The present invention relates to a flat panel display, particularly to a flat panel display package method.
Compared with the traditional CRT (Cathode Ray Tube), FPD (Flat Panel Display), such as LCD (Liquid Crystal Display) and OLED (Organic Light Emitting Diode) displays, has the advantages of lightweight and high brightness and has been widely accepted by users. Among them, EPD (ElectroPhoretic Display) is an outstanding one and features flexibility, bistability, self-luminescence and power efficiency. At present, EPD has been applied to electronic tags, electronic signboards, smart cards, e-books, and time display devices. However, EPD is very sensitive to humidity. Once humidity permeates EPD, the electrodes cannot normally drive the ink particles thereinside, which will decrease the mobility and degrade the picture quality. In such a case, the stability and lifetime of EPD is unlikely to satisfy the requirements of the market, and the popularization of EPD should be handicapped. The traditional solution to the humidity damage on EPD is applying a water-proof film onto the surface of EPD. However, humidity permeation is omnidirectional. Thus, humidity can still permeate EPD from the lateral and back sides. Therefore, the traditional solution cannot effectively protect EPD from humidity damage.
The primary objective of the present invention is to completely prevent external humidity from permeating a flat panel display. To achieve the abovementioned objective, the present invention proposes a flat panel display package method comprising steps:
The flat panel display may be an EPD (ElectroPhoretic Display). The first package film covering the flat panel display needs a light transmittance of over 70% to present the pictures of the flat panel display. Each of the first and second package films is a multi-layer film containing a metal layer. The metal layer of the second package film contains aluminum or copper, or the metal layer of the second package film is a stainless-steel layer. A first joiner adhesive is disposed between the first package film and the flat panel display, and a second joiner adhesive is disposed between the second package film and the electronic baseplate, whereby the first package film and the second package film are respectively firmly stuck onto the flat panel display and the electronic baseplate.
In step (b), the first and second join regions have a width of at least 1 mm to attain a better bonding. In step (c), the hot-pressing temperature is between 75 and 95° C., and the hot-pressing pressure is between 0.8 and 1.2 kg/cm2, and the time for hot-pressing is between 7 and 13 seconds. The hot-pressing machine can be a roller-type or bar-type hot-pressing machine.
Via the flat panel display package method of the present invention, the first and second package films are airtightly sealed by hot pressing the first and second join regions. Thus, external humidity is impossible to enter the space formed by the first and second package films. Thereby, the flat panel display and the electronic baseplate are protected.
Below are described in detailed the technical contents of the preset invention in cooperation with the drawings.
Refer to
The flat panel display may be an EPD (ElectroPhoretic display). The first package film covering the flat panel display needs a light transmittance of over 70% to present the pictures of the flat panel display. A first joiner adhesive is disposed between the first package film and the flat panel display, and a second joiner adhesive is disposed between the second package film and the electronic baseplate, whereby the first package film and the second package film are respectively firmly stuck onto the flat panel display and the electronic baseplate.
In this preferred embodiment, each of the first and second package films is a multi-layer film containing a soft plastic layer, a metal layer, etc. The soft plastic layer is made of PE (polyethylene), PA (polyamide), PET (polyethylene terephthalate), PU (polyurethane), PVA (polyvinyl alcohol), or polyester. The metal layer contains aluminum or copper, or the metal layer is a stainless-steel layer.
Refer to
As shown in
In conclusion, the first package film and the second package film respectively cover the flat panel display and the electronic baseplate, whereby external humidity cannot enter the display module from the front side and back side of the display module. Further, the first and second join regions along the circumference of the display module are sealed airtightly with a hot-pressing method, whereby external humidity cannot enter the display module from the lateral sides. Thus, the flat panel display and electronic baseplate packaged inside the first and second package films are fully protected from the damage of external humidity.
From the abovementioned description, it is known that the present invention indeed possesses novelty and non-obviousness and meets the conditions for a patent. Thus, the Inventor files the application for a patent. It will be appreciated if the patent is approved fast.
The embodiments described above are only to exemplify the present invention but not to limit the scope of the present invention. Therefore, any equivalent modification or variation according to the spirit of the present invention is to be also included within the scope of the present invention.