1. Field of the Invention
The present invention relates to a forging die apparatus for processing a forging material arranged in a cavity formed by a die member so that the forging material is subjected to forging in accordance with a pressurizing action of a punch.
2. Description of the Related Art
A die apparatus has been hitherto known, in which a forging material is inserted into a cavity formed by an upper die and a lower die which are joined to one another, and a pressurizing force is applied to the forging material by the aid of a punch so that the forging material is forged to have a predetermined shape.
A cold forging die suggested by the present applicant is shown in
The cold forging die 1 comprises a lower die 3 and an upper die 4 which are joined to one another by the aid of a clamping means 2 and which are installed on a die holder 5. A cavity 7, which is charged with a forging material 6, is formed by the lower die 3 and the upper die 4. A punch 8 is provided to pressurize the forging material 6 charged in the cavity 7.
A general forging die apparatus including the cold forging die 1 is usually designed, as shown in
In this case, if the clearance A is small, the following inconvenience arises. That is, the punch 8 generates heat as the number of shots is increased. As a result, scuffing occurs on an outer circumferential surface of the punch 8 and on an inner wall surface of the hole 9 of the upper die 4 respectively.
Since the clearance A is provided, the upper die 4 and the lower die 3 are assembled in a state of involving any centering deviation within a range of the clearance A. Further, if any unbalanced load is applied in the lateral direction to the punch 8 during the forging, the pressurizing force is applied to the forging material 6 in a state in which the punch 8 is deviated in the lateral direction within the range of the clearance A.
As described above, the clearance A causes the centering deviation between the punch 8 and the cavity 7 which is formed by the upper and lower dies 4, 3. For example, when an outer cup for constructing a constant velocity universal joint is formed by forging, an inconvenience arises in that the axis of a cup of the outer cup is not coincident with the axis of a shaft thereof, i.e., the centering deviation occurs.
In the case of the cold forging die 1 described above, a clearance (not shown) is formed during the forming process at a joining surface (dividing surface) 10 (see
An unillustrated clearance for assembling is provided at a joined section 11 based on a step section between the upper die 4 and the lower die 3 (see
The present applicant has already suggested a method for cooling a die which makes it possible to greatly enhance the cooling effect and improve the service life of the die (life of the die) (see Japanese Laid-Open Patent Publication No. 61-255737).
That is, as shown in
A mechanical press 31 as shown in
A material 38 is arranged on a die member 37 on the upper surface of the bolster 32. A punch 39, which is fixed to the ram 36, performs reciprocating motion in the vertical direction integrally with the ram 36 to apply a pressurizing force to the material 38. Thus, the material 38 is forged to have a predetermined shape.
In the crank press, the rotary driving force of the motor is transmitted to the crank shaft 34, and the force is converted into the reciprocating motion of the ram 36 and the punch 39 by the aid of the connecting rod 35 connected to the crank shaft 34 to generate the forming load to be applied to the material 38.
When the forging is performed by using the well known mechanical press 31 as described above, any elongation occurs, for example, in the frames 33a, 33b, the connecting rod 35, and the ram 36 for constructing the mechanical press 31. For this reason, the bottom dead center of the punch 39 which makes the vertical reciprocating motion is varied. As a result, an inconvenience arises in that any dispersion occurs in the dimension of an obtained forged product in the thickness direction.
For example, when an outer cup for constructing a constant velocity universal joint is formed by forging by using the mechanical press 31, dispersion occurs in the bottom thickness dimension of a cup of the outer cup due to the influence of the elongation.
Therefore, the conventional technique involves an inconvenience that cutting processing should be applied after the forging in order to obtain a constant bottom thickness dimension of the cup of the outer cup.
If the forming load, which is applied to the material, hugely exceeds a preset value due to the influence of the elongation (if a overloaded forming load is applied), the mechanical press 31 is stopped in a locked state, resulting in an inconvenience that it is impossible to perform continuous forming.
Further, the conventional die apparatus generally adopts a method in which a forged product is taken out by the aid of a knockout pin 43 provided movably back and forth in a hole 42 of a lower die 41. As shown in
When an outer cup for constructing a constant velocity universal joint is produced by using such a die apparatus, it is necessary to form an unillustrated centering hole at a center of one end of a shaft of the outer cup in order to apply finishing processing such as polishing. In this procedure, the centering hole is formed by mechanical processing by using a cutting tool such as a drill (including a machining center).
In view of the function of the constant velocity universal joint, the centering hole serves as a reference, for example, when grinding processing is performed for a portion for which the coaxial accuracy is required. Therefore, a high coaxial accuracy is required between the center of the centering hole and the cup and the shaft for constructing the outer cup.
