This application claims the benefit of Chinese Patent Applications No. 201420464396.0 filed on Aug. 18, 2014 and No. 201410405859.0 filed on Aug. 18, 2014 in the State Intellectual Property Office of China, the entire disclosures of which are incorporated herein by reference.
The present application is a divisional application of U.S. application Ser. No. 14/636,458, filed on Mar. 3, 2015, the entire disclosure of which is incorporated herein by reference.
The present disclosure generally relates to a technical field of electronics, in particular to an electronic apparatus and a method for producing a housing.
A housing of an electronic apparatus is a protective layer of the electronic apparatus and a coat of the electronic apparatus. Thus, it is desired that the housing not only has a good shatter and compression resistance, but also has an elegant appearance and a good hand feeling.
For appearance, implementation of multilayer colors in the housing is a main scheme.
An intermediate frame, a front panel arranged in front of it and a rear panel (i.e., back casing) mounted behind the intermediate frame are provided to form the housing of the electronic apparatus such as a cell phone, a tablet computer.
However, it causes a complex producing process and degrades the hand feeling and appearance of the housing due to the difficulty of assembling such electronic apparatus caused by three components (the front panel, the rear panel and the intermediate frame).
It provides an electronic apparatus comprising M electronic elements; a housing having an accommodating space in which the M electronic elements are fixed and arranged, the housing provided with N through-holes from which N electronic elements of the M electronic elements are exposed, M>N≥1 and M and N are both positive integers, wherein the housing comprises: a side wall forming the accommodating space and having an outer surface which is divided into K appearance layers, where K is a positive integer greater than or equal to 3, and wherein borderlines between adjacent layers in the K appearance layers are parallel to each other. The outer surface has an attractive visual effect because of its divided K appearance layers.
In another aspect, an embodiment of the present application also provides a method for producing a housing of an electronic apparatus, the method comprises: forming a first frame body by injection moulding in a first mold, the first frame body forming a first portion of the side wall of the housing; moulding inserts by K−1 times: in the moulding inserts at first time, putting the first frame body as a first insert into a second mold and forming a second frame body by injection moulding, the second frame body constituting a second portion of the side wall of the housing, the second portion including the first portion and forming two appearance layers, wherein the first portion forms one appearance and the part of the second portion other than the first portion forms the other appearance; and do so, in the moulding inserts at the (K−1)th time, putting the (K−1)th frame body as a (K−1)th insert into a Kth mold and forming a Kth frame body by injection moulding, the Kth frame body constituting the side wall of the housing, the side wall forming K appearance layers, wherein K is a positive integer greater than or equal to 3.
In order to explain the embodiments of the present application, the drawings that are needed to be used in the description of the embodiments are explained simply below. Apparently, the following drawings only illustrate some embodiments of the present application by way of examples. The skilled person in the art can envisage other drawings from the following ones without inventive concepts.
Embodiments of the present application will be described hereinafter in more detail with reference to figures of the attached drawings, so that the objects, technical solutions and advantages of the present application will be more apparent.
An embodiment of the present application provides an electronic apparatus. As illustrated in
As shown in
The electronic elements 101 shown in
In the embodiment of the present application, the housing is designed to have an accommodating space in which the M electronic elements are fixed and arranged, the housing provided with N through-holes from which N electronic elements of the M electronic elements are exposed, M>N≥1 and M and N are both positive integers, wherein the housing comprises: a side wall forming the accommodating space and having an outer surface which is divided into K appearance layers, where K is a positive integer greater than or equal to 3, and wherein borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides an electronic apparatus. As illustrated in
M electronic elements 201; and a housing 202 having an accommodating space 203 in which the M electronic elements 201 are fixed and arranged, the housing 202 provided with N through-holes from which N electronic elements 201 of the M electronic elements 201 are exposed, M>N≥1 and M and N are both positive integers.
