Claims
- 1. A flame retardant comprising phosphorus-containing condensation products of an organophosphorus compound represented by Formula I, ##STR10## wherein X, Y and Z each is hydrogen or halogen, R.sub.1 and R.sub.2 each is hydrogen or methyl and R.sub.3 is hydrogen or an alkyl group with a polyhydric alcohol having at least three alcoholic hydroxyl groups selected from the class consisting of glycerine, polyglycerines, trimethylol ethane, trimethylol propane, pentaerythritol, dipentaerythritol, tripentaerythritol, tetrapentaerythritol, mannite and sorbite, where said condensation products have a phosphorus content of 6.0 to 10.7% by weight and a softening point of 55.degree.-155.degree. C.
- 2. A flame retardant phosphorus-containing condensation product wherein said condensation product is obtained by an addition reaction between acrylic, methacrylic or crotonic acid esters of a polyhydric alcohol having at least three alcoholic hydroxyl groups selected from the class consisting of glycerine, polyglycerines, trimethylol ethane, trimethylol propane, pentaerythritol, dipentaerythritol, tripentaerythritol, tetrapentaerythritol, mannite and sorbite, and an organophosphorus compound of Formula II, ##STR11## wherein X, Y and Z each is hydrogen or halogen.
- 3. The flame retardant of claim 1 wherein said condensation products are a reaction product in a ratio of 35-130 of the Formula I compound relative to 100 of number of hydroxyl groups in the polyhydric alcohol.
- 4. A flame retardant resin composition comprising 100 parts by weight of a thermoplastic resin and 3 to 50 parts by weight of phosphorus-containing condensation products of an organophosphorus compound represented by Formula I, ##STR12## wherein X, Y and Z each is hydrogen or halogen, R.sub.1 and R.sub.2 each is hydrogen or methyl and R.sub.3 is hydrogen or an alkyl group with a polyhydric alcohol having at least three alcoholic hydroxyl groups, where said condensation products have a phosphorus content of 6.0 to 10.7% by weight and a softening point of 55.degree.-155.degree. C.
- 5. The flame retardant resin composition of claim 4 wherein said thermoplastic resin is selected from the group consisting of polystyrene, acrylonitrile-styrene resins, acrylonitrile-butadiene-styrene resins, polyvinyl chloride, polyterephthalate resins, polycarbonate resins, polyphenylene oxide resins and polyamide resins.
- 6. A flame retardant resin composition comprising 100 parts by weight of a thermosetting resin and 3 to 50 parts by weight of phosphorus-containing condensation products of an organophosphorus compound represented by Formula I, ##STR13## wherein X, Y and Z each is hydrogen or halogen, R.sub.1 and R.sub.2 each is hydrogen or methyl and R.sub.3 is hydrogen or an alkyl group with a polyhydric alcohol having at least three alcoholic hydroxyl groups, where said condensation products have a phosphorus content of 6.0 to 10.7% by weight and a softening point of 55.degree.-155.degree. C.
Priority Claims (1)
Number |
Date |
Country |
Kind |
53-61047 |
May 1978 |
JPX |
|
CROSS REFERENCE TO RELATED APPLICATIONS
This application is a continuation-in-part of our copending application Ser. No. 039,769, now abandoned, filed May 17, 1979 for "Flame Retardants."
US Referenced Citations (11)
Foreign Referenced Citations (3)
Number |
Date |
Country |
2034887 |
Oct 1975 |
DEX |
50-17979 |
Jun 1975 |
JPX |
1256180 |
Dec 1971 |
GBX |
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
39769 |
May 1979 |
|