However, in the case of the die apparatus concerning the conventional technique, any backlash occurs in a direction perpendicular to the axis when the knockout pin 43 makes forward and backward movement, resulting from the clearance C between the knockout pin 48 and the hole 42 of the lower die 41. Therefore, even if a projection (not shown) for forming the centering hole is provided at one end of the knockout pin 48 for constructing the die apparatus concerning the conventional technique, an inconvenience arises in that it is impossible to correctly form the centering hole at the center of one end of the shaft of the outer cup formed by the forging. As a result, the die apparatus concerning the conventional technique involves the following inconvenience. That is, the center of the centering hole formed by the projection of the knockout pin 43 is not coincident with the axis of the outer cup due the backlash as described above. Therefore, it is necessary to apply lace processing based on the reference of the centering hole to the outer circumferential surface of the outer cup formed by the forging in order to allow the center of the centering hole to coincide with the axis of the outer cup.
In this case, if the clearance C is made zero in order to avoid the backlash of the knockout pin 43, the knockout pin 43 is fastened by the hole 42, making it impossible to perform forward and backward movement. On the other hand, if the clearance C is made narrow, another inconvenience arises in that it is difficult to perform forward and backward movement of the knockout pin 48 due to the action of sliding friction with respect to the hole 42.
A general object of the present invention is to provide a forging die apparatus which makes it possible to maintain a highly accurate coaxial degree of a forged product obtained by forging.
A principal object of the present invention is to provide a forging die apparatus which makes it possible to suppress occurrence of scuffing between a punch and a die.
Another object of the present invention is to provide a forging die apparatus which makes it possible to assemble an upper die and a lower die in an integrated manner so that the coaxial degree is maintained highly accurately between the upper die and the lower die.
Still another object of the present invention is to provide a forging die apparatus which makes it possible to avoid occurrence of burr at a joining surface between an upper die and a lower die.
Still another object of the present invention is to provide a forging die apparatus which makes it possible to improve durability of a main punch body and a sleeve member by suppressing thermal expansion of the main punch body in accordance with the cooling action for the main punch body, which would be otherwise caused due to heat generated during forging of a material to which a pressurizing force is applied.
Still another object of the present invention is to provide a forging die apparatus which makes it possible to avoid any overloaded forming load without requiring any cutting processing and maintain a highly accurate thickness accuracy of an obtained forged product.
Still another object of the present invention is to provide a forging die apparatus which makes it possible to form a centering hole simultaneously with forging for a forging material and allowing a center of the centering hole formed by the forging to correctly coincide with an axis of the forging material.
The above and other objects, features, and advantages of the present invention will become more apparent from the following description when taken in conjunction with the accompanying drawings in which a preferred embodiment of the present invention is shown by way of illustrative example.
With reference to
A thick-walled forcible insertion ring 120, which is formed in an integrated manner, is fixed on the second die holder 116 by the aid of a clamping means 122. An upper die 126 and a lower die 128 are integrally joined in a hole 119 of the forcible insertion ring 120 via a sleeve 124 which is formed to have a thin-walled cylindrical configuration.
As shown in
A tapered inclined surface 121, in which the diameter is gradually reduced toward the upper end edge, is formed at an upper portion of the inner circumferential surface of the sleeve 124. The inclined surface 121 exerts a pressing force directed downwardly in the assembled state, and thus it functions to increase the surface pressure at the contact surface between the upper die 126 and the lower die 128.
As shown in
As shown in
As shown in
As shown in
As shown in
The first ring member 134 is formed of, for example, a cemented carbide material, and it is in a state of being strongly tightened toward the center by the second ring member 136 which has been subjected to the shrinkage fitting treatment. The first ring member 134 and the second ring member 136 are tightened by a tapered section 141 of a clamping ring 140 which is screwed into a screw hole 139 of the forcible insertion ring 120. Thus, the first ring member 134 and the second ring member 136 are joined to the upper die 126, the lower die 128, and the sleeve 124 in an integrated manner.
In this embodiment, a cavity 142 is formed by the first ring member 134, the upper die 126, and the lower die 128. A knockout pin 144 for extruding a forged product is arranged on the lower side of the cavity 142, which is movable back and forth along a hole 146 formed through the second die holder 116 and the third die holder 118. A secondary formed product 148 as shown in
An elevating member 150, which is connected to the ram 36 of the mechanical press 31 shown in
As shown in
The cylindrical member 154 is formed of a metal material such as SKD11, FC25, or FC30 (according to JIS). The first ring member 134 is preferably formed of a material harder than that for the cylindrical member 154 in order to avoid occurrence of scuffing.
The punch 130 is provided displaceably in the vertical direction integrally with the elevating member 150 in accordance with the guiding action of the plurality of guide means 112a to 112d provided vertically on the first die holder 114.
