The present invention relates to a touch panel, and in particular, to an embedded capacitive touch panel.
A current market has a large demand for touch panels. In the technologies of the touch panels, because a capacitive touch panel has advantages such as high reliability and a high reaction speed, the technology of the capacitive touch panel becomes the main development technology. A structure of the capacitive touch panel usually includes a liquid crystal display module (LCM) at a lower layer, a cover lens as a protection layer at an upper layer, and a transparent conductive layer sandwiched between a liquid crystal panel and the cover lens. According to a composition manner between the liquid crystal panel, the cover lens, and the transparent conductive layer, the capacitive touch panel is classified into an out-cell capacitive touch panel and an embedded capacitive touch panel. In the out-cell capacitive touch panel, a sensing electrode is made on a substrate, and the substrate having the sensing electrode is attached to an outer surface of a display. Therefore, the out-cell capacitive touch panel increases a total thickness of the touch panel, which is unfavorable for the display to be thin and light. On the contrary, the embedded capacitive touch panel is combined with a display panel during manufacturing of the display panel, and the entire system is relatively thin and light. In addition, the cover lens only needs to be removed and changed when broken by an external force, and not any other component of the touch panel, for example, a transparent electrode, needs to be made again. Therefore, in comparison with the out-cell capacitive touch panel, the embedded capacitive touch panel has relatively low maintenance costs. In general, most touch panel technologies pursue thinning and lightness of touch panels. However, when it comes to a commercial display apparatus (for example, an automated teller machine) provided in a public occasion, it further needs to be considered whether the touch panel can withstand a relatively large external force in the long term. Therefore, currently, a good touch panel that can withstand an external force still needs to be developed, so that the product is more competitive.
The present invention relates to an embedded capacitive touch panel that uses thick glass (for example, glass having a thickness of more than 3 mm) as a cover lens. An area of each of first electrodes and an area of each of second electrodes in the touch panel have a ratio relationship. Because the thick cover lens in the disclosure can protect the touch panel, when an external force is applied to the touch panel, it is relatively not easy for the touch panel to be broken. In addition, because the area of each of the first electrodes and the area of each of the second electrodes in the touch panel (for example, a ratio of the area of each of the first electrodes to the area of each of the second electrodes ranges from 0.37 to 0.41) have a ratio relationship, a relatively large induction signal can be obtained according to the ratio relationship, and a problem that an induction signal is insufficient due to use of the thick glass can be solved. Therefore, the touch panel in the disclosure can withstand a relatively large external force and an inductive effect is also excellent.
According to an aspect of the disclosure, a touch panel is provided. The touch panel comprises a substrate, a plurality of first electrode in a first series, and a plurality of second electrode in a second series. The substrate has a first surface. The first electrode series are disposed on the first surface. Each of the first electrode series extends along a first direction and comprises a plurality of first electrodes. The second electrode series are disposed on the first surface. Each of the second electrode series extends along a second direction and comprises a plurality of second electrodes. In a unit area of the touch panel, a relationship between an area of each of the second electrodes and an area of each of the first electrodes satisfies Formula 1 and Formula 2:
A2=R×A1 Formula 1; and
0.37<R<0.41 Formula 2, wherein
A1 indicates the area of each of the first electrodes in the unit area, A2 indicates the area of each of the second electrodes in the unit area, and R indicates a ratio of A2 to A1.
For a better understanding of the foregoing and other aspects of the present invention, embodiments are provided below with reference to the accompanying drawings to give detailed descriptions.
The present invention relates to an embedded capacitive touch panel that uses thick glass (for example, glass having a thickness of 3 to 5 mm) as a cover lens. When the touch panel is applied to a commercial display apparatus, even if an external force is applied to the touch panel for a long time, it is still relatively not easy for the touch panel to be broken. Therefore, the maintenance costs required due to destruction by an external force can be reduced. In addition, shapes of first electrodes and second electrodes and an area ratio of each of the first electrodes to each of the second electrodes in the touch panel in the disclosure are specially designed, so that the touch panel using thick glass can still have a good inductive effect.
