The invention relates to an external electrode for a piezoceramic actuator.
Multilayer piezoceramic actuators are produced as monoliths, that is to say the active material, on which the internal electrodes are applied by a screen printing method before sintering, is assembled as a so-called green film into a stack which is pressed to form a green body. The green body is generally pressed by lamination under the effect of temperature and pressure in laminating moulds.
In the case of external electrodes on the surface 10 of an actuator 1 which are constructed as described above, strong tensile stresses during operation act on the inactive region, that is to say the insulating region 14 which lies below the base metallization 11. Since this insulating region 14 forms a homogeneous unit together with the base metallization 11 and the connecting layer 13, the said unit fails and cracks are formed when the tensile strength of the weakest component is exceeded. The cracking process in question occurs after about 106 working cycles. Owing to the stresses which are encountered, the cracks 15 generally propagate from the brittle base metallization 11 of low tensile strength into the insulating region 14, where they are absorbed by regions with high tensile stresses, preferably at the electrode tips 16 of the electrodes 3 not touching the base metallization 11, or they begin in the regions of maximum tensile stress at the electrode tips 16 and propagate in the direction of the base metallization 11. The spreading of a crack 17 along an internal electrode 3 which touches the base metallization 11 is categorised as uncritical since such a cracking process does not impair the function of the actuator. If the base metallization 11 is split by a crack, then the resilient three-dimensionally structured electrode 12 acts as an electrical bridge so that the crack does not affect the properties or the life of the actuator 13. Cracks 15 which propagate uncontrolled through the insulating region 14, however, are highly critical since they reduce the insulation distance and greatly increase the likelihood of an actuator failure due to arcing.
Moreover, the electrodes constructed in such a way lead to problems when attaching a conductive connection through which an electrical voltage is intended to be delivered.
According to the prior art, a wire 6 is soldered or welded to a three-dimensionally structured electrode 12 at the contact point 18 as represented in
It is known from DE 100 26 005 A1 that the three-dimensionally structured electrode may protrude beyond the actuator and the electrical contact can be soldered there, optionally on the folded or rolled electrode. The protruding ends are insulated by shrink-fit tubing. This type of terminal is elaborate and leads to a complicatedly constructed external electrode. Notch effects can occur at the bending points of the electrode.
It is known from DE 199 09 452 C1 to provide a piezoelectrically inactive region on one side of the actuator, for example at the foot, and to apply the electrical contact in this region. The passive foot leads to a significantly reduced stiffness and expansion for an equivalent overall length of the component, because the passive foot acts like a stiff spring and shortens the active region.
It is an object of the present invention to improve the attachment of the voltage supply lead to the external electrodes by means of the configuration of the electrodes.
The object is achieved in that the external electrode consists of conductive material layers and nonconductive material layers arranged alternately above one another, in that one of the two outlying conductive material layers is connected to the base metallization of the actuator and the other is connected to the voltage supply lead, and in that the conductive material layers are electrically connected to one another.
Since the conductive material layers and nonconductive material layers are arranged alternately above one another, the conductive material layers are mechanically decoupled from each other. The electrical interconnection is established separately, or is obtained by folding a continuous foil as the conductive material. The lower conductive layer, which is connected to the base metallization by soldering or adhesive bonding, can therefore move independently of the upper layers within certain limits and thus compensate for stresses which occur.
A soldered or welded electrical contact is connected only to the top conductive layer. This avoids soldering through the layer.
Therefore, the contact of the terminal wire with the outer conductive layer of the external electrode no longer stiffens the electrode. The forces acting on the external electrode via the base metallization are advantageously attenuated owing to the layered structure, so that they have no effect at the connection position.
On actuators which have external electrodes according to the invention, electrical contacts may be applied at any place on the external electrode without this having any effect on the life or other properties of the actuator. It is therefore possible to produce compact actuator modules without elaborate or disruptive protection measures, such as those which are known from the prior art.
An external electrode constructed according to the invention consists of at least two layers of a conductive material and a layer of a nonconductive material arranged between them.
The conductive material may consist of metal foils, which are easy to process owing to their small thickness. The thickness of the foils is approximately between 30 μm and 200 μm, preferably between 50 μm and 100 μm. The foils may also be structured, for example by stamping. Their overall thickness can thereby be increased to three times the foil thickness.
The conductive material layers may also be three-dimensionally structured. They will not then be solid layers, but instead will consist of metal gauze or fabric, of a mesh or of metal foam.
The gauzes, fabrics or meshes of metal wires have a thickness of about 100 μm to 200 μm. The lattice width of the fabrics or meshes is between about 100 μm and 200 μm, with wire diameters of between about 50 μm and 100 μm.
The nonconductive material layers consist of a resilient plastic, preferably a thermoplastic such as polytetrafluoroethylene (Teflon) or polyimide. The layers are films with a thickness of about 10 μm to about 100 μm.
The conductive material of a layer may also be coated with the nonconductive material of a layer. They may, for example, be foils coated with plastic on one side. These, for example, can be folded to form an external electrode according to the invention. Conductive material layers and nonconductive material layers may furthermore be laminated together alternately.
The individual conductive material layers may consist of different metallic materials. For example, the conductive material, at least of the layer which is soldered or adhesively bonded to the actuator material, may be selected so that it has a coefficient of thermal expansion matched to the ceramic material of the actuator.
