This application claims priority to and the benefit of Korean Patent Application No. 10-2010-0054983 filed in the Korean Intellectual Property Office on Jun. 10, 2010, the entire contents of which are incorporated herein by reference.
1. Field of the Disclosure
The described technology relates to a fuel cell stack. More particularly, it relates to a structure of a separator of a fuel cell stack.
2. Description of the Related Technology
A fuel cell system includes a fuel cell stack generating electrical energy by an electrochemical reaction between a fuel (hydrocarbon fuel, pure hydrogen or reformed gas rich in hydrogen) and an oxidant (air or pure oxygen). A direct oxidation fuel cell uses a liquid or gaseous hydrocarbon fuel. A polymer electrode fuel cell uses pure hydrogen or a hydrogen-rich reformed gas as a fuel.
A membrane-electrode assembly generally includes an electrolyte membrane, an anode formed on one surface of the electrolyte membrane and a cathode formed on the other surface of the electrolyte membrane. A first separator positioned on the anode side of the membrane electrode assembly has a fuel channel formed on a surface facing the anode. A second separator positioned on the cathode side of the membrane electrode assembly has an oxidant channel formed on a surface facing the cathode. Two fuel manifolds and two oxidant manifolds are formed on the corners of each separator. The fuel channel is connected to the two fuel manifolds and the oxidant channel is connected to the two oxidant manifolds.
The fuel channel and the oxidant channel include recessed grooves having a cross-sectional area much smaller than that of the fuel manifolds and the oxidant manifolds. Accordingly, when a fuel enters the fuel channel from the fuel manifolds and an oxidant enters the oxidant channel from the oxidant manifolds, the flow path (of the fuel or the oxidant, respectively) is abruptly narrowed such that a flow rate and a pressure rise.
High fluid pressure causes stress on the system concentrated in an area of the anode into which the fuel is introduced and also in an area of the cathode into which the oxidant is introduced. Moreover, the high fluid pressure at the entrance of the fuel channel and the entrance of the oxidant channel makes it difficult to uniformly distribute the fuel and the oxidant along the fuel channel and the oxidant channel.
Further, since the oxidant supplied to the fuel cell stack is not humidified, the area of the cathode into which the oxidant is first introduced operates in a very dry state. This gives rise to a condition in which radicals (produced during the operation of a membrane-electrode assembly) exist within the membrane-electrode assembly for unusually long periods of time. The increased number of radicals results in deterioration of the membrane-electrode assembly.
In one aspect, a fuel cell stack includes, for example, a membrane-electrode assembly, an anode separator, a cathode separator and a filing member. In some embodiments, the membrane-electrode assembly includes an electrolyte membrane, an anode formed on a first surface of the electrolyte membrane and a cathode formed on a second surface of the electrolyte membrane. In some embodiments, the anode separator includes a fuel channel, a fuel inlet manifold in fluid communication with the fuel channel and a fuel outlet manifold in fluid communication with the fuel channel. In some embodiments, the anode separator is positioned proximate to the anode. In some embodiments, the cathode separator includes an oxidant channel, an oxidant inlet manifold in fluid communication with the oxidant channel, and an oxidant outlet manifold in fluid communication with the oxidant channel. In some embodiments, the cathode separator is positioned proximate to the cathode. In some embodiments, the filling member is positioned in at least one of the fuel inlet manifold and the oxidant inlet manifold.
In some embodiments, the filling member is formed of a porous member having a pore density of about 30% to about 70%. In some embodiments, the porous member includes, for example, a plurality of bead members, a porous annular member having a hollow center, or a porous honeycomb member formed of an array of honeycomb-like cells. In some embodiments, the plurality of bead members and the porous annular member are formed of at least one of sand, zeolite, silica, aluminum oxide, titanium oxide, porous polyethylene, porous polypropylene, and a methyl methacrylate ionomer. In some embodiments, the porous honeycomb member is formed of at least one of sand, zeolite, silica, aluminum oxide, titanium oxide, porous polyethylene, porous polypropylene, and a methyl methacrylate ionomer. In some embodiments, the porous honeycomb member has a density of about 100 cpi to about 1000 cpi.
