The present invention relates to a method for controlling an electric discharge machining apparatus and to such an electric discharge machining apparatus.
Generally, in known electrical discharge machining, electric energy is applied in the form of discrete electrical impulses across a machining gap filled with a machining fluid or liquid dielectric (e.g. oil). The discrete electrical impulses cause a succession of electrical discharges between a tool electrode and a workpiece. The narrow space between the tool electrode and the workpiece defines the machining gap also referred to as working gap. The electrical discharges lead to a material removal from the workpiece and, additionally, to wear of the tool electrode.
Typically, as material removal proceeds the tool electrode is advanced relatively to the workpiece by servo feed means. The machining gap distance is continuously controlled according to the instantaneous process conditions. A signal representing the current working gap distance (e.g. the ignition delay and/or mean voltage) is compared with a value representing a desired working gap distance (reference value) and the resulting error between these values is computed to generate a new command value for the drive motor in order to adjust the correct working gap distance. In this way the control of the relative position of workpiece and electrode allows the creation of consecutive material-removal discharges.
The material-removal and the discharges lead to a contamination of the machining gap region with erosion debris, process byproducts, thermal decomposition products of the dielectric and gases. It is known to remove such contaminations by flushing the machining gap region with fresh machining fluid and by cyclically retracting the tool electrode away from the workpiece.
From U.S. Pat. No. 4,288,675 A it is known to use (discharge) impulse trains which each consist of multiple machining impulses and to vary the duration and/or the off-time of consecutive impulse trains to reduce electrode wear. The impulse duration of each single impulse and the off-time between each single impulse of the impulse train are preset before machining and depend, e.g. on the electrode materials. The duration or on-time of an impulse train and/or the off-time between consecutive impulse trains is adjusted during machining in accordance with a detected rate of relative advance movement of the tool electrode so as to maintain the current density along machining surfaces substantially constant at a desired value in spite of change in the machining area during relative advance movement of the tool electrode.
From U.S. Pat. No. 4,503,309 A it is known to use increased current pulses intermittently in an impulse train in order to achieve desired current density and increase process stability.
As mentioned, typically the tool electrode is prone to wear. Already from U.S. Pat. No. 3,558,842 A it is known that a protective film forms on the tool electrode under specific conditions in an electric discharge machining process. The protective film is formed, e.g. by products of the working liquid and/or by products resulting from the discharge across the machining gap.
The formation of a protective film can be used to protect the tool electrode and to thereby reduce wear of it. For instance, the article “Zero wear—The “Perpetuum Mobile” of die-sinking EDM”, downloadable on http://www.gfac.com/fileadmin/user_upload/dev-agiecharmilles/News/Result_today—4/Results_today—04_E_arti cle11.pdf, describes on page 28 an electric discharge machining where a graphite electrode is used in die-sinking EDM. Graphite does not melt, but it sublimes. According to this document, as soon as the EDM process begins, the material removed wanders with the decomposition products from the carbon content dielectric to the graphite electrode. By controlling the reduction in temperature during the process, carbon precipitates on the electrode surface. Thereby a layer is formed on the electrode which protects the original electrode. The EDM process is such controlled that the growth of the layer on the electrode and the wear caused by discharge impulses taking place on the protective layer is in balance. Thus, the wear of the electrode can be reduced.
However, in particular in the meso- and micro-machining, i.e. for example in the meso-scale (instantaneous electrode surface area 10 mm2 to 1 mm2) and in the micro-scale (instantaneous electrode surface area between 1 mm2 to 0.010 mm2 or smaller or smallest dimension on electrode below 1 mm), the electrode wear is also with the above-mentioned machining processes considerable. The instantaneous electrode surface is defined as the projection surface area of the electrode surface over which a electric discharge (spark) is occurring and the smallest dimension of the tool electrode may refer to structures of electrodes, e.g. ribs, where a thickness of the ribs is below 1 mm (irrespective of the length and width of the ribs).
Thus, it is an object of the present invention to provide an improved method for controlling an EDM process, in particular for meso-micro machining, and an improved electric discharge machining apparatus, in particular for meso-micro machining.