As shown in
A plurality of arrays of holes 168 are formed substantially in parallel to one another along the axial direction in the guide ring 164. Rolling members 170 each having a substantially columnar configuration are rollably arranged in the holes 168. As shown in
In this embodiment, the rolling members 170 roll in a state of making line-to-line contact with the first rolling surfaces 172 and the second rolling surfaces 174 respectively. Accordingly, the cover member 160 connected to the elevating member 150 and the guide ring 164 engaged with the cover member 160 are displaced in an integrated manner along the axial direction of the main post body 158.
Alternatively, the following arrangement may be also available. That is, the rolling member 170 is not provided in the hole 168 of the guide ring 164. The guide ring 164 is formed to surround the outer circumferential surface of the main post body 158. The guide ring 164 is formed to make relative sliding displacement while making line-to-line contact with the main post body 158.
The forging die apparatus 100 according to the first embodiment of the present invention is basically constructed as described above. Next, its operation, function, and effect will be explained. The following embodiment will be described as exemplified by a case in which an outer cup for constructing a constant velocity universal joint is formed as a forged product obtained by forging.
A primary formed product 178, which has different diameters respectively with an intermediate step section as shown in
The forging die apparatus 100 according to the embodiment of the present invention further applies tertiary forging to the secondary forged product 148 as the forging material.
At first, a preparatory operation is performed in a state in which the punch 130 externally fitted with the cylindrical member 154 is inserted into the hole 132 of the first ring member 134. In this state, the upper die 126, the lower die 128, the sleeve 124, the forcible insertion ring 120, and other components are integrally assembled as described later on. Thus, the punch 130 is positioned with respect to the cavity 142 formed by the upper die 126 and the lower die 128.
The secondary formed product 148 as the forging material is charged in the cavity 142 in a state in which the punch 130 is arranged at an unillustrated lifted position. The punch 130 is lowered integrally with the elevating member 150 connected to the ram 36 in accordance with the driving action of the mechanical press 31 to give the state as shown in
When the punch 130 is lowered integrally with the elevating member 150, any unbalanced load in the lateral direction is appropriately absorbed by the plurality of (for example, four of) guide means 112a to 112d provided between the elevating member 150 and the first die holder 114. Accordingly, the punch 130 is smoothly inserted under pressure toward the center of the first ring member 134.
When the forging is started, the cylindrical, member 154, which is externally fitted to the part of the outer circumferential surface of the punch 130, proceeds in accordance with the guiding action of the annular groove 138 formed at the upper end of the hole 132 of the first ring member 134 (see
The punch 130 is lowered as described above, and it arrives at the forging end position shown in
After the forging is completed as described above, the punch 130 is lifted to the predetermined position integrally with the elevating member 150 connected to the ram 36 in accordance with the driving action of the mechanical press 31. Accordingly, the punch 130 and the cylindrical member 154 are separated from the hole 132 of the first ring member 134 to give a waiting state for the next step. The forged product 184 (see
In the embodiment of the present invention, when the pressurizing force is applied to the forging material, the cylindrical member 154, which is externally fitted to the punch 130, is in the state of being forcibly inserted into the hole 132 of the first ring member 134. The punch 130 is lowered while maintaining the forcibly inserted state.
Therefore, in the embodiment of the present invention, the pressurizing force is applied to the forging material in the state in which the punch 130 is forcibly inserted into the hole 132 of the first ring member 134 by the aid of the cylindrical member 154, and the punch 130 does not cause any centering deviation in the lateral direction. Accordingly, as shown in
Further, the cylindrical member 154 and the first ring member 134 are formed of metal materials which are different from each other. Moreover, the lubricating characteristic is appropriately maintained by the aid of the graphite 156 embedded in the cylindrical member 154. Thus, it is possible to suppress occurrence of scuffing on the sliding surfaces of the cylindrical member 154 and the first ring member 134.
The cylindrical member 154 is detachably attached to the punch 130 by the aid of the jig 152. Therefore, an advantage is obtained in that the cylindrical member 154 can be conveniently exchanged with another new cylindrical member 154.
Additionally, for example, an advantage is obtained in that the outer circumferential surface of the cup 186 of the outer cup as an attachment site for a pulser (not shown) can be directly subjected to grinding.
Next, explanation will be made for an assembling step for the dies for constructing the forging die apparatus 100.
As shown in
Subsequently, as shown in
After the sleeve 124, the upper die 126, and the lower die 128 are forcibly inserted into the hole 119, the forcible insertion ring 120 is inverted upside down to give a state shown in
Further, the forcible insertion of the sleeve 124 into the tapered hole 119 allows the compressive stress to act so that the sleeve 124 is tightened in the direction directed toward the center. The clearance 123 disappears between the inner circumferential surface of the sleeve 124 and the outer circumferential surfaces of the upper die 126 and the lower die 128 which are in the unlubricated condition. Thus, a state is given, in which the inner circumferential surface of the sleeve 124 makes mutual surface-to-surface contact with the outer circumferential surfaces of the upper die 126 and the lower die 128.