Referring to
Referring to
In this embodiment, the substrate 110 may be an LCM. The first electrodes 142 and the second electrodes 144 may be formed by a same material, for example, indium tin oxides (ITO), indium zinc oxide (IZO), or another transparent conductive material. Because the gap between each of the first electrodes 142 and each of the second electrodes 144 may cause a problem of visibility of electrode patterns caused by a refractive index difference (a refractive index difference caused by a transparent conductive material and air), each of the imaginary-part electrodes 146 is disposed between each of the first electrodes 142 and each of the second electrodes 144. Therefore, visibility of each of the first electrodes 142 and each of the second electrodes 144 is reduced. The imaginary-part electrodes 146 may be made of a material having a same refractive index as that of the first electrodes 142 and the second electrodes 144. In an embodiment, the material of the imaginary-part electrodes 146 may alternatively be the same as a material of the first electrodes 142 and the second electrodes 144, and the imaginary-part electrodes 146, the first electrodes 142, and the second electrodes 144 may be made in a same process, thereby reducing the costs.
In an embodiment, a material of the first bridge patterns 142b may be different from a material of the second bridge patterns 120. For example, the material of the first bridge patterns 142b may be a transparent conductive material that is the same as that of the first electrodes 142, and the first bridge patterns 142b and the first electrodes 142 may be an integrally molded structure formed by using a same process. The second bridge patterns 120 may be formed by a metal, for example, a metal layer formed by Ti/Al/Ti or Mo/Al/Mo. In comparison with a comparative example in which the second bridge patterns are formed by using a transparent conductive material, the second bridge patterns 120 in the disclosure may be formed by a metal.
In this embodiment, first metal meshes 152 and second metal meshes 154 may respectively cover the first electrodes 142 and the second electrodes 144. That is, the first metal meshes 152 and the second metal meshes 154 may be respectively electrically connected to the first electrodes 142 and the second electrodes 144. A cover lens 160 may cover the first metal meshes 152, the second metal meshes 154, the first electrodes 142, the second electrodes 144, and the imaginary-part electrodes 146. An air gap may exist between the cover lens 160, the first electrodes 142, and the second electrodes 144. In comparison with a comparative example in which the first electrodes and the second electrodes do not have the first metal meshes and the second metal meshes, because the first metal meshes 152 and the second metal meshes 154 in this embodiment respectively cover the first electrodes 142 and the second electrodes 144, resistance values of the first electrodes 142 and the second electrodes 144 decrease, which facilitates electrical conduction, may reduce the signal transmission time (RC loading), and may reduce visibility of the metal second bridge patterns.
Referring to
A2=R×A1 Formula 1; and
0.37<R<0.41 Formula 2, where
A1 indicates the area of each of the first electrodes in the unit area, A2 indicates the area of each of the second electrodes in the unit area, and R indicates a ratio of A2 to A1. The unit area corresponds to an area range touched by a user with a finger, for example, a unit area of a rectangle formed by sides each having a length of 5 to 7 mm.
In
Referring to
Referring to
In addition, the first mesh angle α1 and the second mesh angle α2 both are different from the imaginary-part electrode angles (for example, the imaginary-part electrode angles θ1, θ2, θ3 and θ4). In comparison with a comparative example in which shapes of the imaginary-part electrodes do not form a plurality of different angles and the imaginary-part electrode angles are the same as the metal mesh angles, because the imaginary-part electrodes 146 in this embodiment have three or more imaginary-part electrode angles that are different from each other, and the first mesh angle α1 and the second mesh angle α2 are different from the imaginary-part electrode angles (for example, the imaginary-part electrode angles θ1, θ2, θ3 and θ4), the visual effect can be improved. Therefore, human eyes are less likely to notice an edge of electrode patterns, and visibility of each of the metal second bridge patterns 120 can also be reduced.
In addition, the density of the first metal meshes 152 on the first electrodes 142 may be different from the density of the second metal meshes 154 on the second electrodes 144. In this embodiment, the density of the first metal meshes 152 on the first electrodes 142 may be greater than the density of the second metal meshes 154 on the second electrodes 144. A ratio of the density of the first metal meshes 152 on the first electrodes 142 to the density of the second metal meshes 154 on the second electrodes 144 is greater than 1 and less than 3.