According to a first aspect, the invention provides a method of controlling an electric discharge machining apparatus having at least a tool electrode and a workpiece, the method comprising the steps of: positioning the tool electrode relative to the workpiece; generating at least one first type discharge impulse and at least one second type discharge impulse, wherein the at least one first type discharge impulse has a longer impulse duration than the impulse duration of the at least one second type discharge impulse, and wherein the first type discharge impulse causes the formation of a protective film against wear on the tool electrode and the second type discharge impulse causes erosion at least on the tool electrode; applying the first and second type discharge impulses to a gap between the tool electrode and the workpiece for material removal from the workpiece, wherein a ratio between the first and second type discharge impulses applied to the tool electrode is such defined that a predefined wear of the tool electrode is caused.
According to a second aspect, the invention provides an electric discharge machining apparatus comprising: a tool electrode, a working table for receiving a workpiece, an impulse generator for generating discharge impulses, and a control for controlling the electric discharge machining apparatus, wherein the control is adapted for performing the method of any one of the preceding claims.
Further aspects of the invention are set forth in the dependent claims, the following description of the drawings.
Embodiments of the present invention are explained by way of example with respect to the accompanying drawings, in which:
a to 2f show different embodiments of impulse trains in accordance with the present invention;
a and 3b illustrate an embodiment with a long discharge impulse in accordance with a first group and a short discharge impulse in accordance with a second group, wherein the impulses have an increasing slope section;
a shows a graph depicting frontal wear values against impulse duration for different impulse types (initial current, final current and path for rise of current) for a given surface area, current per impulse and other process parameters;
b shows a graph depicting lateral wear values against impulse duration for different impulse types (initial current, final current and path for rise of current) for a given surface area, current per impulse and other process parameters;
a to 6c show different sequences of a long discharge impulse belonging to a first group and short discharge impulses belonging to a second group for forming impulse trains in accordance with the present invention;
a and 8b show an embodiment in which the ratio of long discharge impulses and short discharge impulses is kept constant.
As already mentioned in the beginning, in electrical discharge machining, electric energy is applied in the form of discrete electrical impulses across a machining gap filled with a machining fluid or liquid dielectric (e.g. oil). The discrete electrical impulses cause a succession of electrical discharges between a tool electrode and a workpiece. The narrow space between the tool electrode and the workpiece defines the machining gap or working gap. The electrical discharges lead to a material removal from the workpiece and, additionally, to wear of the tool electrode.
Typically, as material removal proceeds the tool electrode is advanced relatively to the workpiece by servo feed means. The machining gap distance is continuously controlled according to the instantaneous process conditions. A signal representing the current working gap distance (e.g. the ignition delay and/or mean voltage) is compared with a value representing a desired working gap distance (reference value) and the resulting error between these values is computed to generate a new command value for the drive motor. In this way the control of the relative position of workpiece and electrode allows the creation of consecutive material-removal discharges.
The material-removal and the discharges lead to a contamination of the machining gap region with erosion debris, process by-products, thermal decomposition products of the dielectric and gases. It is known to remove such contaminations by flushing the machining gap region with fresh machining fluid and by cyclically retracting the tool electrode away from the workpiece.
From U.S. Pat. No. 4,288,675, mentioned in the outset, it is known to use (discharge) impulse trains which each consist of multiple machining impulses and to vary the duration and/or the off-time of consecutive impulse trains to reduce electrode wear. The impulse duration of each single impulse and the off-time between each single impulse of the impulse train are preset before machining and depend, e.g. from the electrode materials. The duration or on-time of an impulse train and/or the off-time between consecutive impulse trains is adjusted during machining in accordance with a detected rate of relative advance movement of the tool electrode so as to maintain the current density along machining surfaces substantially constant in spite of change in the machining area during relative advance movement of the tool electrode.
Also, from U.S. Pat. No. 4,503,309 it is known to use increased current pulses intermittently in an impulse train in order to achieve desired current density and increase process stability.