In some embodiments, the fuel cell stack includes, for example, an auxiliary filling member interspersed in at least one of the fuel outlet manifold and the oxidant outlet manifold. In some embodiments, the auxiliary filing member is configured to facilitate moisture discharge. In some embodiments, the auxiliary filling member is formed of a porous member having a higher pore density than that of the filling member. In some embodiments, the auxiliary filling member may include a hydrophilic coating layer. In some embodiments, the porous member may include a plurality of bead members, a porous annular member having a hollow center, or a porous honeycomb member formed of an array of honeycomb-like cells. In some embodiments, the plurality of bead members and the porous annular member are formed of at least one of sand, zeolite, silica, aluminum oxide, titanium oxide, porous polyethylene, porous polypropylene, and a methyl methacrylate ionomer. In some embodiments, the porous honeycomb member is formed of at least one of sand, zeolite, silica, aluminum oxide, titanium oxide, porous polyethylene, porous polypropylene, and a methyl methacrylate ionomer.
In some embodiments, the membrane-electrode assembly may include a plurality of membrane electrode assemblies spaced apart from each other with a bipolar plate positioned between each of the membrane-electrode assemblies. In some embodiments, the bipolar plate may include the anode separator and the cathode separator bonded together. In some embodiments, the anode separator has a first connecting channel formed on an inner surface confronting the cathode separator and in fluid communication with the fuel inlet manifold and the fuel channel. In some embodiments, the first connecting channel is in fluid communication with the fuel outlet manifold and the fuel channel. In some embodiments, the cathode separator has a second connecting channel formed on an inner surface confronting the anode separator and in fluid communication with the oxidant inlet manifold and the oxidant channel. In some embodiments, the second connecting channel is in fluid communication with the oxidant outlet manifold and the oxidant channel. In some embodiments, the anode separator and the cathode separator each have a plurality of cooling channels formed on inner surfaces and facing each other. In some embodiments, the anode separator contacts the anode. In some embodiments, the cathode separator contacts the cathode. In some embodiments, the plurality of bead members may include beads of varied sizes.
In another aspect, a fuel cell stack is provided with separators configured to reduce deterioration of a membrane-electrode assembly by alleviating pressure occurring in the inlet of a fuel channel and the inlet of an oxidant channel and by more uniformly distributing the fuel and the oxidant along the fuel channel and the oxidant channel.
In some embodiments, the pressures and flow rates of the fuel passing through the fuel inlet manifold and the oxidant passing through the oxidant inlet manifold can be reduced by the filling member. In some embodiments, deterioration of the membrane-electrode assembly can be prevented by alleviating stress concentration occurring in an area of the anode into which the fuel is introduced first and an area of the cathode into which the oxidant is introduced first. In some embodiments, the contact efficiency between the anode and the fuel can be increased because the fuel can be distributed more uniformly along the fuel channel. In some embodiments, the contact efficiency between the cathode and the oxidant can be increased because the oxidant can be distributed more uniformly along the oxidant channel. In some embodiments, electricity generation efficiency of the membrane-electrode assembly can be improved.
Features of the present disclosure will become more fully apparent from the following description and appended claims, taken in conjunction with the accompanying drawings. It will be understood these drawings depict only certain embodiments in accordance with the disclosure and, therefore, are not to be considered limiting of its scope; the disclosure will be described with additional specificity and detail through use of the accompanying drawings. An apparatus, system or method according to some of the described embodiments can have several aspects, no single one of which necessarily is solely responsible for the desirable attributes of the apparatus, system or method. After considering this discussion, and particularly after reading the section entitled “Detailed Description of Certain Inventive Embodiments” one will understand how illustrated features serve to explain certain principles of the present disclosure.