Therefore, the tightening force acts to make mutual tight surface-to-surface contact between the inner circumferential surface of the sleeve 124 and the outer circumferential surfaces of the upper die 126 and the lower die 128 in accordance with the action of the compressive stress. Thus, the joined state of the upper die 126 and the lower die 128 is locked. Accordingly, the upper die 126 and the lower die 128 are held in a state in which the surface pressure at the joining surface is increased.
As described above, in the embodiment of the present invention, the upper die 126 and the lower die 128 are maintained in the state in which the surface pressure at the joining surface is increased. Thus, it is possible to avoid occurrence of burr at the joining surface between the upper die 126 and the lower die 128, and it is possible to highly accurately maintain the coaxial degree between the upper die 126 and the lower die 128. Therefore, as shown in
As shown in
As shown in
Subsequently, the first ring member 134 and the second ring member 136 are arranged on the upper die 126 and the sleeve 124 respectively. The clamping ring 140 is screwed along the screw hole 139 of the forcible insertion ring 120. Thus, the first ring member 134 and the second ring member 136 are integrally assembled with the upper die 126, the lower die 128, and other components in accordance with the tightening action of the tapered section 141 of the clamping ring 140 (see
As clearly understood from
In the embodiment shown in
The modified embodiment shown in
Next, a forging die apparatus 200 according to a second embodiment is shown in
The forging die apparatus 200 comprises a forging punch unit 211 fixed to the bottom surface of the elevating member 150 by the aid of a holder 252. The forging punch unit 211 is provided displaceably along the vertical direction integrally with the elevating member 150 in accordance with the guiding action of the plurality of guide means 112a to 112d provided vertically on the first die holder 114.
As shown in
The cylindrical member 154 is held detachably by the aid of a lock ring 255 which engages with a step section of the cylindrical member 154 and which is screwed into a screw portion of the main punch body 230. As shown in
As shown in
As shown in
As shown in
In this embodiment, each of the first to seventh passages 262a to 2628 is substantially composed of a groove having a circular arc-shaped cross section formed on the outer circumferential surface of the main punch body 230. The first to seventh passages 262a to 2628 are formed to make communication with each other. Reference numerals 264a, 264b indicate seal rings for holding the communication passage 257 in an air-tight manner or in a liquid-tight manner. Reference numeral 266 indicates blank caps for closing ends of the first passage 262a and the seventh passage 2628.
The forging die apparatus 200 according to the second embodiment of the present invention is basically constructed as described above. Next, its operation, function, and effect will be explained.
As a preparatory operation, the cooling medium supply source (not shown) is energized beforehand to previously supply the cooling medium via the unillustrated tube to the communication passage 257 formed between the cylindrical member 154 and the main punch body 230.
The secondary formed product 148 (see
When the main punch body 230 is lowered integrally with the elevating member 150, any unbalanced load in the lateral direction is appropriately absorbed by the plurality of (for example, four of) guide means 112a to 112d (see
When the forging is started, the cylindrical member 154, which is externally fitted to the part of the outer circumferential surface of the main punch body 230, proceeds in accordance with the guiding action of the annular groove 138 formed at the upper end of the hole 132 of the first ring member 134. The main punch body 230 is further lowered, and thus the main punch body 230 and the cylindrical member 154 are integrally displaced in a state of being forcibly inserted into the hole 132 of the first ring member 134.
The main punch body 230 is lowered as described above, and it arrives at the forging end position shown in
In this embodiment, the main punch body 230 is directly cooled by the cooling medium flowing through the first to seventh passages 262a to 2628 formed between the cylindrical member 154 and the main punch body 230. The frictional force, which is generated when the forging material is forged, can be appropriately absorbed owing to the cooling action exerted on the main punch body 230. Therefore, it is possible to suppress thermal expansion of the main punch body 230 which would be otherwise caused by the frictional heat. It is possible to further increase the durability of the main punch body 230.
The frictional heat, which is generated on the forcible insertion surface of the cylindrical member 154 forcibly inserted into the hole 132 of the first ring member 134, is also appropriately absorbed in accordance with the cooling action described above. Therefore, it is possible to improve the durability of the cylindrical member 154.
After the forging is completed as described above, the main punch body 230 is lifted to the predetermined position integrally with the elevating member 150 connected to the ram 36 in accordance with the driving action of the mechanical press 31. Accordingly, the main punch body 230 and the cylindrical member 154 are separated from the hole 132 of the first ring member 134 to give a waiting state for the next step. The forged product 184 (see
As clearly understood from
For example, in the case of the main punch body 230 and the cylindrical member 154 provided with the cooking means 253, the portion provided with the first to seventh passages 262a to 2628 for allowing the cooling medium to flow therethrough is cooled to be not more than 20° C. On the contrary, the portion of the main punch body 277 corresponding to the foregoing portion has a relatively high temperature which is not more than 120° C.