As discussed, typically the tool electrode is prone to wear. Already from U.S. Pat. No. 3,558,842 and the family member CH 466 452 it is known that a protective film forms on the tool electrode under specific conditions in an electric discharge machining process. The protective film is formed, e.g. by products of the working liquid and/or by products resulting from the discharge across the machining gap. U.S. Pat. No. 3,558,842 describes to periodically repeat at least three impulses of voltage and current characterised by certain duration, amplitude and form of voltage including its sequence to cause high material removal on the workpiece and to form the protective film on the tool electrode surface. The three types of impulses, namely igniting, thermal and protective type, are united in one impulse, which is the main drawback of this method, in particular for meso-micro scale machining. The reasons are that the highest material removal rate per pulse is achieved for short pulses with time duration about 20-40 μs (depending on other technology parameters) and also that the specified technique is not compatible for lower currents required for small dimensions of meso-micro scale machining. Another drawback is the so-called wear budgeting where different impulses packed within a single impulse are difficult to monitor with process control to achieve low or zero tool wear. Moreover, displacement of the discharge channel causes form distortion.
In contrast to this document, the inventor recognized that higher form accuracy can be achieved by selecting such a technology that wear neutral impulse trains are located in a single region, thereby keeping the original form of the tool electrode intact.
Also in electric discharge physics carbon deposition on electrode surfaces has been observed, especially for a temperature reaching above 1400° C. when pyrolysis of carbon begins. Depending on the temperature and pressure carbon builds up from decomposition products through pyrolysis.
The formation of a protective film can be used to protect the tool electrode and to thereby reduce wear of it, as disclosed in the above mentioned article “Zero wear—The “Perpetuum Mobile” of die-sinking EDM”. As discussed in the outset, during the electrical discharge, carbon is formed in form of graphite on the electrode surface(s). The formed graphite type depends on the temperatures involved in the process and current control during electrical discharges. The deposited carbon on the electrode surface (anode and/or cathode) may also contain erosion products or debris formed during and at the end of the discharge. Thereby a layer is formed on the electrode from graphite and erosion products including dielectric decomposition products which protect the original electrode. The EDM process is such controlled that the growth of the layer on the electrode and the wear caused by discharge impulses taking place on the protective layer is in balance. Thus, the wear of the electrode can be reduced.
In this known method impulse trains may be used, which consist of, for example, three identical discharge impulses having the same impulse duration and the same off-time between them. The off-time between the impulse trains according to this method is larger than the off-time between the single discharge impulses of a single impulse train.
Moreover, with this method it is not possible to apply a high discharge current, e.g. above 8 A, for composite electrodes (electrode having multiple different structures, e.g. in the meso- and micro-scale), without causing a high wear on the tool electrode. Hence, with the above methods, the overall machining rate is small.
Here, the process can be seen at multiscale:
In some embodiments, the growth of carbon on the tool electrode can be mainly characterized as lateral growth and frontal growth in dependence on the direction of motion of the tool electrode during erosion. By controlling the current applied to the electrical discharge over the machining gap (also referred to as “spark”) during initial few microseconds (1-30 μs) of the spark, a high initial temperature on the electrode surfaces can be reduced whereas rest of the pulse duration increases the surface temperatures of the electrode which lead to carbon formation on the tool electrode surface(s).
As mentioned earlier, at temperatures above 1400° C. pyrolysis of carbon begins which may be a primary factor for the formation of the protection layer containing graphite and erosion products on electrodes surface(s). The formed layer may be porous or it can be even harder than the base material of the tool electrode, thereby protecting it against thermal and/or abrasive forces typically causing wear of the tool electrode. In some embodiments the average temperature of the tool electrode surface and the discharge region is controlled by controlling a duty factor or an average current density, whereby the volume of the carbon build-up on the graphite electrode can be controlled.
In some embodiments, the current level per spark can be regulated with three main parameters: initial current (0.01-25 A), final current (0.1-120 A) and the path between them i.e. different slopes or gradients in current rise. Thus, the rate at which the carbon builds up is based on all these effects including anode/cathode material properties such as specific heat, thermal conductivity and electrical resistivity. In some embodiments, the profile of the current rise per spark, the current slopes and the initial current can reduce wear of the tool electrode and can increase the radial growth of the carbon protection layer on the tool electrode surface. Also, the geometric scale effect of electrode dimension plays a role in the carbon growth rate and the characteristics of the carbon build up.
