The present invention relates to a heater used as, for example, an ignition or flame detection heater for in-vehicle heating apparatuses, an ignition heater for burning appliances including an oil fan heater, a glow plug heater of an automobile engine, a heater for sensors including an oxygen sensor, or a heater for heating measuring instruments, and to a glow plug including the same.
For example, a glow plug heater of an automobile engine has been known which includes an insulating base, a resistor embedded in the insulating base, and a lead embedded in the insulating base. The lead is joined to the resistor at one end thereof and the other end is led out as a terminal portion on the surface of the insulating base.
More specifically, a known glow plug heater has the structure in which a lead for an anode has at least two bent portions in longitudinal section, and is led out as a terminal portion disposed at, for example, the back end of the insulating base (see, for example, PTL 1). The lead is led out as the terminal portion, keeping the diameter thereof at the two bent portions.
[PTL 1] Japanese Unexamined Patent Application Publication No.
In recent years, a heater capable of more rapid heating has been desired, and accordingly, a need has occurred for increasing the electric power (inrush power) supplied through the terminal portion so that a large current is applied to the resistor at the start (at the start of the engine).
However, if you try to increase the inrush power of the heater, the load of the inrush power is concentrated particularly on the outer side of the curve of the bent portion of the lead, and this load-concentrated portion is locally heated to expand thermally. This undesirably causes a micro-crack in the interface between the lead and the insulating base.
The present invention is proposed in view of the above issue, and an object of the invention is to provide a highly reliable, durable heater in which micro-cracks caused by stress concentration resulting from local expansion are suppressed even when a large current flows through the bent portion of the lead, for example, for rapid heating, and to provide a glow plug including the heater.
A heater of the present invention includes an insulating base, a resistor embedded in the insulating base, a lead embedded in the insulating base. One end of the lead is joined to the resistor, and the other end is led out as a terminal portion on a surface of the insulating base. The lead in longitudinal section has at least two bent portions. The bent portions in cross-section each have an aspect ratio larger than the aspect ratio of the terminal portion.
A glow plug of the present invention includes a heater having the above-described structure, and a metallic holding member electrically joined to the terminal portion and holding the heater.
According to the heater of the present invention, the load of inrush power placed on the two bent portions is dispersed from the outer sides of the curves of the bent portions, and micro-cracks in the interface between the lead and the insulating base are thereby suppressed.
An embodiment of the heater of the present invention will now be described in detail with reference to the drawings.
The heater 1 of the present embodiment includes an insulating base 2, a resistor 3 embedded in the insulating base 2, a lead 4 embedded in the insulating base 2. One end of the lead 4 is joined to the resistor 3, and the other end is led out as a terminal portion 5 on a surface of the insulating base 2. The lead 4 in longitudinal section has at least two bent portions 41 and 42. The bent portions 41 and 42 in cross-section each have an aspect ratio larger than the aspect ratio of the terminal portion 5.
The insulating base 2 of the heater 1 of the present embodiment has been formed in, for example, a rod-like shape. In the insulating base 2, the resistor 3 and the lead 4 are embedded. Preferably, the insulating base 2 is made of a ceramic. Consequently, the heater 1 can be highly reliable in rapid heating. More specifically, examples of the ceramic include oxide ceramics, nitride ceramics, carbide ceramics, and other electrically insulating ceramics. Preferably, the insulating base 2 is made of a silicon nitride-based ceramic. This is because silicon nitride, which is the main constituent of silicon nitride-based ceramics, is superior in strength, toughness, insulation, and heat resistance. For forming the insulating base 2 made of a silicon nitride-based ceramic, for example, 3% to 12% by mass of a rare-earth metal oxide as a sintering agent, such as Y2O3, Yb2O3, or Er2O3, 0.5% to 3% by mass of Al2O3, and SiO2 are mixed to 100% by mass of the main constituent silicon nitride. The amount of SiO2 added is such that the SiO2 content in the sintered compact can be 1.5% to 5% by mass. The mixture is formed into a predetermined shape and then subjected to hot plate sintering at 1650 to 1780° C. The insulating base 2 has a length of, for example, 20 to 50 mm and a diameter of, for example, 3 to 5 mm.
If the insulating base 2 is made of a silicon nitride-based ceramic, it is preferable to add MoSi2, WSi2, or the like and disperse it in the ceramic. These materials can bring the thermal expansion coefficient of the base matrix or silicon nitride-based ceramic close to the thermal expansion coefficient of the resistor 3, thereby enhancing the durability of the heater 1.