As shown in
In the embodiment, all of points on a first borderline 2051 between a first layer 2041 in the K appearance layers located on the top of the outer surface of the side wall 204 and a second layer 2042 adjacent to the first layer 2041 have the same vertical distance from a top side of the outer surface of the side wall.
Further, all of vertical distances between any two adjacent borderlines are equal.
In the embodiment, each of the K appearance layers has a different appearance from those of others of the K appearance layers.
In particular, the different appearance may be achieved by the following means:
all of the K appearance layers have the same material, but have different colors from each other. In producing process, it may be moulded by a single color injection machine and then by sprayed with multiple colors to achieve the multilayer colored housing. The details of the producing process will be explained in the Fifth Embodiment.
In the embodiment of the present application, the housing is designed to have an accommodating space in which the M electronic elements are fixed and arranged, the housing provided with N through-holes from which N electronic elements of the M electronic elements are exposed, M>N≥1 and M and N are both positive integers, wherein the housing comprises: a side wall forming the accommodating space and having an outer surface which is divided into K appearance layers, where K is a positive integer greater than or equal to 3, and wherein borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides an electronic apparatus. As illustrated in
M electronic elements 301; and a housing 302 having an accommodating space 303 in which the M electronic elements 301 are fixed and arranged, the housing 302 provided with N through-holes from which N electronic elements 301 of the M electronic elements 301 are exposed, M>N≥1 and M and N are both positive integers.
As shown in
In the embodiment, all of points on a first borderline 3051 between a first layer 3041 in the K appearance layers located on the top of the outer surface of the side wall 304 and a second layer 3042 adjacent to the first layer 3041 have the same vertical distance from a top side of the outer surface of the side wall.
Further, all of vertical distances between any two adjacent borderlines are equal.
In the embodiment, each of the K appearance layers has a different appearance from those of others of the K appearance layers.
In particular, the different appearance may be achieved by the following means:
each of the K appearance layers has a different material from those of the others of the K appearance layers.
Or, two of the K appearance layers have the same material, but have different colors from each other, and a layer between the two layers has different material from the two layers. In producing process, a product having two color effects may be moulded at one time by a double colors injection machine and then “a waistband” is assembled between the two colors to form a three-colors housing. The details of the producing process will be explained in the Sixth Embodiment.
In the embodiment of the present application, the housing is designed to have an accommodating space in which the M electronic elements are fixed and arranged, the housing provided with N through-holes from which N electronic elements of the M electronic elements are exposed, M>N≥1 and M and N are both positive integers, wherein the housing comprises: a side wall forming the accommodating space and having an outer surface which is divided into K appearance layers, where K is a positive integer greater than or equal to 3, and wherein borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides an electronic apparatus. As illustrated in
M electronic elements 401; and a housing 402 having an accommodating space 403 in which the M electronic elements 401 are fixed and arranged, the housing 402 provided with N through-holes from which N electronic elements 401 of the M electronic elements 401 are exposed, M>N≥1 and M and N are both positive integers.
As shown in
In the embodiment, all of points on a first borderline 4051 between a first layer 4041 in the K appearance layers located on the top of the outer surface of the side wall 404 and a second layer 4042 adjacent to the first layer 4041 have the same vertical distance from a top side of the outer surface of the side wall.
Further, all of vertical distances between any two adjacent borderlines are equal.
In the embodiment, each of the K appearance layers has a different appearance from those of others of the K appearance layers.
In particular, the different appearance may be achieved by the following means: each of the K appearance layers has a different material from those of the others of the K appearance layers. The details of the producing process will be explained in the Seventh Embodiment and the Eighth Embodiment.
