Claims
- 1. A process for the hydrogenolysis of a halocarbon starting compound selected from the group consisting of CF.sub.3 CC1.sub.2 F, CF.sub.3 CHC1F, CF.sub.3 CC1FCF.sub.3, CC1F.sub.2 CC1F.sub.2, CF.sub.3 CC1.sub.3 and CF.sub.3 CC1F.sub.2 comprising contracting said halocarbon starting compound with at least 0.1 mole of hydrogen per mole of said halocarbon starting compound in an empty reaction vessel of nickel, iron or their alloys at a pressure within the range of from 0 psig to 1000 psig, at a temperature within the range of from 350.degree. C. to 700.degree. C. and for a time sufficient to produce a hydrogenolysis product wherein at least one chlorine has been replaced by hydrogen, at least 90% of the product of said hydrogenolysis containing the same number of fluorines as said halocarbon starting compound.
- 2. The process of claim 1 wherein the halocarbon starting compound is selected from CF.sub.3 CC1.sub.2 F, CF.sub.3 CHC1F and CC1F.sub.2 CC1F.sub.2.
- 3. The process of claim 1 wherein the reaction vessel is nickel or a nickel alloy.
- 4. The process of claim 1 wherein the temperature ranges from 400.degree. C. to 700.degree. C.
- 5. The process of claim 4 wherein the pressure is 0 to 500 psig.
- 6. The process of claim 5 wherein the halocarbon starting compound is CC1F.sub.2 CC1F.sub.2, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 to 8 minutes.
- 7. The process of claim 5 wherein the halocarbon starting compound is CF.sub.3 CC1.sub.2 F, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 and 8 minutes.
- 8. The process of claim 5 wherein the halocarbon starting compound is CF.sub.3 CHC1F, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 and 8 minutes.
- 9. The process of claim 5 wherein the halocarbon starting compound is CF.sub.3 CC1F.sub.2, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 and 8 minutes.
- 10. The process of claim 5 wherein the halocarbon starting compound is CF.sub.3 CC1.sub.3, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 and 8 minutes.
- 11. The process of claim 5 wherein the halocarbon starting compound is CF.sub.3 CC1FCF.sub.3, the reaction vessel is nickel or a nickel alloy, and the reaction time is between 0.2 and 8 minutes.
- 12. The process of claim 1 wherein the reaction vessel is either an alloy containing about 76 percent nickel, about 15.5 percent chromium and about 8 percent iron or an alloy containing about 59 percent nickel, about 15.5 percent chromium, about 16 percent molybdenum and about 3.75 percent tungsten.
- 13. The process of claim 1 wherein a halocarbon starting compound selected from CF.sub.3 CC1.sub.2 F, CF.sub.3 CHC1F, CC1F.sub.2 CC1F.sub.2, CF.sub.3 CC1.sub.3 and CF.sub.3 CC1F.sub.2, is contacted with at least about 2 moles of hydrogen per mole of said starting compound in a nickel alloy reaction vessel.
- 14. The process of claim 1 wherein the halocarbon starting compound is selected from CF.sub.3 CC1.sub.2 F, CC1F.sub.2 CC1F.sub.2 and CF.sub.3 CC1.sub.3 and wherein the hydrogenolysis is conducted at a temperature within the range of from 350.degree. C. to 700.degree. C. for a time sufficient to produce as the major product of the hydrogenolysis, hydrogenolysis product wherein just one chlorine has been replaced by hydrogen.
- 15. A process for the hydrogenolysis of a halocarbon starting compound selected from the group consisting of CF.sub.3 CC1.sub.2 F, CF.sub.3 CHC1F, CF.sub.3 CC1FCF.sub.3, CC1F.sub.2 CC1F.sub.2, CF.sub.3 CC1.sub.3 and CF.sub.3 CC1F.sub.2 comprising contacting said starting compound with at least 0.1 mole of hydrogen per mole of said halocarbon starting compound in an empty chrome plated reaction vessel at a pressure within the range of from 0 psig to 1000 psig, at a temperature within the range of from 350.degree. C. to 700.degree. C. and for a time sufficient to produce a hydrogenolysis product wherein at least one chlorine has been replaced by hydrogen, at least 90% of the product of said hydrogenolysis containing the same number of fluorines as said halocarbon starting compound.
- 16. The process of claim 15 wherein the temperature ranges from 400.degree. C. to 700.degree. C.
- 17. The process of claim 16 wherein the pressure is 0 to 500 psig.
- 18. A process for the hydrogenolysis of CC1F.sub.2 CC1F.sub.2, comprising contacting said CC1F.sub.2 CC1F.sub.2 with at least 0.1 mole of hydrogen per mole of said CC1F.sub.2 CC1F.sub.2 in an empty chrome-plated reaction vessel at a pressure within the range of from 0 psig to 1000 psig, at a temperature within the range of from 400.degree. C. to 700.degree. C. and for a reaction time between 0.2 to 8 minutes sufficient to produce a hydrogenolysis product wherein at least one chlorine has been replaced by hydrogen at least 90% of the product of said hydrogenolysis containing the same number of fluorines as said CC1F.sub.2 CC1F.sub.2.
CROSS-REFERENCE TO RELATED APPLICATION
This application is a continuation of U.S. application Ser. No. 07/847,987 filed Apr. 9, 1992, now abandoned, a national filing of PCT application No. PCT/U.S. 90/05637 filed Oct. 9, 1990 claiming priority (continuation in part) of U.S. patent application Ser. No. 07/418,832 filed Oct. 10, 1989, now abandoned.
US Referenced Citations (8)
Foreign Referenced Citations (5)
Number |
Date |
Country |
0253410 |
Jan 1988 |
EPX |
0305019 |
Mar 1989 |
EPX |
1-93549 |
Apr 1989 |
JPX |
698386 |
Oct 1953 |
GBX |
1578933 |
Nov 1980 |
GBX |
Non-Patent Literature Citations (1)
Entry |
111:11473h Chemical Abstract. |
Continuations (1)
|
Number |
Date |
Country |
Parent |
847987 |
Apr 1992 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
418832 |
Oct 1989 |
|