1. Technical Field
The present invention relates to injection molding articles and, particularly to a dual-injection molding article and a method for making same.
2. Description of the Related Art
Many kinds of workpieces, such as injection molding articles are fabricated by means of injection molding. Typically, dual-injection molding articles are used to create a plastic part made of two different materials or two different colors of the same material.
A typical dual-injection molding article 90, as shown in
However, if the second material has a higher melting point than that of the first material, when the melted second material is injected into the mold, there's a risk that the first portion 92, which is molded in the mold previously, may be melted and mixed by the second material due to its high temperature. Therefore, the joint/connection area of the first portion 92 and the second portion 95 may become distorting and ambiguous, as shown in
Therefore, an improved dual-injection molding article and method for making same is desired in order to overcome the above-described problems.
In one aspect, a dual-injection molding article is provided. The dual-injection molding article includes a first molding portion, a second molding portion, and a groove. The first molding portion has a hole defined therein, and an inside surface surrounding the hole. The second molding portion includes a base plate and a protruding portion. The base plate is integrally formed on the first molding portion. The protruding portion is integrally formed on the base plate, and is received in the hole. The groove is defined between a peripheral sidewall of the protruding portion and the inside surface of the first molding portion.
In another aspect, a method for making the dual-injection molding member is provided. The method includes the following steps: providing a mold; injecting a first material into the mold to form a first molding portion having a hole defined therein and an inside surface surrounding the hole; placing a block member inside the hole of the first molding portion, and the blocking member having an opening defined therein; and injecting a second material into the mold to form a second molding portion having a base plate integrally formed on the first molding portion, and a protruding portion integrally formed on base plate and being received inside the opening.
Other advantages and novel features will become more apparent from the following detailed description when taken in conjunction with the accompanying drawings.
Many aspects of the present dual-injection molding article and method for making same can be better understood with reference to the following drawings. The components in the drawings are not necessarily drawn to scale, the emphasis instead being placed upon clearly illustrating the principles of the dual-injection molding article and method for making same. Moreover, in the drawings, like reference numerals designate corresponding parts throughout the several views.
The present dual-injection molding article is suitable for portable electronic devices such as mobile phones, personal digital assistants (PDAs) and so on. Referring now to the drawings in detail,
Also referring to,
The second molding portion 30 includes a base plate 31, and a protruding portion 33 integrally formed on an upper surface of the base plate 31. The base plate 31 has an outer perimeter equal to that of the frame section 21. The protruding portion 33 has an upper side 331 positioned opposite to the upper surface of base plate 31, and a peripheral sidewall 333 protruding from the upper surface of the base plate 31. The peripheral sidewall 333 has a peripheral dimension smaller than that of the inside surface 214 of the frame section 21. The height of the protruding portion 33 is approximately equal to that of the frame section 21.
The upper surface of the base plate 31 is integrally formed on the bottom surface 212 of frame section 21. The protruding portion 33 is inserted into the hole 213 of the frame section 21 with the supper side 331 is flushed with the top surface 211 of the frame section 21. A groove 40 is thereby formed between the peripheral sidewall 333 of the protruding portion 33 and the inside surface 214 of the frame section 21. The protruding portion 33 can act as a display screen, since it is made of transparent material.
Referring to
providing a mold;
injecting the PC material (a first material) to form a first molding portion 20;
placing a block member 50 with an opening 53 defined therein inside a hole 213 of the first molding portion 20;
injecting the PMMA material (a second material) to form a second molding portion 30 having a base plate 31 connecting to the first mold portion 20 and a protruding portion 33 received in the opening 53 of the first mold portion 20;
cooling; and
removing the block member 50 from the molding article 10.
The block member 50 is a frame member in shape, and includes an outer side 51, an inner side 52, and an opening 53 defined therein. The outer side 51 of the block member 50 has a profile similar to the inside surface 214 of the frame section 21 with a dimension approximately equal to that of the inside surface 214 of the frame section 21. The inner side 53 of the block member 50 has a profile similar to that of the outer sidewall 333 of the protruding portion 33 with a dimension approximately equal to that of the peripheral sidewall 333 of the protruding portion 33. In the molding process, the block member 50 is sandwiched between the inside surface 214 of the frame section 21 and the peripheral sidewall 333 of the protruding portion 33, and thus prevents the first material and the second material from blending/mixing/pervasion with each other. After the block member 50 is removed, the groove 40 is defined between the inside surface 214 of the frame section 21 and the peripheral sidewall 333 of the protruding portion 33. The boundaries of the first and second molding portions 20, 30 are clear, and the aesthetic visibility of the molding article 10 will not be affected.
It is to be understood that the block member 50 can be placed in the mold before the step of injecting the first material.
It is further to be understood that the block member 50 can be made of decorating material and used as decorating member of the molding article 10. Thus, the step of removing the block member 50 can be omitted, and the bar member 50 can remain in the molding article 10 to increase aesthetic visibility of the molding article 10.
It is to be understood, however, that even though numerous characteristics and advantages of the present invention have been set forth in the foregoing description, together with details of the structure and function of the present invention, the disclosure is illustrative only, and changes may be made in detail, especially in matters of shape, size, and arrangement of parts within the principles of present invention to the full extent indicated by the broad general meaning of the terms in which the appended claims are expressed.