Referring to Table 1 (as shown below), Table 1 shows that the number of points falling within a visible area of moiré in a first comparative example (the ratio of the density of the first metal meshes on the first electrodes to the density of the second metal meshes on the second electrodes is 1), a first experimental example (the ratio of the density of the first metal meshes 152 on the first electrodes 142 to the density of the second metal meshes 154 on the second electrodes 144 is 2), and a second comparative example (the ratio of the density of the first metal meshes on the first electrodes to the density of the second metal meshes on the second electrodes is 3) is measured by using an invisible curve of the moiré effect as a judgment criterion. A larger number of the points in the visible area of moiré indicates a more apparent interference stripe and a stronger moiré effect.
In comparison with the first comparative example and the second comparative example, the smaller number of the points falling within the visible area of moiré in the first experimental example indicates a relatively less apparent interference stripe. If a density difference of the metal meshes is excessively large, an interference effect may be affected again, and the visual effect is degraded. It can be learned that because the ratio of the density of the first metal meshes 152 on the first electrodes 142 to the density of the second metal meshes 154 on the second electrodes 144 in the disclosure is greater than 1 and less than 3, the interference phenomenon can be relieved, the moiré effect can be reduced, and a good visual effect can be achieved.
According to the foregoing descriptions, an embodiment of the disclosure provides a touch panel. In a unit area of the touch panel, the ratio of the area of each of the second electrodes to the area of each of the first electrodes is greater than 0.37 and less than 0.41. In comparison with a comparative example in which the area of each of the second electrodes is the same as the area of each of the first electrodes, the area ratio of each of the first electrodes to each of the second electrodes in the disclosure is specially designed. Even if thick glass (for example, glass having a thickness greater than 3 mm) is used as the cover lens, the touch panel can still have a high induction signal and a relatively low noise value, and have a good touch sensing quality. In addition, the second electrodes in the disclosure are connected by the metal second bridge patterns, and have a relatively high capability of withstanding high pressure in comparison with the comparative example of the second bridge patterns made of a transparent conductive material. Moreover, the first metal meshes and the second metal meshes that have different densities respectively cover the first electrodes and the second electrodes, each of the imaginary-part electrodes having the three or more angles is disposed between each of the first electrodes and each of the second electrodes, and the imaginary-part electrode angles are different from the angles of the first metal meshes and the second metal meshes. In this way, the RC loading can be reduced, visibility of the metal second bridge patterns and electrode patterns can also be reduced, and the moiré effect can be reduced. Therefore, the touch panel in the disclosure can withstand a relatively large external force and an inductive effect is also excellent, and a visual effect is not affected.
Based on the above, although the present invention has been disclosed by using the embodiments, the embodiments are not intended to limit the present invention. A person of ordinary skill in the art of the present invention may make various modifications and variations to the present invention without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention should be defined by the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
106144111 A | Dec 2017 | TW | national |
Number | Name | Date | Kind |
---|---|---|---|
8519967 | Chien et al. | Aug 2013 | B2 |
9489914 | Ha | Nov 2016 | B2 |
10296153 | Nakase | May 2019 | B2 |
10310688 | Xie | Jun 2019 | B2 |
20050036091 | Song | Feb 2005 | A1 |
20140085261 | Lu | Mar 2014 | A1 |
20140293163 | Ju | Oct 2014 | A1 |
20170108975 | Zhang | Apr 2017 | A1 |
20170344141 | Lee | Nov 2017 | A1 |
20180275801 | Nakayama | Sep 2018 | A1 |
20190004657 | Koudo | Jan 2019 | A1 |
20190008041 | Nakamura | Jan 2019 | A1 |
20190012011 | Wang | Jan 2019 | A1 |
20190034010 | Lee | Jan 2019 | A1 |
20190051711 | Lee | Feb 2019 | A1 |
20190064964 | Choi | Feb 2019 | A1 |
Number | Date | Country |
---|---|---|
104111759 | Oct 2014 | CN |
106249963 | Dec 2016 | CN |
M523908 | Jun 2016 | TW |
Entry |
---|
Taiwan Intellectual Property Office, “Office Action”, dated Feb. 5, 2018. |
Number | Date | Country | |
---|---|---|---|
20190187825 A1 | Jun 2019 | US |