Further, as shown in
By means of the above design of the inner surface, the forces applied to the first to the (K−1)th layers are decreased to avoid the breaking of the side wall of the housing. As in the embodiment, each layer is made from the material different from those of the other layers, there is a certain, but not very strong, interface bonding force between two materials in moulding inserts. Thus, it has a certain risk of breaking. In the embodiment, the Kth layer of the bottom frame, the bottom surface and the inner surface are made from the same material and moulded at one time. Its mechanical properties may meet the normal mechanical requirements (for the same thickness of the side wall, the tensile strength of the side wall of the single injection member is greater than the interface bonding force between two materials of the side wall moulded by inserts), and it may be the primary stressed member. A display screen, an inner main board and other electronic elements are fixed on the member (the bottom frame, the bottom surface and the inner surface). In contrast to it, the interface between the first layer and the second layer, . . . , the interface between the (K−2)th layer and the (K−1)th layer are subject to tiny forces, and thus, a risk of breaking in the side wall of the housing will not occur in use.
In the embodiment of the present application, the housing is designed to have an accommodating space in which the M electronic elements are fixed and arranged, the housing provided with N through-holes from which N electronic elements of the M electronic elements are exposed, M>N≥1 and M and N are both positive integers, wherein the housing comprises: a side wall forming the accommodating space and having an outer surface which is divided into K appearance layers, where K is a positive integer greater than or equal to 3, and wherein borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
Besides the above embodiments.
Further, as illustrated in
Further, the intermediate bar 23 in transited into the first layer 22 smoothly at the borderline 21 between the intermediate bar 23 and the first layer 22, and the intermediate bar 23 in transited into the second layer 24 smoothly at the borderline 21 between the intermediate bar 23 and the second layer 24. In this way, the appearance surface of the side wall 2 conforms to the customs of the user in visual.
Further, in the electronic apparatus, the housing 1 further includes a bottom surface (not shown). The bottom surface has the same appearance as that of the bottom layer on the appearance surface of the side wall 2. In an embodiment, the bottom surface of the housing 1 and the bottom layer on the appearance surface of the side wall 2 are moulded integrally to form the back casing of the housing. Then, the same appearance may be provided on the back casing. In this way, the processing is easier and the cost may be reduced. In an embodiment, the bottom surface may have the appearance of wood grains or skin grains.
Further, as shown in
Further, in the above electronic apparatus, all of the K appearance layers are made of the same material with different color parameter appearance respectively. In particular, all of the K appearance layers are made of the same material and the outer surfaces of all of the K appearance layers are coated with different colors such that all of appearance layers have different appearance.
Further, in another embodiment, in the above electronic apparatus, all of the K appearance layers are made of different materials respectively and all of different materials have different appearance respectively. In this example, the K appearance layers represent different appearance by different materials.
Further, in another embodiment, as shown in
An embodiment of the present application provides a method for producing a housing of an electronic apparatus. As shown in
Step 501: forming a raw housing by injection moulding at one time by a single color injection machine.
Step 502: processing the raw housing by multiple colors shield spraying such that the outer surface of the side wall is divided into K appearance layers, where K is a positive integer greater than or equal to 3 and borderlines between adjacent layers in the K appearance layers are parallel to each other.
In this example, the multiple colors shield spraying is to shield the specific part of the side wall by a specific shielding jig and to spray the unshielded part with colors. The multilayer colors housing may be obtained by the shield spraying by multiple times.
In the embodiment of the present application, the raw housing is processed by the multiple colors shield spraying such that the outer surface of the side wall is divided into K appearance layers, where K is a positive integer greater than or equal to 3 and borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides a method for producing a housing of an electronic apparatus. As shown in
Step 601: forming a product having two colors effects by injection moulding at one time by a double colors injection machine, the product being provided an art groove at the intermediate position of the side wall thereof.
Step 602: assembling an opened thin frame (waistband) with the third color in the art groove to obtain the three layer colors housing.
In the embodiment of the present application, the raw housing is processed by the multiple colors shield spraying such that the outer surface of the side wall is divided into K appearance layers, where K is a positive integer greater than or equal to 3 and borderlines between adjacent layers in the K appearance layers are parallel to each other. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides a method for producing a housing of an electronic apparatus. As shown in
Step 701: forming a first frame body by injection moulding in a first mold, the first frame body forming a first portion of the side wall of the housing;
Step 702: moulding inserts by K−1 times.
