This application claims the priority benefit under 35 U.S.C. §119 of Japanese Patent Application No. 2006-353194 filed on Dec. 27, 2006, which is hereby incorporated in its entirety by reference.
1. Field
The presently disclosed subject matter relates to a filament electrode and to a fluorescent lamp using the same. More particularly, the disclosed subject matter relates to a filament electrode that can connect a filament coil with a pair of lead wires with confidence and can be employed even if an inner diameter of the light source is thin. The disclosed subject matter also relates to a fluorescent lamp using the above connection structures that can decrease both end areas which do not emit light and can allow emission with a wider range.
2. Description of the Related Art
A conventional hot-cathode fluorescent lamp (HCFL), cold-cathode fluorescent lamp (CCFL) and the like can include respective electrodes for supplying a power supply at both ends of a light tube that can include a glass tube, silica tube, quartz tube, or other type of arc/luminescence tube. The conventional filament electrode is composed of, for example, a filament coil that is connected to a pair of lead wires. The respective filament coils can be encapsulated in the light tube that includes a filler gas. Respective pairs of lead wires can extend from the light tube to an area outside of the light tube along and can be sealed within the tube structure in an air proof state. Therefore, when supplying the respective filament coils with a power supply via the respective pairs of lead wires, the conventional HCFL, CCFL and the like emit by generating a discharge in the light tube.
The filament coil 3 is attached to the pair of lead wires 2a, 2b as shown in
However, according to the conventional filament electrode 1 shown in
Therefore, an electrode structure as shown in
The filament coil 5 includes: each of the two connecting parts 5b, 5c thereof contacting each end of the pair of lead wires 2a, 2b in line with each other; each of the two connecting parts 5b, 5c thereof being welded with each end of the pair of lead wires 2a, 2b using a spot welding, a laser welding and the like. Therefore, each of the two connecting parts 5b, 5c are fixed to each end of the pair of lead wires 2a, 2b. Thus, the filament coil 5 is attached to the pair of lead wires 2a, 2b by welding each of the two connecting parts 5b, 5c thereof with each end of the pair of lead wires 2a, 2b. In the above described electrode structure, heat generated from the filament coil 5 during light-emission is directly transmitted to the pair of lead wires 2a, 2b and is radiated.
A revised example of the above described filament electrode 4 is disclosed in, for example, Patent Document No. 1 (Japanese Patent Application Laid Open No. JP2005-235749).
An exemplary electrode structure of a fluorescent lamp is disclosed in Patent Document No. 2 (Japanese Patent Application Laid Open No. Hei04-245161).
An exemplary electrode structure of a halogen bulb is disclosed in Patent Document No. 3 (Japanese Patent Application Laid Open No. Hei11-297272).
The above-referenced Patent Documents are listed below and are incorporated herein by reference.
1. Patent Document No. 1: Japanese Patent Application Laid Open JP2005-235749
2. Patent Document No. 2: Japanese Patent Application Laid Open Hei04-245161
3. Patent Document No. 3: Japanese Patent Application Laid Open Hei11-297272
However, in the electrode structure of the filament electrode 4 shown in
In the above-described electrode structures of
In the fluorescent lamp 8 in accordance with Patent Document No. 2, the electrode 8a fixes the lead wire 8e by being sintered with the metallic pipe 8b and by fixing the back end of the metallic pipe 8b to the lead wire 8e with a pressure bonding. However, because the sinter bonding process for fixing the electrode 8a to the metallic pipe 8b is required, the process for manufacturing becomes complex.
In the electrode structure of the halogen bulb 9 in accordance with Patent Document No. 3, because the pipe 9c expands bigger than both the electrode 9a and the lead wire 9b during light-emission of the halogen bulb 9, a gap appears between the electrode 9a and the lead wire 9b. Thus, heat generated from the electrode 9a is not transmitted efficiently to the lead wire 9b because of the gap between the electrode 9a and the lead wire 9b, and the gap prevents the electrode 9a from oxidizing. However, because a transmission of the heat is shielded by the slight gap caused during light-emission of the halogen bulb 9 due to the difference of CTE between materials of both the electrode 9a and the lead wires 9c and a material of the pipe 9c, the heat-shield operation may be unstable or unpredictable, and electrical contact between the electrode 9a and the lead wire 9b may also become defective.
