Claims
- 1. A method of manufacturing a filling material, comprising the steps of:
obtaining down; washing the down in accordance with a predetermined washing process to produce prepared down; obtaing Lyocell fiber; blending the prepared down with the obtained Lyocell fiber in accordance with a predetermined blending process to produce the filling material.
- 2. The method of claim 1, wherein the blending step is carried out by blending the prepared down 70% by weight with 30% by weight Lyocell fiber.
- 3. The method of claim 1, wherein the washing step is carried out by the sub-steps of:
(a) washing the down with hot soapy water; (b) rinsing the down with hot water; (c) rinsing the down with cold water; (d) drying the rinsed down; and (e) dedusting and cooling the dried down.
- 4. The method of claim 3, wherein the drying sub-step is carried out by drying 40 pounds of washed down for substantially 20 minutes at a temperature of substantially 220 degrees Fahrenheit
- 5. The method of claim 3, wherein the dedusting and cooling sub-step further includes injecting ozone into the down.
- 6. The method of claim 3, wherein the dedusting and cooling sub-step is carried out utilizing a screened centrifuge.
- 7. The method of claim 3, wherein each of the washing and two rinsing sub-steps further includes applying the down to a centrifuge cycle.
- 8. The method of claim 1, wherein the blending step is carried out by the sub-steps of:
(a) washing the down with hot soapy water; (b) rinsing the down with hot water; (c) adding the Lyocell fiber to the washed and rinsed down to produce a mixture; (d) rinsing the mixture with cold water; (e) drying the rinsed mixture; and (f) dedusting and cooling the dried mixture.
- 9. The method of claim 8, wherein the rinsing the mixture sub-step includes applying the rinsed mixture to a centrifuge cycle, and repeating the rinsing and centrifuge cycles multiple times.
- 10. The method of claim 8, wherein the adding sub-step is carried out by adding 30% by weight Lyocell fiber to the washed and rinsed down.
- 11. The method of claim 8, wherein the drying sub-step is carried out by drying substantially 40 pounds of the rinsed mixture for substantially 20 minutes at a temperature of substantially 200 degrees Fahrenheit.
- 12. The method of claim 8, wherein the dedusting and cooling sub-step includes injecting of ozone into the dried mixture.
- 13. The method of claim 1, wherein the blending step is carried out by a dry process.
- 14. The method of claim 1, further comprising the step of filling a pillow with the produced filling material.
- 15. The method of claim 1, further comprising the step of filling a comforter with the produced filling material.
- 16. A filling material, comprising:
down; and Lyocell fiber blended with the down.
- 17. The filling material of claim 16, wherein the filling material includes 70% by weight of the down and 30% by weight of the Lyocell fiber.
- 18. The filling material of claim 16, wherein the down includes a minimum of 75% new down cluster.
- 19. A pillow, comprising:
a blend of down and Lyocell fiber; and a pillow filled with the blend of down and Lyocell fiber.
- 20. A comforter, comprising:
a blend of down and Lyocell fiber; and a comforter filled with the blend of down and Lyocell fiber.
RELATED APPLICATION
[0001] This application claims the benefit of U.S. Provisional Application Ser. No. 60/440,596, filed Jan. 16, 2003.
Provisional Applications (1)
|
Number |
Date |
Country |
|
60440596 |
Jan 2003 |
US |