Although, only the thermal aspect is mentioned here, in some embodiments, the nature of carbon growth may also be attributed to other aspects such as electro-magnetic field, physical—chemical vapour deposition, cathode/anode spot generation, high current density (0.1-20A or higher) over time and/or surface area, etc.
However, in some embodiments, in particular in the meso- and micro-machining, i.e. for example in the meso-scale (instantaneous electrode surface area 10 mm2 to 1 mm2) and in the micro-scale (instantaneous electrode surface area between 1 mm2 to 0.010 mm2 or smaller or smallest dimension structures at the tool electrode which are below 1 mm), the electrode wear is also with the above-mentioned machining processes considerable.
The inventor recognized that, in particular in the above-defined meso- and micro-machining scale, the wear of the tool electrode can be considerably reduced, whereas material removal rate and process stability can be increased, by introducing at least two types of discharge impulses. A first type discharge impulse is configured for forming a protective layer on the tool electrode and a second type discharge impulse is configured for causing wear/erosion on the tool electrode and the workpiece, respectively. By applying a defined ratio of first and second type discharge impulses for material removal from the workpiece, the wear of the tool electrode can be controlled. Moreover, the first and second type discharge impulse can form a specific impulse train, where for each impulse train the wear is nearly zero. Also the impulse train comprises a predefined ratio of first type and second type discharge impulses.
The first type discharge impulse has a longer impulse duration than the second type discharge impulse. The sequence and combination of the two different types of impulses may be set or generated in any order, also within an impulse train. An impulse train can be defined as a group of discharge impulses, wherein each group, i.e. each impulse train, is separated by a pause time from the previous and consecutive group of discharge impulses (impulse train) or an impulse train can also be defined by a specific pattern of discharge impulses during machining.
In some embodiments, the first type discharge impulse primarily causes the formation of a protective film against wear on the tool electrode radially and/or frontally on the tool electrode. The second type discharge impulse causes erosion on the tool electrode surface(s). Mainly depending on the parameters such as current, duty factor, electrode dimension, anode—cathode material properties and dielectric; short pulse duration may also result in higher material removal rate (MRR), higher electrode wear while keeping process stable. In some embodiments, an impulse train may be separated from a consecutive impulse train by a pause duration which is longer than any one of the pause duration values used between same or different types of impulses within the impulse train.
In some embodiments, the least two discharge types can belong to a first and a second group, respectively (e.g. group 1 and group 2 as shown in
From
Thus, two discharge type groups can be formed:
At the same time, i.e. the same impulse duration value at which the frontal wear reaches a zero value, the same type of discharge with increasing pulse duration reaches a value where the lateral wear of the tool electrode becomes zero (marked with reference sign 35 in
In some embodiments, it is possible that at the pulse duration value for a specified current impulse, the frontal wear on the tool electrode reaches zero but lateral wear has not reached zero yet. Thus, in some embodiments, also two groups can be defined on the basis of lateral wear values, where with increasing pulse duration, a pulse duration value is reached where lateral wear becomes zero or near to zero (35):
In some embodiments, based on the two distinct pulse duration groups (group 1,2) defined for a specified impulse type (with given initial current, final current and path for rise of current) based on frontal wear and/or lateral wear, a specific impulse train is formed comprising at least one impulse with an impulse duration from group 1 and at least one impulse with an impulse duration from group 2 and applied to gap between two electrodes (anode, cathode) which results in low or near zero tool wear, high material removal rate and stable process.
In some embodiments, the impulse train comprises at least two impulses, a first type discharge impulse belonging to group 1 and a second type discharge impulse belonging to group 2 separated by a specific impulse pause duration. In some embodiments, first type discharge impulses (group 1, e.g.