The disclosed subject matter has been devised to consider the above and other problems and characteristics. Thus, embodiments of the disclosed subject matter can include a filament electrode and associated stem that do not cause (or depreciates) some or all of the above-described various problems and can connect a filament coil with a pair of lead wires with confidence and strength. In addition, the filament electrode can be employed even if an inner diameter of a light source is very thin. The disclosed subject matter can also include a fluorescent lamp using the filament electrode that is configured to decrease that portion of the end areas that do not emit light, and to emit light with a wide range.
The presently disclosed subject matter has been devised in view of the above and other problems and characteristics in the conventional art, and to make certain changes to the existing electrode structures. An aspect of the disclosed subject matter includes providing a filament electrode and associated stem that can connect a filament coil with a pair of lead wires with confidence and strength for supplying a power supply absolutely and which prevents leaks in a sealing portion. Furthermore, the filament electrode can be used even in a thin inner diameter tube.
Another aspect of the disclosed subject matter includes providing a fluorescent lamp using the above described filament electrode that can decrease both end areas which are not configured for emission of light and which can emit light with a wider range. Thus, because the fluorescent lamp can be formed to be thin and can extend a light-emission area thereof, it can be employed as a light source for a back light unit, etc.
According to an aspect of the disclosed subject matter, a filament electrode can include: a pair of connecting pipes formed in a tubular manner; a pair of lead wires located parallel with respect to each other, each with an end thereof attached to a respective end of the pair of connecting pipes in a telescoped state via pressure bonding, and each with an opposite respective end thereof exposed in order to supply a power supply; and a filament coil including two connecting parts, each of the two connecting parts attached to each of the opposite respective ends of the pair of connecting pipes in a telescoped state via pressure bonding so as not to contact the ends of the pair of lead wires in each of the pair of connecting pipes.
In the above described exemplary filament electrode, the filament electrode can also include the pair of connecting pipes that are composed of a conductive material having a coefficient of thermal conductivity that is smaller than that of the pair of lead wires. The pair of connecting pipes can also include a squeezing part between each end thereof and each respective other end thereof. The squeezing part can be formed in a tapered shape so as to shrink from each first end thereof towards each respective other end thereof. In addition, the pair of connecting pipes can also function as a getter, for example, by being made of certain reactive materials to ensure and maintain proper atmospheric chemical make-up and pressure qualities within the tube.
In the above described exemplary filament electrode, the filament electrode can further include a glass bead formed in a circular manner, wherein the glass bead is provided around a proximal portion of each exposed end of the pair of lead wires and can achieve an air proof state between the glass bead and the pair of lead wires. The above filament electrode including the glass bead can be a convenient structure for manufacturing a fluorescent lamp as described later.
According to the above described exemplary filament electrode, because each of the two connecting parts of the filament coil can connect each corresponding end of the pair of lead wires via the pair of connecting pipes, a power supply can be provided to the filament coil with great consistency. In that case, because each of the two connecting parts of the filament coil can align each of the pair of lead wires via each of the pair of connecting pipes in line with a direction parallel or co-axial with a longitudinal axis or length of the tube, the filament electrode can be installed in the tube with confidence even if an inner diameter of tube is thin.
In addition, because each of the two connecting parts of the filament coil can firmly attach to each of the pair of connecting pipes via pressure bonding, the fixing intensity does not weaken due to recrystallization of tungsten of the filament coil. Thus, the filament coil is not prone to detachment from the pair of lead wires and can be confidently supplied with a power supply.
Furthermore, when the pair of connecting pipes is composed of a material for which the coefficient of thermal conductivity is smaller than that of the pair of lead wires, because heat generated from the filament coil is then not transmitted efficiently to the pair of lead wires, a gap that may otherwise be caused between the glass bead and the pair of lead wire can be prevented and therefore a filler gas in the glass tube can be prevented from leaking out.
Another aspect of the disclosed subject matter includes a fluorescent lamp using the immediately above-described filament electrode that can include: a glass, quartz or other tube formed in a tubular fashion, an inner surface thereof forming a phosphor layer, and both ends thereof providing respective filament electrodes so as to be located opposite to each other and so as to be fixed between both ends of the tube and the respective glass beads provided at the respective pairs of lead wires in their respective air proof state; and a filler gas can be located in the tube.