For example, in the embodiment shown in
The resistor 3 may be made of a material mainly containing a carbide, a nitride or a silicide of W, Mo, Ti or the like. If the insulating base 2 is made of a silicon nitride-based ceramic, tungsten carbide (WC) is most suitable of those materials as the material of the resistor 3 because it has a small difference in thermal expansion coefficient from the insulating base 2, and has a high heat resistance and a low specific resistance. If the insulating base 2 is made of a silicon nitride-based ceramic, it is more preferable that the resistor 3 contain mainly WC, which is an inorganic electroconductive material, and, in addition, 20% by mass or more of silicon nitride. The resistor 3 in the insulating base 2 of, for example, a silicon nitride-based ceramic is in general under the condition where a stress is placed thereon because the electroconductive material of the resistor 3 has a larger thermal expansion coefficient than silicon nitride. However, by adding silicon nitride to the resistor 3, the thermal expansion coefficient is brought close to that of the insulating base 2 to reduce the stress resulting from the difference in thermal expansion coefficient produced during the heating or cooling of the heater 1. Also, if the silicon nitride content in the resistor 3 is 40% by mass or less, the resistance of the resistor 3 can be relatively low and stable. The silicon nitride content in the resistor 3 is preferably 20% by mass to 40% by mass. More preferably, the silicon nitride content is 25% by mass to 35% by mass. As an alternative to silicon nitride, 4% by mass to 12% by mass of boron nitride may be added as a similar additive of the resistor 3.
The lead 4 embedded in the resistor 2 is joined to the resistor 3 at one end thereof, and the other end is led out as a terminal portion 5 on the surface of the insulating base. In the embodiment shown in
The leads 4 are made of the same material as the resistor 3, and their resistance per unit length is set lower than the resistor 3 by, for example, increasing the sectional area relative to that of the resistor 3, or by reducing the content of the insulating base 2 material relative to the that in resistor 3. In particular, WC is suitable as the material of the lead 4 because WC has a small difference in thermal expansion coefficient from the insulating base 2, and has a high heat resistance and a low specific resistance. Preferably, the lead 4 mainly contains an inorganic electroconductive material WC, and further contains silicon nitride with a content of 15% by mass or more. As the silicon nitride content is increased, the thermal expansion coefficient of the lead 4 comes close to that of the silicon nitride of the insulating base 2. Also, the lead 4 containing silicon nitride with a content of 40% by mass or less has a stable, low resistance. The silicon nitride content is preferably 15% by mass to 40% by mass. More preferably, the silicon nitride content is 20% by mass to 35% by mass.
One of the leads 4 in longitudinal section has at least two bent portions 41 and 42. The bent portions 41 and 42 in cross section each have an aspect ratio larger than the aspect ratio of the terminal portion 5.
The lead 4 described here refers to the lead 4 shown in
The terminal portion 5 refers to the end of the lead 4 not joined to the resistor, and may be formed of the same material as the other portion of the lead 4 in one body or a different body, or may be formed of a different material.
The load of inrush power from the terminal portion 5 tends to increase at the outer side of the bends of the bent portions 41 and 42 in section, that is, at the A2 side shown in
In this instance, when the cross sections of the bent portions 41 and 42 has aspect ratios of, for example, 1.2 to 5.0, the load of inrush power can be dispersed effectively without allowing excess stress to concentrate in the longer axis direction.
Preferably, the bent portions 41 and 42 have oval cross sections. Since oval sections do not have corners and therefore allow stress to disperse easily, the occurrence of micro-cracks can be further suppressed.
In the embodiment shown in
Preferably, the aspect ratios of the bent portions 41 and 42 in cross section are gradually increased in the direction from the terminal portion 5 toward the resistor 3, as shown in
Furthermore, it is preferable that the cross sections of the bent portions 41 and 42 have the same area. Since this form does not have any portion on which load is concentrated in a stationary state, the occurrence of micro-cracks can be further suppressed.
The cross sections may have any shape without being limited to the shapes shown in
The heater 1 described above can be used for a glow plug. More specifically, a glow plug of the present invention includes the heater 1, and a metallic holding member 6 (metallic sheath) electrically joined to the terminal portions 5 of the leads 4 of the heater 1 and holding the heater 1, as shown in
An exemplary process for manufacturing the heater 1 of the present embodiment will now be described.
The heater 1 of the present embodiment may be produced by, for example, injection molding using metallic molds having the shapes corresponding to the resistor 3, the leads 4 and the insulating base 2.
First, an electroconductive paste containing an electroconductive ceramic powder and a resin binder is prepared for forming the resistor 3 and the lead 4, and a ceramic paste containing an insulating ceramic powder and a resin binder is prepared for forming the insulating base 2.
Subsequently, a compact (compact a) having a predetermined pattern of the electroconductive paste that will be used as the resistor 3 is formed by injection molding or the like using the electroconductive paste. Then, a compact (compact b) having a predetermined pattern of the electroconductive paste that will be used as the leads 4 is formed by introducing the electroconductive paste into the metallic mold with the compact a kept therein. Thus a state is established in which the compact a and the compact b joined to the compact a are held in the metallic mold.
Subsequently, after a part of the metallic mold, in which compact a and the compact b are held, is replaced with a mold for forming the insulating base 2, the ceramic paste for forming the insulating base 2 is introduced to the mold. Thus a compact (compact d) of the heater 1 is prepared in which the compact a and the compact b are covered with the compact (compact c) of the ceramic paste.