In order to establish the electrical connection between the metallic material layers, contacts are made via or around these layers. For this purpose, the layers are electrically connected to one another on each of their long sides, for example by soldering their protruding sides.
It is also possible for a conductive material, preferably in the form of a foil or a gauze, to be folded into a meandering or spiral shape so that the nonconductive material respectively lies as a layer between the folds, or inside a turn. The following effect is achieved by this: interrupting the layers of the foil or the gauze with plastic layers ensures that a soldered or welded electrical contact is only connected to the upper conductive layer. This avoids soldering through and stiffening the layers.
The production of an actuator according to the invention will be described below. A low-sintering piezoceramic according to DE 198 40 488 is prepared with an organic binder system as a 125 μm thick film. An internal electrode paste of silver-palladium powder in a weight ratio of 70/30 and a suitable binder system is applied to this film by means of screen printing. A multiplicity of such films are stacked and pressed to form a laminate. The laminate is divided into individual rod-shaped actuators, which are pyrolyzed at about 400° C. and sintered at about 1100° C. The actuator preforms are then mechanically processed on all sides.
The base metallization, for example consisting of a suitable silver-palladium termination paste, is applied by means of a screen printing/burn-in process.
A structured and folded external electrode according to the invention is soldered onto this base metallization.
The electrical connection may then be applied, for example by soldering or welding. This working step may also be delayed, for example if a contact pin is applied to the folded electrode before soldering onto the actuator. The actuators are subsequently protected by a layer of varnish. It is also possible for the contact not to be established until after the varnishing, in which case the soldering or welding region generally needs to be kept free of varnish. The actuators are subsequently polarised and electrically measured.
The present invention will be explained in more detail with reference to exemplary embodiments.
The production of the external electrodes according to the invention will be explained with reference to four exemplary embodiments.
As indicated above, actuator preforms 1 are prepared with dimensions of 10 mm×10 mm (base area) and a length of 30 mm. The thickness of a single ceramic layer 2 is 100 μm after the sintering, and the thickness of an internal metallization layer is 2 μm. The base metallization 3 is produced by screen printing using a commercially available termination paste, and burnt in for 30 minutes at 750° C. in air. The layer thickness after burning in is from 10 μm to 12 μm. These actuator preforms are then processed in the following way:
According to
External electrodes 20, 21 of this type are soldered at the opposite terminal surfaces onto the base metallization 11 of the actuator preform, for example by a reflow soldering method. A solder point 18 for the terminal wires 6 is respectively applied to the opposite external electrodes 20, 21 in the vicinity of one actuator end face. This procedure represents the prior art. The soldering time is 10 minutes at 240° C.
According to
External electrodes of this type are soldered onto the base metallization of the actuator preform, for example by a reflow soldering method. A solder point 18 for the terminal wires 6 is respectively applied to the opposite external electrodes 23, 24 in the vicinity of an actuator end face. The soldering time is 10 minutes at 240° C.
According to
External electrodes of this type are soldered onto the base metallization 11 of the actuator preform, for example by a reflow soldering method, so that the doubled-up metal mesh layer faces away from the actuator. A solder point 18 for the terminal wires 6 is respectively applied to the opposite external electrodes 26, 27 in the vicinity of an actuator end face. The soldering time is 10 minutes at 240° C.
According to
The matched coefficient of thermal expansion of the mesh material and the already preformed terminal pin are advantageous in this embodiment,
External electrodes of this aforementioned type are soldered onto the base metallization of the actuator preform, for example by a reflow soldering method. The soldering time is 10 minutes at 240° C.
The four variants are coated with silicone varnish by a suitable method, for example by immersion or spraying.
After the varnish has been dried and set, the varnish is removed from the solder points of variants 1 to 3 and a terminal wire is soldered on.
The actuators are prestressed with 2000 N in test frames and driven with a trapezoidal signal. The drive voltage is increased from 0 V to 200 V in 100 μs, kept at 200 V for 1 μs and then reduced to 0 V in 100 μs. The repetition frequency is 200 Hz. The actuators reach operating temperatures of from 150° C. to 160° C. during this.
Example 1 already shows significant detachment of the mesh electrode from the ceramic in the vicinity of the solder points at 107 cycles. After 2·107 cycles, the actuator is destroyed by arcing at the solder points.
Examples 2 to 4 show mutually identical behaviours, which differ significantly from Example 1. Even at 109 cycles, no mesh detachment or arcing occurs in any of the examples.
The person skilled in the art may select various methods when producing the external electrodes according to the invention. For example, the external electrodes may be folded from thin sheet metal coated with plastic or, as described, they may be folded as metal mesh around a plastic strip. Production similar to a printed circuit board is also possible, by laminating the plastic and metal layers onto one another and making electrical contact via them. For example, this printed circuit board may also enclose and protect the entire actuator as preformed flexboard. Instead of soldering the external electrodes onto the actuator, it is also possible to use conductive adhesives. The materials to be used depend essentially on the intended working conditions. PTFE and polyimide materials, and expansion alloys such as FeNi42, are suitable in particular for high temperatures and a rapid temperature change.
Number | Date | Country | Kind |
---|---|---|---|
102 33 057.3 | Jul 2002 | DE | national |
103 27 902.4 | Jun 2003 | DE | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP03/07893 | 7/18/2003 | WO | 6/17/2005 |