According to the above described exemplary fluorescent lamp, because the pair of lead wires is not heated to an extreme degree as describe above, the one end of the pair of lead wire can be located near the end of the tube. Thus, the fluorescent lamp can be configured to decrease the portions of the end areas at which light is not emitted and can be configured to emit a light with a wide area.
These and other characteristics and features of the disclosed subject matter will become clear from the following description with reference to the accompanying drawings, wherein:
FIGS. 7(A)-(C) are a schematic perspective view for a description of misalignment in a sideward direction of two connecting parts of a filament coil to a pair of connecting pipes in the filament electrode shown in
FIGS. 8(A)-(B) are schematic perspective views showing a conventional electrode structure, wherein
Exemplary embodiments of the disclosed subject matter will now be described in detail with reference to
The pair of lead wires 11, 12 can be composed of a conductive metallic material and can be located parallel with respect to each other. The filament coil 13 can be composed of, for instance, a tungsten (W), a rhenium tungsten (W—Re), a doped tungsten and the like.
The above filament coil 13 can include a coil body 13a formed in a double helical and two connecting parts 13b, 13c extending from both ends of the coil body 13a in a direction parallel with a central axis thereof (downwards in
The above-described pair of connecting pipes 14, 15 can be composed of a conductive metallic material and can be formed in a hollow tubular configuration. The pair of connecting pipes 14, 15 can be composed of a metallic material for which the coefficient of thermal conductivity is smaller than that of the pair of lead wires 11, 12, such as a nickel and an iron metal, for which the coefficient of thermal conductivity is less than 115 W/m·K.
The pair of connecting pipes 14, 15 can be configured as and function as a getter. When the pair of connecting pipes 14, 15 is composed of a material having a getter function or is formed with a material having a getter function coated on an inner surface or an outer surface of the pair of connecting pipes 14, 15, the getter function can be activated in the pair of connecting pipes 14, 15. The getter material can be coated via vapor deposition or other known coating or fixation method.
When the pair of connecting pipes 14, 15 includes a getter function, the pair of connecting pipes 14, 15 can be composed of, for example, a material of titanium series and a material of zirconium series. When a surface of the pair of connecting pipes 14, 15 is formed of a comparatively low conductive material having a getter function, the material can form an outer surface of the pair of pipes 14, 15.
A description of the specific electrode structure for the filament electrode 10 will now be given. Each first end 14a, 15a of the pair of connecting pipes 14, 15 can be telescoped onto an end of the pair of lead wires 11, 12 located therein as shown in
Each opposite end 14b, 15b of the pair of connecting pipes 14, 15 can be telescoped onto two connecting parts 13b, 13c of the filament coil 13 as shown in
In the above-described two attachment configurations for the pair of connecting pipes 14, 15, pair of lead wires 11, 12, and two connecting parts 13b, 13c of the filament coil 13, either of the ends can be the first to be attached and/or both of the ends can be attached at the same time. However, when each end of the pair of lead wires 11, 12 is attached to each first end 14a, 15a of the pair of connecting pipes 14, 15 with a weld, for example, after fixing with the weld, the filament coil 13 can be attached to the pair of connecting pipes 14, 15 via pressure bonding. The reason why the weld is carried out first because it can absolutely eliminate an effect of transmitting heat to the filament coil 13 during the weld process.
The filament electrode 10 in accordance with an exemplary embodiment of the disclosed subject matter can be constituted as described above. A manufacturing process for the filament electrode 10 can include: providing the pair of connecting pipes 14, 15 with each first end 14a, 15a telescoped over respective ends of the pair of lead wires 11, 12; attaching each end of the pair of lead wires 11, 12 to respective first ends 14a, 15a of the pair of connecting pipes 14, 15 with a weld or via pressure bonding; attaching each of the opposite ends 14b, 15b of the pair of connecting pipes 14, 15 by telescoping them over each end of two connecting parts 13b, 13c of the filament coil 13; and attaching each end of the two connecting parts 13b, 13c of the filament coil 13 to respective opposite ends 14b, 15b of the pair of connecting pipes 14, 15 via pressure bonding.