As for the cylindrical member 154 concerning the characteristic curve J, the forcible insertion margin for the first ring member 134 is set to be about 0.03 mm. As for the cylindrical member 154 concerning the characteristic curve K, the forcible insertion margin is set to be about 0.01 mm. As for the cylindrical member 154 concerning the characteristic curve L, the forcible insertion margin is set to be about 0.01 mm.
In the case of the cylindrical member 154 concerning the characteristic curve L provided with the cooling means 253, the increase in temperature is suppressed, and the temperature is maintained to be substantially constant at a low temperature (about 20° C.) even when the number of forging shots is increased. Therefore, no scorch occurs on the first ring member 134. On the contrary, in the case of the cylindrical members 154 concerning the characteristic curves J and K not provided with the cooling means 253, the temperature is increased in accordance with the increase in the number of forging shots, and scorch occurs on the cylindrical members 154.
As described above, in the embodiment of the present invention, the frictional heat generated by the forging material and the main punch body 230 is appropriately absorbed by the aid of the cooling means 253. Accordingly, the thermal expansion can be suppressed, and it is possible to further improve the durability of the main punch body 230.
Since the cooling means 253 is constructed by the simple mechanism, it is possible to respond to mass production.
Further, in the embodiment of the present invention, the pressurizing force is applied to the forging material in the state in which the main punch body 230 is forcibly inserted into the hole 132 of the first ring member 134 by the aid of the cylindrical member 154, and thus the main punch body 230 does not cause any centering deviation in the lateral direction. Accordingly, as shown in
Furthermore, the cylindrical member 154 and the first ring member 134 are formed of metal materials which are different from each other. Moreover, the lubricating characteristic is appropriately maintained by the aid of the graphite 156 embedded in the cylindrical member 154. Thus, it is possible to suppress occurrence of scuffing on the sliding surfaces of the cylindrical member 154 and the first ring member 134.
Moreover, the cylindrical member 154 is detachably attached to the main punch body 230 by the aid of the lock ring 255. Therefore, an advantage is obtained in that the cylindrical member 154 can be conveniently exchanged with another new cylindrical member 154.
Next, a modified embodiment of the forging punch unit 211 according to the embodiment of the present invention is shown in
A forging punch unit 280 according to the modified embodiment is different from the forging punch unit 211 shown in
That is, a cooling medium supply port 258a and a cooling medium discharge port 258b, which are opposed to one another, are formed on the upper side of the intermediate member 286. A first communication passage 288, which communicates with the cooling medium supply port 258a, is formed to make circumscription in a helical configuration between the cylindrical member 282 and the intermediate member 286. Further, a second communication passage 290, which communicates with the cooling medium discharge port 258b, is formed to make circumscription in a helical configuration between the main punch body 284 and the intermediate member 286.
In this embodiment, as shown in
The structure, the function, and the effect of this embodiment other than the above are equivalent to those of the forging punch unit 211 shown in
Next, a forging die apparatus 300 according to a third embodiment of the present invention is shown in
The forging die apparatus 300 comprises a first die holder 314 on which a plurality of guide means 112a to 112d (see
A thick-walled forcible insertion ring 320, which is formed in an integrated manner, is fixed on the second die holder 316 by the aid of a clamping means 122. An upper die 326 and a lower die 328 are integrally joined in a hole of the forcible insertion ring 320 via a sleeve 324 which is formed to be thin-walled.
A first ring member 334 formed with a hole 332, a second ring member 336 externally fitted to the first ring member 334, and a clamping ring 338 for holding the first ring member 334 and the second ring member 336 are provided in an annular recess 330 formed at an upper portion of the forcible insertion ring 320. The first ring member 334 and the second ring member 336 are formed on the upper side of the forcible insertion ring 320, and they are inserted under pressure into a hole 337 processed coaxially with a cavity 346 described later on, with a good coaxial degree. In this embodiment, the first ring member 334 and the second ring member 336 may be integrally formed as an unillustrated ring member without constructing them as the separate members respectively.
A first plate 344 for regulating the displacement amount of a punch 340 by making abutment against a second plate 342 which is displaceable integrally with the punch 340 as described later on is provided on upper surfaces of the upper die 326 and the sleeve 324.
The first ring member 334 is formed of, for example, a cemented carbide material, and it is in a state of being strongly tightened toward the center by the second ring member 336 which has been subjected to the shrinkage fitting treatment. The first ring member 334 and the second ring member 336 are forcibly inserted into the hole 337 processed coaxially with the cavity 346. Further, the first ring member 334 and the second ring member 336 are tightened by a tapered section of the clamping ring 338 which is screwed into a screw hole of the forcible insertion ring 320. Thus, the first ring member 334 and the second ring member 336 are integrally joined to the recess 330 of the forcible insertion ring 320 with a good coaxial degree with respect to the cavity 346.
