A section of the disclosure of this patent document and its figures contain material subject to copyright protection. The copyright owner has no objection to the facsimile reproduction by anyone of the patent document, but otherwise reserves all copyrights whatsoever.
The present invention generally relates to doors and the manufacture thereof. The present invention more particularly relates to the manufacture of a door having a split frame.
Manufacturers of composite doors strive to create a door skin that closely resembles a real wood door. They must also strive to reduce the cost of manufacturing such a door. Manufacturers have implemented a variety of manufacturing processes to achieve these sometimes conflicting goals.
For example, U.S. Pat. No. 6,485,800 to Littschwager, et al (hereinafter “Littschwager”, which is assigned to the assignee of the present application, discloses one process for manufacturing a composite door. In the process disclosed in Littschwager, the door manufacturer creates a silicone mold from an original wood door, referred to as the “plug.” The manufacturer then laminates a skin on the mold. The skins may comprise various materials.
Once the manufacturer has laminated a skin, the manufacturer places a temporary frame on the inner surface of the skin. The frame comprises at least a pair of horizontal pieces, called rails, and at least a pair of vertical pieces called stiles. Typically, when the frame is placed, the manufacturer simply lays the frame down on top of the skin; however, the manufacturer may use adhesive or vacuum pressure to hold the temporary frame in place. The temporary frame acts as a dam when the core material is subsequently applied.
According to the process described in Littschwager, the manufacturer next applies the core material. The core material may comprise various materials, such as wood block, particleboard, medium density fiberboard, or urethane. The manufacturer pours the core material onto the inner surface of the skin within the temporary frame. The core material is carefully measured so that when it rises, the depth of the material will exceed the thickness of the frame. In other words, the core material extends slightly above the frame when the partially completed door is lying on the skin. A machine applies the core, using a timed pouring. For example, in one process, a ninety-second pour provides enough core material for a standard 36″×96″ door to allow for expansion or rise above a one and a half inch frame.
Once the core has cured, but prior to fully cooling, the manufacturer removes the temporary frame. The remaining part, comprising a skin and core, is now ready for machining. Two of these parts are used to assemble a finished door. In a conventional one-and-three-quarter-inch-thick composite door, each part is machined to be seven eighths of an inch thick, including the one-eighth inch skin and three quarters of an inch core.
Once machining is complete, the part (skin and core combination) is removed from the mold (demolded) and placed in a medium density fiberboard (MDF) assembly tray. The assembly tray is a mirror image or the door to be assembled. Every design element of the door is routed into the assembly board so that the skin fits firmly in place.
Final assembly of the composite door involves three components: two machined skin-core combinations and one frame. The manufacturer places a first skin-core combination on the assembly board, applies adhesive to the frame, and sets the frame on the skin-core combination. The manufacturer then applies adhesive to the other side of the frame and places another skin-core combination on top of the frame. The manufacturer then places another assembly board on top of the upper skin and applies pressure or a combination of both heat and pressure to the components to complete the assembly process.
Composite doors manufactured by the method described above as well as by other, conventional methods suffer from several disadvantages. Due to the use of the temporary frame and other factors, the manufacturer has difficulty maintaining close tolerances. As a result, the finished door may not meet quality standards. For example, composite doors manufactured using conventional methods may comprise telegraphing visible or tactile irregularities in the surface of the door. Telegraphing may be evidenced by a noticeable depression or raised area in the transition from frame to core. Since many of the conventional composite doors are pre-finished with a high-gloss topcoat, any irregularities are accentuated, and therefore, the manufacturer cannot sell the door.
Also, in a conventional process for manufacturing composite doors, considerable material is wasted. For example, in a conventional one-and-three-quarter-inch composite door, the temporary frame, or dam, used to hold the core material in place on a skin while it cures is one-and-one-half-inches thick, and the core is poured to a depth greater than this temporary frame. However, the manufacturer must machine the cured core to a thickness of only three quarters of an inch in order to combine one skin-core combination with another to create the one-and-three-quarter-inch composite door. Therefore, more than half of the core material applied to each door section is wasted. In addition, it can be difficult to roll a fiberglass skin accurately.