In particular, in the moulding inserts at first time, putting the first frame body as a first insert into a second mold and forming a second frame body by injection moulding, the second frame body constituting a second portion of the side wall of the housing, the second portion including the first portion and forming two appearance layers, wherein the first portion forms one appearance and the part of the second portion other than the first portion forms the other appearance; and do so,
in the moulding inserts at the (K−1)th time, putting the (K−1)th frame body as a (K−1)th insert into a Kth mold and forming a Kth frame body by injection moulding, the Kth frame body constituting the side wall of the housing, the side wall having K appearance layers, where K is a positive integer greater than or equal to 3.
The housing produced by the embodiment has a very clear layer to layer border, has no layer to layer gaps and has no breaking beds, in contrast to the housing produced by the Fifth embodiment.
In contrast to the housing produced by the Sixth embodiment, the embodiment uses the single color injection machine to produce the housing such that the cost is significantly reduced in comparison with the double colors injection machine. The housing produced by the embodiment has a very clear layer to layer border, has no layer to layer gaps and has no breaking beds.
In the embodiment of the present application, a first frame body by injection moulding is formed in a first mold and then inserts are moulded by K−1 times. In particular, in the moulding inserts at first time, the first frame body as a first insert is put into a second mold and a second frame body is formed by injection moulding, and do so, in the moulding inserts at the (K−1)th time, the (K−1)th frame body is put as a (K−1)th insert into a Kth mold and a Kth frame body is formed by injection moulding, the Kth frame body constituting the side wall of the housing, the side wall forming K appearance layers, where K is a positive integer greater than or equal to 3. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
An embodiment of the present application provides a method for producing a housing of an electronic apparatus. As shown in
Step 801: forming a first frame body by injection moulding in a first mold, the first frame body forming a first portion of the side wall of the housing.
In particular, the first mold includes a first fixed mold 80 (see
The structure of the first frame body 90 is shown in
Step 802: moulding inserts by K−1 times.
In particular, in the moulding inserts at first time, putting the first frame body as a first insert into a second mold and forming a second frame body by injection moulding, the second frame body constituting a second portion of the side wall of the housing, the second portion including the first portion and forming two appearance layers, wherein the first portion forms one appearance and the part of the second portion other than the first portion forms the other appearance; and do so,
in the moulding inserts at the (K−1)th time, putting the (K−1)th frame body as a (K−1)th insert into a Kth mold and forming a Kth frame body by injection moulding, the Kth frame body constituting the side wall of the housing, the side wall having K appearance layers, where K is a positive integer greater than or equal to 3.
In particular, the second mold includes a second fixed 100 (see
In addition, the first cover in the first mold and the second cover in the second mold may have the same shape. In order to save the cost, they may be implemented as the same cover. The cover has the main function of covering the groove in the mold in injection.
The structure of the second frame body 110 is shown in
In particular, the Kth mold includes the Kth fixed mold 120 (as shown in
In particular, the housing produced by the step 602 (i.e., the Kth frame body) is shown in
In the embodiment, the bottom surface 150b of the housing 150 is formed by moulding inserts at the (K−1)th time.