In this embodiment, the cavity 346 is formed by the upper die 326 and the lower die 328. A knockout pin 348 for extruding a forged product is arranged on the lower side of the cavity 346, which is movable back and forth along a hole 350 formed through the second die holder 316 and the third die holder 318. A secondary formed product 148 as shown in
An elevating unit 354, which is connected to the ram 36 of-the mechanical press 31 shown in
The elevating unit 354 has a buffering mechanism 356 which is provided in order that the punch 340 abuts against the forging material to start the forging, and the upper and lower dies make abutment before arrival at the bottom dead center to complete the forging for the forging material so that the residual displacement amount is absorbed thereafter until arrival at the bottom dead center.
The buffering mechanism 356 has a pressure chamber 358 formed therein, and it comprises a cylindrical block member 362 with a bottom having a piston 360 which is provided vertically displaceably along the pressure chamber 358, and a pair of connecting blocks 366a, 366b which are coupled to the block member 362 in a liquid-tight manner and which are formed with a passage 364 communicating with the pressure chamber 358. A ring-shaped stopper 368 is fixed on the bottom surface of the block member 362 in order to prevent the piston 360 from descending movement.
A check valve 371 and a pressure oil supply source 373 are connected via a tube 370 to one connecting block 366a. A relief valve 377 and a tank 379 for storing the pressure oil are connected via a tube 375 to the other connecting block 366b. A predetermined amount of pressure oil, which is supplied from the pressure oil supply source 373, is charged in the pressure chamber 358 and the passage 364. A ring-shaped high pressure packing 372, a low pressure packing 374, and a wear plate 376 are installed to annular grooves on the outer circumference of the piston 360 respectively.
A punch plate 378 is fixed on the bottom surface of the piston 360. A punch 340 is fixed on the punch plate 378 by the aid of a holder 380 which surrounds a part of the outer circumferential surface. A cylindrical member 382, which is formed of a cylindrical metal material, is externally fitted to the outer circumference of the holder 380. A second plate 342 is fixedly provided on the bottom surface of the holder 380.
The cylindrical member 382 is formed of a metal material such as SKD11, FC25, or FC30 (according to JIS). The first ring member 334 is preferably formed of a material harder than that for the cylindrical member 382.
The punch 340 is provided displaceably in the vertical direction integrally with the elevating unit 354 in accordance with the guiding action of the plurality of guide means 112a to 112d provided vertically on the first die holder 314.
The forging die apparatus 300 according to the third embodiment of the present invention is basically constructed as described above. Next, its operation, function, and effect will be explained.
At first, the following preparatory operation is performed. That is, the punch 340 is allowed to be in a state of being positioned with respect to the cavity 346 formed by the upper die 326 and the lower die 328. The pressure chamber 358 is previously charged with a predetermined amount of pressure oil via the passage 364 communicating with the check valve 371 in accordance with the driving action of the pressure oil supply source 373.
Subsequently, the secondary formed product 148 as the forging material is charged in the cavity 346 in a state in which the punch 340 is arranged at an unillustrated lifted position. The punch 340 is lowered integrally with the elevating unit 354 connected to the ram 36 in accordance with the driving action of the mechanical press 31 to give the state as shown in
When the punch 340 is lowered integrally with the elevating unit 354, any unbalanced load in the lateral direction is appropriately absorbed by the plurality of guide means 112a to 112d provided between the elevating unit 354 and the first die holder 314. Accordingly, the punch 340 can be smoothly inserted under pressure toward the center of the hole 332 of the first and second ring members 334, 336 arranged coaxially with the cavity 346 by the aid of the cylindrical member 382.
When the forging is started, the cylindrical member 382, which is externally fitted to the part of the outer circumferential surface of the punch 340, proceeds in accordance with the guiding action of the annular groove 138 formed at the upper end of the hole 332 of the first ring member 334. The punch 340 is further lowered, and thus the punch 340, the holder 380, and the cylindrical member 382 are integrally displaced in a state of being forcibly inserted into the hole 332 of the first ring member 334.
When the ram 36 of the mechanical press 31 is displaced downwardly from the predetermined lifted position, and the punch 340, the second plate 342, and other components are lowered integrally with the ram 36, then the spacing distance of separation R between the first plate 344 on the fixation side and the second plate 342 on the displacement side is gradually decreased. The piston 360 is held by the stopper 368, and it is in a state of being prevented from downward displacement. The pressure of the pressure oil charged in the pressure chamber 358 is gradually increased after the start of the forging in accordance with the increase in load applied to the punch 340.
The operating pressure for the relief valve 377 is set such that the reaction force of the piston 360 is not less than the forging load on the forging material, and it is not more than the overloaded forging load. The forging load on the forging material is supported by the pressure oil charged in the pressure chamber 358.