Subsequently, the resulting compact d is sintered at a temperature of 1650° C. to 1780° C. and a pressure of 30 MPa to 50 MPa to yield the heater 1. The sintering is preferably performed in an atmosphere of hydrogen gas and a non-oxidizing gas.
A heater of the Example of the present invention was prepared as described below.
First, an electroconductive paste containing 50% by mass of tungsten carbide (WC) powder, 35% by mass of silicon nitride (Si3N4) powder, and 15% by mass of a resin binder was injected into a metallic mold to form a compact a for a resistor having the shape shown in
Subsequently, the same electroconductive paste for forming a lead was introduced into the mold with the compact a kept therein, thereby joining to the compact a. Thus a compact b was formed for the lead having the shape shown in
Subsequently, a ceramic paste containing 85% by mass of silicon nitride (Si3N4) powder, 10% by mass of ytterbium oxide (Yb2O3) as a sintering agent, and 5% by mass of tungsten carbide (WC) for bringing the thermal expansion coefficient close to that of the resistor and the lead was injected into the metallic mold with the compact a and compact b kept therein. Thus, a compact d was formed in which the compact a and the compacts b were embedded in a compact c for the insulating base.
Subsequently, the resulting compact d was sintered by hot press at a temperature of 1700° C. and a pressure of 35 MPa in an atmosphere of a non-oxidizing gas containing nitrogen gas in a carbon cylindrical mold. Thus the heater of the Example of the present invention was completed. In the heater (sample of the Example of the present invention), the lead had two bent portions, and the sections of the bent portions had aspect ratios increasing in the direction toward the resistor. The section of the portion between the bent portions had aspect ratios increasing gradually in the direction from the terminal toward the resistor. Also, the sections were in an oval shape, and the sectional areas of the two bent portions were the same. The insulating base had a diameter of 3.2 mm. The bent portion closer to the terminal portion had a shorter axis of 1.1 mm in length and an aspect ratio (length of longer axis/length of shorter axis) of 1.5, while the bent portion distant from the terminal portion had a shorter axis of 0.8 mm and an aspect ratio (length of longer axis/length of shorter axis) of 3.5.
Then, a cylindrical metallic holding member was welded to the end (terminal portion) of a lead extracted from the side near the back end of the resulting heater to yield a glow plug.
On the other hand, another glow plug was prepared as the Comparative Example. This glow plug included a lead having two bent portions whose sections each had the same aspect ratio as the aspect ratio of the sections of the terminal portion and the resistor. The terminal portion, the bent portions and the resistor of this sample had oval sections of 1.2 mm in shorter length and an aspect ratio (length of longer axis/length of shorter axis) of 1.1.
The glow plugs were subjected to heat cycle test. The heat cycle test was performed under the conditions where the voltage applied to the heater was set so that the temperature of the resistor could be increased to 1400° C., and a cyclic operation including: (1) supplying power for 5 minutes; and (2) suspending power supply for 2 minutes was repeated 10 thousand times.
The variation between the resistances of the heater before and after the heat cycle test was measured. For the Example of the invention, the variation in resistance of the sample was 1% or less. In addition, there was no sign showing local heating or micro-cracks at the interface between the lead and the insulating base in the sample.
For the Comparative Example, on the other hand, the variation in resistance was 5% or more, and a micro-crack was observed.
Number | Date | Country | Kind |
---|---|---|---|
2011-186180 | Aug 2011 | JP | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/JP2012/071591 | 8/27/2012 | WO | 00 | 2/28/2014 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2013/031728 | 3/7/2013 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
5362944 | Hatanaka | Nov 1994 | A |
5883360 | Tatematsu | Mar 1999 | A |
5948306 | Konishi | Sep 1999 | A |
6013898 | Mizuno | Jan 2000 | A |
6025579 | Tanaka | Feb 2000 | A |
6049065 | Konishi | Apr 2000 | A |
6111223 | Tatematsu | Aug 2000 | A |
6204481 | Ito | Mar 2001 | B1 |
20020162830 | Taniguchi | Nov 2002 | A1 |
20020162831 | Taniguchi | Nov 2002 | A1 |
20060011602 | Konishi | Jan 2006 | A1 |
20090008383 | Kurono | Jan 2009 | A1 |
20090320782 | Hiura | Dec 2009 | A1 |
20110068091 | Hiura | Mar 2011 | A1 |
Number | Date | Country |
---|---|---|
2006049279 | Feb 2006 | JP |
2001280640 | Oct 2011 | JP |
2009096477 | Aug 2009 | WO |
Entry |
---|
International Search Report, PCT/JP2012/071591, Sep. 18, 2012, 1pg. |
Number | Date | Country | |
---|---|---|---|
20140224783 A1 | Aug 2014 | US |