The inner surface 150c of the housing 150 is formed by moulding inserts at the (K−1)th time and the (K−1)th frame body is arranged around the inner surface 150c and the inside of the (K−1)th frame body is combined to the outside of the inner surface 150c together. Further, the bottom frame 150a is also formed upon moulding inserts at the (K−1)th time. The bottom frame 150a is connected to an edge of the bottom surface 150b and the inner face 150c is provided on the bottom frame 150a. The design of the above inner surface may reduce the force to which the first to (K−1)th layers are subject to avoid breaking of the side wall of the housing. As each of the layers is made from the material different from those of the others in the embodiment, there is a certain, but not very strong, interface bonding force between two materials. Thus, it has a certain risk of breaking. In the embodiment, the Kth layer of the bottom frame, the bottom surface and the inner surface are made from the same material and moulded at one time. Its mechanical properties may meet the normal mechanical requirements (for the same thickness of the side wall, the tensile strength of the side wall of the single injection member is greater than the interface bonding force between two materials of the side wall moulded by inserts), and it may be the primary stressed member. A display screen, an inner main board and other electronic elements are fixed on the member (the bottom frame, the bottom surface and the inner surface). In contrast to it, the interface between the first layer and the second layer, . . . , the interface between the (K−2)th layer and the (K−1)th layer are subject to tiny forces, and thus, a risk of breaking on the side wall of the housing will not occur in use.
In the moulding inserts at the (K−1)th time, putting the (K−1)th frame body as the (K−1)th insert into the Kth mold 140 having deformed portion and forming the Kth frame body by injection moulding to form the side wall of the housing, the deformed portion being configured to counteract the deformation of the frame body in the moulding inserts by the K−1 times, during the injection moulding.
In particular, the Kth mold 140 has grooves and protrusions that are formed by arc-shape faces, the arc-shape faces having curvatures designed on the basis of the deformation quantity of the housing obtained by moulding inserts by K−1 times by general molds.
In a general injection moulding, (the average condition of most of manufacturers without limited by resources), the insert moulding products have relatively large deformations. Without predeformation of the mold, the deformation may be corrected in a certain case by adjusting the injection process, however, it cannot be corrected at all in another case, in particular when the insert moulding products are made from the materials having large difference in physical properties (for example, thermal expansion coefficient, thermal conduct coefficient, melt mobility, melt temperature) or from special materials, the insert moulding products will have very serious warpage deformation that cannot be solved only by adjusting the injection process. For example, two materials for injection have very large difference in thermal expansion coefficients, e.g., the material injected later has the thermal expansion coefficient significantly greater than that of the material as the insert, the final product obtained by insert moulding tends to have large deformation, even to break directly. In this circumstance, the warpage deformation cannot be solved only by adjusting the injection process conditions. However, the process of “predeformation” can solve the technical problem.
Thus, the housing produced by the embodiment will not generate the warpage deformation in comparison with those produced by the Fifth Embodiment and the Sixth Embodiment.
In particular, when the predeformation is designed, its parameter (curvature) may be obtained by the following means:
In one method, the insert moulding is carried out in a general process conditions by means of easy dismountable cavity modules (no predeformation, the cavity is an ideal product state). At that time, the insert moulding products will be deformed to some extent. The parameter for deformation of the product is tested and reverse design is carried out on the basis of the parameter in the extent of deformation (for example, if the insert moulding products projects outwards to deform, the normal mold insert cavity will be designed to be recessed to the corresponding extent) in the normal mold insert cavity design, and thus the desired parameter will be obtained. In final moulding, it may be adjusted slightly by the variation of the moulding process parameters. In this way, the housing product with little deformation or without deformation may be obtained. In another method, the warpage deformation data of the insert moulding products may be simulated and calculated by simulation analysis software (such as Moldflow) and the mold is designed reversely on the basis of it.
Further, in the step 802, in the insert moulding, the insert position at which a melt material enters in a high temperature is controlled to correspond to the insert position at which it enters in the moulding inserts at the last previous time.
Generally, in the insert moulding, the moulding runner may cause local melt deformation near the inserts due to fast high pressure impacts on the high temperature melt plastics (in this circumstance, it can be seen from appearance that there is a certain curve deformation of the layer-to-layer border of the two materials and the insert may be concaved slightly in local), but the region that it affects is not large. As long as the region where the melt deformation occurs is designed in the part which will be removed subsequently by CNC, the deformation of the border between two colors may be avoided to be left on the final housing. For example, if the moulding runner is designed outside the side wall and the part outside the side wall will be cut out by CNC, the layer to layer border of the housing will be linear without deformation. Certainly, the moulding runner may also be designed at other position as long as the position corresponds to the position cut out by the CNC. That is, the form, number and position of the moulding runner of the mold may be designed flexibly. In combination the operation of removing redundant part of the moulding member by CNC, the curve deformation of the color border among the multicolors may be avoided completely.