The second plate 342 abuts against the first plate 344 immediately before the punch 340 arrives at the bottom dead center after the punch 340 is further lowered from the state shown in
The compression of the die enables the punch 340 to be lowered after abutment of the first plate 344 and the second plate 342. Since the force of the mechanical press 31 is extremely large, the components such as the first through third die holders 314, 316, 318, the forcible insertion ring 320, the sleeve 324, and the upper die 326, the lower die 328 assembled into the die are pressed together just a little. Though the substantial movement of the punch 340 is restricted by the abutment between the first plate 344 and the second plate 342, the compression of the die components enables the punch to be displaced downwardly by the minute distance (Δt) (see
During this process, in the embodiment of the present invention, the amount of variation, which is brought about, for example, by elongation of the connecting rod 35 and the frames 33a, 33b of the mechanical press 31 to cause variation in thickness dimension of the forging material in ordinary cases, is absorbed as the change in stroke amount of the piston 360. Further, the thickness dimension of the forging material is determined by the abutment between the upper die and the lower die. Therefore, no influence is exerted by the elongation of the frames 33a, 33b and other components.
As described above, the dimension of the bottom thickness T (see
Next,
The punch 340 is lowered as described above, and it arrives at the forging end position shown in
After the forging is completed as described above, the punch 340 is lifted to the predetermined position integrally with the elevating unit 354 connected to the ram 36 in accordance with the driving action of the mechanical press 31. Accordingly, the punch 340, the holder 380, and the cylindrical member 382 are separated from the hole 332 of the first ring member 334 to give a waiting state for the next step. The forged product 392 as a tertiary formed product (hereinafter also referred to as “tertiary formed product 392”, if necessary) (see
In the embodiment of the present invention, the second plate 342 disposed on the displacement side abuts against the first plate 344 on the fixation side, and the distance of separation therebetween R becomes zero, immediately before the punch 340 arrives at the bottom dead center. Accordingly, the downward displacement of the punch 340 is regulated. Thus, it is possible to obtain a substantially constant dimension of the bottom thickness T of the cup 394 of the outer cup obtained as the forged product 392. Therefore, it is possible to highly accurately maintain the thickness accuracy of the obtained forged product 392.
In the embodiment of the present invention, it is unnecessary to perform, after the forging, the cutting processing which has been required for the conventional technique in order to obtain a constant bottom thickness dimension of the cup 394 of the outer cup. Accordingly, it is possible to simplify the production process and improve the production efficiency.
In the embodiment of the present invention, the forming load applied to the forging material can be set to be larger than the minimum forming load which is actually required and smaller than the overloaded forming load. Therefore, it is possible to prevent the mechanical press 31 from being stopped in the locked state, and it is possible to continuously perform the forging.
In the embodiment of the present invention, the buffering mechanism 356 is provided at the elevating unit 354 disposed on the displacement side. However, there is no limitation thereto. The buffering mechanism 356 may be provided on the fixation side, for example, on the upper die 326 and the lower die 328.
Next, a forging die apparatus 400 according to a fourth embodiment of the present invention is shown in
The forging die apparatus 400 comprises a first die holder 414 on which a plurality of guide means 112a to 112d (see
A cylindrical first die member 420 is fixed on the second die holder 416 by the aid of a clamping means 122. A cylindrical second die member 426, which has a smaller diameter than the first die member 420, is integrally joined to a step section of a first hole 424 of the first die member 420.
As shown in
In this embodiment, a cavity 430 (see
A shoulder 438, which has a curved configuration with a predetermined radius of curvature, is formed at an upper portion of the second hole 428 of the second die member 426. A tapered hole 440, which has its diameter gradually increasing in the upper direction over a predetermined range, is formed at a lower portion of the second hole 428. A portion of the second hole 428, which is disposed over the tapered hole 440, is formed to have a diameter larger than the increased diameter of the tapered hole 440.
As shown in
A diametrally expanded pin 448 is arranged under the knockout pin 432 while being separated by a predetermined clearance W. An unillustrated displacement member is connected to the diametrally expanded pin 448. The diametrally expanded pin 448 and the knockout pin 432 can be moved back and forth in an integrated manner in accordance with the energizing action of the displacement member.
The knockout pin 432 has its tapered section 444 which is engaged with the tapered hole 440 of the second die member 426. The clearance W is formed between the knockout pin 432 and the diametrally expanded pin 448. Accordingly, the knockout pin 432 is suspended in a state of being positioned beforehand so that the projection 446 is arranged at the center of the tapered hole 440.
An elevating member 450, which is connected to the ram 36 of the mechanical press 31 described above for making displacement along the vertical direction integrally with the ram 36 in accordance with the driving action of the mechanical press 31, is provided at an upper position separated by a predetermined distance from the first die member 420. A punch 454 is fixed to the elevating member 450 by the aid of a jig 452. A cylindrical member 456, which is formed of a cylindrical metal material, is externally fitted to a predetermined portion of the outer circumference of the punch 454.
