The present invention relates to the field of display technology, in particular to a display substrate, a method for manufacturing the same and a liquid crystal display device.
Liquid crystal display device (LCD) has become a mainstream product of the current flat panel display device because of its characteristics such as small size, low power consumption and no radiation. The liquid crystal display panel is an important element in a liquid crystal display device. A liquid crystal display panel includes an array substrate and a color film substrate disposed oppositely, and a liquid crystal layer is located between the array substrate and the color film substrate.
When the liquid crystal display panel is not energized, in order to maintain a specific orientation for the liquid crystal in the liquid crystal display panel, rubbing alignment should be performed on the surfaces of the array substrate and the color film substrate facing each other to form grooves having a certain orientation. The grooves are typically formed by rubbing with a rubbing cloth.
In the rubbing process for the alignment layer of the liquid crystal display substrate, rubbing mura is apt to occur. This is due to poor consistency of rubbing when the surface of the alignment layer is rubbed by the rubbing cloth, which leads to poor consistency of the formed grooves. The inventor also notes that mura typically occurs on a position opposite to the data line, affecting the display quality of the liquid crystal display panel seriously.
Embodiments of the invention provide a display substrate, a method for manufacturing the same and a liquid crystal display device, which can eliminate the mura phenomenon, simplify the process and ensure the adhesive force in the sealing region.
The display substrate provided by the embodiment of the invention includes a display region and a non-display region. The non-display region includes at least a sealing region surrounding the display region. The sealing region includes a segment difference padding layer, and the segment difference padding layer includes several through holes.
In a display substrate, a certain segment difference may exist between the display region and the non-display region. By applying the segment difference padding layer in the sealing region, the segment difference between the non-display region and the display region of the display substrate can be eliminated, thereby eliminating the rubbing mura. The segment difference padding layer is applied only in the sealing region, the manufacturing process of the display substrate is thus simplified. Further, since the segment difference padding layer includes the through holes, the fluffs on the rubbing cloth can thus be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. The through holes can be filled with a sealing material to ensure the sealing function of the sealing region.
Optionally, a material of the segment difference padding layer is resin.
Compared with a passivation layer, a resin material can be applied by a relatively simple process (e.g., but not limited to: deposition, spin coating). The resin material also has better optical and mechanical properties.
Optionally, the through holes are circular through holes.
The circular through holes can comb the fluffs on the rubbing cloth, so as to avoid poor rubbing alignment caused by messy fluffs of the rubbing cloth.
Optionally, a diameter of each circular through hole is in a range of 1-10 μm.
By applying the through holes with a certain diameter, a sealant can be filled in the through holes to ensure sufficient adhesive strength at the edge of the display substrate.
Optionally, a distribution density of the circular through holes decreases as a distance from the display region decreases.
With a gradually changed distribution density, the fluffs on the rubbing cloth can be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, a cross sectional area of the through hole decreases as a distance from the display region decreases.
With gradually changed sectional areas of the through holes, in a range from the segment difference padding layer to the display region, the fluffs on the rubbing cloth can be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, a total area of the several through holes is 5-50% of an area of the segment difference padding layer.
The sealant can be filled in the through holes, the total area of the several through holes thus can ensure sufficient adhesive strength between the segment difference padding layer and the substrate.
Optionally, a cross section of the through hole has a stripe shape. By setting the cross section of the through hole as a stripe shape, the segment difference padding layer has a comb-like arrangement. The sealant can thus be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate. Moreover, such an arrangement can also comb the fluffs on the rubbing cloth, reducing the damage to the fluffs on the rubbing cloth caused by the segment difference.
Optionally, a width of the through hole is smaller than or equal to an interval between two directly adjacent strip shaped through holes.
With such an arrangement, more sealant can be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate.
Optionally, the display substrate further includes a sealant filling the through holes and covering the segment difference padding layer. Similarly, a passivation layer can also be used for covering the segment difference padding layer, a sealant can then be filled into the through holes, and the sealant covers the passivation layer.
With the sealant, a cell aligning process can be performed. The sealant is also permeable to the through hole, increasing the adhesive strength between the segment difference padding layer and the substrate.