In some embodiments, the impulse train comprises at least one first type discharge impulse (of group 1) and at least one second type discharge impulse (of group 2). In such embodiments, a pause duration between two consecutive impulse trains is larger than any pause duration used between consecutive pulses within the impulse train (see also
In some embodiments, for example, in the case of a single or a simple tool electrode geometry, an arc suppression method, which is generally known to the skilled person, is used and modified by introducing a dynamic arc suppression voltage level and adapting it as a dynamic pulse suppression method. In such embodiments the stated pulse train pause condition is no more valid. Thus, in some embodiments, the amount of second type discharges (group 2 discharges) with respect to first type discharges (group 1 dischargers) is determined and a constant ratio between first and second type discharges is maintained (within a given tolerance). In such embodiments, the at least two types of discharge impulses with different properties may be generated based on various algorithms or adaptive process control with voltage/current characteristics and other impulse characteristics, e.g. delay time, open voltage, fall time from open voltage to discharge voltage, high-frequency component of the discharge voltage, etc. Hence, e.g. based on a regulation of an arc suppression level, two or more types of discharge impulses (group 1, 2) can be generated during the erosion. In such embodiments, the protection layer build-up and the wear process can be performed on multi spark level without creating explicit impulse trains (see also
The specific parameters of the first type (group 1) and second type (group 2) discharge impulses, e.g. of the impulse train, such as initial current, final current, path of current rise between initial and final current, pulse duration(s), pause duration(s) within the impulse train and number of first type (group 1) discharge impulses and second type (group 2) discharge impulses including their sequence within an impulse train depends in some embodiments on fixed parameters, e.g., the surface structure and/or dimensions of the tool electrode, the electrode material, the machining liquid, gap condition, depth of erosion etc.
Accordingly, some embodiments pertain to a method of controlling an electric discharge machining (EDM) apparatus, in particular a die-sinking EDM apparatus or drilling EDM apparatus or milling EDM apparatus. The EDM apparatus has at least a tool electrode and a workpiece and, e.g. other units or elements, which are known to the skilled person, such as a generator, a control, a working table, etc.
The tool electrode is relatively positioned to the workpiece, such that a machining gap is defined between the tool electrode and the workpiece.
The tool electrode can have different shapes, such as known to the skilled person. For instance, the tool electrode can be a single electrode, a batch electrode which has multiple identical structures, a composite electrode which has multiple different structures or a special electrode which can have any shape.
In some embodiments, the tool electrode has at least one portion which has an instantaneous surface area/dimension in the meso- or micro-scale region as defined above.
At next at least one first type discharge impulse and at least one second type discharge impulse are generated, e.g. by the generator of the EDM apparatus. The at least one first type discharge impulse has a longer impulse duration than the impulse duration of the at least one second type discharge impulse and the first type discharge impulse causes the formation of a protective film against wear on the tool electrode and the second type discharge impulse causes erosion at least on the tool electrode. As discussed above, the first type discharge impulse belongs in some embodiments to the first group and the second type discharge impulse to the second group.
Although the function of the first type discharge impulse is to cause a formation of a protective layer on the tool electrode, which can be grown laterally and/or radially on the tool electrode, as also discussed above, the first type discharge impulse could also cause in addition other effects than the formation of the protection layer (such as material removal from workpiece). The same is true for the second type discharge impulse, which can also cause other effects than only causing wear on the tool electrode and/or material removal on the workpiece (such as process stability).
The first and second type discharge impulses are applied to the tool electrode for material removal from the workpiece. The ratio between the first and second type discharge impulses applied to the tool electrode is defined such that a predefined wear of the tool electrode is caused.
In some embodiments, a plurality of first and second type discharge impulses is applied to the tool electrode. Thus, the ratio between first type and second type discharge impulses is calculated by the number of first type and second type discharge impulses, respectively.
By defining a specific ratio of first and second type discharge impulses a predefined balance between build-up of the protection layer on the tool electrode and the amount of wear of the tool electrode can be achieved, thereby controlling the wear of the tool electrode.
In some embodiments, the sequence of first and second type discharge impulses can be in any order. In other embodiments, the first and second type discharge impulses are arranged in a predefined order, e.g. one first type discharge impulse is followed by at least one second type discharge impulse, wherein the first and second type discharge impulses are separated by a process pause from each other.