Step 803: removing a redundant part of the housing at its periphery by using a numerical control processing.
In the embodiment, the step of removing a redundant part of the housing at its periphery by using a numerical control processing comprises:
cutting in a longitudinal direction at the position of the redundant part of the housing at its periphery to remove the part in which the borderlines between layers are deformed in the injection moulding, that is, carrying out the cutting process by CNC process.
After the moulding defects (for example, margin/fin at the border of different color materials, blank and breaking bend at the runner) caused by moulding inserts by multiple times are milled by CNC as described in the step 803, the remaining part has a very clear layer to layer border, has no layer to layer gaps and has no breaking beds.
Further, in the steps 801 and 802 of moulding, decoration particles with diameters of tens of micrometers to hundreds of micrometers may be added into the material. After the step 803, some decoration particles may be cut out to represent the special appearance, to have a distinguishing feature.
Step 804: shining and polishing the processed housing of the electronic apparatus and then spraying protective paint onto a surface of the housing of the electronic apparatus.
By means of the above steps 803 and 804, the appearance and hand feeling of the housing may be improved.
In the embodiment of the present application, a first frame body by injection moulding is formed in a first mold and then inserts are moulded by K−1 times. In particular, in the moulding inserts at first time, the first frame body as a first insert is put into a second mold and a second frame body is formed by injection moulding, and do so, in the moulding inserts at the (K−1)th time, the (K−1)th frame body is put as a (K−1)th insert into a Kth mold and a Kth frame body is formed by injection moulding, the Kth frame body constituting the side wall of the housing, the side wall forming K appearance layers, where K is a positive integer greater than or equal to 3. As the housing includes the side wall forming the accommodating space, it may avoid assembling the intermediate frame and the back casing in the prior art and thus may reduce the complexity of producing process and facilitate assembling. Division of the outer surface of the side wall into the K appearance layers enhances the appearance of the housing. Parallel borderlines between adjacent layers in the K appearance layers are may improve the hand feeling of the housing.
The numerals of the embodiments of the present application are provided only by way of examples, instead of representing the quality of the embodiments.
The above embodiments are only those of the present application by way of examples instead of limiting the present application. Any modifications equal replacements, and variations may be envisaged without departing from the principles and spirits of the disclosure should fall within the scope of the present application.
Number | Date | Country | Kind |
---|---|---|---|
2014 1 0405859 | Aug 2014 | CN | national |
2014 2 0464396 U | Aug 2014 | CN | national |
Number | Name | Date | Kind |
---|---|---|---|
20060118999 | Cooper | Jun 2006 | A1 |
20090194308 | Cheng et al. | Aug 2009 | A1 |
20090301748 | Hsu et al. | Dec 2009 | A1 |
20100061040 | Dabov et al. | Mar 2010 | A1 |
20100326720 | Tsao et al. | Dec 2010 | A1 |
20110005796 | Wu et al. | Jan 2011 | A1 |
20110048754 | Xiong et al. | Mar 2011 | A1 |
20120003489 | Ying | Jan 2012 | A1 |
20120097412 | Wennemer et al. | Apr 2012 | A1 |
20120241185 | Hsu et al. | Sep 2012 | A1 |
20140077410 | Takatsugi | Mar 2014 | A1 |
20140125551 | Chen et al. | May 2014 | A1 |
Number | Date | Country | |
---|---|---|---|
20170262023 A1 | Sep 2017 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 14636458 | Mar 2015 | US |
Child | 15602768 | US |