Optionally, several recesses are formed on the surface of the segment difference padding layer.
The recesses formed on the surface of the segment difference padding layer can also be filled with the sealant, thereby increasing the adhesive strength between the segment difference padding layer and the substrate.
An embodiment of the invention further provides a method for manufacturing a display substrate. The method includes the following steps: forming a segment difference padding layer in a sealing region surrounding a display region of the display substrate, and forming several through holes in the segment difference padding layer.
In a display substrate, a certain segment difference may exist between the display region and the non-display region. By applying the segment difference padding layer in the sealing region, the segment difference between the non-display region and the display region of the display substrate can be eliminated, thereby eliminating the rubbing mura. The segment difference padding layer is applied only in the sealing region, the manufacturing process of the display substrate is thus simplified. Further, since the segment difference padding layer includes the through holes, the fluffs on the rubbing cloth can thus be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. The through holes can be filled with a sealing material to ensure the sealing function of the sealing region.
Optionally, the method further includes: performing a rubbing alignment process on the display substrate.
A rubbing alignment process using a rubbing cloth can be performed to the display substrate to form an alignment layer, thereby determining an initial orientation of the liquid crystal molecules.
Optionally, the method further includes: after performing a rubbing alignment process on the display substrate, filling the through holes and covering the segment difference padding layer with a sealant.
With the sealant, a cell aligning process can be performed. The sealant is also permeable to the through hole, increasing the adhesive strength between the segment difference padding layer and the substrate.
An embodiment of the present invention also provides a liquid crystal display device. The liquid crystal display device includes the display substrate in the above mentioned embodiments.
In order to more clearly illustrate the technical solutions in embodiments of the invention or in the prior art, the appended drawings needed to be used in the description of the embodiments or the prior art will be introduced briefly in the following. Obviously, the drawings in the following description are only some embodiments of the invention, and for those of ordinary skills in the art, other drawings may be obtained according to these drawings under the premise of not paying out creative work.
In the following, the technical solutions in the embodiments of the invention will be described clearly and completely in connection with the drawings in the embodiments of the invention. Obviously, the described embodiments are only part of the embodiments of the invention, and not all of the embodiments. Based on the embodiments in the invention, all other embodiments obtained by those of ordinary skills in the art under the premise of not paying out creative work pertain to the protection scope of the invention.
As shown in
Typically, the non-display region of the display substrate can also include a pad region and/or a wiring region as indicated by “pad” in
In the context of the present invention, the term “display substrate” can refer to a monolithic substrate with a plurality of display regions prior to cutting (for example, as shown in
Optionally, a material of the segment difference padding layer 104 is resin.
Compared with a passivation layer, a resin material can be applied by a relatively simple process (e.g., but not limited to: deposition, spin coating). The resin material also has better optical and mechanical properties.
Optionally, as shown in
The circular through holes can comb the fluffs on the rubbing cloth, so as to avoid poor rubbing alignment caused by messy fluffs of the rubbing cloth.
Optionally, a diameter of each circular through hole 105 is in a range of 1-10 μm.
By applying the through holes with a certain diameter, a sealant can be filled in the through holes to ensure sufficient adhesive strength at the edge of the display substrate.
Optionally, as shown in
With a gradually changed distribution density, the fluffs on the rubbing cloth can be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, as shown in
With gradually changed sectional areas of the through holes, in a range from the segment difference padding layer to the display region, the fluffs on the rubbing cloth can be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, a total area of the several through holes 105 is 5-50% of an area of the segment difference padding layer 104.
The sealant can be filled in the through holes, the total area of the several through holes thus can ensure sufficient adhesive strength between the segment difference padding layer and the substrate.
Optionally, as shown in
By setting the cross section of the through hole as a stripe shape, the segment difference padding layer has a comb-like arrangement. The sealant can thus be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate. Moreover, such an arrangement can also comb the fluffs on the rubbing cloth, reducing the damage to the fluffs on the rubbing cloth caused by the segment difference.
Optionally, a width of the through hole 105′ is smaller than or equal to an interval between two directly adjacent strip shaped through holes.
With such an arrangement, more sealant can be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate.