Addressing telegraphing, also referred to as telescoping, and other quality problems resulting from conventional manufacturing methods results in much wasted time, materials, and money. Doors must be repaired in the field, reworked in the factory, or scrapped. These problems also result in increases in warranty costs as low-quality doors that are shipped to customers must be fixed or replaced. These quality problems and the measures taken to address them all serve to decrease the profitability of manufacturing the doors.
An efficient method of manufacturing a high-quality door is needed.
Embodiments of the present invention comprise doors and methods of manufacturing doors. An exemplary embodiment of the present invention comprises a composite door having a pair of complementary sections attached to one another. In one embodiment, each of the sections comprises a molded skin, which forms the face panel of the completed door and a rectangular frame laminated to the skin. In another embodiment, each section includes a core material poured on the inner surface of the skin, between the stiles and rails of the rectangular frame.
In one embodiment, each section comprises one half of the total thickness of the door. To increase the strength of the attach between the pair of sections and to simplify the process of aligning the two sections, the stiles or other structure of the frames may comprise a depression, such as a groove, for accommodating a corresponding projection, such as a tongue, on the frame of the other section.
One method for manufacturing a door according to the present invention comprises making the first section, making the second corresponding section, and attaching the two sections together.
In an exemplary embodiment, a manufacturer constructs a first section by first molding a skin to form a composite face panel of the composite door. The manufacturer then adhesively laminates the skin to a rectangular frame. During the lamination, the manufacturer may vacuum press the frame to the skin. Next, the manufacturer pours a core material the volume defined between the inside surface of the skin and the inside surfaces of the stiles and the rails. The manufacturer then repeats these steps to construct a second section.
Once the manufacturer has allowed the cores to cure, the manufacturer machines the backs of the sections—the side opposite the skins—to attain a desired thickness. Preferably, the manufacturer machines each section to half of the desired thickness of a complete composite door or slightly less to account for the thickness of the adhesive. Once the sections are complete, the manufacturer attaches the two sections together to form a door. In one embodiment, the manufacturer applies pressure. In another embodiment the manufacturer applies both heat and pressure.
Embodiments of the present invention provide numerous advantages over conventional composite doors and conventional methods of manufacturing composite doors. For example, in one embodiment of the present invention, a hollow door manufacturer is able to compensate for variations in the thickness of a skin by milling each section of the frame prior to joining the sections together. Additional advantages include increases in efficiency and quality. For example, in an embodiment of the present invention, tolerances are minimized leading to enhanced quality of the finished doors. Improved quality results in a reduction in refits and remakes due to telegraphing and other imperfections in the doors. In addition returns and associated warranty costs are reduced as are the number of field repairs, internal reworks, and scrap. Minimal tolerances and reduced scrap also help to increase the yield of finished doors per quantity of input materials. Reductions in cost and increase in yields all serve to increase the profitability of the composite doors to the manufacturer.
In addition, an embodiment of the present invention may also create a stronger door. And a door according to and embodiment of the present invention is less susceptible to extremes in climate, including areas that are hot and dry, areas with high humidity, and areas that experience extreme freeze and thaw cycles.
Further details and advantages of embodiments of the present invention are set forth below.
These and other features, aspects, and advantages of the present invention are better understood when the following Detailed Description is read with reference to the accompanying drawings, wherein:
Embodiments of the present invention comprise a door and a method of manufacturing a door. In one embodiment of the present invention, a door comprises a pair of sections attached to one another. Each section comprises a skin and a frame. In another embodiment, each section comprises a skin, a frame, and a core material present on the inside surface of the skin. In one embodiment, each section comprises one half of a door. For example, in one embodiment, a composite door that is one-and-three-quarter-inches thick comprises two sections, each having a one-eighth inch skin and a three-quarter inch frame and core. Thus the door has a “split frame.”
Referring now to the figures, in which like numbers indicate like elements throughout the several figures,
Once the skin (102) has been molded, the manufacturer attaches a frame (103) to the skin (102) 404. In one embodiment, the manufacturer laminates the skin (102) to the frame (103) with a pliers-grip adhesive. The manufacturer uses a vacuum press to hold the frame (103) while aligning it to and attaching it with the skin (102).