As shown in
The cylindrical member 456 is formed of a metal material such as SKD11, FC25, or FC30 (according to JIS). The first die member 420 is preferably formed of a material harder than that for the cylindrical member 456 in order to avoid occurrence of scuffing.
The punch 454 is provided displaceably in the vertical direction integrally with the elevating member 450 in accordance with the guiding action of the plurality of guide means 112a to 112d (see
The forging die apparatus 400 according to the fourth embodiment of the present invention is basically constructed as described above. Next, its operation, function, and effect will be explained.
The forging die apparatus 400 according to the embodiment of the present invention is used to further apply quaternary forging to the tertiary formed product 392 shown in
The tertiary formed product 392 as the forging material is charged in the cavity 430 as shown in
When the punch 454 is lowered integrally with the elevating member 450, any unbalanced load in the lateral direction is appropriately absorbed by the plurality of (for example, four of) guide means 112a to 112d provided between the elevating member 450 and the first die holder 414.
When the forging is started, the cylindrical member 456, which is externally fitted to the part of the outer circumferential surface of the punch 454, proceeds along the first hole 424 of the first die member 420. The punch 454 is further lowered, and thus the punch 454 and the cylindrical member 456 are integrally displaced in a state of being forcibly inserted into the first hole 424 of the first die member 420.
The punch 454 is lowered as described above, and it arrives at the forging end position shown in
When the pressurizing force is applied to the forging material by the aid of the punch 454, a hole is made at one end of the shaft 474 of the forging material (see
In this embodiment, the knockout pin 432 is inserted in the state of being positioned beforehand so that the projection 446 is arranged at the center of the tapered hole 440. Therefore, the centering hole 476 can be correctly made at the center of one end of the shaft 474 of the forging material. In other words, the center of the centering hole 476 formed simultaneously with the forging can be allowed to correctly coincide with the axis of the forging material.
After the formation of the centering hole 476 is started, the clearance W between the knockout pin 432 and the diametrally expanded pin 448 becomes zero on account of the forming load applied to the knockout pin 432. The forming load is supported by the abutment therebetween (see
After the forging is completed as described above, the punch 454 is lifted to the predetermined position integrally with the elevating member 450 connected to the ram 36 in accordance with the driving action of the mechanical press 31. Accordingly, the punch 454 and the cylindrical member 456 are separated from the first hole 424 of the first die member 420 to give a waiting state for the next forging material. The forged product 474 as a quaternary formed product (see
In the embodiment of the present invention, when the pressurizing force is applied to the forging material, the cylindrical member 456, which is externally fitted to the punch 454, is in the state of being forcibly inserted into the first hole 424 of the first die member 420. The punch 454 is lowered while maintaining the forcibly inserted state.
Therefore, in the embodiment of the present invention, the pressurizing force is applied to the forging material in the state in which the punch 454 is forcibly inserted into the first hole 424 of the first die member 420 by the aid of the cylindrical member 456, and the punch 454 does not cause any centering deviation in the lateral direction. Accordingly, it is possible to highly accurately maintain the coaxial degree among the center line Z of the centering hole 476, the axis X of the cup 480, and the axis Y of the shaft 484 of the outer cup obtained as the forged product 478 (see
Number | Date | Country | Kind |
---|---|---|---|
9-335893 | Dec 1997 | JP | national |
9-335912 | Dec 1997 | JP | national |
9-335916 | Dec 1997 | JP | national |
9-335923 | Dec 1997 | JP | national |
9-335931 | Dec 1997 | JP | national |
This application is a continuation-in-part of applicatiton Ser. No. 09/487,880, filed on Jan. 20, 2000, now abandoned, which in turn is a divisional application of application Ser. No. 09/177,364, filed on Oct. 23, 1998, now U.S. Pat. No. 6,035,688. The entire contents of each of the above-identified applications are hereby incorporated by reference and priority is claimed under 35 U.S.C. § 120.
Number | Name | Date | Kind |
---|---|---|---|
1689500 | Rode | Oct 1928 | A |
2200609 | Week Jr. | May 1940 | A |
4030336 | Grigorenko et al. | Jun 1977 | A |
4426872 | Gatny | Jan 1984 | A |
4466266 | Gardner et al. | Aug 1984 | A |
Number | Date | Country |
---|---|---|
61-255737 | Nov 1986 | JP |
7-178493 | Jul 1995 | JP |
Number | Date | Country | |
---|---|---|---|
20030213277 A1 | Nov 2003 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 09177364 | Oct 1998 | US |
Child | 09487880 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 09487880 | Jan 2000 | US |
Child | 10437074 | US |