In the following detailed description, only certain exemplary embodiments have been shown and described, simply by way of illustration. As those skilled in the art would realize, the described embodiments may be modified in various different ways, all without departing from the spirit or scope of the present disclosure. Accordingly, the drawings and description are to be regarded as illustrative in nature and not restrictive. In addition, when an element is referred to as being “on” another element, it can be directly on the another element or be indirectly on the another element with one or more intervening elements interposed therebetween. Also, when an element is referred to as being “connected to” another element, it can be directly connected to the another element or be indirectly connected to the another element with one or more intervening elements interposed therebetween. Hereinafter, like reference numerals refer to like elements. Certain embodiments will be described in more detail with reference to the accompanying drawings, so that a person having ordinary skill in the art can readily make and use aspects of the present disclosure.
Referring to
In operation, the membrane-electrode assembly 10 is supplied with a fuel and an oxidant, and is configured to generate electrical energy by an electrochemical reaction of the fuel and the oxidant. The separators 20 are configured to support the membrane-electrode assemblies 10 by pressing the membrane-electrode assemblies 10 having low mechanical strength, and also electrically connecting the membrane-electrode assemblies 10. The fuel cell stack 100 may use liquid or gaseous hydrocarbon fuels (methanol, ethanol, liquefied petroleum gas, liquefied natural gas, gasoline, or butane gas), or may use hydrogen or a hydrogen-rich gas generated by reforming a hydrocarbon fuel in a reformer. The fuel cell stack 100 may be configured to use pure oxygen stored in separate storage means or oxygen-containing air as an oxidant.
A pair of end plates 30 is provided on the outermost sides of the fuel cell stack 100. The end plates 30 are configured for fixing the membrane-electrode assemblies 10 and the separators 20. Either one or both of the end plates 30 may be provided with a fuel injection port 31 for supplying a fuel, an oxidant injection port 32 configured for supplying an oxidant, a fuel exhaust port 33 configured for exhausting unreacted fuel, and an oxidant exhaust port 34 configured for exhausting moisture and unreacted air. Although
As depicted in
As depicted in
In the illustrated embodiment of
Cooling channels 43 may be formed on the inner surface of the anode separator 210 and the inner surface of the cathode separator 220. The cooling channels 43 are in fluid communication with a blowing unit, which is not shown. In operation, outside air enters the cooling channels 43 by force created by the blowing unit. The temperature of the fuel cell stack 100 can be lowered by heat exchange between the outside air and the fuel cell stack 100. Instead of (or in addition to) an air-cooled structure, the anode separator 210 and the cathode separator 220 may have a cooling water manifold (not shown) for circulating cooling water.
As the inner surface of the anode separator 210 is positioned with respect to the flat inner surface of the cathode separator 220 in the vicinity of the first connecting channel 23, the fuel manifolds 411 and 412 and the fuel channel 21 can be connected through the first connecting channel 23 without fuel leakage in other directions.
Although
The two fuel manifolds 411 and 412 at each anode separator 210 are divided into a fuel inlet manifold 411 and a fuel outlet manifold 412. In operation, the fuel supplied to the fuel injection port 31 (see, for example,
The fuel cell stack 100 of the first exemplary embodiment includes a filling member 50 positioned in the fuel inlet manifold 411 of the anode separator 20. The filling member 50 is positioned and configured to alleviate the pressure and decrease flow rate of the fuel. The filling member 50 is a member configured to provide predetermined resistance to fuel flow without preventing the movement of the fuel, and may also be configured to reduce the pressure and flow rate of the fuel put into the first connecting channel 23 (or the fuel channel 21 if there is no first connecting channel) from the fuel inlet manifold 411. To this end, the filling member 50 may be formed as a porous member having a predetermined pore density.
