foamed material with a completely closed hole structure, the second sub-buffer layer is made of a foamed material with a half-open and half-closed hole structure, and the third sub-buffer layer is made of a foamed material with a completely open hole structure, which can improve point impact resistance of falling pen test. When performing a falling ball test on the display device, the buffer layer can have a certain buffer effect on an impact force of the falling ball test. Therefore, it can improve the impact resistance of the display device and ensure the display device passing falling ball test successfully, thereby improving a yield of the display device.
The present disclosure provides a display device. To make the objectives, technical solutions, and effects of the present disclosure clearer, the present disclosure is further described in detail below with reference to the embodiments accompanying with drawings. It should be understood that specific embodiments described herein are merely for explaining the present disclosure, and the present disclosure is not limited thereto.
Specifically, referring to
In the present disclosure, a preferred material of the buffer layer is foam. Wherein, the greater a hardness of the foam is, the better a buffer rate of the buffer layer is. In addition, factors affecting the buffer rate of the foam include density, type of hole structure, and material ratio. In some embodiments, the material of the buffer layer is selected from at least one of chemical crosslinked polyethylene (XPE) foam or expandable polyethylene (EPE) pearl cotton. In other embodiments, the material of the buffer layer includes but is not limited to the foam and other soft porous materials.
In the present disclosure, the buffer layer may be made of foam with any one type of three different types of holes including a completely open hole structure, a completely closed hole structure, and a half-open and half-closed hole structure. A compression ratio and the hardness of the foam with different types of holes are different, and thus impact absorption capacity of the different types of holes are different. Wherein, the compression ratio of the foam refers to a ratio of a thickness of a compressed part of the foam to an original thickness of the foam. The greater the compression ratio of the foam is, the softer the foam is. Specifically, the compression ratio of the foam with the completely closed hole structure is less than that of the foam with the half-open and half-closed hole structure, and the compression ratio of the foam with the half-open and half-closed hole structure is less than that of the foam with the completely open hole structure. Conversely, the hardness of the foam with the completely closed hole structure is greater than that of the foam with the half-open and half-closed hole structure, and the hardness of the foam with the half-open and half-closed hole structure is less than that of the foam with the completely open hole structure.
In the present disclosure, as a preferred embodiment, a buffer rate of the first sub-buffer layer 110 ranges from 12.76% to 16.84%. Furthermore, the buffer rate of the first sub-buffer layer 110 may be preferably but not limited to at least one of 16.84%, 16.75%, or 12.76%.
Referring to
Sequentially referring to
In the preferred embodiment, a buffer rate of the second sub-buffer layer 120 ranges from 2.61% to 9.11%. Furthermore, the buffer rate of the second sub-buffer layer 120 may be preferably but not limited to at least one of 9.11%, 3.71%, or 2.61%.
Referring to
In the embodiment, due to the compression ratio of the foamed material with the half-open and half-closed hole structure being greater than that of the foam with the completely closed hole structure, that is, the hardness of the first sub-buffer layer 110 is greater than that of the second sub-buffer layer 120, the buffer rate of the first sub-buffer layer 110 is better than that of the second sub-buffer layer 120. That is, the buffer rate of the first sub-buffer layer 110 with the completely closed hole structure is greater than that of the second sub-buffer layer 120 with the half-open and half-closed hole structure. Therefore, on the basis of good buffer rate of the first sub-buffer layer 110, the second sub-buffer layer 120 has a function of further improving the impact resistance of the buffer layer.
Referring to
As shown in
In some embodiment, a buffer rate of the third sub-buffer layer 130 ranges from 1.53% to 1.95%. Furthermore, the buffer rate of the third sub-buffer layer 130 may be preferably but not limited to at least one of 1.95%, 1.53%, 0.97%, 0.79%, or 0.41%.
Referring to
In the embodiment, when the third sub-buffer layer 130 is made of the foamed material with a completely open hole structure, the hardness of the first sub-buffer layer 110 is greater than that of the third sub-buffer layer 130, so that the buffer rate of the first sub-buffer layer 110 is greater than that of the third sub-buffer layer 130 in the embodiment. Therefore, on the basis of better buffer performance and better impact resistance of the first sub-buffer layer 110, the third sub-buffer layer 130 has a function of further improving the buffer performance of the buffer layer.
In the embodiment, the third sub-buffer layer 130 made of the foamed material with the completely open hole structure is configured to replace the second sub-buffer layer 120 made of the foamed material with the half-open and half-closed hole structure in the previous embodiment. Because in most cases, the hardness of the foamed material with the half-open and half-closed hole structure is greater than that of the foamed material with the completely open hole structure, and the greater the hardness is, the higher the price of the foamed material is. Therefore, on the basis of realizing that the buffer layer has a good buffering effect, the preferred embodiment can further save costs to a certain extent.
Referring to
In the above-mentioned embodiment of the disclosure, the first sub-buffer layer 110 mainly serves as a buffering role, and the second sub-buffer layer 120 and the third sub-buffer layer 103 are equivalent to forming a structure for preventing an impact force absorption layer. So the embodiment has better buffer performance and better impact resistance, which can further enhance the impact resistance of the display panel 108.
In the above embodiments of the present disclosure, the buffer layer is configured to buffer damage to the display panel 108 when the display device is under external impact, which can effectively protect the display device, and the buffer layer can also be configured to improve resistance to point impact of the falling pen test.
In the present disclosure, the back plate 102 and the first sub-buffer layer 110 are bonded together by an adhesive.
