Claims
- 1. A method for cleaning coal comprising
- (a) submerging coal containing ash and pyrite in liquid sulfur dioxide for a time sufficient for a discrete float-sink separation to occur, and
- (b) recovering the float portion, a coal product reduced in ash and pyrite.
- 2. The method of claim 1 wherein the specific gravity of the liquid sulfur dioxide is adjusted by the addition of a quantity of an inert material to effect an improved float-sink separation of coal from ash and pyrite.
- 3. The method of claim 1 wherein coal is submerged for a period of from ten minutes to ten hours.
Parent Case Info
This is a continuation, division, of application Ser. No. 786,912, filed Apr. 12, 1977.
US Referenced Citations (5)
Divisions (1)
|
Number |
Date |
Country |
Parent |
786912 |
Apr 1977 |
|