The filling member 50 may have a filling density of between about 30% to about 70%. In this case, the pore density of the filing member 50 is also set to a range of between about 30% to about 70%. If the filling density of the filling member 50 is less than about 30%, a resistance effect on fuel flow is negligible, thus making it difficult to reduce the pressure and flow rate of the fuel. On the other hand, if the filling density of the filling member 50 is greater than about 70%, the resistance effect on the fuel flow becomes excessive, thus preventing the movement of the fuel. In some embodiments, the density of the filing member 50 is about 35%, about 40%, about 45%, about 50%, about 55%, about 60% or about 65% or any number in between. Indeed, the filling density of the filling member 50 can be easily adjusted by appropriately selecting the size and quantity of the bead members 51 in consideration of the type and supply pressure of the fuel put into the fuel cell stack 100.
Referring again to
As the inner surface of the cathode separator 220 is positioned in proximity to the flat inner surface of the anode separator 210 in the vicinity of the second connecting channel 24, the oxidant manifolds 421 and 422 and the oxidant channel 22 can be in fluid communication through the second connecting channel 24 without oxidant leakage in other directions.
Although
The two oxidant manifolds 421 and 422 at each cathode separator 220 are divided into an oxidant inlet manifold 421 and an oxidant outlet manifold 422. In operation, the fuel supplied to the oxidant injection port 32 (see, for example,
Like the anode separator 210, a filling member 50 is positioned in the oxidant inlet manifold 421 of the cathode separator 220. The filling member 50 is configured to provide resistance to oxidant flow passing through the oxidant inlet manifold 421 and positioned and configured to alleviate the pressure and decrease flow rate of the oxidant. The filling member 50 includes a plurality of integrally fixed bead members 51. The filling member 50 may include one type of bead members 51 having the same size, or at least two different types of bead members 51 with different sizes. For example,
In operation, a concentration of stress on the system occurs in an area of the cathode 13 into which the oxidant is introduced first. Thus, as the pressure and flow rate of the fuel passing through the oxidant inlet manifold 421 are reduced by the filling member 50, the concentration of system stress is alleviated, which ultimately decreases deterioration of the membrane-electrode assembly 10. Also, since the oxidant can be distributed more uniformly along the oxidant channel 22, the contact efficiency between the cathode 13 and the oxidant may be increased. When contact efficiency between the cathode 13 and the oxidant is increased the electricity generation efficiency of the membrane-electrode assembly 10 may be improved.
While the above description has been made with respect to a case where the filling member 50 is positioned in both the fuel inlet manifold 411 and the oxidant inlet manifold 421, the filling member 50 may be positioned in either one or both of the fuel inlet manifold 411 and the oxidant inlet manifold 421. That is, the filling member 50 may be selectively positioned in the inlet manifold that supplies either the fuel or the oxidant, which causes stress concentration on the membrane-electrode assembly 10 due to high supply pressure and flow rate.
Of the aforementioned filling members 50, 510, 520, and 530, the bead members 51, the porous annular member 52, and the porous honeycomb member 53 may be formed of one or more materials selected from the group including sand, a ceramic material such as zeolite, silica, aluminum oxide, or titanium oxide, a porous polymer material such as polyethylene or polypropylene, and a high-absorbent ionomer such as a methyl methacrylate ionomer. The porous honeycomb member 53 may be also formed of a metal foam, for example an iron-chrome-aluminum alloy foam.
The filling density of the filling members 50, 510, 520, and 530 may be between about 30% to about 70%, as noted above. In some embodiments, the density of the filling members 50, 510, 520, and 530 is about 35%, about 40%, about 45%, about 50%, about 55%, about 60% or about 65% or any number in between. The porous honeycomb member 53 may have a density of between about 100 cpi and about 1000 cpi. Here, cpi is an abbreviation for cell/in2, which indicates the number of cells per unit area (1 in2). If the density of the porous honeycomb member 53 is less than about 100 cpi, the pressure and flow rate of the fuel or oxidant may not be sufficiently reduced, and if the density of the porous honeycomb member 53 is greater than about 1000 cpi, movement of the fuel or oxidant may be blocked.