In the present disclosure, the back plate 102 needs to have good thermal conductivity, and the material of the back plate 102 includes but is not limited to any one of polyimide (PI) materials, polyethylene terephthalate (PET) materials, nylon, and other plastic materials. The material of the back plate 102 may also include a mixture of metal copper foil, graphite heat sink, and at least two of the above plastic materials.
In the present disclosure, the display device further includes a frame (not shown), and the frame and the back plate 102 are integrally connected or assembled. The frame is disposed around the back plate 102 and defines an accommodation space (not shown) with the back plate 102, and the accommodation space is configured to accommodate the display panel 108.
In the present disclosure, the display panel 108 can emit light by using liquid crystal technology, organic light-emitting technology, and electroluminescence technology, etc. The display panel 108 may be an organic light-emitting diode (OLED) display panel, a liquid crystal display panel, and light-emitting diode (LED), etc. For example, when the display panel 108 is an OLED display panel, the display panel 108 includes a thin film transistor array substrate, the touch layer 106 may be an on-cell structure, and the touch layer 106 is disposed on the thin film transistor array substrate of the display panel 108. The touch layer 106 is connected to the thin film transistor array substrate of the display panel 108, and the thin film transistor array substrate includes a thin film transistor array layer, an OLED light-emitting layer, and a thin film package layer in turn. The OLED light-emitting layer includes an anode, a hole injection layer, a hole transport layer, an organic light-emitting layer, an electron transport layer, an electron injection layer, and a cathode formed in turn above the thin film transistor array layer. And the thin film package layer covers the OLED light-emitting layer. In addition, in other embodiments, when the display panel 108 is an OLED display panel, the touch layer 106 may also is an in-cell structure, and a position of the touch layer 106 is replaced by interior of the thin film transistor array substrate embedded in the OLED display panel.
In the disclosure, when the display panel 108 is a liquid crystal display panel, the display module further includes a backlight source and an optical film. The backlight source is an LED, and the optical film includes a light guide plate, a reflection film, a diffusion plate, a brightness enhancement film, and a double-sided adhesive tape, etc. The optical film is disposed on a side of the back plate 102 away from the display panel 108.
In the present disclosure, when the display panel 108 is a liquid crystal display (LCD) panel, the display module 101 further includes the polarizer layer 105 (POL, Polarizing Film). The polarizer layer 105 is configured to convert non-polarized natural light into polarized light, and to control whether or not light passes through by utilizing torsion characteristics of liquid crystal molecules, which makes the liquid crystal display panel display images normally.
In the disclosure, the cover plate 103 (or a cover plate module) is a glass cover plate or a 3D cover plate, and an outer diameter of the cover plate 103 is greater than an outer diameter of the display panel 108. A side of the cover plate 103 away from the display panel 108 is an arc surface, and the arc surface includes an arc chamfer. The cover plate 103 may be processed and shaped by hot bending process, which can make the appearance of the display device beautiful and smooth, and make the visual effect significantly better.
As shown in
In other embodiments, the first adhesive layer 104 and the second adhesive layer 107 may further include but are not limited to at least one of OCA or water adhesive. Wherein, the water adhesive is configured to reduce reflection at the interface, suppress a light leakage at the splicing place, and enhance a light transmission ability of the display module.
In some embodiments, the display panel 108 further includes a light-transmitting area 1032, and an open hole (not shown) is defined in the polarizer layer 105 corresponding to the light-transmitting area 1302, and the open hole is filled with the OCA or the water adhesive. The OCA in the open hole is configured to make the cover plate 103, the first adhesive layer 104, and the polarizer layer 105 closely adhere to each other to prevent the formation of an air layer at the open hole, thereby preventing a phenomenon of full emission of some light rays at the open hole.
Please sequentially refer to
The present disclosure further provides a display device, which includes the display components as described above, and further includes optical components such as a camera. And the camera is corresponding to the blind hole or the through hole area of the light-transmitting area 1032.
During performing the falling ball test on the display module described in the disclosure, when a solid steel plate is used in the test, a bright spot is present at a falling pen height of 1.5 cm, and when a lower part of the steel plate is avoided, a bright spot is present at a falling pen height of 11 cm.
For specific implementation of the foregoing operations, refer to the foregoing embodiments. Details are not further described herein.
In summary, the display device provided by the disclosure, the buffer layer is disposed on a side of a back plate 102 away from a cover plate 103. The buffer layer includes at least one of at least one first sub-buffer layer 110, at least one second sub-buffer layer 120, and at least one third sub-buffer layer 130. The first sub-buffer layer 110 is made of a foamed material with a completely closed hole structure, the second sub-buffer layer 120 is made of a foamed material with a half-open and half-closed hole structure, and the third sub-buffer layer 130 is made of a foamed material with a completely open hole structure to improve point impact resistance of falling pen test. When performing the falling ball test on the display device, the buffer layer can buffer an impact force of falling ball test to a certain extent. Therefore, it can improve the impact resistance of the display device and ensure the display device passing falling ball test successfully, thereby improving the yield of the display device.
It can be understood that, for those skilled in the art, equivalent replacements and modifications can be made according to the technical solution and disclosure ideas thereof of the present disclosure, and all these modifications or replacements are considered within the protection scope of the attached claims of the present disclosure.
Number | Date | Country | Kind |
---|---|---|---|
202010566142.X | Jun 2020 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2020/103493 | 7/22/2020 | WO | 00 |