Optionally, the display substrate further includes a sealant 106 filling the through holes 105 and covering the segment difference padding layer 104. Similarly, a passivation layer can also be used for covering the segment difference padding layer 104, a sealant can then be filled into the through holes 105, and the sealant covers the passivation layer.
With the sealant, a cell aligning process can be performed. The sealant is also permeable to the through hole, increasing the adhesive strength between the segment difference padding layer and the substrate.
Optionally, as shown in
The recesses formed on the surface of the segment difference padding layer can also be filled with the sealant, thereby increasing the adhesive strength between the segment difference padding layer and the substrate.
An embodiment of the invention further provides a method for manufacturing a display substrate. As shown in
S201: forming a segment difference padding layer in a sealing region surrounding a display region of the display substrate, and
S202: forming several through holes in the segment difference padding layer.
In a display substrate, a certain segment difference may exist between the display region and the non-display region. By applying the segment difference padding layer in the sealing region, the segment difference between the non-display region and the display region of the display substrate can be eliminated, thereby eliminating the rubbing mura. The segment difference padding layer is applied only in the sealing region, the manufacturing process of the display substrate is thus simplified. Further, since the segment difference padding layer includes the through holes, the fluffs on the rubbing cloth can thus be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. The through holes can be filled with a sealing material to ensure the sealing function of the sealing region.
Optionally, in the step of forming several through holes in the segment difference padding layer, the through holes 105 can be formed in the segment difference padding layer by applying, for example, a photolithography process.
Optionally, as shown in
The circular through holes can comb the fluffs on the rubbing cloth, so as to avoid poor rubbing alignment caused by messy fluffs of the rubbing cloth.
Optionally, as shown in
By applying the through holes with a certain diameter, a sealant can be filled in the through holes to ensure sufficient adhesive strength at the edge of the display substrate.
Optionally, as shown in
With a gradually changed distribution density, the damage to the fluffs on the rubbing cloth can be reduced. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, as shown in
With gradually changed sectional areas of the through holes, in a range from the segment difference padding layer to the display region, the fluffs on the rubbing cloth can be smoothed, thereby further avoiding poor rubbing alignment caused by messy fluffs of the rubbing cloth. Meanwhile, sufficient adhesive strength at the edge of the display substrate can also be ensured.
Optionally, a total area of the several through holes 105 is 5-50% of an area of the segment difference padding layer 104.
The sealant can be filled in the through holes, the total area of the several through holes thus can ensure sufficient adhesive strength between the segment difference padding layer and the substrate.
Optionally, as shown in
By setting the cross section of the through hole as a stripe shape, the segment difference padding layer has a comb-like arrangement. The sealant can thus be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate. Moreover, such an arrangement can also comb the fluffs on the rubbing cloth, reducing the damage to the fluffs on the rubbing cloth caused by the segment difference.
Optionally, a width of the through hole 105′ is smaller than or equal to an interval between two directly adjacent strip shaped through holes.
With such an arrangement, more sealant can be filled into the intervals between the strip-like portions of the segment difference padding layer, thereby increasing the cohesive force and preventing the segment difference padding layer from being peeled off from the substrate.
Optionally, the method further includes: performing a rubbing alignment process on the display substrate.
A rubbing alignment process using a rubbing cloth can be performed to the display substrate to form an alignment layer, thereby determining an initial orientation of the liquid crystal molecules.
Optionally, the method further includes: after performing a rubbing alignment process on the display substrate, filling the through holes 105 and covering the segment difference padding layer 104 with a sealant 106 (as shown in
With the sealant, a cell aligning process can be performed. The sealant is also permeable to the through hole, increasing the adhesive strength between the segment difference padding layer and the substrate.
An embodiment of the present invention also provides a liquid crystal display device. The liquid crystal display device includes the display substrate in the above mentioned embodiments. As shown in
Apparently, the person skilled in the art may make various alterations and variations to the invention without departing the spirit and scope of the invention. As such, provided that these modifications and variations of the invention pertain to the scope of the claims of the invention and their equivalents, the invention is intended to embrace these alterations and variations.
Number | Date | Country | Kind |
---|---|---|---|
201610151993.1 | Mar 2016 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|