In some embodiments, the first and second type discharge impulses are grouped in a specific discharge impulse pattern, for example, into an impulse train, as also mentioned above. In such embodiments, the EDM generator generates at least one impulse train including at least one first type discharge impulse and at least one second type discharge impulse. The second type discharge impulse(s) are generated in any sequence to the first type discharge impulse e.g. the one single first type discharge impulse comes first in the impulse train and at least one second type (group 2) discharge impulse(s) follow after the first type discharge impulse (as also shown in
The at least one impulse train is applied to the tool electrode for material removal. In some embodiments, a plurality of impulse trains is generated and applied to the tool electrode for material removal.
As discussed, the first type discharge impulse (belonging to group 1) primarily causes the generation or formation of a protective film or protective layer against wear on the tool electrode. The protective film can be formed, as discussed above in connection with U.S. Pat. No. 3,558,842, by reaction particles of the machining fluid and/or of the tool electrode and/or of the workpiece, e.g. by pyrolysis. In some embodiments, the tool electrode protective film comprises graphite or graphite embedded with erosion products. In such embodiments, the first type discharge impulse (group 1) is adapted to form or generate a pyrolytic graphite layer on the tool electrode which may have higher degree of hardness compared to the base electrode material. In some embodiments, the protective layer is formed in particular in a front region of the tool electrode, e.g. by frontal growth, where most of the discharges take place.
The second type discharge impulse (belonging to group 2) causes erosion at least on the tool electrode and, additionally, on the workpiece. As the tool electrode is mainly protected by the protection film produced by the single first type discharge (group 1) impulse, the tool electrode itself is not worn or marginally worn, while mostly the protective layer which has been formed on it is worn out.
As mentioned, the single first type discharge impulse (group 1), e.g. of each impulse train, has longer impulse duration than the second type discharge impulse (group 2). The particular impulse duration values at which first type and second type discharge impulses (i.e. group 1 and group 2 discharge impulse) can be separated depends on the impulse type/characteristic (initial current, final current, path for rise of current) and associated process parameters (e.g. electrode surface area, dielectric oil, workpiece material, electrode material, pause duration between two consecutive impulse trains, etc.). For a given impulse type having specific characteristics (see also
In some embodiments, a first group (group 1) of time durations embracing the first type discharge impulses and a second group (group 2) of time durations embracing the second type discharge impulses are each defined, e.g. based on the characteristics discussed above. The time duration of the discharge impulses of the first and/or second group are determined by at least one of the following process parameters: electrode surface area, pulse type (initial current, final current, path), electrode-workpiece materials, pause duration between consecutive impulse trains, dielectric oil, gap between tool electrode and workpiece, time interval between two flushing cycles, machining depth, discharge voltage and/or current. In some embodiments, at least some of these parameters are taken into account in order to specify the first and/or second type discharge impulse.
In some embodiments, the time duration of the second type discharge impulse is chosen from the second group of discharge impulses and the time duration of the first type discharge impulse is chosen from the first group of discharge impulses.
In some embodiments, the first and/or second type discharge impulse is specified at least by an initial current value, a final current, and a path taken for a rise of current, thereby also the specific curve of the impulse is defined. In some embodiments, pulse type of impulses within an impulse train may be different. E.g. pulse type for impulses belonging to group 1 and group 2 may be different where group 1 impulse may have increasing slope current for faster carbon growth and group 2 impulses may have rectangular current shape for higher material removal from tool electrode and/or workpiece.
In some embodiments, within one impulse train the protective film against wear on the tool electrode generated by the first type discharge impulse is nearly completely eroded by the second type discharge impulses of the impulse train.
The impulse train with the first and second type discharge impulses is applied to the tool electrode such that a corresponding discharge takes place across the machining gap between the tool electrode and the workpiece. Thus, in embodiments, where the protective layer produced within one impulse train is eroded within one impulse train, the tool electrode has (nearly) the original shape after application of each impulse train. In other words, in some embodiments, the impulse train is wear neutral due to combination of group 1 and 2 impulses, while mostly achieving even higher material removal rate and process stability due to group 2 impulse(s).
