Claims
- 1. A method for repairing an irregular surface texture material, the method comprising the steps of:storing a hardenable texture material for application to a patch surface surrounded by a stucco-like material having an irregular surface texture in a fluid-tight aerosol dispensing container, the hardenable texture material comprising a mixture of, a liquid base wherein the liquid base consists essentially of a water-resistant material, the liquid base having a composition by percentage weight of 10% to 80% of the hardenable texture material, and a stucco filler substance having large particulates resembling stucco wherein the stucco filler substance consists essentially of a mixture of limestone and clay, the limestone of the stucco filler substance having a composition percentage weight of approximately 35% to 65% of the hardenable texture material, and the clay of the stucco filler substance having a composition percentage weight of approximately 5% to 25% of the hardenable texture material, and the large particulates having a particulate size of approximately {fraction (1/30)} cubic inches ({fraction (1/30)} in.3) to ⅛ cubic inches (⅛ in.3), wherein the fluid-tight aerosol dispensing container has a nozzle attached to the fluid-tight aerosol dispensing container for dispensing the hardenable texture material using a pressure from the fluid-tight aerosol dispensing container in the form of an aerosol spray; and selectively dispensing the hardenable texture material onto the patch surface such that the hardenable texture material forms a layer having a bumpy, irregular surface texture after being dispensed that matches and is compatible with the stucco-like material surrounding the patch surface.
- 2. The method for repairing the irregular surface texture material according to claim 1, wherein the water-resistant material is a vinyl.
- 3. The method for repairing the irregular surface texture material according to claim 1, wherein the water-resistant material is an acrylic.
- 4. The method for repairing the irregular surface texture material according to claim 1, wherein the water-resistant material is polyvinyl alcohol.
- 5. The method for repairing the irregular surface texture material according to claim 1, wherein the water-resistant material is a resin.
- 6. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises an aggregate wherein the aggregate consists essentially of perlite, the aggregate having a composition percentage weight of approximately 5% to 30% of the hardenable texture material.
- 7. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises an aggregate wherein the aggregate consists essentially of sand, the aggregate having a composition percentage weight of approximately 5% to 30% of the hardenable texture material.
- 8. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises an aggregate wherein the aggregate consists essentially of silica sand, the aggregate having a composition percentage weight of approximately 5% to 30% of the hardenable texture material.
- 9. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises an aggregate wherein the aggregate consists essentially of glass beads, the aggregate having a composition percentage weight of approximately 5% to 30% of the hardenable texture material.
- 10. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises an anti-freeze.
- 11. The method for repairing the irregular surface texture material according to claim 10, wherein in the step of storing the hardenable texture material for application to a patch surface, the anti-freeze consists essentially of propylene glycol.
- 12. The method for repairing the irregular surface texture material according to claim 1, wherein in the step of storing the hardenable texture material for application to a patch surface, the hardenable texture material further comprises a fungicide.
- 13. A method for repairing an irregular surface texture material, the method comprising the steps of:storing a hardenable texture material for application to a patch surface surrounded by a stucco-like material having an irregular surface texture in a fluid-tight aerosol dispensing container, the hardenable texture material comprising a mixture of, a liquid base wherein the liquid base consists essentially of a water-resistant material, the liquid base having a composition by percentage weight of 10% to 80% of the hardenable texture material, a stucco filler substance having large particulates resembling stucco wherein the stucco filler substance consists essentially of a mixture of limestone and clay, the limestone of the stucco filler substance having a composition percentage weight of approximately 35% to 65% of the hardenable texture material, and the clay of the stucco filler substance having a composition percentage weight of approximately 5% to 25% of the hardenable texture material, and the large particulates having a particulate size of approximately {fraction (1/30)} cubic inches ({fraction (1/30)} in.3) to ⅛ cubic inches (⅛ in.3), an aggregate wherein the aggregate is a material selected from the group consisting of sand, perlite, silica sand, and glass beads, the aggregate having a composition percentage weight of approximately 5% to 30% of the hardenable texture material, an anti-freeze, and a fungicide, wherein the fluid-tight aerosol dispensing container has a nozzle attached to the fluid-tight aerosol dispensing container for dispensing the hardenable texture material using a pressure from the fluid-tight aerosol dispensing container in the form of an aerosol spray; and selectively dispensing the hardenable texture material onto the patch surface such that the hardenable texture material forms a layer having a bumpy, irregular surface texture after being dispensed that matches and is compatible with the stucco-like material surrounding the patch surface.
- 14. The method for repairing the irregular surface texture material according to claim 13, wherein the water-resistant material is a vinyl.
- 15. The method for repairing the irregular surface texture material according to claim 13, wherein the water-resistant material is an acrylic.
- 16. The method for repairing the irregular surface texture material according to claim 13, wherein the water-resistant material is polyvinyl alcohol.
- 17. The method for repairing the irregular surface texture material according to claim 13, wherein the water-resistant material is a resin.
- 18. The method for repairing the irregular surface texture material according to claim 13, wherein the anti-freeze consists essentially of propylene glycol.
Parent Case Info
This is a divisional of application Ser. No. 09/312,554, filed May 14, 1999 U.S. Pat. No. 6,225,393
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
5450983 |
Stern et al. |
Sep 1995 |
A |
6112945 |
Woods |
Sep 2000 |
A |