In this case, each end of the two connecting parts 13b, 13c of the filament coil 13 can be configured to telescope into respective opposite ends 14b, 15b of the pair of connecting pipes 14, 15 while also not contacting respective ends of the pair of lead wires 11, 12 which telescope into respective first ends 14a, 15a of the pair of connecting pipes 14, 15. This is accomplished by allowing each end of the two connecting parts 13b, 13c of the filament coil 13 to telescope within the opposite ends 14b, 15b of the connecting pipes 14, 15 so as to maintain a predetermined interval between each end of the two connecting parts 13b, 13c and each end of the pair of lead wires 11, 12 in each of the pair of connecting pipes 14, 15. Thus, the filament coil 13 and the pair of lead wires 11, 12 can be fixed with respect to each other at a predetermined interval via the pair of connecting pipes 14, 15 in the filament electrode 10.
In the above-described structure, because the filament coil 13 can be attached in each of the opposite ends 14b, 15b of the pair of connecting pipes 14, 15 via pressure bonding, recrystallization of a material such as tungsten and the like composing the filament coil 13 cannot create a weld-like structure. Thus, because the fixing intensity in the filament electrode 10 does not become weak, the filament coil 13 should not become detached from the ends of the pair of lead wires 11, 12 and, therefore, reliability of the filament electrode 10 can increase.
Furthermore, because each end of the two connecting parts 13b, 13c of the filament coil 13 can be attached to respective ends of the pair of lead wires 11, 12 via the pair of connecting pipes 14, 15, the filament electrode 10 can extend in a direction parallel with a longitudinal axis of the tube. Thus, even if a diameter of the tube is thin, the filament electrode 10 can be easily installed in the thin tube.
The fluorescent lamp 16 can include: a tube 17 configured in a tubular shape from glass, quartz, or the like, an inner surface of the tube 17 can include a phosphor layer, and both ends 17a of the tube 17 can include respective filament electrodes 10 so as to be located opposite to each other and so as to be fixed between both ends 17a of the glass tube 17 and the respective glass beads 18 provided on the respective pairs of lead wires 11, 12 in their respective air proof states. A filler gas can be located in the tube 17.
When a power supply is provided between respective ends of the pairs of lead wires 11, 12, the respective filament coils 13 can be heated and can operate as respective heaters. Thus, because the fluorescent lamp can generate a discharge in the tube 17 with a discharge voltage between each of the filament electrodes 10 attached to both ends 17a of the tube 17, the fluorescent lamp 16 can emit light.
In this case, when the pair of connecting pipes 14, 15 is composed of a material having a smaller coefficient of thermal conductivity than that of the pair of lead wires 11, 12, it is difficult to transmit heat generated from the filament coil 13 during light-emission of the fluorescent lamp 16 to the pair of lead wires 11, 12 via the pair of connecting pipes 14, 15. Thus, in the sealing portions of both ends 17a of the tube 17 and the respective beads 18 (and between the respective pairs of lead wires 11, 12 and the respective glass beads 18) the filler gas in the tube 17 can be prevented from leaking out due to a gap caused by differences of CTE between the ends 17a of the tube 17 and the respective beads 18, and/or based on differences of CTE between the respective pairs of lead wires 11, 12 and the respective beads 18.
In addition, because the pair of lead wires 11, 12 are not extremely heated, each end of the respective pairs of lead wires 11, 12 can be located near respective ends 17a of the tube 17. Thus, when manufacturing a fluorescent lamp using other conventional types of filament electrodes in a tube as long as the tube 17, the above-described fluorescent lamp using the filament electrode 10 can emit brighter light than the other conventional fluorescent lamp.
Furthermore, because the filament coil 13 can be coated with an emissive material, the emissive material can emit an electron in the tube 17 by heating the filament coil 13 and the discharge in the tube 17 can be accelerated. In addition, because the pair of connecting pipes 14, can be configured to function as a getter, the pair of connecting pipes 14, 15 can absorb gas molecules such as impure substances and the like located in the tube 17. Therefore, the fluorescent lamp 16 can improve its discharging state, its sputter and the like in the tube 17.