The filling members 50, 510, 520, and 530 may contain water by absorbing moisture from the outside air because of the high absorbance of the material itself when the fuel cell stack 100 is not in operation. In this case, when the fuel cell stack 100 is in operation, the fuel or oxidant may receive moisture while passing through the filling members 50, 510, 520, and 530. Accordingly, it is possible to suppress deterioration of the membrane-electrode assembly 10 due to dry fuel or dry oxidant and simultaneously to improve the electricity generation efficiency of the membrane-electrode assembly 10.
The filling member may be formed in shapes other than the shape as described above, and any structure capable of reducing the pressure and flow rate of fluid by providing resistance to fuel or oxidant flow is applicable.
Referring to
In operation, an unreacted fuel to be discharged to the fuel outlet manifold 412 and an unreacted oxidant to be discharged to the oxidant outlet manifold 422 may contain a large amount of moisture. The auxiliary filling member 60 may thus be configured to facilitate the discharge of the moisture contained in the unreacted fuel and the unreacted oxidant. To this end, the auxiliary filling member 60 is formed to have a structure similar to that of the filling member 50 provided in the corresponding separator with a higher density. That is, the pore density of the auxiliary filling member 60 is greater than the pore density of the filling member 50. Accordingly, the auxiliary filling member 60 is configured to absorb the moisture of the unreacted fuel and the unreacted oxidant. The auxiliary filing member 60 may be formed of a material having a high absorbance. The auxiliary filing member 60 may also be configured to facilitate discharge of the moisture with the aid of its high pore density. The auxiliary filling member 60 may include a plurality of bead members integrally fixed by adhering means, such as an adhesive. The auxiliary member may be formed with a structure or material which is less dense than that of the filling member 50. Also, the auxiliary filling member 60 may include a hydrophilic coating layer 62. The coating layer 62 may be configured to further facilitate moisture discharge.
The bead members 61 constituting the auxiliary filling member 60 may be accommodated in the porous case 54 depicted in
While the above description has been made with respect to a case where the auxiliary filling member 60 is positioned in both the fuel inlet manifold 412 and the oxidant inlet manifold 422, it will be understood that the auxiliary filling member 60 may also be positioned in either one or both of the fuel inlet manifold 412 and the oxidant inlet manifold 422.
While this invention has been described in connection with certain exemplary embodiments, it will be appreciated by those skilled in the art that various modifications and changes may be made without departing from the scope of the present disclosure. It will also be appreciated by those of skill in the art that parts included in one embodiment are interchangeable with other embodiments; one or more parts from a depicted embodiment can be included with other depicted embodiments in any combination. For example, any of the various components described herein and/or depicted in the Figures may be combined, interchanged or excluded from other embodiments. With respect to the use of substantially any plural and/or singular terms herein, those having skill in the art can translate from the plural to the singular and/or from the singular to the plural as is appropriate to the context and/or application. The various singular/plural permutations may be expressly set forth herein for sake of clarity. Thus, while the present disclosure has described certain exemplary embodiments, it is to be understood that the disclosure is not limited to the disclosed embodiments, but, on the contrary, is intended to cover various modifications and equivalent arrangements included within the spirit and scope of the appended claims, and equivalents thereof.
Number | Date | Country | Kind |
---|---|---|---|
10-2010-0054983 | Jun 2010 | KR | national |
Number | Name | Date | Kind |
---|---|---|---|
7842426 | Tighe et al. | Nov 2010 | B2 |
20080118809 | Tighe et al. | May 2008 | A1 |
20110053011 | Owejan et al. | Mar 2011 | A1 |
Number | Date | Country |
---|---|---|
3113340 | Sep 2000 | JP |
2008-153212 | Jul 2008 | JP |
10-2004-0100139 | Feb 2004 | KR |
10-2006-0086983 | Jan 2006 | KR |
10-2009-0072536 | Jul 2009 | KR |
Entry |
---|
KIPO OA (Korean Only) in related KR-10-2010-0054983 dated Oct. 19, 2011. |
Number | Date | Country | |
---|---|---|---|
20110305960 A1 | Dec 2011 | US |