Due to this shape accuracy characteristic in some embodiments, also structures in the defined domain of meso and micro scale can be machined with high accuracy and form precision with even lesser number of required electrodes for machining leading to higher productivity, lower resource requirements and thus overall cost saving for any type of machining (complex features, combination electrodes including high aspect ratios up to 3:1 and above) in macro-meso-micro scale for numerous engineering materials (e.g. Steel, Stainless Steel, Nickel alloys, Titanium alloys, Aluminium, Ceramics, Silicon, etc.).
In some embodiments, the time duration of the second type discharge impulse is below 30 microseconds. Pulse duration value depends on various parameters such as electrode surface area, gap conditions, applied current per spark, average current, etc. This allows a fast machining of the anode and/or cathode region, in particular in comparison with the known “zero wear” method or single type discharge process technologies described above.
In some embodiments, the discharge current during spark is in the range of 0.1 A to 120 A, and, in particular, above 8 A, and in particular for the second type of discharge impulses (group 2 pulse durations). Such a high discharge current also allows a higher wear on tool electrode and may also result in faster machining process, in particular in comparison with the “zero wear” method described above, since in this described method the wear of the tool electrode is very high, in particular in the case of a high discharge current and small electrode surface area which is below 10 mm2 or smallest electrode dimension below 1 mm (e.g. Ribs).
In some embodiments, the first type and/or the second type discharge impulse has a square shape, an increasing slope section and/or a falling slope section with main parameters: initial current, final current and path used for current rise/fall between these two points. In some embodiments, an increasing slope section, in particular an increasing edge has the effect that the discharge impulse starts with a lower current and increase over impulse duration. This allows using a higher peak current and/or current density for a discharge impulse in some embodiments for given surface area of electrode and may also facilitate faster carbon growth on tool electrode. Similarly, the falling slope section, in particular a falling edge, has the effect that a higher peak current of a discharge impulse is only present for a short time. Thus, such impulse shapes allow the application of a higher peak discharge current.
In some embodiments, the second type discharge impulse (
In some embodiments, the first type discharge impulse(s) and the second type discharge impulse(s) have positive polarity, while in other embodiments the first type discharge impulse has a positive polarity and the second type discharge impulse(s) have a negative polarity. The negative polarity can increase the removal of the protective layer from the tool electrode.
The second type discharge impulses can also be generated by a capacitive discharging (see
As mentioned, some embodiments pertain to machining in the meso-scale and/or micro-scale or even smaller surface area (nano scale). In such embodiments, the tool electrode has at least one section or surface area or smallest dimension structure which is smaller than 10 mm2, respectively 1 mm, in some embodiments even smaller than 0.010 mm2.
In some embodiments, an off-time between two consecutive impulse trains is larger than the pause duration(s) used between different pulses within a single impulse train. The inventor has recognized that in some embodiments the overall machining rate can be improved by introducing longer pauses or off-times (>200 as) between consecutive impulse trains, since the longer pauses can allow a better recovery of the machining gap, and primarily depends on pulse type (initial current, final current, path for rise of current) and process parameters (such as electrode surface area, time interval between two flushing cycles, dielectric oil, workpiece and electrode materials).
In some embodiments such as single electrodes in meso-micro scale, single impulse trains can be replaced by algorithms which maintain a specific ratio of pulses belonging to group 1 (longer pulse duration) with pulses belonging to group 2 (shorter pulse duration), as discussed above. The generation of two distinct discharge types can be done with preset programming or dynamically through adaptive current control algorithms e.g. using arc suppression level.
In some embodiments, the ratio of first and second type discharge impulses is controlled at a desired value, e.g. maintained constant, in order to provide a predefined amount of wear of the tool electrode.
Some embodiments pertain to an electric discharge machining apparatus, in particular a die-sinking EDM apparatus or drilling EDM apparatus, which is adapted to perform at least some steps of the control method as described above.
Such an EDM apparatus comprises parts which are typically known to the skilled person, such as a tool electrode, a working table for receiving a workpiece, an impulse generator for generating discharge impulses, and a control for controlling the EDM apparatus. The control is adapted for performing the method as described above.
