Claims
- 1. An aqueous pulp slurry containing a thermosetting epoxidized polyamide wet strength resin in an amount sufficient to impart wet strength to said pulp in the manufacture of paper and molded pulp products and lecithin in an amount sufficient to increase the internal bonding strength and to inhibit sticking of said polyamide on heated drying surfaces in the manufacture of paper and molded pulp products.
- 2. An aqueous pulp slurry of claim 1 wherein the quantity of said polyamide is from about 0.1 to 5 percent by weight based on the weight of dry pulp solids.
- 3. A composition of claim 2 wherein the quantity of lecithin varies from about 2 percent to about 10 percent by weight based on the weight of the said polyamide resin.
- 4. A process for making paper and molded pulp products which comprises forming a mat or sheet of pulp from an aqueous pulp slurry containing thermosetting epoxidized polyamide resin in an amount sufficient to impart wet strength to said mat or sheet upon drying of said mat or sheet on heated surfaces and curing of said resin, said slurry also containing lecithin in an amount sufficient to prevent said resin from sticking to said heated surfaces and for increasing the internal bonding strength of said paper and molded pulp products.
- 5. The process of claim 4 for making molded pulp products wherein said products have a permanent contour and a thickness of about 0.1 to 0.4 inches.
- 6. A molded pulp product comprising pulp containing a thermoset epoxidized polyamide wet strength resin in an amount sufficient to impart wet strength to said product and lecithin in an amount sufficient to increase the internal bonding strength of said pulp.
- 7. A molded product of claim 6 having a thickness of from about 0.1 to 0.4 inches.
Parent Case Info
This is a divisional of copending application Ser. No. 411,704 filed on 9/25/89, now U.S. Pat. No. 4,970,250.
US Referenced Citations (16)
Non-Patent Literature Citations (3)
| Entry |
| Japanese Patent Publication JP55-139430 (Publn. & Abstract) of 10/31/80 to Matsushita Elec. Works. |
| Jap. Pat. Pub. J.P.64-45894 (Abstract and Publication) of 2/20/89 to Oji Paper KK. |
| Jap. Pat. Pub. JP88-057206 (English Abstract & Publication) of 11/10/88 to Kobe. |
Divisions (1)
|
Number |
Date |
Country |
| Parent |
411704 |
Sep 1989 |
|