A second exemplary embodiment of the disclosed subject matter will now be given with reference to FIGS. 5(A)-(B). Relevant parts of the filament electrode 20 of the second exemplary embodiment are shown in FIGS. 5(A)-(B), wherein the same or similar elements shown in
According to the second exemplary embodiment, when each of the two connecting parts 13b, 13c of the filament coil 13 telescopes into each of the opposite ends 14b, 15b of the pair of connecting parts 14, 15, the pair of squeezing parts 14c, 15c can operate as stoppers of the two connecting parts 13b, 13c of the filament coil 13. In addition, when each end of the pair of lead wires 11, 12 telescopes into each first end 14a, 15a of the pair of connecting parts 14, 15, the pair of squeezing parts 14c, 15c can operate as stoppers of the lead wires 11. 12 with respect to the pair of connecting parts 14, 15. Thus, contact between each of the two connecting parts 13b, 13c of the filament coil 13 with each end of the pair of lead wires 11, 12 located in the pair of connecting parts 14, 15 can be avoided without exception.
In addition, because it can become harder for heat generated from the filament coil 13 during light-emission of the fluorescent lamp 16 to be transmitted via connecting pipes 14, 15 to the pair of lead wires 11, 12, each of the ends of the pair of lead wires 11, 12 can be located nearer respective ends 17a of the tube 17. Thus, those end areas in which light is not emitted in the tube 17 can be made smaller and the fluorescent lamp can thus emit light with a wider range.
A third exemplary embodiment of the disclosed subject matter will now be described with reference to
According to the third exemplary embodiment, when the diameter of each of the apertures of the opposite ends 31b, 32b corresponds with a respective diameter of the two connecting parts 13b, 13c of the filament coil 13, the filament coil 13 can be exactly attached to the pair of lead wires 11, 12 so that each of the two connecting parts 13b, 13c thereof aligns with each of the pair of connecting pipes 31, 32. Therefore, a problem in that each of the two connecting parts 13b, 13c of the filament coil 13 is misaligned with each of the pair of connecting pipes 14, 15 by an amount “d” as shown in
Thus, the disclosed subject matter can provide a filament electrode that can connect a filament coil with a pair of lead wires with confidence and strength and with minimal or no leakage at the sealing portions, which can be the result and benefits of an effective heat-shield operation. The filament electrode can also be employed in a thin inner diameter tube. Furthermore, the disclosed subject matter can provide a fluorescent lamp using a filament electrode that can decrease both end areas in which light is not typically able to be emitted such that light can be emitted with a wider range.
In the above-described exemplary embodiments, the pair of connecting pipes 14, 15 can include materials or be configured of materials that provide a getter function. However, it is possible to provide separate or other structures that function as a getter. In addition, the connecting pipes 14, 15 are shown as cylindrical with a circular cross-section. However, this shape can be varies greatly and remain within the spirit and scope of the disclosed subject matter. For example, the pipes 14, 15 can be configured to have a polygonal cross-section, non-symmetrical cross-section, oval cross-section or other cross section. In addition, the shape of the pipes 14, 15 can change along the longitudinal axis of the pipes 14, 15. In particular, the wall thickness and shape can vary at different locations along the pipes 14, 15 to facilitate pressure bonding and the like. The filament coil 13 can be formed in a double helical shape. However, it is contemplated that the shape of the filament coil 13 can be formed in various other shapes and configurations without limitation. In addition, the electrodes 10, 20 and 30 of the exemplary embodiment can be configured for use in a fluorescent lamp. However, these electrodes can also be configured for use in other types of bulbs and the like without departing from the spirit and scope of the presently disclosed subject matter.
While there has been described what are at present considered to be exemplary embodiments of the invention, it will be understood that various modifications may be made thereto, and it is intended that the appended claims cover such modifications as fall within the true spirit and scope of the invention. All conventional art references described above are herein incorporated in their entirety by reference.
Number | Date | Country | Kind |
---|---|---|---|
2006-353194 | Dec 2006 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
3733508 | Rainone et al. | May 1973 | A |
4370589 | DeCaro et al. | Jan 1983 | A |
5057735 | Zalar et al. | Oct 1991 | A |
20070228913 | Horikoshi et al. | Oct 2007 | A1 |
Number | Date | Country |
---|---|---|
03098254 | Apr 1991 | JP |
4245161 | Sep 1992 | JP |
11297272 | Oct 1999 | JP |
2005183267 | Jul 2005 | JP |
2005235749 | Sep 2005 | JP |
Number | Date | Country | |
---|---|---|---|
20080157676 A1 | Jul 2008 | US |