Returning to
The die-sinking EDM apparatus 1 has a control block 2 for performing the EDM process described above. The control block 2 has a general control module 7, a generator control module 8 for controlling an impulse generator 4, a machining gap control module 9 for controlling a machining gap 13 between a tool electrode 11 and a workpiece 12, and a gap acquisition module 10 for receiving machining gap related data during the machining process.
The tool electrode 11 and the workpiece 12 are located in a machining block 3. The positioning of the tool electrode 11 relative to the workpiece 12 is performed over an interpolator module 6 and a drive module 5 which drives positioning members, such as servo-feeds, in the c, x, y and z-direction as indicated in the machining block 3 of
a to 2f illustrate examples of different impulse trains which can be used in the die-sinking EDM 1 for machining the workpiece 12. The
a illustrates an impulse train 14 which has in the first position one first type discharge impulse 15 (group 1) for primarily forming a protective layer on the tool electrode 11, as discussed above, and three consecutive second type discharge impulses 16 (group 2) for eroding the workpiece 12 and the protective layer on the tool electrode 11, as also discussed above. The discharge impulses 15 and 16 here have a rectangular shape, i.e. an initial current is the same as a final current for a single impulse. The discharge current is the same for the discharge impulses 15 and 16 of the impulse train 14.
Moreover, also the off-times between the discharge impulse 15 for forming the protective layer and the first erosion discharge impulse 16 as well as between the single erosion discharge impulse 16 are identical in the present embodiment.
Between the application of each impulse train 14 an off-time can be used. During the off-time the machining gap, the tool electrode and the workpiece recover such that in some embodiments the overall machining rate is higher than in embodiments where no or only a short off-time is present between single impulse trains.
As mentioned above, the impulse durations, the off-times between the impulses, the number of the erosion discharge impulses, the discharge current, the off-time between impulse trains, etc., depend i.e. on the materials used for the tool electrode and the workpiece, gap conditions and the shape of the tool electrode 11, etc. These parameters can be pre-stored and/or pre-set in the die-sinking EDM apparatus 1 for group 1 and group 2 discharge impulses. In other embodiments, these parameters can be dynamically determined, e.g. by analyzing machining parameters, such as variations in the discharge voltage or current characteristics.
In some embodiments, also other impulse trains can be used:
For example, in some embodiments an impulse train 17, as illustrated in
As illustrated in
As illustrated in
In order to further reduce wear at the tool electrode or achieve faster radial growth of graphite protective layer, in some embodiments and as illustrated in
A short erosion discharge impulse 30 (group 2), as illustrated in
The above discussed shapes of the long impulse 27 (
As illustrated in
In the following, the differentiation between group 1 and group 2 discharge impulses is exemplary discussed in connection with
As illustrated in
As illustrated in
The following discussion of
As illustrated in
a illustrates an impulse train 46 having in the three first positions three second type discharge impulses 48 causing erosion followed by a longer first type discharge impulse 47. In this impulse train 47 the wear caused by the second type discharge impulses 48 is balanced by the first type discharge impulse 47 causing the formation of a protective layer on the tool electrode.
b illustrates an impulse train 49, where on the first two positions two second type discharge impulses 51 are located, followed by a first type discharge impulse 50, which, in turn, is followed by a single second type discharge impulse 51. In this impulse train 49, the first type discharge impulse 50 is interposed between at least two second type discharge impulses 51.
c illustrates an impulse train 52, where on a first position a single second type discharge impulse 54 is located, followed by a single first type discharge impulse 53, which, in turn, is followed by two second type discharge impulses 54.
As illustrated in
In such embodiments, also the ratio between at least these two different impulse types of group 1 and 2 is maintained constant. The ratio can be pre-programmed or dynamically calculated, using one or more process condition information, e.g. dynamic arc suppression level to achieve low tool wear and/or high material removal rate.
Although the present invention is described in connection with a limited number of embodiments, it is evident that there may be allowed modifications and variants that do not depart from the concept and scope of the invention, which will be readily understood by those skilled in the art. All these modifications and variants are considered not to depart from the concept and scope of the invention, as defined by the appended claims.
Number | Date | Country | Kind |
---|---|---|---|