Once the skin (102) and frame (103) are removed from the vacuum press, the manufacturer pours the core material onto the inner face of the skin (102) to a thickness just greater than that of the frame (103) 406. In an embodiment in which the manufacturer pours the core material, the core material must be in a liquid state when poured, such as urethane heated beyond its melting point. When the core material contacts the inner surface of the skin (102), it begins attaching with the skin (102). The manufacturer then allows the core material to cure 408. The core material preferably reaches a green tier state before it is machined. In an embodiment in which urethane is utilized as the core material, the core material typically reaches a green tier state before reaching room temperature.
Once the core material has cured, the manufacturer machines the door section (100) 410. In one embodiment, the manufacturer uses a computer numerical cutter (CNC) with a live cut insert tooling blade to machine the door section (100). The CNC essentially shaves the back of the section (100)—the side opposite the skin (102)—to a desired thickness. The CNC may also create a groove or tongue in the section (100) to simplify and improve the process of combining multiple sections to finish assembly of a composite door.
In the embodiment shown, once the section (100) has been machined, it is demolded or removed from the mold 412. In other embodiments, the section (100) is removed from the mold before machining. In the embodiment shown in
The manufacturer then combines the two sections 416. The manufacturer combines the sections by placing the first section (100) in an assembly tray horizontally with the skin (102) down, applying adhesive to the frame (103) and core material of the section (100), placing the second, corresponding section on top of the first section with the skin on top, aligning the sections using the tongue and groove if present, and clamping the sections together. The manufacturer may apply pressure or a combination of heat and pressure to ensure a strong attach is created between the sections.
One embodiment of the present invention is a standard one and three quarter inch thick composite door, comprising two sections of equal thickness. In such an embodiment, each section of the finished door comprises a one eighth inch skin and a three quarter inch frame and core.
In one such embodiment, when the manufacturer produces the frame for each section, the frame is somewhat thicker than three quarters of an inch. The additional material provides a degree of flexibility during the machining process. In such an embodiment, the manufacturer pours a urethane core material to a level that is, or will be after rising, slightly thicker than the three quarter inch frame. Once the core material cures, the manufacturer machines the frame and the core material to three quarters of an inch thick, resulting in a section, including the skin, that is seven eights of an inch thick. The manufacturer combines the two sections and the resulting door is one-and-three-quarter-inches thick, preferably within plus or minus one sixteenth of an inch.
In another embodiment of the present invention, a manufacture produces a hollow door. The manufacture molds the skin. The manufacturer then attaches a frame to the skin. Once the frame has been attached to the skin, the manufacturer machines the section to a predetermined width. The manufacturer repeats the process for a second section. By machining each half separately, the manufacturer is able to compensate for any variances in the thickness of the skin or other materials used to manufacture the door.
In other embodiments, the manufacturer varies the order of the steps for manufacturing a door. For example, in one embodiment, the manufacturer molds a skin, attaches a first frame to the skin, attaches a second frame to the first frame, inserts core material, and then attaches the second skin to the second frame.
The foregoing description of the preferred embodiments of the invention has been presented only for the purpose of illustration and description and is not intended to be exhaustive or to limit the invention to the precise forms disclosed. Numerous modifications and adaptations thereof will be apparent to those skilled in the art without departing from the spirit and scope of the present invention.
Number | Name | Date | Kind |
---|---|---|---|
2178729 | Shields | Nov 1939 | A |
2825674 | Werner | Mar 1958 | A |
3225505 | Lytz | Dec 1965 | A |
4015393 | Warwick | Apr 1977 | A |
4103467 | Lindal | Aug 1978 | A |
4236365 | Wheeler | Dec 1980 | A |
4343127 | Greve et al. | Aug 1982 | A |
4602466 | Larson | Jul 1986 | A |
5074087 | Green | Dec 1991 | A |
5239799 | Bies et al. | Aug 1993 | A |
5318734 | Palmersten et al. | Jun 1994 | A |
5369869 | Bies et al. | Dec 1994 | A |
5537789 | Minke et al. | Jul 1996 | A |
5782055 | Crittenden | Jul 1998 | A |
6092343 | West et al. | Jul 2000 | A |
6132540 | Barber et al. | Oct 2000 | A |
6485800 | Liittschwager et al. | Nov 2002 | B1 |
Number | Date | Country |
---|---|---|
525520 | May 1931 | DE |
460611 | Feb 1937 | GB |
WO 0104448 | Jan 2001 | WO |
Number | Date | Country | |
---|---|---|---|
20040231285 A1 | Nov 2004 | US |